Zpc Zhejiang Petroleum Chemical Hdpe M 3606

ZPC (Zhejiang Petroleum & Chemical) HDPE M-3606

    • Product Name: ZPC (Zhejiang Petroleum & Chemical) HDPE M-3606
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 102123
    Density 0.960 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 6.0 g/10 min
    Tensile Strength At Yield 30 MPa
    Elongation At Break 600%
    Flexural Modulus 1200 MPa
    Notched Izod Impact Strength 50 J/m
    Vicat Softening Temperature 125°C
    Heat Deflection Temperature 75°C
    Melting Point 130°C
    Shore Hardness 60 Shore D
    Mold Shrinkage 1.5-3.0%
    Brittleness Temperature -70°C
    Water Absorption <0.01%
    Dielectric Strength 20 kV/mm
    Volume Resistivity >10^16 ohm·cm

    As an accredited ZPC (Zhejiang Petroleum & Chemical) HDPE M-3606 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing ZPC HDPE M-3606 is packaged in 25 kg polypropylene woven bags or 1,000 kg jumbo bulk bags.
    Container Loading (20′ FCL) 20′ FCL can load 25 MT loose or 20 MT palletized ZPC HDPE M-3606 in 25 kg bags.
    Shipping ZPC (Zhejiang Petroleum & Chemical) HDPE M-3606 is shipped as non-hazardous virgin polyethylene pellets, normally in 25 kg PP woven bags or 500–1000 kg jumbo bags, palletized/containerized. Typical 20' FCL load: 25–28 MT. No special dangerous goods handling required. Store dry, cool, away from sunlight.
    Storage Store ZPC HDPE M-3606 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and moisture. Keep original packaging sealed, palletized, and avoid excessive stacking. Maintain clean, segregated storage, separate from strong oxidizers, acids, and solvents. Prevent dust and static buildup; use grounding where required. Inspect containers regularly. Follow the manufacturer’s SDS and local regulations.
    Shelf Life ZPC HDPE M-3606 shelf life: 12 months from production when stored dry, cool, ventilated, in original packaging, away from sunlight.
    Application of ZPC (Zhejiang Petroleum & Chemical) HDPE M-3606

    ZPC HDPE M-3606, a narrow-molecular-weight injection grade with a nominal density of 0.960 g/cm³ (ISO 1183-1:2019) and a nominal melt flow rate of 3.6 g/10 min (ISO 1133-1:2022, 190 °C, 2.16 kg), is used in high-cavitation thin-wall production of dairy tubs, portion cups and press-on lids. In this segment the resin is blended at 96.5–98.5 wt% with 1.0–2.0 wt% slip/antiblock masterbatch and 0.5–1.5 wt% TiO₂ white masterbatch to reduce denesting force and scuffing without exceeding food-contact additive limits. Compliance for the finished dairy-contact articles is assessed under FDA 21 CFR 177.1520(c), with overall migration testing under EU Regulation (EU) No 10/2011 and its amendment (EU) 2020/1245, using food simulants A, B and D2 for aqueous, acidic and fatty foods respectively. Downstream processing is performed on 250–450 t high-speed injection moulding machines equipped with 32-cavity hot-runner stack moulds. The material is processed at a melt temperature of 210–240 °C, a mold temperature of 7–15 °C, injection pressure of 80–120 MPa, holding pressure of 55–80 MPa, and a total cycle time of 4.5–8.0 s. Screw geometry is typically 20:1–24:1 L/D with compression ratio 2.5:1. Wall sections from 0.30–0.55 mm produce flow-length-to-thickness ratios approaching 200:1–300:1; this creates a processing conflict in which injection velocity below 300 mm/s generates hesitation marks on the sidewall, while velocity above 400 mm/s can produce peripheral vent flash. Terminal finished products in this scenario are 150–500 mL tubs, lids, portion cups and deli containers.

    What Controls Wall-Section Consistency in UN-Classified Industrial Pail Injection?

