Zpc Zhejiang Petroleum Chemical Hdpe Hd5502s

ZPC (Zhejiang Petroleum & Chemical) HDPE HD5502S

    • Product Name: ZPC (Zhejiang Petroleum & Chemical) HDPE HD5502S
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 581874
    Melt Flow Rate Mfr 0.35 g/10 min
    Density 0.954 g/cm³
    Tensile Strength At Yield 28 MPa
    Elongation At Break >600 %
    Flexural Modulus 1200 MPa
    Notched Izod Impact Strength 200 J/m
    Vicat Softening Temperature 124 °C
    Melting Temperature 132 °C
    Environmental Stress Crack Resistance Escr >1000 h
    Hardness Shore D 65
    Bulk Density 0.55 g/cm³
    Moisture Content <0.05 %
    Ash Content <0.03 %

    As an accredited ZPC (Zhejiang Petroleum & Chemical) HDPE HD5502S factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing ZPC (Zhejiang Petroleum & Chemical) HDPE HD5502S is packaged in 25 kg woven bags or 1,000 kg jumbo bags.
    Container Loading (20′ FCL) Container Loading (20′ FCL) for ZPC HDPE HD5502S: 25 kg bags, palletized, shrink-wrapped, securely stowed, approx. 20 MT net for export.
    Shipping ZPC (Zhejiang Petroleum & Chemical) HDPE HD5502S is shipped as non-hazardous polyethylene pellets in 25 kg PP woven bags or 500–1000 kg jumbo bags, palletized and stretch-wrapped. It is transported by sea in 20- or 40-foot containers, kept dry and away from direct sunlight, heat, and moisture. Standard export documentation applies.
    Storage Store ZPC (Zhejiang Petroleum & Chemical) HDPE HD5502S in a cool, dry, well-ventilated warehouse at ambient temperature, preferably on pallets in original sealed bags. Keep away from direct sunlight, moisture, rain, heat, sparks, and strong oxidizers. Avoid contamination, physical damage, and excessive stacking pressure. Maintain clean handling areas, follow local regulations, and use oldest stock first.
    Shelf Life Stored dry and ventilated in original packaging, away from sunlight, ZPC HDPE HD5502S has a shelf life of 24 months.
    Application of ZPC (Zhejiang Petroleum & Chemical) HDPE HD5502S

    Accumulator-head extrusion blow moulding of UN 1H1 industrial jerricans

    The commercial route for ZPC (Zhejiang Petroleum & Chemical) HDPE HD5502S in chemical packaging is accumulator-head extrusion blow moulding of tight-head jerricans and open-head drums under UN 1H1 or UN 1H2 design type approval. In this sector, the governing failure mode is environmental stress cracking at the pinch-off weld or along the flash line after sustained contact with hydrocarbons, surfactants, aggressive cleaning agents, or oxidising fluids. HD5502S is processed at melt temperatures of 190–210°C, with an accumulator head shot mass of 5–15 kg, a die gap of 1.8–2.4 mm, and blow-up ratios of 2.8:1–3.4:1. Parison programming is adjusted continuously, with a die-gap reduction of 25–45% at the top and bottom pinch zones to prevent excessive material accumulation in the weld. Production-scale accumulator-head lines fitted with barrier screws of L/D 24:1–30:1 and grooved feed bushes show the least shot-to-shot variation; lines without closed-loop parison control commonly exhibit wall-thickness variation of 0.4 mm or more in 20 L jerricans, particularly at the handle pinch-off. Clamp force on 20 L jerrican tools should be maintained at no less than 500 kN, while mould temperature is held at 25–40°C. Chilled moulds below 15°C can create oriented skin layers that reduce environmental stress crack resistance and are therefore avoided unless the tool design compensates with thicker sidewalls. Surface moisture from outdoor silo storage must be removed by dried-air hopper or pre-drying at 70–80°C for 1–2 h when ambient relative humidity exceeds 60%; the resin is not hygroscopic, but surface condensation can generate splay and parison surface defects.

