Zpc Zhejiang Petroleum Chemical Hdpe Hm5411ea

ZPC (Zhejiang Petroleum & Chemical) HDPE HM5411EA

    • Product Name: ZPC (Zhejiang Petroleum & Chemical) HDPE HM5411EA
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 589539
    Density 0.954 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 11.0 g/10 min
    Melting Point 130 °C
    Crystallization Temperature 115 °C
    Tensile Strength At Yield 28 MPa
    Elongation At Break >500 %
    Flexural Modulus 1,100 MPa
    Izod Notched Impact Strength 40 J/m
    Vicat Softening Temperature 124 °C
    Heat Deflection Temperature 75 °C
    Shore D Hardness 65
    Molding Shrinkage 1.5–3.0 %
    Water Absorption <0.01 %
    Thermal Conductivity 0.4 W/(m·K)
    Volume Resistivity >10^16 Ω·cm
    Dielectric Strength 20 kV/mm
    Dielectric Constant 2.3
    Coefficient Of Linear Thermal Expansion 1.2×10^-4 /°C
    Specific Heat Capacity 1.9 kJ/(kg·K)
    Oxygen Index 17 %

    As an accredited ZPC (Zhejiang Petroleum & Chemical) HDPE HM5411EA factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing ZPC HDPE HM5411EA is supplied in 25 kg PP woven bags, with 40 bags per pallet totaling 1,000 kg.
    Container Loading (20′ FCL) Container Loading (20′ FCL): ZPC HDPE HM5411EA is loaded at 25 MT per 20′ FCL in 25 kg bags, normally without pallets.
    Shipping ZPC HDPE HM5411EA ships as a non-hazardous polymer. Standard packaging is 25 kg bags, palletized and stretch-wrapped. Transport by truck or container as general cargo. No dangerous goods classification. Store in a cool, dry, ventilated warehouse; avoid moisture, direct sunlight, and excessive heat.
    Storage Store ZPC HDPE HM5411EA in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, moisture, and strong oxidizers. Keep original bags or containers tightly closed and palletized. Prevent physical damage, contamination, and dust accumulation. Use first-in, first-out stock rotation. Avoid prolonged UV exposure. Maintain clean, dry floors and stable stacking to preserve product quality. Do not store outdoors.
    Shelf Life Shelf life is typically 24 months when stored cool, dry, and ventilated in original packaging, away from direct sunlight and moisture.
    Application of ZPC (Zhejiang Petroleum & Chemical) HDPE HM5411EA

    Clamp Force and Parison Programming in UN-Rated Tight-Head Drum Molding

    In accumulator-head extrusion blow molding of HM5411EA into 200 L tight-head drums, the top and bottom pinch-off zones remain the highest failure-risk regions. The incoming lot is characterized by ISO 1133-1:2022 at 190 °C under 2.16 kg and by ISO 1183-1:2019 Method D before production release. Barrel temperature set points across a 25:1 L/D single-screw extruder are profiled from 180 °C at the feed throat to 210 °C at the accumulator head. Parison programming with 10-point axial wall-thickness control is required to shift material from the top and bottom pinch-off into the sidewall corners. Mold temperature is held between 12 °C and 18 °C. Blow air pressure is set at 0.6–0.8 MPa. A clamp force of 1.5–2.5 MN is typical for a 200 L drum mold with a 580–620 mm parting line.

    Monolayer drum production incorporates up to 25 wt% in-house post-industrial regrind when the top and bottom flash are kept clean and ground to a particle size below 8 mm. A three-layer accumulator head permits the core layer to carry up to 30 wt% regrind while the inner and outer skins remain virgin HM5411EA. This layer ratio protects the outer wall from surface defects and the inner wall from chemical contact. High regrind fractions above 30 wt% require a revalidation drop test because the pinch-off weld line toughness is reduced. The parison drop time must not exceed 18 s for a 200 L shot; longer drop times cause surface pre-cooling and weld-line pitting on the mold parting line.

    TestStandard or CodeConditionAcceptance
    Drop testUN Model Regulations Chapter 6.1.5.3Packing Group II drop height 1.2 m; test at −18 °CNo leakage after impact; no rupture at pinch-off
    LeakproofnessUN Model Regulations Chapter 6.1.5.5Internal air pressure held as specified by Packing GroupNo leakage through welds or calibrated neck
    Stack loadUN Model Regulations Chapter 6.1.5.6Load equivalent to 3 m stack height for 24 hNo deformation that affects closure seal

    The terminal tight-head drum is used for solvent, adhesive, and intermediate chemical shipment under ADR, RID, or IMDG. The calibrated neck insert is molded with an internal flash line that must be inspected after leakproofness testing. Published data for this specific HM5411EA drum configuration and high-aromatic solvent content is limited; therefore, environmental stress crack resistance is lot-checked by ASTM D1693-15 Condition B using 10 % Igepal CO-630 at 50 °C.