    In the production of open-top and closed-head industrial containers for lubricants, agrochemicals and cleaning concentrates, wall-section consistency at the handle bosses and sidewall-to-bottom transition controls the UN drop-test outcome. The formulation addition ratio is typically 97.0–98.5 wt% M-3606, 1.0–2.0 wt% carbon black masterbatch with nominal 50% carbon black content, and 0.5–1.0 wt% processing aid/antioxidant masterbatch. This loading yields sufficient carbon black dispersion for outdoor storage without shifting the melt viscosity beyond the hot-runner pressure envelope. Compliance is evaluated under UN Model Regulations Chapter 6.1 for 1H2 open-top plastics drums and 3H1 non-removable-head jerricans, IMDG Code Chapter 6.1, and ADR/RID 6.1.5, including drop impact from 1.2 m for packing group II and 0.8 m for packing group III, followed by stacking at 40 °C for 28 days. Downstream, the pails are moulded on 500–1200 t clamp force injection machines with accumulator-assisted injection. Melt temperature is set at 200–230 °C, mold temperature at 10–20 °C, injection pressure at 60–110 MPa, and hold pressure at 40–70 MPa applied through 3–4 valve-gated hot runners. Sidewall thickness is 2.5–3.5 mm; the handle boss can reach 6–10 mm local thickness, requiring a two-stage pack-and-hold profile to avoid internal voids and sink marks. Total cycle time is 18–35 s. Terminal products include 10 L, 15 L, 20 L and 25 L pails, 20 L and 25 L jerricans, and injection-moulded UN closures. Avoid calcium carbonate loadings above 5 wt% in drop-tested pails; the filler reduces environmental stress-crack resistance and can produce brittle hinge failure at the handle boss.

    TestStandardConditionAcceptance criterion
    Drop impactUN Model Regulations 6.1.5.31.2 m for packing group II, 0.8 m for packing group IIINo leakage, rupture, or thread dislocation
    Stacking loadUN Model Regulations 6.1.5.640 °C for 28 daysNo buckling, collapse, or leakage
    Environmental stress crack resistanceASTM D1693-15e110% Igepal CO-630, 50 °CF50 monitored against process control baseline
    Melt flow rateISO 1133-1:2022190 °C, 2.16 kgWithin site-specific release band

    Beverage Crate Regrind Stability and Low-Temperature Impact

    Beverage crate and logistics tray moulding imposes a closed-loop regrind constraint because the impact performance of the part at low storage temperatures depends on the molecular degradation introduced by repeated high-shear processing. The addition ratio is 82–90 wt% virgin M-3606, 8–15 wt% post-industrial regrind from sprues, runners and rejected crates, and 1.5–2.5 wt% colour/UV masterbatch. Regrind above 15 wt% can reduce notched impact strength at -20 °C and increase the incidence of gate-area stress cracking; moulders therefore stabilize the regrind fraction and dry it at 70–80 °C for 2 h when stored in humid environments. Compliance for the structural performance of the crate is assessed with ISO 527-1:2019 tensile testing, ISO 179-1:2023 Charpy notched impact at -20 °C, ASTM D256-10 Izod impact, and ISO 1183-1:2019 density checks. Colourant systems must comply with REACH (EC) No 1907/2006. Downstream injection is performed on 800–1600 t clamp force machines with sequential valve-gated multi-gate systems to relocate weld lines away from the centre of the crate base. Melt temperature is held at 190–215 °C to minimize regrind degradation, mold temperature at 12–25 °C, injection pressure at 80–130 MPa, and total cycle time at 22–40 s. Terminal finished products include 24-bottle soft drink crates, 300×400 mm logistics trays, bakery trays, fish crates and fork-liftable lightweight pallets.

    For pressure piping components, injection-moulded electrofusion sockets and spigot fittings utilise M-3606 in an application where slow-crack-growth resistance and long-term hydrostatic strength are controlled by the base resin molecular architecture and carbon black dispersion. The addition ratio is 94–97 wt% M-3606, 2–4 wt% carbon black masterbatch to achieve a final carbon black concentration of 2.0–2.5 wt%, and 0.2–0.5 wt% antioxidant masterbatch. Compliance requirements follow ISO 17885:2021 for pressure fittings, EN 12201-3:2011+A1:2022 for water supply fittings, ISO 9080:2012 hydrostatic design stress classification, and ISO 1167:2006 hydrostatic pressure testing. Downstream injection moulding of thick-wall fittings is performed on 250–600 t clamp machines with nozzle shut-off and multi-cavity tooling. Melt temperature is 205–235 °C, mold temperature 20–40 °C, injection pressure 70–120 MPa, and hold pressure 40–80 MPa. Wall sections of 8–25 mm require cooling times of 60–120 s to avoid sink marks and internal shrinkage voids. Terminal products include 20–630 mm electrofusion couplers, spigot fittings, saddle tees, tapping tees and end caps.