    Compliance is anchored to the performance-oriented packaging framework of ADR Chapter 6.1.5 and 49 CFR Part 178.509, with design type tests including drop, leakproofness, hydraulic pressure, and stacking. For liquid filling with specific gravity exceeding 1.2, hydraulic test pressure is commonly set at 250 kPa for 30 min, while leakproofness testing is performed at 20 kPa. The UN marking on the finished jerrican, for example 1H1/Y1.8/250, identifies package type, packing group, maximum gross mass, and test pressure. For resin qualification, the relevant stress-cracking test is ASTM D1693-15 Method B at 50°C in 100% Igepal CO-630; high-molecular-weight blow-moulding HDPE grades of this class typically show F50 values beyond 600 h, although published data specific to HD5502S should be obtained from the producer’s certificate of analysis for each lot. Lot-to-lot variability in ESCR is influenced mainly by comonomer incorporation and molecular weight distribution; a drop in F50 below 200 h is an early warning of inconsistent resin supply and should trigger a pre-shipment audit of incoming HD5502S lots before UN design type testing is repeated.

    Formulation ratios for industrial chemical containers are kept deliberately simple to preserve ESCR. A 40% carbon black masterbatch in LDPE carrier is added at 2.0–2.5 wt% to achieve UV weatherability and opacity; the carbon black content in the final part remains around 0.8–1.0 wt%. Antioxidant masterbatch is dosed at 0.03–0.06 wt%, and a fluoropolymer processing aid is used only when melt fracture appears on the parison surface at high output rates, typically 0.01–0.03 wt%. Regrind generated from trimmed flash and rejected containers can be incorporated up to 25 wt% for UN-certified designs provided it is from the same HD5502S source and the resulting container passes the design type tests. Higher regrind fractions, especially with mixed HDPE scrap, lower the F50 ESCR and increase the probability of brittle failure at the pinch-off after drop testing. Processing limitations include the need to keep the melt temperature above 190°C to avoid weak pinch-off welds and below 215°C to avoid thermal degradation, odour formation, and loss of parison melt strength. The terminal product range covers 5 L, 10 L, 20 L, 25 L, and 30 L jerricans, as well as 30–220 L open-head drums with clamp-ring or lever-lock lids.

    Continuous shuttle blow-moulding lines running HD5502S for household detergent, bleach, and personal care bottles operate under a different constraint: wall-thickness distribution must remain tightly controlled at short cycle times, while the resin must resist environmental stress cracking from sodium hypochlorite, caustic, and anionic surfactant formulations. High-density polyethylene of this class is processed at melt temperatures of 175–205°C, with blow-up ratios of 2.0:1–2.8:1, in-line flash trimming, and cooling water set at 10–20°C. The molecular weight distribution of HD5502S controls parison sag, allowing multi-cavity shuttle machines with 8–12 moulds to produce bottles from 500 mL to 5 L at cycle times of 8–25 s. The critical production failure mode in this segment is not ESCR alone, but thickness variation in the handle pinch-off and base corners; when the parison die gap is not profiled for the bottle geometry, these zones can thin by 30–40% and fail filled-bottle drop impact tests. On high-speed shuttle lines, reciprocating extruders of L/D 24:1–28:1 are used, and calibrated neck inserts must be maintained within 0.05 mm roundness; ovality beyond this value produces cap leakage after torque application.

    Compliance for this packaging segment is tied to mechanical integrity standards rather than dangerous goods regulation. ASTM D2463-15 drop impact resistance testing evaluates filled bottle performance, while ASTM D2911-10 controls dimensional tolerance for blow-moulded bottles. Where the bottle envelope has incidental food-contact status under FDA 21 CFR 177.1520 or where REACH Article 33 declarations are required for exported cleaning products, the base resin and colour masterbatch must be selected from approved components; heavy metals and phthalate-containing carriers are specifically excluded. Formulation addition ratios for household chemical bottles are typically 3.0–5.0 wt% titanium dioxide white masterbatch for opacity, 0.05–0.20 wt% slip or antiblock masterbatch, and 0.03–0.08 wt% antioxidant masterbatch. When a pearlescent or pastel visual effect is specified, 0.5–2.0 wt% effect pigment masterbatch is added, but this must be evaluated for screw mixing quality because high-shear dispersion of lamellar pigments can develop melt fracture on the parison surface. The terminal part range includes 500 mL, 750 mL, 1 L, 2 L, 3 L, and 5 L bottles with standard neck finishes, many converted into trigger-spray packaging or closed with push-pull and disc-top closures. The operational boundary for bleach packaging is hot filling not exceeding 60°C; above this temperature, bottle deformation and stress-cracking acceleration are observed, particularly around the handle and base pinch-off.