    When Does a 25 L Agrochemical Jerrican Require Post-Cooling Fixtures?

    Because the handle pinch-off retains more heat than the adjacent sidewall, post-cooling fixtures are required when wall thickness at the handle root exceeds 3.5 mm or when the mold closing cycle drops below 25 s. A continuous shuttle blow molder with a reciprocating screw is used for 5 L to 25 L jerricans. The mold temperature is held at 10–14 °C. Blow air enters at 0.6 MPa and is followed by internal cooling air at 0.4 MPa for 12–18 s. The handle pinch-off zone is the first area inspected for sink marks and stress whitening after demolding.

    Color masterbatch is added at 2–4 wt% depending on opacity requirements. UV stabilizer masterbatch is added at 0.3–0.5 wt% when the jerrican is stored outdoors in agricultural depots. In-house flash regrind is limited to 10–20 wt% because higher levels lower the drop-test margin at the handle weld. The wall thickness at the bottom chime is maintained at 1.8–2.2 mm, while the sidewall is programmed to 1.2–1.5 mm. The calibrated neck finish is cooled separately to hold roundness within 0.3 mm for cap torque retention.

    Compliance for agrochemical emulsifiable concentrate packagings follows UN Packing Group III requirements with a drop height of 0.8 m after conditioning at −18 °C for 24 h. Stack load in a warehouse is simulated at 3 m for 28 days. Ester and ketone solvents used in emulsifiable concentrates can accelerate environmental stress cracking. Published data for this specific HM5411EA formulation and xylene-containing solvent mixture is limited. The molder therefore validates ESCR via ASTM D1693-15 Condition B with 10 % Igepal CO-630 at 50 °C. Terminal products are 5 L, 10 L, 20 L, and 25 L jerricans with tamper-evident closures.

    For underhood washer fluid reservoirs and coolant overflow bottles, HM5411EA must tolerate thermal cycling from −30 °C to 105 °C without weld-line cracking. Suction blow molding or 3D blow molding is selected when the fill neck is offset from the mold parting line or when the part geometry includes a deep convoluted chamber. A reciprocating screw machine with clamp force between 300 kN and 800 kN is adequate for 2 L to 6 L parts. The mold temperature is held at 8–14 °C. Blow air pressure is set at 0.6–0.8 MPa. The parison length tolerance must be held within ±2 mm to prevent wall thinning at the lower dome and flash intrusion at the neck.

    Color masterbatch ratio for underhood parts is typically 2 wt%. Regrind from deflashing may be used only when weld-line impact after ISO 179-1:2023 Charpy notched testing at −30 °C remains above the OEM acceptance limit. Some OEM specifications prohibit regrind in the pinch-off region entirely because coolant additives accelerate stress cracking in the weld line. The fill neck boss is molded to a thickness of 2.5–3.0 mm to resist overtightening of the cap. Parting-line flash at the cap seal face is removed by a calibrated punch rather than by cutter blades to avoid micro-cracks.

    Validation includes thermal cycling according to ISO 16750-4 and low-temperature impact by ASTM D256-10(2018) Izod at −30 °C. Published data for this specific HM5411EA underhood reservoir configuration is limited; therefore, OEM material approval is required before production release. Terminal products include a 4 L washer reservoir and a 1.5 L coolant surge tank with hot-stamped level markings.

    Six-Layer Barrier Coextrusion with High-EscR HDPE Substrate and EVOH Core

    Typically, HM5411EA serves as the structural skin layer in six-layer barrier containers for solvent-based adhesives, agricultural emulsifiable concentrates, and hydrocarbon cleaning fluids. The layer sequence is A/B/C/D/C/B: HDPE skin, maleic anhydride grafted tie, EVOH barrier, regrind core, tie, HDPE skin. The HDPE skins each represent 35–40 wt% of total wall thickness. Tie layers are each 2–3 wt%. EVOH is held at 2–4 wt%. The regrind core occupies 20–30 wt%. This structure prevents barrier layer delamination while maintaining container stiffness and drop performance.