    TestStandardConditionRelevance
    Hydrostatic strength of assembled fittingISO 17885:2021Water-in-water, 20 °C and 80 °CPressure leak tightness
    Long-term hydrostatic design stressISO 9080:2012Multiple temperatures, regression analysis to 50 yearsPE100 grade classification
    Hydrostatic pressure testISO 1167:2006End closures restrainedBurst and creep resistance
    DensityISO 1183-1:2019Method A, 23 °CCompound quality control

    Battery Container Moulding Demands a Controlled Post-Mould Shrinkage Window

    Lead-acid automotive battery containers and lids require a controlled post-mould shrinkage window because lid fit, terminal sealing and internal cell alignment depend on dimensional stability after demoulding. The formula addition ratio is 93–97 wt% M-3606, 3–7 wt% ethylene-propylene impact modifier to improve puncture resistance at -20 °C, and 0.2–0.5 wt% heat stabilizer/antioxidant masterbatch. Exceeding 7 wt% impact modifier lowers tensile yield stress and prolongs cycle time due to increased relaxation; below 3 wt%, cold drop failure rates increase on thin-wall cell partitions. Compliance testing for the moulded parts follows ASTM D638-22 tensile properties, ASTM D256-10 notched Izod at -20 °C, ASTM D792-20 density, and UL 94 HB flammability classification. Complete lead-acid battery systems are assessed under EN 50342-1 for automotive starter batteries. Downstream production uses 600–2000 t two-platen injection moulding machines with sequential valve gating across the container length to eliminate weld lines at the intercell partition. Melt temperature is 200–235 °C, mold temperature 15–30 °C, injection pressure 80–140 MPa, and total cycle time 35–60 s. Post-mould shrinkage is monitored for 48 h before lid fit; typical total shrinkage is 1.2–2.5%. Terminal products include 12 V SLI automotive battery containers, lids, venting plugs and terminal covers.

    Where the injection-moulded component sits inside drinking-water contact equipment, the polymer must satisfy extraction limits rather than only mechanical fit. M-3606 is formulated at 96–99 wt% with 1–4 wt% cobalt-blue or carbon black masterbatch, and the finished housings are tested to NSF/ANSI 61, FDA 21 CFR 177.1520, and EU Regulation (EU) No 10/2011 where applicable. Production uses 300–800 t injection presses with hot-runner multi-cavity tools, melt temperature 205–235 °C, mold temperature 15–30 °C, injection pressure 80–120 MPa, and cycle time 30–50 s. Terminal components include under-sink filter housings, filter sumps and gravity-fed water treatment chambers.

    Free Quote

    Competitive ZPC (Zhejiang Petroleum & Chemical) HDPE M-3606 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    ZPC (Zhejiang Petroleum & Chemical) HDPE M-3606 is a high-density polyethylene injection-molding grade supplied as free-flowing pellets. The material is classified under ISO 1043-1:2011 as PE-HD and under ASTM D4976-24 as a polyethylene injection-molding material with a nominal density of 0.960 g/cm³ and a nominal melt mass-flow rate of 6.0 g/10 min at 190 °C/2.16 kg. The grade designation M-3606 follows the producer’s internal nomenclature: the M prefix identifies injection-molding utility, while the numerical suffix distinguishes the melt-flow set point from ZPC extrusion and blow-molding grades. Because additive formulation is proprietary, certificates of analysis rather than generic class data are required for lot-specific compliance decisions.

    Table 1 lists representative supplier-reported values associated with ZPC HDPE M-3606. These values are not specification limits and do not replace incoming inspection against ISO 1133-1:2022 or the relevant lot certificate.

    PropertyNominal value or rangeTest method
    Melt mass-flow rate (190 °C/2.16 kg) 6.0 g/10 min ISO 1133-1:2022 / ASTM D1238-20 Procedure A
    Density 0.960 g/cm³ ISO 1183-1:2019 / ASTM D1505-18
    Tensile stress at yield 26–28 MPa ISO 527-2:2012 Type 1A, 50 mm/min
    Tensile strain at yield 8–10% ISO 527-2:2012 Type 1A
    Flexural modulus 1,000–1,150 MPa ISO 178:2019, 2 mm/min
    Charpy notched impact strength, 23 °C 4–6 kJ/m² ISO 179-1:2010/1eA
    Vicat softening temperature A50 122–126 °C ISO 306:2013, 10 N, 50 K/h
    Deflection temperature under load B, 0.45 MPa 72–76 °C ISO 75-2:2013 method B, flatwise

    These values correspond to a medium-flow high-density polyethylene with the fast crystallisation behaviour typical of injection-molding grades. The combination of a 6.0 g/10 min melt flow rate and 0.960 g/cm³ density establishes a balance between injection pressure demand and solid-state stiffness, but the material is not characterised by the elevated environmental stress-crack resistance of high-molecular-weight grades.