    What limits regrind incorporation in coextruded automotive fuel tank outer layers?

    Regrind incorporation in six-layer automotive fuel tank coextrusion is limited by the loss of slow-crack-growth resistance in the outer virgin layer, not by short-term tensile or impact strength. In manufacturing, HD5502S is run as the outer HDPE layer on coextrusion accumulator-head machines with six-layer die heads, shot masses of 15–28 kg, and melt temperatures of 210–230°C. The parison length approaches 1.8–2.2 m, requiring high melt strength; excessive parison sag results in wall-thickness variation along the tank periphery. A die gap of 2.0–3.0 mm and blow-up ratio of 1.5:1–2.2:1 are used. The outer HD5502S layer is kept virgin or at regrind content not exceeding 20 wt%; the inner HDPE layer and the post-industrial regrind core layer may contain up to 45–50 wt% defined hydrocarbon-contamination-free regrind. This asymmetric regrind distribution maintains the required -40°C drop impact performance and suppresses rapid crack propagation from outer-surface scratches. Production lines use 3D blow moulding or suction blow moulding to control wall thickness in the complex saddle geometry; wall-thickness measurement at the pinch weld and the fill-pipe interface is performed by ultrasonic scanning every 2 h.

    Compliance for automotive fuel tank extrusion is dominated by type approval and permeation standards. UNECE Regulation No. 34 Annex 5 sets mechanical tests for plastic fuel tanks, including fire resistance, impact, and internal pressure, while FMVSS 301 governs fuel system integrity under crash. Evaporative emission limits under CARB LEV III and EPA Tier 3 require multi-material structures with ethylene vinyl alcohol or low-permeation polyamide barrier layers; HD5502S alone does not meet those permeation limits and is used as the structural outer layer. Chemical resistance testing is performed under ISO 175:2010 with ASTM Fuel B or CE10 test fluids; dimensional change after immersion should remain within the design tolerance of the tank shell. Formulation addition ratios for the outer layer are carbon black masterbatch at 2.0–2.5 wt% for UV protection, antioxidant masterbatch at 0.03–0.08 wt%, and fluoropolymer processing aid at 0.01–0.03 wt%. Adhesive tie layers between HDPE and EVOH are maleic anhydride-modified polyethylene, typically 40–70 µm thick, and the EVOH barrier layer is 1.5–3.0 wt% of the total tank. The terminal product type is the 40–120 L multilayer plastic fuel tank for passenger vehicles and commercial vehicles. The processing boundary is that HD5502S should not be processed above 230°C for extended residence times because oxidative degradation increases gel formation and reduces outer-layer surface quality; gels visible on the outer surface are cause for immediate charge rejection.

    Agrochemical container qualification on HD5502S often proceeds through the FAO/WHO storage-durability and UN combination-packaging framework, where the main differentiator from industrial jerricans is stack-load creep under tropical warehouse conditions and compatibility with solvent-based pesticide formulations. Extrusion blow moulding of 1 L and 5 L agrochemical bottles on single-station and shuttle machines uses melt temperatures of 185–205°C, die gaps of 1.2–2.0 mm, and blow-up ratios of 2.5:1–3.0:1. Sidewall thickness is maintained at 0.6–1.4 mm, and the top shoulder is thickened by 15–25% through parison programming to support the closure and induction-seal liner. Field failures in this segment commonly appear as stress cracks around the neck finish after prolonged tightening or as panel deformation at the sidewall label recess after 28-day stacking at 40°C. For 5 L containers with handle pinch-off, the pinch-off weld must survive 1.2 m drop testing without splitting; a split at the handle weld is typically caused by melt temperature below 190°C or excessive regrind.

