Zpc Zhejiang Petroleum Chemical Hdpe 9255b

ZPC (Zhejiang Petroleum & Chemical) HDPE 9255B

    • Product Name: ZPC (Zhejiang Petroleum & Chemical) HDPE 9255B
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 411961
    Grade ZPC HDPE 9255B
    Polymer Type High-density polyethylene (HDPE)
    Density 0.955 g/cm³
    Melt Flow Rate 0.05 g/10 min (190°C/2.16 kg)
    Tensile Yield Strength ≥25 MPa
    Tensile Strength At Break ≥30 MPa
    Elongation At Break ≥600%
    Flexural Modulus ≥1000 MPa
    Notched Izod Impact Strength ≥20 kJ/m²
    Vicat Softening Temperature ≥125°C
    Brittleness Temperature ≤-70°C
    Environmental Stress Cracking Resistance >1000 h
    Melting Point 130-135°C
    Hardness 60-65 Shore D
    Bulk Density ≥0.50 g/cm³
    Ash Content ≤0.03%
    Moisture Content ≤0.15%

    As an accredited ZPC (Zhejiang Petroleum & Chemical) HDPE 9255B factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing ZPC HDPE 9255B is supplied in 25 kg PE-lined PP woven bags, palletized, stretch-wrapped, and labeled for shipment.
    Container Loading (20′ FCL) Container loading (20′ FCL): ZPC HDPE 9255B in 25kg bags, palletized, stretch-wrapped, labeled, and secured inside container for ocean shipment.
    Shipping ZPC HDPE 9255B ships as non-hazardous polyethylene resin pellets, typically in 25 kg PP bags, 1 MT jumbo bags, or bulk containers. Transport in clean, dry, ventilated conditions; protect from moisture, direct sunlight, and contamination. No dangerous goods documentation required. HS code: 3901.20. Standard international freight handling applies.
    Storage Store ZPC HDPE 9255B in original packaging in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and open flames. Keep bags or containers sealed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Maintain clean handling areas, use appropriate PPE, and follow local regulations and manufacturer storage guidance.
    Shelf Life Shelf life is 24 months from production when stored dry, cool, ventilated, and away from direct sunlight in original packaging.
    Application of ZPC (Zhejiang Petroleum & Chemical) HDPE 9255B

    On shuttle-type extrusion blow-molding equipment with grooved-barrel extruders of 24:1–30:1 L/D, ZPC HDPE 9255B is processed at melt temperatures of 190–220 °C, with die-head zones held at 205–215 °C and mold circuits held between 10 °C and 25 °C. The formulation for household chemical containers consists of pelletized color masterbatch at 1.5–3.0 wt%, fluoroelastomer-based processing aid at 0.03–0.08 wt%, and, where dry-fill detergents are packaged, an antistatic additive at 0.1–0.5 wt%; closed-loop regrind is limited to 30 wt% because higher loading has been observed on shuttle machines to increase parison length variation and pinch-off failure frequency. Compliance for this application is anchored to FDA 21 CFR 177.1520 for olefin polymers and EU No 10/2011 for dual-use food-contact retention, with the finished-article overall migration limit of 10 mg/dm² requiring converter-level extraction testing rather than resin certification alone. Downstream conversion uses parison programming of 15–35% radial wall-thickness adjustment, blow-air pressure of 0.6–0.8 MPa, pinch-edge clearances of 0.3–0.6 mm, and cycle times of 12–18 s for a 1-L bottle. Terminal finished articles include 0.5–5 L detergent bottles, bleach containers, fabric-softener bottles, all-purpose-cleaner packs, and liquid hand-soap containers.

    Pre-drying is not normally required when warehouse relative humidity remains below 60%; if surface moisture is visible, the resin is to be dried at 80 °C for 2 h. Processing outside the 190–220 °C melt window increases odor and plate-out on accumulator heads, and die-lip temperatures above 220 °C should be avoided with antistatic packages. For bleach-containing formulations, the converter is to run environmental stress-crack resistance screening on the finished bottle per ASTM D1693 Condition A because the aggressive packaged liquid, not the base resin alone, controls stress-cracking; the failure criterion is set by the brand owner, often as an F50 value above 100 h.