    Thermal Degradation Thresholds at Elevated Residence Time

    Melt processing of M-3606 is bounded by a barrel-temperature window from 200 °C to 240 °C, with nozzle set points commonly 220–230 °C. At melt temperatures above 240 °C and residence times exceeding 5 minutes, thermo-oxidative chain scission becomes measurable as an increase in melt flow rate, yellowing, and loss of notched impact strength. The degradation pathway is radical-mediated and accelerates under oxygen ingress at the feed throat or when regrind carries oxidised surfaces. On production-scale injection-molding machines with general-purpose polyolefin screws of compression ratio 2.0:1–2.5:1 and L/D 18:1–22:1, melt temperature is controlled by barrel profile, screw speed, and back pressure. Recommended back pressure is 0.5–1.5 MPa; screw speed of 60–120 rpm for screw diameters 30–60 mm is typical, but the actual value should be set to avoid excessive shear heating.

    Mould temperature is maintained between 15 °C and 40 °C for most rigid packaging and industrial containers. Lower mould temperatures shorten cycle time but increase orientation and differential shrinkage; higher mould temperatures improve surface gloss and reduce frozen-in stress at the cost of cooling time. Injection velocity is normally set in the range 100–250 mm/s for parts with wall sections 1.5–4.0 mm. Holding pressure of 50–70% of peak injection pressure is held until gate freeze; premature drop-off produces sink marks, while excessive holding pressure increases moulded-in stress and demoulding force.

    Pre-drying is not mandatory for HDPE at ambient storage conditions because the resin is non-hydroscopic. Nevertheless, surface moisture from cold-to-warm transfer or storage under condensation risk can generate silver streaking and should be removed with hopper drying at 70 °C for 1 h. For pre-compounding of pigment or additive concentrates based on M-3606, co-rotating twin-screw extruders with L/D 40:1 and side feeders prevent excessive residence time distribution; melt temperature measured at the die plate should remain below 230 °C.

    Industrial containers, crates, totes, pails, and housewares constitute the principal conversion sector for M-3606. The resin displays adequate flow length-to-wall-thickness ratio for stackable tote moulds with projected areas of 0.5–1.5 m² on clamping units of 8,000–25,000 kN. In pail injection molding, wall thicknesses of 2–3 mm are filled with the 6.0 g/10 min melt flow rate without excessive injection pressure, while productivity is obtained from rapid solidification of the spherulitic structure. Drop-impact performance of pails at 0 °C should be verified according to ASTM D5276-19 or ISTA Series test protocols rather than assumed from room-temperature Charpy data.

    Food-contact containers require separate migration testing under the applicable jurisdiction. M-3606 can be evaluated under FDA 21 CFR 177.1520 for olefin polymers when supported by manufacturer compliance certification and end-use extraction testing; for China food-contact use, GB 4806.6-2016 and GB 9685-2016 apply. The material is not supplied with an automatic universal food-contact approval, because final additive formulation and conversion conditions affect regulatory status.

    During production campaigns on hot-runner moulds with valve-gated drops, the low melt viscosity of M-3606 permits filling of multi-cavity tools at moderate injection pressures; however, hot-runner temperature should be held at 220–240 °C to avoid premature gate freeze and stringing. Use of externally heated manifolds with independent tip temperature control is recommended for part-weight consistency below ±0.5% when moulding tight-tolerance caps and closures.

    What Distinguishes M-3606 from High-Molecular-Weight Blow-Moulding and Film Grades?

    The primary differentiator is melt mass-flow rate. M-3606 at 6.0 g/10 min occupies a much lower melt viscosity region than high-molecular-weight blow-molding HDPE, which typically ranges from 0.2 g/10 min to 0.8 g/10 min under the same ISO 1133-1:2022 condition. This viscosity reduction allows shorter injection fill time and lower cavity pressure, but it also reduces parison melt strength, making M-3606 unsuitable for continuous extrusion blow molding of large containers. Converter trials show that a material with this melt flow has limited bubble stability in blown film; ZPC designates separate film grades where molecular architecture and additive packages are optimised for bubble stability, gel control, and melt strength.

    Environmental stress-crack resistance is lower in injection-molding grades than in high-molecular-weight blow-molding or pipe grades. While blow-molding HDPE used in detergent bottles may exhibit ESCR values exceeding 600 h in ASTM D1693-21 stress-crack testing, M-3606 is not intended for that performance envelope and published ESCR data for this specific configuration is limited. Components exposed to aggressive surfactants, mineral oil, or polar organic liquids should be tested under end-use strain because stress-cracking is a function of moulded-in stress, wall thickness, and service temperature, not merely resin class.

