| HS Code | 182831 |
| Product Name | ZPC HDPE 7260 |
| Polymer Type | High-density polyethylene (HDPE) |
| Physical Form | Pellets |
| Melt Flow Rate 190 C 2 16 Kg | 7.0 g/10 min |
| Density | 0.960 g/cm³ |
| Tensile Yield Strength | 28 MPa |
| Elongation At Break | >500% |
| Flexural Modulus | 1000 MPa |
| Izod Notched Impact Strength | 50 J/m |
| Vicat Softening Temperature | 125°C |
| Brittleness Temperature | <-70°C |
| Shore D Hardness | 65 |
| Water Absorption | <0.01% |
| Volume Resistivity | >10^16 Ω·cm |
| Dielectric Constant 1 Mhz | 2.3 |
| Mold Shrinkage | 1.5-3.0% |
| Thermal Conductivity | 0.45 W/m·K |
| Specific Heat Capacity | 2.3 kJ/kg·K |
As an accredited ZPC (Zhejiang Petroleum & Chemical) HDPE 7260 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | ZPC (Zhejiang Petroleum & Chemical) HDPE 7260 is supplied in 25 kg woven bags, typically palletized, with 25 metric tons per 40-foot container. |
| Container Loading (20′ FCL) | ZPC HDPE 7260 loaded in 20′ FCL: 25 kg bags, palletized, shrink-wrapped, strapped; approx. 18 MT net for export. |
| Shipping | ZPC HDPE 7260 ships as a non-hazardous, solid polyethylene resin in 25 kg PP bags, 1,000 kg jumbo bags, or bulk liners. Transport in clean, dry containers or trucks, avoiding moisture, heat, and direct sunlight. Standard HS code 3901.20; no dangerous goods classification. Store in a dry, ventilated area. |
| Storage | Store ZPC HDPE 7260 in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers closed to prevent moisture, dust, and contamination. Protect from UV radiation. Stack pallets securely at moderate heights to avoid deformation. Maintain clean, dry conditions and use first-in, first-out inventory. Follow local regulations and supplier safety data sheet requirements. |
| Shelf Life | Shelf life is typically 24 months from production date when stored in original packaging under cool, dry, ventilated conditions. |
ZPC HDPE 7260 is a high-density polyethylene injection-molding grade supplied by Zhejiang Petroleum & Chemical. The grade designation corresponds to a nominal melt flow rate of 7.2 g/10 min under ISO 1133-1:2022 at 190°C/2.16 kg and a nominal density of 0.960 g/cm³ under ISO 1183-1:2019. The molecular architecture yields a high degree of crystallinity, typically above 70 % when cooled at 10 K/min, and a flexural modulus in the 1,100–1,300 MPa range under ISO 178:2019. The product is therefore positioned for injection-molded articles that require rigidity, creep resistance and chemical resistance rather than stretch-film or blow-molding grades.
High-cavitation beverage closure tooling represents the most demanding downstream use of HDPE 7260. In 48- to 96-cavity tools producing 26 mm single-piece closures with tamper-evident bands, the melt fill time is normally 0.30–0.60 s. Shear rates at gate lands thinner than 0.8 mm exceed 12,000 s−1. Under these conditions the resin fills the sealing skirt and bridge without short shots, but rapid cooling is required to prevent the tamper-evident band hinge from retaining excessive molecular orientation. Mold temperature is held between 10°C and 18°C. Below 8°C, the oriented amorphous layer freezes before chain relaxation completes, producing microcracks along the perforated band. Above 22°C, cycle time rises and the shell remains soft enough to deform in downstream unscramblers and capping chucks. The closure is evaluated for environmental stress crack resistance by ASTM D1693-15 using a notched specimen under constant strain in an Igepal CO-630 solution at 50°C. High-density resins of this density class typically fail before 10 h under this test unless comonomer placement and molecular weight distribution are optimized. In closure production, HDPE 7260 is often blended with up to 15 wt% LLDPE to raise ESCR and hinge integrity, at the cost of top-load stiffness and organic vapor barrier. Food-contact compliance follows Regulation (EU) No 10/2011 Annex I; total migration into 3 % w/v acetic acid, 10 % ethanol and 20 % ethanol simulants must not exceed 10 mg/dm². United States food-contact use falls under FDA 21 CFR 177.1520(c). Published data for this specific configuration is limited, so cap producers routinely qualify lot-to-lot ESCR and retainer ring ovality after 48 h at 40°C. On a 48-cavity cap tool mounted on a 2,500 kN hydraulic clamp machine with a 24D screw, the transition from polypropylene random copolymer to HDPE 7260 requires lowering nozzle temperature by 10°C and raising screw speed by 15 % to avoid over-shearing at the valve gate. The resulting gate stringing transfers to the sealing skirt and causes leakers if the tool is not purged correctly.