    What UN 3H1 Certification Changes in Extrusion Blow Molding at 30-L Scale?

    Accumulator-head lines running ZPC HDPE 9255B for UN-rated lube-oil and hydraulic-fluid jerry cans require melt temperatures of 195–220 °C and die-head temperatures of 200–215 °C. The formulation is adjusted for outdoor and industrial fluid exposure with a high-molecular-weight hindered-amine light stabilizer at 0.1–0.4 wt%, pelletized carbon black or pigment masterbatch at 1.0–2.5 wt%, and an antioxidant masterbatch at 0.03–0.08 wt%; regrind is held at or below 20 wt% because the drop-test and hydraulic-pressure qualification of UN 3H1 packaging is no longer automatically valid above this loading unless the design-type test is repeated with the regrind composition. The production route for a 30-L jerry can uses an accumulator head with shot capacity of 1.2–1.5 kg, extruder L/D of 24:1–30:1, blow-air pressure of 0.7–0.9 MPa, clamp force of 300–800 kN, and cooling times of 25–45 s depending on mold efficiency and ambient temperature. Parison programming in the 30–45% range is required to maintain body wall thickness at 1.0–1.8 mm and neck pinch-off consistent with the UN design-type test. Terminal articles include 10/20/25/30 L UN 3H1 jerry cans for lube oil, hydraulic oil, coolants, diesel exhaust fluid, and agrochemical intermediate liquids.

    The governing compliance framework consists of the UN Model Regulations Chapter 6.1 design-type tests as referenced by ADR/RID 6.1.5 and 49 CFR §178.509; each converter must hold the relevant UN packaging certificate for the specific mold and parison program. Re-qualification is required when regrind loading moves above 20 wt%, when the parison program changes by more than 5% in the neck region, or when mold cooling channel geometry is modified, because the UN certificate is tied to the exact design-type test sample.

    Design-type testReferenceConditionPass requirement
    DropUN Model Regulations 6.1.5.3; ADR/RID 6.1.5Packing group II: 1.2 m at 18 °CNo leakage after impact
    LeakproofnessUN Model Regulations 6.1.5.420 kPa internal air for 10 minNo leakage
    Hydrostatic pressureUN Model Regulations 6.1.5.5100 kPa for 30 minNo leakage or rupture
    StackingUN Model Regulations 6.1.5.6Load equivalent to 3.0 m stack height for 24 h at 40 °CNo deformation affecting containment

    When a Six-Layer Die Head Receives EVOH and Maleic-Anhydride-Grafted Tie Resins

    A six-layer coextrusion blow-molding line running ZPC HDPE 9255B as the structural skin layer for oxygen-sensitive agrochemical and food packaging typically positions the HDPE skin at 60–75 wt% of the total parison wall, maleic-anhydride-grafted polyethylene tie layers at 2–5 wt% per tie layer, and an ethylene-vinyl alcohol copolymer core at 3–6 wt%; if a regrind layer is added, the layer sequence becomes HDPE/regrind/tie/EVOH/tie/HDPE and the regrind layer is restricted to 20–30 wt% of total weight. Compliance for food-contact use is evaluated under FDA 21 CFR 177.1520 for the HDPE skin, FDA 21 CFR 177.1360 for the EVOH layer, and EU No 10/2011 for the finished multi-material article; oxygen transmission rate is measured on the blown bottle by ASTM F1307 or on flat film by ASTM F1249, with converter-level barrier qualification needed because layer thickness deviation directly controls the transmission value.

    Processing is performed with separate extruders feeding gear pumps to maintain layer thickness variation at or below ±10%, a die-head temperature of 190–220 °C, die gap of 0.8–1.4 mm, blow-up ratio of 2.2–3.0:1, and cooling times of 10–18 s for a 1-L bottle; melt pumps are mandatory when the EVOH extrusion temperature must remain below 225 °C while the HDPE skin is run at the upper end of its melt window. Published data for this specific six-layer configuration is limited to converter-level barrier qualifications; resin datasheet oxygen transmission values are not a substitute. Terminal products manufactured by this route include 0.5–5 L agrochemical bottles, crop-protection containers, edible-oil bottles, sauce packs, and barrier pharmaceutical containers requiring oxygen ingress control.