    Compliance is defined by UN design type testing for packing group II or III liquids and the FAO/WHO Guidelines for the Storage and Transport of Pesticides. For a 1 L pesticide bottle, the UN drop height for packing group II is 1.2 m, and stacking is assessed at a minimum load corresponding to 3 m warehouse height for 28 days. No single ISO standard covers all crop protection formulations; qualification therefore uses the UN protocol plus supplier-specific chemical compatibility immersion tests with the actual formulation at 40°C for 7 days. Formulation ratios for agrochemical containers include UV stabilizer masterbatch at 0.5–1.0 wt%, pigment concentrate at 1.5–3.0 wt%, and antistatic masterbatch only when powdered formulations are packed, at 0.5–1.0 wt%. Fluoropolymer processing aid is omitted unless melt fracture from high-viscosity masterbatch occurs. The resin must be protected against high shear heating during extrusion; melt temperature excursions above 215°C can create gels that later fail the hydraulic pressure test. The terminal product range covers 1 L, 2 L, 5 L, 10 L, and 20 L agrochemical HDPE containers, often with standard 38 mm or 63 mm neck finishes and induction-sealed closures. A specific operational limitation is that HD5502S should not be used with solvents that swell HDPE by more than 3% in 7-day immersion testing; otherwise, closures lose torque retention and the container can deform under stack load.

    When accumulator head shot mass exceeds 25 kg for IBC inner bottles

    When accumulator head shot mass exceeds 25 kg for 1000 L intermediate bulk container inner bottles, the process window narrows because parison sag, blow ratio, and pinch-off weld strength become mutually constrained. HD5502S is processed on dedicated large-part blow moulding machines with 120–150 mm grooved-feed extruders, L/D 30:1, shot masses of 25–40 kg, and clamp forces of 800–1200 kN. Melt temperatures are controlled at 200–220°C; die gaps range from 3.0–5.0 mm, and blow-up ratios are held at 2.0:1–2.5:1 to avoid excessive hoop orientation. The wall thickness of the finished inner bottle is 2.5–4.0 mm, with top and bottom pinch-off welds requiring complete fusion. Production lines use post-mould cooling fixtures and internal cooling air to reduce cycle time from 180–300 s while preventing warpage at the top opening. The most frequent field failure is crack initiation at the bottom pinch-off after long-term stacking; this is mitigated by maintaining a minimum pinch-off weld thickness of 2.0 mm and verifying weld quality by sectioning each shift.

    Regulatory compliance follows the UN 31H2 composite IBC framework, ADR Chapter 6.5.5, and 49 CFR Part 178.705, with design type tests including bottom lift, top lift, stacking, leakproofness, and hydraulic pressure. A 1000 L composite IBC for liquid dangerous goods is required to pass a hydraulic test of 100 kPa for 10 min and a leakproofness test at 20 kPa. Stacking is evaluated for 28 days at 40°C under the full gross mass load. Formulation addition ratios are kept low to preserve ESCR: carbon black masterbatch at 1.0–2.0 wt%, antioxidant masterbatch at 0.05–0.10 wt%, and processing aid at 0.02–0.05 wt%. Regrind from rejected IBC inner bottles is incorporated up to 30 wt% for non-hazardous service, but UN 31H2 certified bottles normally require 100% virgin HD5502S or a defined same-resin regrind stream validated by the design type tests. The terminal product is the 1000 L blow-moulded HDPE inner bottle used inside a galvanized steel frame or plastic outer cage composite IBC. The main limitation is that the top fill opening should be cooled with internal mandrels; without internal cooling, the neck region can shrink 1–2% and fail the leakproofness test.

    Food-contact compliance under EU 10/2011 is not the only limiting factor in edible-oil bottle production

    Edible-oil bottle haze and the oxidation induction time threshold define acceptance criteria for non-beverage food-contact extrusion blow moulding using HD5502S. In this application, the resin is processed at melt temperatures of 175–200°C, with blow-up ratios of 2.2:1–3.0:1, and mould temperatures of 10–25°C to control gloss and wall-thickness uniformity on 500 mL to 5 L containers. The main technical challenge is not processing instability but the balance between light-protective pigmentation and visual clarity; fully transparent HDPE bottles are not produced from this grade, so edible-oil packers specify white or tinted bottles to limit photo-oxidation of unsaturated oil. Product-specific failure modes include surface whitening at the base crease and stress cracking from oil contact, which is evaluated by ASTM D1693-15 in a test medium representative of edible oil or by direct storage tests with the actual product at 60°C. Oxidation induction time under ISO 11357-6 at 200°C, as a measure of retained antioxidant content, is commonly specified at not less than 20 min for stabilised HDPE bottles intended for long shelf-life edible oils; if the value falls below 10 min, the compound is judged deficient in stabiliser and is rejected for oxygen-sensitive oil filling.