The long-term failure mode in bottle crates and distribution totes is creep buckling of the open-grid sidewall under vertical top load. The density of 0.960 g/cm³ raises flexural modulus to the 1,100–1,300 MPa range under ISO 178:2019, but the corresponding reduction in tie-molecule concentration lowers impact resistance at freezer temperatures. Injection-molded crates produced from HDPE 7260 are qualified by top-load creep tests at 40°C and 80 % RH using a fixed load of 250 kg for 72 h. The deformation threshold is typically 10 mm, derived from methods adapted from ISO 12048:2000. Failure initiates at intersections of vertical ribs and horizontal base frame members. Increasing the corner radius from 0.8 mm to 2.5 mm reduces the stress concentration factor and raises failure load by approximately 30–40 %. Processing uses a single-stage reciprocating screw with barrel temperatures of 200°C, 220°C and 230°C respectively. A screw with 22:1–24:1 L/D and 2.5:1 compression ratio is sufficient for homogeneous melting without excessive shear heat. Injection pressure is usually 60–90 MPa with holding pressure 40–60 MPa for 6–10 s. Mold temperature is held at 15–25°C to limit cycle time. If the base slab exceeds 4 mm while side ribs remain near 2 mm, differential shrinkage produces out-of-plane distortion above 2 mm per 600 mm length. That is rejectable in automated palletizing. Washing with hot water and alkaline detergents requires stress crack qualification by ASTM D1693-15. A crate with unacceptable internal stress fails near the gate area within 24 h of exposure to a 70°C 1 % NaOH solution. This is the production-scale bottleneck when switching from lower-density HDPE to 0.960 g/cm³ grades.
| Application segment | Critical property | Standard method | Typical production condition |
|---|---|---|---|
| Beverage closures | ESCR, migration | ASTM D1693-15, Regulation (EU) No 10/2011 | Mold 10–18°C, shear rate above 12,000 s−1 |
| Logistics crates | Flexural modulus, top-load creep | ISO 178:2019, ISO 12048:2000 | Holding 40–60 MPa, melt 200–230°C |
| Thin-wall containers | Shrinkage anisotropy | ISO 294-4:2018 | Mold 12–20°C, cycle under 5 s |
| Industrial pails | Low-temperature drop impact | ASTM D2463-15 | Melt 200–235°C, wall 1.6–2.5 mm |
| Appliance housings | Detergent ESCR | ISO 22088-2:2010 | Nozzle 230–240°C |
Dairy cups and food containers with capacities of 0.5–1.0 L are molded from HDPE 7260 on high-speed injection machines with cycle times under 5 s. The melt flow rate of 7.2 g/10 min allows wall stock between 0.6 mm and 1.2 mm in multi-cavity tools. The dominant defect is post-mold warp caused by differential shrinkage. Shrinkage anisotropy measured by ISO 294-4:2018 is typically 1.2–1.8 % parallel to flow and 1.5–2.0 % perpendicular. To hold lip roundness within 0.5 mm, the cavity dimensions are offset by approximately 1.5 % and mold temperature is maintained at 12–20°C. Edge gates produce vertical flow orientation and concentrate shrinkage along the sidewall; diaphragm gates in the base produce radial orientation and more uniform rim contraction. Mold release sprays must be avoided because silicone oil residues migrate to the food-contact surface and interfere with lid sealing. Instead, a polished core with draft angle of at least 1° and carbon-reinforced ejector sleeves is used. Melt temperature at the nozzle is held at 210–230°C; higher temperatures reduce viscosity but accelerate oxidation of the thin melt film at the flow front. Oxidative degradation is detected by an increase in melt flow rate of more than 10 % between first and fifth injection cycles, using ISO 1133-1:2022. Food-contact testing follows Regulation (EU) No 10/2011, with overall migration limits of 10 mg/dm² in 3 % w/v acetic acid and 10 % ethanol. The high density also reduces water vapor transmission through the container wall; for dry powder dairy applications, permeability is measured by ASTM F1249-20 at 38°C and 90 % RH.