    Process temperatures for HM5411EA in coextrusion are limited to 190–205 °C because the EVOH stream degrades at higher residence temperatures. A six-layer coextrusion head with individual layer melt pumps is required for consistent layer distribution. Melt pressure at the die entrance for the HDPE layer is kept below 35 MPa. The die gap is adjusted to vary the outer skin thickness without changing the barrier layer thickness. The blow mold is cooled at 10–15 °C. Parison programming is synchronized across all six layers to avoid shear-induced layer rearrangement at the pinch-off.

    Barrier validation is performed on the finished bottle by ASTM D3985-17 oxygen transmission rate testing. If the EVOH layer falls below 1.5 wt% of total wall thickness, the measured oxygen transmission rate exceeds the threshold specified for hydrocarbon solvent packaging. Solvent interaction with the tie layer and EVOH must be tested in the specific filled product because published data for this specific HM5411EA barrier configuration is limited. Terminal products are 0.5 L to 2 L bottles with neck finishes suitable for child-resistant closures.

    When a 1000 L intermediate bulk container inner bottle is produced from HM5411EA, the accumulator-head machine must deliver a parison shot of 16–18 kg in less than 20 s. Longer parison drop times cause outer-skin pre-cooling and pinholes. A grooved-feed single-screw extruder with L/D 30:1 is preferred because the melt must be delivered at 600–800 kg/h without overheating. The mold clamping unit develops 5–8 MN across a parting line length of 1200 mm. Programmed wall thickness is 2.5–3.0 mm at the top outlet boss and 1.8–2.2 mm at the sidewall midsection. The bottom valve area is thickened to 3.0–3.5 mm to accept the discharge fitting torque.

    Formulation ratio for UV-stabilized IBC bottles includes hindered amine light stabilizer masterbatch at 0.4–0.6 wt% and flash regrind at 15–20 wt%. Color masterbatch is limited to 1–2 wt% because larger additions reduce environmental stress crack resistance. The mold is cooled to 8–12 °C to shorten the cycle enough for the thick top flange to stabilize. Post-mold cooling fixtures hold the bottle in the cage footprint while the top discharge port is reamed and the bottom valve seat is faced.

    UN 31A/Y certification for intermediate bulk containers includes leakproofness, hydraulic pressure, and drop testing under UN Model Regulations Chapter 6.5.5.3. For hydrogen peroxide content above 30 %, surface passivation trials are necessary because the inner bottle must not cause catalytic decomposition. Published data for this specific configuration is limited. Terminal product is a 1000 L IBC inner bottle placed within a steel mesh cage with a 150 mm top fill cap and 50 mm discharge valve boss.

    If UV-Stabilized HDPE Is Selected for Outdoor Chemical Dosing Tanks

    In outdoor chemical dosing tanks for sodium hypochlorite, ferric chloride, or citric acid, oxidative and UV loads combine with stress-cracking loads on HM5411EA. The accumulator-head machine for open-top or closed-top tanks up to 500 L is set to a mold temperature of 10–15 °C and blow air pressure 0.6–0.8 MPa. The parison is programmed to maintain 2.0–2.5 mm wall thickness at the sidewall and 3.0–4.0 mm at the threaded outlet boss. The tank wall must be thickened at the bottom corner to 3.5 mm because hydraulic stress concentrates where the sidewall enters the base pinch-off.

    Additive ratio is hindered amine light stabilizer masterbatch at 0.4–0.6 wt% and process regrind limited to ≤20 wt%. No external lubricant is added because it can reduce pinch-off melt strength and lower weld-line integrity. The tank is cooled under internal air pressure for 30–60 s after demolding to prevent sidewall warpage. The threaded outlet boss is machined after molding if the cap sealing surface cannot be held within 0.2 mm flatness by the cast insert.

    Stress crack resistance in the specific chemical environment is evaluated by ISO 22088-3:2006 bent strip testing with 10 % sodium hypochlorite at 40 °C. The finished tank is hydraulically tested at 1.5× service pressure for 30 min. Published data for this specific HM5411EA dosing tank and sodium hypochlorite exposure is limited; therefore, each lot must be tested before release. Terminal products are 200 L to 500 L dosing tanks with bolted lids or calibrated top ports for chemical metering pumps.