    Food-contact compliance for edible oil packaging is governed by EU Regulation (EU) No 10/2011, with overall migration below 10 mg/dm² or 60 mg/kg; U.S. FDA 21 CFR 177.1520 for olefin polymers; and China GB 4806.6-2016. The resin and additive package must use only listed substances, and the final bottle must pass overall migration testing under fatty food simulant D2 or 95% ethanol for oil-in-water emulsions. Formulation addition ratios include white titanium dioxide masterbatch at 3.0–4.5 wt%, antioxidant masterbatch at 0.03–0.08 wt%, and optionally a UV absorber masterbatch at 0.5–1.0 wt% for extended shelf-life. The terminal product type covers 0.5 L, 1 L, 2 L, 3 L, and 5 L edible-oil bottles, soy sauce containers, and viscous food containers. The operational boundary is hot-filling; this grade should not be used for hot-fill temperatures above 70°C unless the bottle is specifically designed with vacuum panels and heat-set moulds, which are not part of standard HD5502S extrusion blow moulding.

    Free Quote

    Competitive ZPC (Zhejiang Petroleum & Chemical) HDPE HD5502S prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The product ZPC HDPE HD5502S is a high-density polyethylene extrusion blow molding grade produced by Zhejiang Petroleum & Chemical Co., Ltd. The grade is supplied as pellets and is defined by a nominal density of 0.955 g/cm3 under ISO 1183-1:2019 and a melt mass-flow rate of 0.20 g/10 min at 190 °C with a 2.16 kg load under ISO 1133-1:2022. The melt index places HD5502S in the high-molecular-weight HDPE class used for parison extrusion, not in the high-flow injection-molding category. The resin is intended for blow molded containers from approximately 0.25 L to 15 L in household and industrial chemical packaging, automotive lubricant bottles, and selected personal care containers. The grade is controlled for balanced die swell and parison melt strength, which reduce wall-thickness variation on continuous shuttle and reciprocating screw blow molding machines. Because the values stated in this document are typical, the lot-specific certificate of analysis should be obtained before process qualification.

    Within the Zhejiang Petroleum & Chemical HDPE range, HD5502S is distinguished by the combination of 0.20 g/10 min melt index and 0.955 g/cm3 density. Injection-molding HDPE grades typically show melt indices from 8 to 50 g/10 min; high-speed film grades generally fall from 0.04 to 0.8 g/10 min with densities between 0.945 and 0.952 g/cm3. HD5502S is therefore not a direct substitute for thin-wall injection-molded closures or high-stalk film lines. The molecular architecture is controlled to avoid the low melt strength and high shrinkage anisotropy of a narrow low-molecular-weight distribution while retaining processability at standard HDPE barrel temperatures. This balance is critical because containers made from grades with insufficient melt strength exhibit excessive parison sag and poor pinch-off weld integrity.

    Table 1 lists typical physical and mechanical properties from the supplier technical datasheet. These values are not release specification limits and should not be used as design maxima or minima without confirmation from a specific lot.

    PropertyTest methodTypical valueUnit
    DensityISO 1183-1:20190.955g/cm3
    Melt mass-flow rateISO 1133-1:20220.20g/10 min
    Tensile stress at yieldISO 527-2:201227MPa
    Elongation at breakISO 527-2:2012>800%
    Flexural modulusISO 178:20191100MPa
    Notched Charpy impact, 23 °CISO 179-1:20108kJ/m2
    Vicat softening temperature A50ISO 306:2013128°C
    ESCR F50, 10 % Igepal CO-630, 50 °CASTM D1693-15 Condition B50h

    Extensional viscosity data generated on a Sentmanat extensional rheometer at 190 °C and strain rates between 0.1 s-1 and 10 s-1 show strain-hardening behavior typical of HDPE blow molding grades. This response supports uniform parison inflation and reduces local thinning at the pinch-off. The strain-hardening magnitude is lower than that of high-molecular-weight film grades; HD5502S cannot be substituted into thin-film processes requiring bubble stability under film test standards such as those used for high-molecular-weight HDPE film.

    How Does HD5502S Differ from Other HDPE Blow Molding and Film Grades?

