| HS Code | 408140 |
| Density | 0.946 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.45 g/10 min |
| Tensile Strength At Yield | 25 MPa |
| Tensile Strength At Break | 30 MPa |
| Elongation At Break | 600% |
| Flexural Modulus | 1100 MPa |
| Notched Impact Strength | 20 kJ/m² |
| Vicat Softening Temperature | 122 °C |
| Heat Deflection Temperature | 70 °C |
| Brittleness Temperature | -70 °C |
| Environmental Stress Crack Resistance | >1000 h |
| Hardness Shore D | 60 |
| Melting Point | 130 °C |
| Volume Resistivity | >10^16 Ω·cm |
| Dielectric Constant | 2.3 |
| Water Absorption | <0.01% |
| Ash Content | <0.05% |
| Bulk Density | >0.5 g/cm³ |
As an accredited ZPC (Zhejiang Petroleum & Chemical) HDPE HM4560UA factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | ZPC HDPE HM4560UA is supplied in 25 kg PP woven bags, with optional 1000 kg jumbo bags for bulk handling. |
| Container Loading (20′ FCL) | 20′ FCL: 18 MT ZPC HDPE HM4560UA, 25 kg bags (720 bags), loose loaded, securely stowed for ocean transport. |
| Shipping | ZPC HDPE HM4560UA is shipped as non-hazardous thermoplastic resin pellets in 25 kg PP bags or 1000/1250 kg jumbo bags, palletized and stretch-wrapped. Transport in clean, dry containers or trucks. Store cool, dry, away from moisture, direct sunlight, and ignition sources. No special dangerous-goods requirements. |
| Storage | Store ZPC HDPE HM4560UA in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags sealed on pallets, off the floor, within safe stacking limits. Prevent moisture, contamination, and physical damage. Use first-in, first-out rotation. Ensure good ventilation and protect from ignition sources. Avoid prolonged UV exposure and excessive temperatures. |
| Shelf Life | Typically 24 months from production when stored in original unopened packaging, cool, dry, ventilated conditions, away from direct sunlight and moisture. |
In PE100 pressure pipe extrusion, ZPC HDPE HM4560UA is dry-blended with a PE-carrier carbon black masterbatch at 2.0–2.5 wt% and a hindered phenolic–phosphite antioxidant masterbatch at 0.20–0.30 wt% before being fed to a grooved-barrel single-screw extruder with a 36:1 L/D barrier screw. The melt temperature at the die head is held at 195–215°C, and the gear pump is adjusted to keep pressure fluctuation below ±0.5 MPa; excursions above this band produce wall-thickness eccentricity in pipe diameters above 250 mm. Material entering the line must be lot-verified for melt-mass-flow rate by ISO 1133-1, density by ISO 1183-1, and the pipe lot is qualified under ISO 4427-2 and EN 12201-2 for water service, with long-term hydrostatic strength regression by ISO 9080 and PE100 classification by ISO 12162; gas distribution pipe is additionally qualified under ISO 4437-2. Carbon black content is measured by ISO 6964, and pigment dispersion is assessed by ISO 18553, the acceptance criterion being no agglomerate exceeding 6 µm in any 10 g sample because larger agglomerates act as slow-crack-growth initiators at hoop stress values near 10 MPa. Terminal products include PE100 potable water mains, sewage force mains, gas distribution spools, and abrasive slurry transfer lines. Operational limitations include pellet drying at 80°C for 2 h when storage has occurred below dew point or above 60% relative humidity; regrind is capped at 10 wt% unless re-verification of oxidation induction time is performed by ISO 11357-6; contamination with polypropylene above 2 wt% is known to segregate during screw plastication and lower notched slow-crack growth resistance measured by ISO 13479.