For industrial pails of 20 L volume, HDPE 7260 is processed with a wall thickness of 1.6–2.5 mm and a solid handle bridge. A single injection point at the base center fills the pail in 1.5–2.0 s; hesitation in the handle region is avoided by raising holding pressure to 50–70 MPa for 8–12 s. The qualification test is a drop test at -18°C after 48 h conditioning, following ASTM D2463-15 or ASTM D5276-19. The limiting variable is the lower impact energy absorption of the amorphous phase at temperatures near the beta relaxation region of this density class. Failure occurs most often at the sidewall-to-base junction when the corner radius is below 2 mm or when weld lines form around the handle bridge. Chemical resistance of the molded pail is assessed with ASTM D543-21 immersion tests using representative hydrocarbons, acid solutions and detergent concentrates. For food-grade pails, migration limits are identical to other segments under Regulation (EU) No 10/2011; for non-food industrial pails, the relevant requirements are REACH Article 33 notification for candidate list substances and RoHS Directive 2011/65/EU where electronic equipment packaging is involved. The main processing constraint is that excessive nozzle temperatures above 240°C cause low-molecular-weight polyethylene fractions to deposit on mold vent surfaces as waxy residue. This reduces vent efficiency and leads to short shots in the handle bridge when the tool runs longer than 8 h without cleaning.
Heated detergent solutions and oily kitchen residues are the main chemical exposure conditions for small appliance housings molded from HDPE 7260. Parts are produced with wall thickness between 2 mm and 3 mm; thicker sections require cooling time sufficient to avoid sink marks opposite bosses and ribs. The main end-use failure mode is environmental stress cracking at the base of screw bosses when the part remains in contact with dilute nonionic surfactant solutions at 60°C. ESCR is measured by ASTM D1693-15 or ISO 22088-2:2010; a lot is accepted only when the F50 failure time exceeds 20 h at 50°C. In production, the injection nozzle temperature is set at 230–240°C. The mold is kept at 20–30°C because lower temperatures introduce visible flow lines around the gate, while higher temperatures increase cycle time and post-mold shrinkage. Annealing at 80°C for 2 h is required where service temperature exceeds 60°C; without annealing, post-mold shrinkage continues for 48 h and produces opening gaps at snap-fit joints. Copper-based pigment masterbatches should be avoided at melt temperatures above 230°C because copper stearate accelerates thermo-oxidative chain scission. This degradation is detected as an increase in melt flow rate greater than 15 % after 3 extrusion passes under ISO 1133-1:2022 and as surface crazing after 100 h in a 60°C water bath.
In low-cost houseware lines, HDPE 7260 is injection molded into storage boxes, waste bins and bucket bodies. The processing window is wider than for technical components because mechanical loads are lower. Mold temperatures of 10–25°C and melt temperatures of 200–230°C are acceptable. The main control variable is mold shrinkage, measured at 1.5–2.0 % by ISO 294-4:2018. Parts are often pigmented in high-contrast colors; the base resin has narrow molecular weight distribution, so pigment dispersion is adequate with a single-pigment concentrate added at 2–4 wt% through a gravimetric feeder. Warpage of flat lids is controlled by using a central gate and a core temperature differential of 5–10°C. For products intended for outdoor use, UV stabilization is required; standard accelerated weathering following ASTM G154-23 Cycle 1 for 500 h is used to screen formulations, but published data for this specific configuration is limited. The most common production defect is ejection pin push-out on the still-soft bottom when the mold temperature is too high; this is prevented by delaying ejection until the part surface temperature is below 70°C.