    Property or attributeHDPE M-3606HMW blow-molding HDPEPE80/PE100 pipe-grade HDPE
    Melt mass-flow rate (190 °C/2.16 kg) 6.0 g/10 min 0.2–0.8 g/10 min 0.3–0.7 g/10 min
    Density 0.960 g/cm³ 0.949–0.955 g/cm³ 0.948–0.952 g/cm³
    Primary conversion process Injection molding Extrusion blow molding Pipe extrusion
    Typical wall thickness relevance 1.5–4.0 mm 0.5–2.5 mm 3–60 mm
    Notched impact at 23 °C 4–6 kJ/m² (ISO 179-1/1eA) 20–40 kJ/m² (ISO 179-1/1eA) 20–50 kJ/m² (ISO 179-1/1eA)
    Long-term hydrostatic strength Not intended Not intended ISO 9080:2012 validated PE80/PE100

    Comparison with polypropylene injection-molding grades reveals a lower flexural modulus and lower short-term heat deflection for HDPE. M-3606 is therefore not selected for hot-fill or dishwasher-intensive applications without thermal verification; under ISO 75-2:2013 method A at 1.80 MPa, the deflection temperature of HDPE is substantially below that of polypropylene. The choice between M-3606 and PP is made after testing flexural modulus, HDT, and cleaning-chemical resistance according to end-use specifications.

    When M-3606 is processed in thin-wall food-service or consumer packaging with nominal wall thickness below 1 mm, cooling-rate gradients dominate dimensional control. The melt is injected at high velocity, typically 200–400 mm/s, to solidify before the flow front freezes. Cavity filling is therefore dependent on machine hydraulic response, gate geometry, and melt temperature uniformity. Mould shrinkage for HDPE of density 0.960 g/cm³ commonly falls within 1.5–2.5% after 48 h at 23 °C when measured to ISO 294-4:2018 or ASTM D955-21, but measured values vary with flow direction, wall thickness, and gate type.

    Mould temperature differentials of more than 10 °C between core and cavity produce anisotropic shrinkage that manifests as bowing or edge curl in flat lids and shallow containers. In production tools, water-line layouts are balanced to keep core and cavity steel within ±5 °C of the set point; conformal cooling channels are used when cycle-time targets require more aggressive heat removal. Packing pressure decay is adjusted so that gate sealing occurs before the crystalline phase completes, but after volumetric compensation of shrinkage. If packing time is truncated by more than 0.3 s from the gate seal time, sink marks and warpage become measurable in thickness transitions.

    For chilling roll or stack mould systems, cycle times are set by the cooling requirement of the thickest section. A thickness increase from 2 mm to 4 mm roughly multiplies cooling time by a factor of 2–3 in conduction-limited HDPE parts; production scheduling uses thermal simulation rather than linear extrapolation.

    Regulatory Boundary Conditions Are Not Substitutes for End-Use Migration Testing

    A supplier regulatory statement for M-3606 may include conformity to the monomer and additive requirements of the relevant food-contact regulation, but the converter remains responsible for end-use compliance. For the United States, the resin may be evaluated within the scope of FDA 21 CFR 177.1520, which covers olefin polymers with density above 0.94 g/cm³; specific extraction limits and end-use temperature limitations are defined in the regulation and should be confirmed with the current formulation. For the European Union, plastic materials and articles intended for food contact are subject to Regulation (EU) No 10/2011, and the final article must undergo overall migration and specific migration testing. Compliance with EU Regulation (EC) No 1907/2006 for REACH distinguishes between the polymer itself, which is exempt from registration under Article 2(9), and the monomers or additives, which may require registration. RoHS Directive 2011/65/EU restricts lead, cadmium, mercury, hexavalent chromium, PBB, and PBDE in electrical and electronic equipment; polymer resins are not directly in scope, but component suppliers must furnish declarations when the final part enters electronic applications.

    The material is not recommended for continuous contact with strong oxidising acids, aromatic solvents, or chlorinated hydrocarbons at elevated temperature; such chemicals can swell the amorphous phase and accelerate environmental stress-cracking under applied strain. Chemical resistance should be tested according to ISO 22088-1:2006 or ASTM D543-21 using the actual strain and temperature of service. Regrind of M-3606 may be reused at levels up to 20 wt% in the same application when the flake is clean, dry, and not degraded by previous heat history; higher regrind fractions require verification of tensile strength, notched impact, and colour stability after moulding.

    Batch-to-batch variance in melt flow rate should be controlled by incoming inspection. A shift from 6.0 g/10 min to 7.0 g/10 min may reduce cavity pressure and cycle time but can also reduce notched impact strength; a shift to 5.0 g/10 min can increase injection pressure and warp due to orientation. The converter should therefore map lot-specific MFR against part weight, clamp force, and post-mould dimensions before a new lot enters production.