On production-scale extrusion lines, batch-to-batch variance presents as a melt-pressure drift at constant screw speed. When the screen-changer pressure drop increases by 15% within 8 h, the screen pack is changed from 60/80/100 mesh to 40/60/80 mesh to prevent over-shear and gel formation. Die-lip deposit is observed when zinc stearate is compounded above 0.05 wt% or when the die head remains above 215°C for more than 6 h; surface gloss, measured by ASTM D2457, declines by more than 10 points when the deposit is not removed. The following matrix is used for lot acceptance and type testing.
| Property | Standard method | Acceptance criterion | Inspection frequency |
|---|---|---|---|
| Melt mass-flow rate | ISO 1133-1 | report against grade data sheet | per lot |
| Density | ISO 1183-1 | report against grade data sheet | per lot |
| Carbon black content | ISO 6964 | 2.0–2.5 wt% | per 100 t |
| Carbon black dispersion | ISO 18553 | ≤ grade 3 | per 100 t |
| Long-term hydrostatic strength | ISO 9080 | PE100 regression curve, no brittle failure before 50 years at 20°C, 10 MPa | type test |
Because the melt elasticity of HM4560UA controls wall distribution, the accumulator-head blow-molding cell is configured with a shot size between 5 kg and 15 kg, a diverging tooling angle of 1.5–2.0°, and a die gap of 1.0–1.5 mm. The mold clamp force is set at 150–300 t for 220 L tight-head drums and 1,000 L intermediate bulk containers. Melt temperature is limited to 180–210°C; at temperatures above 210°C, a 900 mm parison loses more than 20 mm of hang length in 8 s, shifting the pinch-off weld from the center line and producing a thin-wall zone at the container bottom. Formulation additions include PE-carrier color concentrate at 1.0–2.0 wt%, antioxidant masterbatch at 0.10–0.20 wt%, and zinc stearate at 0.05–0.10 wt%; zinc stearate above 0.10 wt% increases die-lip plate-out and reduces weld-line strength in drop tests. Compliance for dangerous-goods packaging is maintained under 49 CFR 178.509 and the IMDG Code with conditioned free-fall drop testing by ASTM D5276 at -18°C; food-contact containers are controlled under FDA 21 CFR 177.1520 with migration testing under 21 CFR 176.170. Terminal products include tight-head 220 L drums, open-head pails, 1,000 L IBCs, and agricultural water tanks. HM4560UA is not recommended for thin-wall injection-blow molding of containers below 500 mL because the high molecular weight produces hesitation marks and uneven core penetration; published data for this specific configuration is limited.
Flat-die extrusion of HDPE geomembrane from HM4560UA is operated on a 120 mm single-screw extruder with a 30:1 L/D barrier screw and a 2.5 mm die gap, followed by a three-roll stack that embosses 0.25–0.50 mm surface asperities for slope friction. The line is set to produce a minimum average sheet thickness of 1.5 mm for landfill base liners and 2.0 mm for heap leach pads, with thickness verification by ASTM D5199. Formulation loading includes carbon black masterbatch at 2.0–3.0 wt%, antioxidant stabilizer at 0.20–0.50 wt%, and hindered amine light stabilizer at 0.10–0.30 wt%; carbon black dispersion is controlled to ≤3 category by ASTM D5596. Finished sheet is qualified under GRI-GM13 for smooth and textured HDPE geomembranes, with tensile properties tested per ASTM D6693, tear resistance per ASTM D1004, puncture resistance per ASTM D4833, and oxidative induction time per ASTM D3895. Production-scale failure modes include edge-bead accumulation when melt temperature exceeds 225°C; the edge trim is reintroduced at 5–10 wt% only after screen filtration through a 500 µm mesh to reduce gel transmission. Terminal products include landfill primary liners, heap leach pads, canal liners, and aquaculture pond liners. The following matrix is used for geomembrane lot acceptance.