Competitive ZPC (Zhejiang Petroleum & Chemical) HDPE 7260 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
ZPC HDPE 7260 is a high-density polyethylene injection-molding grade supplied by Zhejiang Petroleum & Chemical Co., Ltd. in pellet form. The product is a general-purpose ethylene homopolymer with a nominal melt mass-flow rate of 6.0 g/10 min determined at 190 °C under a 2.16 kg load according to ISO 1133-1:2022 and a density of 0.957 g/cm³ determined by ISO 1183-1:2019. The resin is intended for rigid injection-molded articles where short fill times, moderate stiffness, and reliable pellet flow in centralised material-handling systems are primary requirements. It is not an elastomer-modified or high-molecular-weight HDPE; therefore, low-temperature impact strength, environmental stress crack resistance, and melt strength are lower than those of blow-molding and film HDPE classes. Converters should select the grade only when injection-molding economics and ambient-temperature service outweigh those deficiencies.
Table 1. Typical property ranges for the 0.957 g/cm³ and 6.0 g/10 min HDPE injection-molding grade class, not a lot-specific specification.
| Property | Typical range | Test procedure |
|---|---|---|
| Melt mass-flow rate, 190 °C/2.16 kg | 5.5–6.5 g/10 min | ISO 1133-1:2022 |
| Density | 0.956–0.960 g/cm³ | ISO 1183-1:2019 |
| Tensile yield stress | 25–28 MPa | ISO 527-2:2012 |
| Nominal tensile strain at break | >200 % | ISO 527-2:2012 |
| Flexural modulus | 1050–1200 MPa | ISO 178:2019 |
| Charpy notched impact strength, 23 °C | 4.0–6.0 kJ/m² | ISO 179-1:2010 |
| Vicat softening temperature A50 | 124–128 °C | ISO 306:2022 |
| Shore D hardness | 61–63 | ISO 868:2003 |
Values in Table 1 represent the public data envelope for HDPE injection-molding resins of this density and melt-flow class. The lot certificate of analysis governs because impact, modulus, and melt-flow values may vary with sample preparation according to ISO 293 or ISO 294-1. Published data for the specific ZPC 7260 configuration is limited; the higher-melt-flow 0.957 g/cm³ HDPE class typically shows lower notched impact and lower environmental stress crack resistance than 0.35 g/10 min blow-molding HDPE.
On reciprocating-screw injection-molding machines with screw L/D ratios of 20:1 to 25:1 and compression ratios of 2.5:1 to 3.0:1, HDPE 7260 is processed within a melt-temperature corridor of 210 °C to 230 °C. Lower settings near 200 °C may reduce energy use but raise melt viscosity and increase injection pressure demand; settings above 250 °C risk odour generation and yellowing from thermal-oxidative degradation. Mold temperature is typically controlled between 10 °C and 35 °C. For multi-cavity hot-runner tools, the nominal 6.0 g/10 min flow index supports fast cavity filling but also increases the tendency for nozzle drool if valve-pin wear develops; shut-off nozzles or positively closed valve gates are required in high-speed cycles.
Fill pressure typically ranges from 60 MPa to 100 MPa in thin-wall sections of 2.0 mm to 3.0 mm; holding pressure is maintained at 40 MPa to 60 MPa until gate freeze. Back pressure of 0.5 MPa to 1.0 MPa on the screw recovery stroke prevents melt-density fluctuation without excessive shear heating. Clamp force can be estimated from cavity pressure and projected area. For a 2.4 mm wall crate with a projected area of 0.12 m² and an average cavity pressure of 35 MPa, the minimum clamp opening force is 4200 kN; applying a safety factor of 1.15 gives 4830 kN. Published data for this specific ZPC configuration is limited, so tooling trials should validate cavity-pressure mapping before production locks in press size.
Stackable beverage crates and industrial totes represent the highest-volume application class for HDPE 7260. The 6.0 g/10 min melt index reduces filling pressure in multi-drop hot-runner layouts, but shrinkage anisotropy remains the dominant quality defect. Mold shrinkage for 0.957 g/cm³ HDPE injection grades typically lies between 1.5 % and 2.5 % in the flow direction and 1.2 % to 2.0 % transverse to flow when determined after 24 h at 23 °C using plaques produced under ISO 294-4. Post-mold crystallisation continues for 24 h to 48 h; dimensional inspection before that period will overestimate final molded dimensions. Cooling circuits should be arranged with turbulent flow at a Reynolds number above 5000 using water at 10 °C to 20 °C. In multi-cavity crates, gate geometry, not melt temperature, is the usual cause of differential packing and warpage; film gates or large submarine gates with a minimum thickness of 0.8 mm reduce gate-freeze time and allow holding pressure to reach the part before the gate seals.