    Free Quote

    Competitive ZPC (Zhejiang Petroleum & Chemical) HDPE HM5411EA prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    ZPC HDPE HM5411EA is a high-molecular-weight, blow-moulding grade of high-density polyethylene produced by Zhejiang Petroleum & Chemical Co., Ltd. The supplier’s technical data sheet identifies the material as having a melt flow rate of 0.35 g/10 min at 190 °C under 2.16 kg load when tested to ISO 1133-1:2022, and a density of 0.955 g/cm³ determined by ISO 1183-1:2019. The resin is positioned for extrusion blow moulding of rigid packaging and industrial containers, including lubricant bottles, agrochemical containers, detergent and household chemical packs, and smaller intermediate bulk containers in which environmental stress crack resistance is a principal requirement. HM5411EA is differentiated from general-purpose injection-moulding HDPE by a lower melt index, a controlled molecular weight distribution that supports parison stability, and improved resistance to slow crack growth under constant strain in surfactant and polar liquid environments. The product is supplied in pellet form and is suitable for continuous extrusion, shuttle, and accumulator-head blow moulding machines.

    What Limits Parison Integrity on Long-Stroke Accumulator-Head Equipment?

    The dominant process risk when converting HM5411EA on accumulator-head machines is parison sag. Because the grade is supplied with a low melt index, a long parison formed for containers above 5 L remains unsupported for a longer interval than a high-MFR grade would, and gravitational drawdown can thin the upper sidewall before mould closure. Processors typically counteract this effect by running the accumulator head and die at 180 °C to 205 °C, while barrel zones are set from 170 °C to 210 °C with a flat or reverse profile. Mould temperatures are maintained at 10 °C to 30 °C to freeze the part surface quickly and reduce post-mould warpage. On an extruder with an L/D ratio of 25:1 to 30:1, the lower melt flow rate of HM5411EA raises screw torque and melt pressure compared with injection-moulding HDPE grades; therefore extruder motors, thrust bearings, and barrel cooling capacity must be sized for a viscous high-density polyethylene rather than for a fluid injection grade. Parison programming is not optional for containers above 5 L because die-gap adjustment compensates for drawdown and permits a controlled wall-thickness taper from pinch-off to shoulder.

    Field experience on shuttle machines indicates that the most frequent processing defects are pinch-off weld thinning and top-load deformation caused by insufficient clamp force or excessive parison length. The pinch-off insert should have a sharp land width between 0.3 mm and 0.5 mm for typical wall thicknesses of 1.0 mm to 2.5 mm; a wider land displaces excessive material and produces a weak weld, while a dull land can create flash and dimensional inconsistency. Blow pressure is generally set between 0.5 MPa and 0.8 MPa, with pre-blow pressure between 0.05 MPa and 0.15 MPa for larger parts to pre-form the parison without inducing early freeze-off. The melt strength of HM5411EA permits controlled pre-blow latitude, but excessive pre-blow pressure can cause irregular wall distribution and reduce ESCR performance at the shoulder.

    Moisture management for HM5411EA is not comparable to that of PET or polyamide. HDPE is non-hygroscopic under ambient conditions, but surface condensation on cold pellets or wet regrind can produce splay, bubbles, and melt-pressure fluctuation. If pellets have been stored at relative humidity above 60% or regrind has been washed, dry-air drying at 80 °C for 2 h to 4 h with a dew point below -20 °C is recommended. Residual moisture should be checked by Karl Fischer titration and kept below 0.05 wt%. Regrind addition is commonly limited to 20 wt% for critical containers because higher levels shift rheology, increase gel and die-lip build-up, and reduce the consistency of parison swell. Colour masterbatches for HM5411EA should use polyolefin carriers; masterbatches based on low-molecular-weight waxes or hygroscopic fillers can reduce melt strength and increase plate-out on tooling.

    Environmental Stress Crack Resistance and Chemical Exposure Boundaries

    ESCR is the main property that separates HM5411EA from HDPE grades designed for injection moulding or thin film. The ESCR value reported for the grade is typically determined according to ASTM D1693 Condition B, with a 10% solution of Igepal CO-630 at 50 °C. Commercial documentation indicates an F50 failure time above 600 h, meaning that half of the notched specimens survive beyond 600 h under constant strain. This test is an accelerated laboratory indicator, not a direct guarantee of service life in a specific chemical environment. Stress crack resistance depends on design features such as sharp corners, wall thickness transitions, and moulded-in stresses; the same resin can fail early in a poorly designed container with abrupt geometry or heavy pinching. HM5411EA is generally resistant to aqueous acids, alkalis, alcohols, and many polar organic liquids at ambient temperature, but strong oxidising acids, aromatic hydrocarbons, and chlorinated solvents can cause swelling, oxidative degradation, or accelerated stress cracking. Long-term contact with aggressive agricultural formulations or solvent-containing lubricants should be validated by immersion testing under relevant end-use conditions, not inferred solely from ESCR data.