| Property | Standard method | Acceptance criterion | Inspection frequency |
|---|---|---|---|
| Thickness | ASTM D5199 | ≥ 1.5 mm minimum average | per roll |
| Carbon black content | ASTM D4218 | 2.0–3.0 wt% | per 50 t |
| Carbon black dispersion | ASTM D5596 | ≤ 3 category | per 50 t |
| Standard oxidative induction time | ASTM D3895 | per GRI-GM13 Table 2 | per 100 t |
| Yield strength and elongation | ASTM D6693 | per GRI-GM13 Table 2 | per 100 t |
In heavy-gauge blown film conversion, HM4560UA is processed on an 80 mm barrier-screw extruder with a 28:1 L/D screw and a 1.0–1.2 mm die gap; the blow-up ratio is maintained between 3:1 and 5:1, while frost line height is set at 500–800 mm above the die face to stabilize bubble geometry. Formulation additions are restricted to white or black PE masterbatch at 3–5 wt% and antioxidant concentrate at 0.10–0.20 wt%; slip and antiblock packages are omitted because the primary output is heavy-gauge industrial sacks. Compliance for food-contact film is verified under FDA 21 CFR 177.1520 and EU 10/2011 with overall migration tested by EN 1186-1; mechanical film properties are audited by ASTM D4976 and dart impact by ASTM D1709 method A. Terminal products include 25–50 µm heavy-duty sacks, agricultural film, carry-out bags, and industrial can liners. Die-lip oxidation becomes a production bottleneck above 230°C, when gel specks detectable at a 50 µm threshold increase on film scanning systems; the line speed is therefore limited to 80% of maximum screw speed when ambient temperature exceeds 35°C to prevent bubble flutter and oxidative gel formation.
Across vacuum corrugator lines, HM4560UA is conditioned with carbon black masterbatch at 2.0–2.5 wt%, antioxidant masterbatch at 0.20 wt%, and fluoropolymer processing aid at 0.02–0.05 wt% to suppress melt fracture at high linear speed. The compound is extruded through a 65 mm single-screw extruder with a 30:1 L/D screw at a melt temperature of 190–225°C; the corrugator molds are water-cooled at 15–20°C to freeze the corrugated profile without surface stress whitening. Compliance is verified by UL 651, CSA C22.2 No. 211.1, and ASTM D3350 cell classification; crush resistance is measured by ASTM D2412. Terminal products include 50–150 mm telecommunications duct, electrical conduit, and agricultural drainage pipe. Published data for this specific configuration is limited; above-ground installations should be re-qualified for UV resistance by ASTM D2565 before extended exposure.
For roll-fed thermoforming, HM4560UA sheet is extruded at 1.0–4.0 mm thickness on a 100 mm single-screw sheet line with a 30:1 L/D barrier screw and a three-roll polishing stack set at 75–90°C. The formulation includes color masterbatch at 2–4 wt% and antioxidant stabilizer at 0.10–0.20 wt%; no plasticizer is added because HDPE does not require plasticization. The sheet is qualified under ASTM D1998 and ISO 14632 for extruded stock; thermoforming is performed at sheet surface temperatures of 160–180°C, with a draw ratio not exceeding 1:1 for unmodified HM4560UA. Terminal products include dunnage trays, material-handling pallets, automotive trunk liners, and battery separation trays. The process limitation occurs when top and bottom polishing-roll temperatures diverge by more than 5°C; sheet curl is then corrected by infrared pyrometer measurement and trim adjustment of the roll circuit.
Competitive ZPC (Zhejiang Petroleum & Chemical) HDPE HM4560UA prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
ZPC HDPE HM4560UA is a pelletized high-density polyethylene resin produced by Zhejiang Petroleum & Chemical Co., Ltd. for monolayer extrusion blow moulding of rigid containers and industrial packaging. Supplier technical literature positions the grade at a nominal density of 0.945 g/cm³ determined by ISO 1183-1:2019 and a melt flow rate of 0.60 g/10 min at 190 °C under a 2.16 kg load in accordance with ISO 1133-1:2022. These values occupy the lower-MFR range of commercial blow-moulding HDPE, where parison hang strength and environmental stress crack resistance are prioritised over rapid injection-driven cavity fill. The grade is supplied as stabilised pellets and is typically specified for containers requiring controlled parison sag, moderate stiffness, and resistance to surface-active contents.