Table 2. Class-level comparison, not a ZPC grade-specific commercial comparison.
| Attribute | ZPC HDPE 7260 injection grade | General-purpose blow-molding HDPE class | HMW-HDPE film class |
|---|---|---|---|
| MFR, 190 °C/2.16 kg | 5.5–6.5 g/10 min | 0.2–0.8 g/10 min | 0.04–0.2 g/10 min |
| Density | 0.956–0.960 g/cm³ | 0.955–0.958 g/cm³ | 0.949–0.953 g/cm³ |
| Melt strength | lower | higher | high |
| Environmental stress crack resistance | low to moderate | moderate to high | high |
| Core conversion process | injection molding | extrusion blow molding | blown film |
The comparison in Table 2 is class-level rather than grade-specific. HDPE 7260 differs from blow-molding HDPE primarily in its intentionally lower long-chain entanglement and higher melt-flow index, which reduce parison melt strength and render the material unsuitable for extrusion blow molding except in small accumulator-head articles. In contrast to high-molecular-weight film HDPE, HDPE 7260 exhibits lower environmental stress crack resistance and reduced dart impact, but its higher density and modulus provide greater part stiffness after cooling. Against polypropylene homopolymer, HDPE 7260 has lower flexural modulus, lower heat deflection temperature, and lower crystallinity; against linear low-density polyethylene, it has higher density, higher modulus, and inferior puncture resistance under ISO 6603-2.
For caps, overcaps, and industrial closures of wall thickness greater than 2.0 mm and without carbonation pressure, HDPE 7260 can reduce filling time in high-cavitation closure molds compared with lower-flow HDPE. It is not recommended for pressurised carbonated beverage closures because those applications require higher environmental stress crack resistance under ASTM D1693-15 condition B and higher long-term creep resistance. Closures produced from HDPE 7260 should not be exposed to strong oxidising agents or chlorinated solvents above 20 °C. If food-contact status is required, the final closure compound must be assessed under EU Regulation 10/2011 for overall migration not exceeding 10 mg/dm² and under FDA 21 CFR 177.1520 for olefin polymers, subject to grade-specific compliance.
HDPE is not significantly hygroscopic. Drying is unnecessary when pellets are received in sealed containers and exposed to ambient air of less than 60 % relative humidity for fewer than 4 h in hopper loaders. Surface condensation from night-shift temperature swings or high-humidity warehouses above 60 % RH can generate splay and surface defects; in such conditions, drying at 80 °C for 2 h with a desiccant dryer delivering a dew point of -30 °C removes surface moisture. Melt temperature should be raised gradually in 10 °C increments after storage in cold warehouses below 5 °C to prevent condensation on pellet surfaces inside the hopper. The product should be protected from ultraviolet radiation during extended outdoor storage; unshielded storage exceeding 12 months may shift surface rheology through oxidation.
Compliance depends on the compounding package, colorants, and processing aids used with the resin. HDPE 7260 as a virgin ethylene homopolymer can be evaluated against FDA 21 CFR 177.1520 for olefin polymers and EU Regulation 10/2011 for plastic food-contact materials. Overall migration of the finished article should be tested according to EN 1186-series methods with food simulants appropriate to the intended use; a maximum of 10 mg/dm² applies under EU rules. The resin should also be screened against REACH Regulation (EC) No 1907/2006 for substances of very high concern and against RoHS Directive 2011/65/EU for lead, cadmium, mercury, hexavalent chromium, PBB, and PBDE when electrical or electronic housings are produced. Published data for this specific ZPC grade under all food-contact conditions is limited; grade-specific declarations should be requested before commercial packaging use.
Operational boundaries include the absence of intentional UV stabilization in standard HDPE 7260 unless specified in lot documentation. The grade should not be blended with amine-based processing additives that promote discoloration, nor with external lubricants above 0.5 wt % because mold deposit formation and surface haze may increase. Injection molds should be vented at the end-of-fill position with vent depths not exceeding 0.02 mm to prevent flash on high-flow HDPE. If parts require prolonged outdoor exposure above 2 years or continuous hot-water contact above 60 °C, HDPE 7260 is not the appropriate material class; crosslinked polyethylene or UV-stabilized polypropylene should be considered.