    HD5502S differs from general-purpose HDPE blow molding grades in density and melt index. A lower density, such as 0.945 g/cm3, reduces stiffness and top-load strength but improves low-temperature impact; a higher density above 0.960 g/cm3 raises modulus while reducing environmental stress crack resistance. HD5502S occupies an intermediate position. The ESCR value of 50 h under ASTM D1693-15 Condition B supports use with household chemical formulations, but the resin is not a high-density pipe compound. Pipe grades such as PE100 require notched pipe testing under ISO 13479:2022 and long-term hydrostatic strength under ISO 9080:2012; HD5502S is not classified for these applications. Film grades, especially bimodal high-density film resins, are evaluated for dart impact and tear resistance under ASTM D1709-16 and ASTM D1922-15; HD5502S does not carry those film performance specifications.

    Table 2 summarizes the process class separation by typical melt index and density ranges. The ranges are generic industry values, not supplier release limits.

    Resin classTypical melt indexTypical densityPrimary processing windowDifference from HD5502S
    Injection molding HDPE8–50 g/10 min0.952–0.965 g/cm3200–260 °CMelt index too high for parison melt strength
    High-molecular-weight film HDPE0.04–0.15 g/10 min0.945–0.952 g/cm3200–260 °C flat dieMelt index and density lower; unsuitable for blow molding
    Pipe HDPE0.2–0.5 g/10 min0.958–0.961 g/cm3200–240 °C annular diePipe grades require hydrostatic strength and slow crack growth not specified for HD5502S
    HD5502S0.20 g/10 min0.955 g/cm3180–210 °C parison extrusionReference grade

    Compared with lower-molecular-weight blow molding grades in the same density range, HD5502S displays lower melt flow and therefore higher parison melt strength, which allows longer parison hang times. This property is measurable by capillary rheometry under ISO 11443:2021. The shear viscosity at 190 °C and 100 s-1 is expected to fall in the range of 10 000 to 15 000 Pa·s for this melt index class; exact values vary with lot. Compared with high-molecular-weight film grades, HD5502S has a broader blow molding processing window but lacks the bubble stability required for thin-gauge film.

    On extrusion blow molding lines with reciprocating screw plastification and screw L/D ratios between 24:1 and 30:1, HD5502S is processed at barrel set temperatures from 180 °C to 210 °C and die head temperatures from 190 °C to 205 °C. The low melt index requires sufficient screw torque and a compression ratio of 2.5:1 to 3.5:1 to generate a homogeneous melt without excessive shear heating. Shear rates at the die land typically fall between 100 s-1 and 1000 s-1; within this window, the material shows pseudoplastic viscosity decay that permits pumping while retaining parison strength. Mold surface temperatures are maintained from 10 °C to 40 °C. Circumferential die swell values are in the range of 25 % to 45 %, depending on die geometry, flow length, and output rate; parison diameter and weight must be adjusted when tooling changes. Excessive melt temperatures above 220 °C degrade the stabilizer package, generate oxidized gels, and reduce parison melt strength, causing sag and poor pinch weld integrity. Converters operating at ambient humidity above 60 % RH should consider a hopper dryer at 70 °C for 2 h only when surface moisture is suspected; continuous drying is not required under normal indoor storage.

    In accumulator-head machines producing 5 L to 15 L containers, parison programming is required to compensate for sag. The gravitational load on the hanging parison increases with time; a 0.20 g/10 min melt retains usable wall thickness up to a length-to-diameter ratio of approximately 15:1 to 20:1 before local thinning becomes unacceptable. For longer parisons, tooling modifications such as diverging die gaps or higher melt pressure reduce sag but increase die swell. Batch-to-batch variation in die swell is usually less than 5 % absolute; if a lot exceeds this value, the extruder barrel temperature profile and die land length should be verified before changing the parison programmer.

    On high-speed rotary wheel blow molding machines, the melt must be distributed through a continuously rotating manifold. The rheology of HD5502S supports wheel configurations where shear rates at the die land exceed 500 s-1, but excessive shear heating can raise the melt temperature above the 210 °C threshold. Thermocouple probes placed at the die exit should be used to verify actual melt temperature, because barrel set points do not account for shear heating under high screw speed.