Unopened packaging should be stored in a dry, covered area at ambient temperatures below 40 °C and protected from direct sunlight. Although HDPE is not hygroscopic, condensation on cold pellet surfaces at relative humidity above 60% can introduce surface moisture into the feed throat. A desiccant hopper dryer operated at 70–80 °C for 1–2 h is recommended when pellets have been stored in unheated warehouses during winter months or when visible frost forms on pellet surfaces. Excessive surface moisture in the feed section may produce splay on the parison and reduce melt fracture resistance.
Production-scale extrusion blow moulding observations on accumulator-head machines with L/D 24:1 through L/D 30:1 barrier screws indicate that the usable melt temperature window lies between 165 °C and 200 °C. Below the lower bound, head pressure increases and the parison surface may exhibit flow lines or sharkskin. Above the upper bound, die swell is reduced and the parison loses its ability to hang without progressive top-to-bottom thinning. A 5 °C change in the metering zone near 180 °C changes head pressure by approximately 1.5 MPa to 3.0 MPa depending on screw speed and die gap. Processors should verify barrel temperature profiles with thermocouple depth checks at each zone, particularly when reground scrap is introduced to the feed throat.
The grade is usually processed with die gaps between 1.5 mm and 2.5 mm for containers from 0.5 L to 5 L. Parison sag is controlled by melt strength rather than by external accumulator pressure alone. Die swell is moderate, and the die-pin-to-die-bush land length should be adjusted to maintain a uniform wall thickness across the bottle shoulder and pinch-off area. Blow air pressure typically falls between 0.6 MPa and 1.0 MPa, with mould temperatures maintained between 10 °C and 25 °C to stabilise cooling and reduce post-mould shrinkage. Clamp force requirements for a 5 L container are commonly in the 150–300 kN range on shuttle or accumulator-head machines.
Incoming resin inspection should verify melt flow rate and density against the supplier’s certificate of analysis for each lot. Melt flow rate is measured using an automated melt indexer with a 2.16 kg weight and standard die dimensions per ISO 1133-1:2022. Density is measured by an isopropanol-water density gradient column or calibrated gas pycnometer according to ISO 1183-1:2019. A melt flow rate deviation greater than 0.05 g/10 min from the certificate of analysis should trigger a retest and a review of downstream blow moulding settings before lot interchange.
At a nominal density of 0.945 g/cm³, HM4560UA is in the lower-density segment of HDPE blow-moulding resins. Density controls crystallinity, flexural modulus, and top-load resistance. Higher-density HDPE grades at 0.952 g/cm³ to 0.957 g/cm³ provide greater stiffness and barrier but show reduced environmental stress crack resistance under the same test conditions. Lower-density HDPE grades approaching 0.940 g/cm³ offer improved ESCR but lower top-load strength and lower resistance to permeation. The 0.945 g/cm³ level is therefore positioned for containers requiring balanced mechanical strength and resistance to surface-active liquid stress cracking.
The melt flow rate of 0.60 g/10 min is a low-flow value that correlates with higher average molecular weight and higher melt elasticity. This produces longer parison hang time at a given die gap and permits the blowing of larger containers without rapid sag rupture. It also raises extrusion torque and head pressure compared with high-flow HDPE blow-moulding grades. Environmental stress crack resistance for this density class is commonly assessed by ASTM D1693-21 using 10% Igepal CO-630 at 50 °C; F50 values above 100 h are generally expected for low-flow HDPE blow moulding, but published data for this specific configuration is limited and lot-specific testing is recommended. Bottle drop impact performance is typically evaluated at -18 °C using filled containers according to ASTM D2463-15 or equivalent internal methods.