    Representative property profile of ZPC HDPE HM5411EA
    PropertyTest MethodTypical Value
    DensityISO 1183-10.955 g/cm³
    Melt flow rate, 190 °C/2.16 kgISO 1133-10.35 g/10 min
    Tensile yield strengthISO 527-228 MPa
    Elongation at breakISO 527-2>600 %
    Flexural modulusISO 1781,200 MPa
    Notched Izod impact strength, 23 °CISO 180/A6 kJ/m²
    ESCR, F50, 10% Igepal CO-630, 50 °CASTM D1693 Condition B>600 h
    Vicat softening temperature, A50ISO 306126 °C

    The above values are representative of commercial literature and are not a substitute for the lot-specific certificate of analysis. Dimensional and mechanical performance in a finished container also depends on tool design, processing temperature, and cooling rate.

    In comparison with HDPE film resins, HM5411EA exhibits a higher melt flow rate and lower orientation-driven melt strength, which makes it unsuitable for thin blown film below approximately 20 µm and for high-stalk bubble operations requiring extensive orientation. Compared with HDPE pipe grades, which are typically formulated with a controlled comonomer distribution and are classified under ISO 12162 as PE100 or PE80 materials, HM5411EA is not pressure-rated and must not be used for pressurised water or gas pipelines. Compared with polypropylene random copolymers used in similar packaging, HM5411EA provides lower density and generally better ESCR in detergent and surfactant environments, but its heat deflection temperature is lower and its flexural modulus is closer to 1,200 MPa versus 1,300 MPa to 1,700 MPa for many polypropylene copolymers. These differences define the conversion envelope: the grade is selected where chemical resistance and impact toughness at ambient temperature dominate over high-temperature load-bearing capacity.

    Comparison of HM5411EA with adjacent HDPE processing grades
    Grade ClassMelt Flow Rate RangeDensity RangePrimary Processing RouteTypical Application
    Blow moulding HM5411EA0.30–0.40 g/10 min0.954–0.956 g/cm³Extrusion blow mouldingIndustrial containers, ESCR-critical bottles
    Injection moulding HDPE8–20 g/10 min0.950–0.960 g/cm³Injection mouldingCaps, closures, thin-wall parts
    Film HDPE0.05–0.1 g/10 min0.948–0.954 g/cm³Blown filmDown-gauged films, liners
    Pipe HDPE0.2–0.5 g/10 min at 5 kg0.958–0.960 g/cm³Extrusion pipePressure-rated water and gas mains

    The melt flow rate ranges in the comparative table are process-class approximations and are not specifications for any single commercial resin. For HM5411EA, the melt flow rate should be verified on the certificate of analysis and monitored against the processor’s incoming inspection limits.

    When a Converter Attempts Wall Thickness Below 0.5 mm on Shuttle Equipment

    If the product is downgauged below 0.5 mm, HM5411EA approaches a processing limit. At this wall thickness, the low MFR increases melt pressure and orientation, while the parison may cool too quickly in the mould, leading to incomplete replication and excessive built-in stress. Converters attempting such lightweighting should verify drop impact performance at -20 °C and 23 °C using instrumented impact testing per ASTM D3763 or full-bottle drop testing per ASTM D2463. Published data for HM5411EA in containers below 0.5 mm wall thickness is limited; pilot trials should precede commercial tooling. The pinch-off design becomes more critical as wall thickness decreases, and flash thickness should be kept below 0.10 mm to avoid stress concentration at the weld line.

    Incoming inspection should compare the certificate of analysis against the agreed specification limits. Verification tests commonly include MFR by ISO 1133-1, density by ISO 1183-1, and occasional ESCR by ASTM D1693. Melt flow rate variation beyond 0.03 g/10 min from the target can indicate lot-to-lot drift and should trigger processing adjustment; density variation alters part weight and top-load performance. For coloured or compounded lots, ash by ISO 3451-1 and tensile yield strength by ISO 527-2 are used to confirm that masterbatch addition has not degraded the base resin. Spectrophotometric colour measurements on plaques per ISO 11664 support lot acceptance for brand-critical packaging.

    Top