    LayerMaterialWeight fractionProcess set point
    External structural skinZPC HDPE 9255B25–35 wt%200–220 °C
    Regrind coreApproved HDPE/EVOH/tie regrind20–30 wt%190–210 °C
    Tie layerMaleic-anhydride-grafted polyethylene2–5 wt%190–210 °C
    Barrier coreEVOH3–6 wt%180–215 °C
    Tie layerMaleic-anhydride-grafted polyethylene2–5 wt%190–210 °C
    Internal structural skinZPC HDPE 9255B25–35 wt%200–220 °C

    Within ISO 14644-1 Class 8 cleanrooms, pharma-grade blow-molding lines processing ZPC HDPE 9255B for ophthalmic and nasal-spray containers are operated with point-of-use HEPA filtration, oil-free blow air, and ionizing bars to control static contamination. The formulation excludes post-consumer regrind and consists of pharmaceutical-grade white masterbatch at 0.5–2.0 wt% and, where die-lip build-up is problematic on continuous runs, a fluoroelastomer processing aid at 0.02–0.05 wt%; slip agents are omitted unless the specific compendial application provides a positive list entry. Compliance is determined by USP <661.1> for plastic packaging systems, Ph. Eur. 3.1.3 for polyolefins, and FDA 21 CFR 177.1520 under the applicable condition of use; extractables profiling follows the finished container, not the base resin, and must be repeated for any color masterbatch change. The downstream process uses mold chillers held at 12–18 °C, parison programming of 10–25% for small neck finishes, and in-line leak detection at 20–30 kPa; cycle times for a 30-mL ophthalmic bottle are commonly 8–15 s. Terminal finished articles include 5–50 mL ophthalmic bottles, 10–30 mL nasal-spray bottles, 100–250 mL oral-liquid containers, and 30–200 mL cosmetic lotion bottles.

    Closed-Loop Regrind Ratios and Melt-Stability Limits

    The closed-loop regrind stream generated from ZPC HDPE 9255B container scrap is reintroduced at 20–40 wt% into non-food blow-molding production, with the balance of 60–80 wt% maintained as virgin HDPE to stabilize parison drawdown and pinch-off tear resistance. An antioxidant masterbatch is added at 0.05–0.2 wt% to offset the thermo-oxidative history of the regrind, and a toner masterbatch is added at 0.1–0.3 wt% only when yellowing must be corrected. Traceability is managed under EN 15343:2007 for plastics recycling input/output verification and ISO 14021:2016 where recycled content is communicated; REACH Article 33 communication applies when any substance of very high concern in the recovered feedstock exceeds 0.1 wt%. The regrind is shredded through a 8–10 mm screen, passed over a high-intensity magnetic separator, dedusted by cyclone, and gravimetrically blended with virgin pellets before entering the extruder throat. After five repeated closed-loop passes, the melt-flow rate by ISO 1133-1:2022 is to be measured; drift exceeding 10% of the virgin lot value triggers antioxidant adjustment or reduction of regrind loading. Terminal articles are restricted to non-food detergent and industrial-fluid containers, automotive fluid packs, and other industrial packaging where compendial or UN food-contact requirements are not applicable.

    Free Quote

    Competitive ZPC (Zhejiang Petroleum & Chemical) HDPE 9255B prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    ZPC HDPE 9255B, produced by Zhejiang Petroleum & Chemical Co., Ltd., is a high-density polyethylene resin intended primarily for extrusion blow moulding of rigid containers. The grade is differentiated from ZPC injection moulding and film resins by a controlled rheology that combines sufficient shear thinning for extrusion with elevated extensional viscosity for parison hanging stability. Publicly available secondary listings place the grade in the density class near 0.955 g/cm³; the certificate of analysis remains the controlling document for lot-release density and melt mass-flow rate. Melt mass-flow rate is reported under ISO 1133-1:2022 at 190 °C and 21.6 kg. Exact numerical limits for ZPC HDPE 9255B are not consistently disclosed across secondary trade databases, and process calculations should therefore not be based on assumed melt index values.