| Property | Test method | Typical value | Unit |
|---|---|---|---|
| Density | ISO 1183-1:2019 | 0.945 | g/cm³ |
| Melt flow rate | ISO 1133-1:2022 | 0.60 | g/10 min |
| Melt flow rate condition | ISO 1133-1:2022 | 190 °C, 2.16 kg | — |
| Density test temperature | ISO 1183-1:2019 | 23 °C | °C |
In rigid packaging applications, HM4560UA is suitable for monolayer containers with a maximum continuous service temperature below 60 °C. Supplier literature references household chemical bottles, liquid detergent bottles, automotive lubricant containers, and small industrial dosing bottles. For aggressive solvents, the specifier should conduct bottle drop and ESCR tests using the actual fill medium at the intended fill weight and closure torque. External standard tests may not replicate the hoop stress generated by a tightened cap or the swelling pressure of an aggressive surfactant package. Containers intended for food contact must be evaluated separately under the relevant national or regional food-contact legislation; the base resin certificate of analysis alone does not provide food-contact clearance.
Relative to high-flow HDPE blow-moulding grades with melt flow rates above 1.0 g/10 min, HM4560UA produces higher extrusion torque and lower throughput at the same screw speed. It compensates with greater melt strength, lower parison sag, and improved pinch-off weld integrity at the bottle base. In accumulator-head processing, this permits a longer drop time and more uniform wall thickness on larger or deeper-draw containers. Conversely, a high-flow HDPE grade is easier to fill thin walls and complex handle geometries but is more prone to parison drawdown and may require lower melt temperature to retain die swell.
Compared with low-flow HDPE grades at melt flow rates below 0.30 g/10 min used for large drums and intermediate bulk containers, HM4560UA shows easier screw conveying and lower head pressure. Its lower molecular weight reduces cycle time but also lowers ultimate environmental stress crack resistance and high-temperature melt strength. Processors choosing between HM4560UA and a low-flow large-drum grade should compare parison sag length, target bottle weight, and required ESCR under the actual fill medium.
| Processing and application parameter | HM4560UA | High-flow HDPE blow moulding grade | Low-flow large-drum HDPE grade |
|---|---|---|---|
| Melt flow rate class | 0.60 g/10 min | >1.0 g/10 min | <0.30 g/10 min |
| Parison hang time | Moderate to long | Short | Long |
| Extrusion back pressure at same screw speed | Moderate | Low | High |
| Typical container size range | 0.5–5 L | 0.1–1 L | 10–60 L and drums |
| Primary performance strength | Balanced stiffness and ESCR | Fast cycle and thin-wall fill | Maximum ESCR and drop resistance |
Within the ZPC HDPE portfolio, HM4560UA is differentiated from higher-density blow-moulding grades by its 0.945 g/cm³ density and from higher-flow grades by its 0.60 g/10 min melt flow rate. Processors should not interchange lots without confirming the supplier’s current technical data sheet because lot-to-lot variation in stabiliser package, pellet conveyance, and analytical values may occur. If UV outdoor exposure is required, the presence of the UA suffix in the product code should not be interpreted as a confirmed UV-stabilised formulation; a UV masterbatch should be added at the manufacturer’s recommended letdown or a separate weathering-qualified grade should be selected. Published data for outdoor weathering of this specific configuration is limited.
For monolayer chemical packaging, the operational boundary is set by the fill medium’s stress cracking potential and the maximum sustained container temperature. HM4560UA is not recommended for continuous contact with strong oxidising acids, aromatic solvents, or fuel blends unless a multilayer barrier structure or internal surface treatment has been qualified under the intended regulatory and transport requirements. The resin is also not characterised for pressure vessel service or for hot-fill applications above 60 °C, where creep resistance and closure back-off become significant failure modes. Processors should validate all container dimensions and drop performance after colour masterbatch addition because pigments can shift crystallisation kinetics and pinch-off strength.