    Melt Temperature Window and Parison Sag Thresholds in Continuous Extrusion Blow Molding

    The usable melt temperature window for HD5502S is bounded at the lower end by melt fracture and at the upper end by thermo-oxidative chain scission. At melt temperatures below 180 °C, sharkskin and die lines appear because the high-molecular-weight fraction does not fully relax at the die exit; at temperatures above 210 °C, the onset of stabilizer consumption and chain scission lowers melt strength and increases the formation of gel particles. The practical window is therefore approximately 190 °C to 210 °C. This narrow window demands close control of extruder barrel zones; a temperature overshoot of only 10 °C in one zone can produce a measurable increase in melt flow rate and a decline in parison hang time. The sag rate is governed by extensional viscosity, which for a 0.20 g/10 min HDPE remains sufficiently high below 210 °C but declines rapidly above 220 °C as chain disentanglement and chain scission occur.

    Capillary rheometry under ISO 11443:2021 is the appropriate control method when adjusting melt temperature. Shifts in shear viscosity of more than 10 % at 100 s-1 compared with the reference lot suggest contamination, excessive regrind, or thermal degradation. If the melt flow rate measured under ISO 1133-1:2022 exceeds 0.25 g/10 min after processing, the melt has been degraded beyond the intended envelope. The result is not solely a viscosity change; degraded HDPE shows lower environmental stress crack resistance and weaker pinch-off welds. Therefore, recycled material should be limited and the barrel residence time kept below the degradation threshold specified by the stabilizer supplier.

    Because of its environmental stress crack resistance and processability, HD5502S is employed in containers that require resistance to aggressive liquid formulations, including bleach-based cleaners, agricultural adjuvants, and motor oil. The ESCR value of 50 h under ASTM D1693-15 Condition B supports lot acceptance for household chemical packaging. Containers up to 1 L are often produced on shuttle blow molding machines with clamp forces from 10 to 20 t; larger containers up to 15 L require accumulator-head machines. Wall-thickness distribution in these tools is influenced by parison programming; the linear transducer die-gap adjustment should be calibrated to the swell characteristics of HD5502S. Converter qualification for food contact must be performed under 21 CFR 177.1520 and, in the European Union, under Regulation (EU) No 10/2011 as amended. The finished article must be tested for overall migration and specific migration of additives, because resin compliance alone does not establish food-contact safety.

    Published data for this specific grade under full notch creep testing is limited; converters designing for long-term exposure to wetting agents should request ISO 16770:2004 or ASTM F2136-18 data rather than relying solely on ASTM D1693-15.

    When high-humidity storage or regrind incorporation is required

    If the resin has been stored in unsealed silos or bags in relative humidity above 60 %, surface moisture can produce splay, pin holes, or weakened weld lines in blow molded parts. Drying at 70 °C for 2 h in a desiccant dryer is generally sufficient; continuous drying is not required for HD5502S under standard indoor storage. Regrind from trimmed flash and rejected containers can be blended with virgin material up to 30 % by weight, provided the regrind is dry, free of oil contamination, and not thermally degraded by multiple passes. Higher regrind fractions reduce ESCR and impact strength because the high-molecular-weight fraction is partially degraded during repeated extrusion. The use of more than 30 % regrind in containers for hazardous liquids should be validated by lot-specific ASTM D1693-15 ESCR testing and top-load creep testing under ASTM D2659-17 or equivalent.

    Published data on the interaction between HD5502S and specific antistatic concentrates is limited; therefore, compatibility trials should be conducted before scale-up. Additive packages based on metal stearates and phenolic antioxidants are typical for this resin class. Amine-based antistatic masterbatches that accelerate oxidation at elevated processing temperatures should be avoided unless the masterbatch supplier has verified compatibility, because the additive can shift the melt flow rate and color of the finished article.

    Compared with lower-density HDPE blow molding grades, the 0.955 g/cm3 density of HD5502S raises top-load strength and chemical resistance but reduces low-temperature impact. Converters filling containers at temperatures below -30 °C should evaluate drop impact resistance according to ASTM D2463-15 or ISTA 1A protocols. The grade is not recommended for continuous service above 60 °C under internal pressure without creep rupture verification. It is also not intended for rotational molding, thermoformed sheet, or blown film; those processes require different molecular weight distributions, melt indices, and additive packages. Processors changing from an existing HDPE blow molding grade should compare shear viscosity using capillary rheometry in accordance with ISO 11443:2021 before modifying die gaps or parison programs. When a line is converted from a higher-MFR HDPE, residue of the previous resin may cause initial surface defects; purging with a commercial HDPE purging compound or with the new material at 210 °C for a minimum of 20 min is a standard line-start procedure.

    Top