    Grade Designation, Density Class, and Molecular Architecture

    The terminal letter in the designation identifies the intended conversion process, separating 9255B from ZPC injection, film, and pipe grades. Published disclosures do not always include the comonomer type or molecular weight distribution. The processing behaviour of high-density blow moulding polyethylene with a density near 0.955 g/cm³ is consistent with a broad or bimodal molecular weight distribution: a lower molecular mass fraction lowers viscosity at the die wall and reduces head pressure, while a higher molecular mass fraction increases zero-shear viscosity and limits parison sag. Environmental stress crack resistance in such systems is controlled by tie-molecule concentration and crystallite thickness distribution rather than by density alone. Quantitative molecular weight data for ZPC HDPE 9255B is limited; the manufacturer’s technical data sheet should be consulted before rheological modelling.

    The specification framework relevant to blow moulding grade evaluation is summarised below. Lot-release values are determined under the listed test methods; the table does not replace the official specification.

    Specification framework for ZPC HDPE 9255B
    ParameterTest methodRole in blow moulding
    DensityISO 1183-1:2019Controls stiffness, top-load strength, and permeation resistance
    Melt mass-flow rateISO 1133-1:2022 at 190 °C, 21.6 kgIndicates shear-thinning behaviour and accumulator head pressure
    Environmental stress crack resistanceASTM D1693-15bPredicts container life in aggressive fluids
    Tensile yield stressISO 527-2:2012, type 1B, 50 mm/minRelates to creep and deformation under load
    Flexural modulusISO 178:2019, 2 mm/minMeasures stiffness contribution to panel rigidity
    Vicat softening temperatureISO 306:2022, method A50Sets upper use temperature for hot-fill and wash-down
    Charpy notched impact strengthISO 179-1:2010, 23 °CIndicates dent resistance and low-temperature ductility

    The density class near 0.955 g/cm³ places the material between lower-density HDPE film grades and higher-density HDPE pipe grades. This position allows higher stiffness than low-density polyethylene while retaining a broader blow moulding window than pipe-grade resins with densities above 0.960 g/cm³. The exact density interval for the current production lot must be taken from the ZPC certificate of analysis because secondary listings may not reflect active production.

    Extrusion blow moulding trials on accumulator-head machinery are normally conducted with a smooth-bore single-screw extruder of 24:1 to 30:1 L/D. A grooved feed section is preferred because it stabilises solids conveyance and prevents surging. Barrel temperatures are profiled from 50 °C at the feed throat to 220 °C at the die head, while the die exit melt temperature is usually held between 180 °C and 210 °C. A melt pump between the extruder and the accumulator head dampens pressure fluctuations. The accumulator head applies a drop pressure typically in the range 20 MPa to 35 MPa; lower pressure is used for thin die gaps and higher pressure for high molecular mass parisons. The parison die gap is adjusted between 1.2 mm and 2.8 mm, depending on finished part weight and trim ratio.

    The material is not hygroscopic in the manner of polyamide or PET. Feeding problems arise from surface condensation when cold silo material enters a warm production hall. At relative humidity above 60%, hopper drying at 80 °C for 2 h reduces screw slip and intermittent parison length variation. Regrind addition up to 25 wt% is common for non-food containers; for food-contact packaging, each lot must be qualified under the applicable national regulation before regrind incorporation. Processing above 220 °C accelerates thermal-oxidative chain scission, which lowers molecular weight and environmental stress crack resistance. Processing below 180 °C increases melt fracture sensitivity and weakens the pinch-off weld. The practical melt-temperature window is consequently narrow, and die-head thermocouple calibration should be verified before each production shift.

    What Processing Parameters Govern Parison Stability?

    Parison stability is governed by three competing rheological responses: shear viscosity in the die land, extensional viscosity in the hanging parison, and elastic recovery at the die exit. In accumulator blow moulding, the parison hangs for a period that increases with container length; gravitational sag reduces wall thickness in the lower region. A qualitative sag resistance index is the ratio of melt strength to zero-shear viscosity, but no single ISO method is adopted. Laboratory evaluations use the Rheotens extensional rheometer to measure draw force as a function of draw speed; published data for ZPC HDPE 9255B on this instrument is limited.

    During drop, the parison diameter increases due to die swell. For HDPE blow moulding grades, die swell ratios of 1.35:1 to 1.70:1 are typical; exact values must be measured on the production die because swell depends on die land length, gap, temperature, and shear history. The die land length is usually set at 10 to 20 times the die gap to relax inlet stresses. A shorter land reduces pressure drop but increases melt fracture sensitivity. Wall shear stress in the die land should be kept below 0.14 MPa to avoid sharkskin and gross melt fracture; published data for the melt fracture threshold of 9255B is limited, so production dies should be validated through incremental pressure-drop and surface-quality trials.

    Parison programming should be used for containers with length-to-diameter ratios above 4:1. The die gap is closed during the initial drop to place additional material near the container top and bottom, then opened in the middle. Modern servo-hydraulic heads execute gap changes within 50 ms; slower response produces visible thickness bands and weld-line weakening. In large-container production, pinch-off design and clamp force are equally critical. Machines of 500 kN to 1500 kN clamp force are commonly used for 200 L drums and intermediate bulk container inner bottles, while shuttle machines below 100 kN are limited to bottles below 5 L. The exact mould clamping requirement for a given container must be calculated from part projected area and blow pressure.

    When 9255B Replaces Conventional Unimodal Blow Moulding HDPE

    When 9255B replaces a conventional unimodal blow moulding HDPE, the main observable difference is lower parison sag at the same container weight. In production trials this allows a reduction in container wall thickness or an increase in drop length without bottom thinning. The environmental stress crack resistance improvement is typically assessed under ASTM D1693-15b condition A or B at 50 °C in 100% Igepal. Unimodal grades of equal density may fail between 50 h and 200 h, while bimodal grades frequently exceed 500 h; specific ZPC HDPE 9255B values must be confirmed from the certificate of analysis or independent testing. These differences are magnified in aggressive liquid service, where interlamellar tie-molecule density becomes the controlling failure variable.

    Compared with ZPC injection moulding HDPE, 9255B has a lower melt flow index and higher elongational viscosity. This makes it unsuitable for thin-wall injection moulding; filling of wall sections below 1.0 mm will require excessive injection pressure and may cause freeze-off before complete packing. Film-grade HDPE is formulated for bubble stability and draw-down at high stalk heights; its molecular architecture differs from blow moulding HDPE, which is optimised for high die swell and parison thickness retention. Pipe-grade HDPE is formulated for long-term hydrostatic strength under ISO 9080 and slow crack growth resistance; it is not interchangeable with 9255B in blow moulding because its high melt viscosity can overload accumulator heads and produce excessive parison sag. The product therefore occupies a narrow specification band: stiff enough for rigid containers, viscous enough for large parisons, and shear-thinning enough for stable extrusion.

    Compliance, Food-Contact Verification, and Storage Boundaries

    Compliance is lot-specific and must be verified through the supplier’s declaration. The resin is typically evaluated against the following standards relevant to rigid polyethylene containers. The table identifies the regulatory boundary; it does not constitute a certificate of compliance for any specific shipment.

    Compliance checklist matrix
    Standard or regulationRelevant clause or test methodApplication boundary
    FDA 21 CFR 177.1520Olefin polymers, paragraph (c) specificationsUS food-contact containers for food types and use conditions specified in the regulation
    GB 4806.6-2016Hygiene standard for food-contact plasticsChina food-contact packaging; overall migration limits under specified simulants
    REACH Regulation (EC) No 1907/2006Annex XVII restrictions and SVHC candidate listEU market; substance-of-concern screening at article level
    RoHS Directive 2011/65/EUAnnex II restricted substancesElectrical and electronic equipment housings; lead, cadmium, mercury, hexavalent chromium limits
    ASTM D1998-15Polyethylene upright storage tanksMoulded tanks for atmospheric storage; not for pressure service

    Resin should be stored in a dry environment below 50 °C and protected from direct sunlight. Ultraviolet exposure of natural resin without UV stabiliser is not recommended for outdoor service; containers expected to be stored outdoors require a carbon black or hindered amine stabiliser package validated by accelerated weathering under ISO 4892-2:2013. Material removed from storage after prolonged exposure to high humidity should be dried as specified above before feeding. The operational boundaries described here are production-control limits, not material specifications; they apply to the conversion of high-density blow moulding polyethylene on standard accumulator-head machinery.