| HS Code | 380527 |
| Density | 0.958 g/cm³ |
| Melt Flow Rate | 0.35 g/10 min |
| Tensile Strength At Yield | 26 MPa |
| Tensile Strength At Break | 30 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 1100 MPa |
| Notched Izod Impact Strength | 25 kJ/m² |
| Vicat Softening Temperature | 125 °C |
| Melting Point | 133 °C |
| Environmental Stress Cracking Resistance | >1000 h |
| Hardness | 62 Shore D |
| Crystallinity | 60% |
As an accredited ZPC (Zhejiang Petroleum & Chemical) HDPE 5831D factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | ZPC HDPE 5831D is packaged in 25 kg polyethylene-lined woven bags, palletized, or 1,000 kg jumbo bags for bulk shipment. |
| Container Loading (20′ FCL) | 20′ FCL: typically 25–28 MT ZPC HDPE 5831D in 25 kg bags; lower if palletized, subject to carrier weight limits. |
| Shipping | ZPC (Zhejiang Petroleum & Chemical) HDPE 5831D is a non-hazardous polyethylene resin, typically packed in 25 kg bags or jumbo bags on pallets. Ship in clean, dry containers by sea or road. No UN number or hazard class; keep cool, dry, and away from ignition sources. |
| Storage | Store ZPC (Zhejiang Petroleum & Chemical) HDPE 5831D in a cool, dry, well-ventilated warehouse using original sealed bags or packaging. Keep away from direct sunlight, heat, ignition sources, and strong oxidizers. Prevent moisture, dust, oil, and chemical contamination. Ensure bags remain closed and avoid prolonged outdoor exposure. Stack pallets securely to avoid deformation or collapse. Follow first-in-first-out inventory and good housekeeping. |
| Shelf Life | Stored cool, dry, ventilated, sealed in original packaging away from sunlight, ZPC HDPE 5831D has a 24-month shelf life. |
Extrusion blow moulding of high-density polyethylene containers in the 0.3 g/10 min melt-flow class begins with continuous plastication on a single-station shuttle machine or a two-station rotary wheel. ZPC HDPE 5831D enters the process as pre-dried only when silo storage humidity exceeds 60 % RH or when regrind moisture exceeds 0.1 wt%; otherwise, melt-phase hydrolysis is not the primary degradation mechanism and vented barrels are not required. For 500 mL to 5 L household detergent, fabric softener, and liquid soap bottles, converters run barrel zone setpoints between 160 °C and 220 °C with die head temperatures held between 195 °C and 215 °C. Melt temperature measured at the die entry typically remains between 200 °C and 220 °C to balance parison sag and surface gloss. Blow mould cooling water circulates at 10 °C to 20 °C; mould surfaces below 8 °C can restrict the pinched weld line and raise flash-pin tear-out defects, while mould temperatures above 30 °C slow crystallisation and extend cycle time without proportional ESCR gain. Wall thickness distribution is corrected through ten-point parison programming, with die gap convergence from 1.2 mm at the top section to 0.9 mm in the pinch-off zone for a 1 L bottle weighing 38 g to 45 g. Finished containers are produced under the territorial packaging and labelling requirements of Regulation (EC) No 1272/2008 for the filled product and the packaging waste framework of Directive 94/62/EC; material compliance is checked against REACH Annex XVII and the latest SVHC candidate list. Because HDPE 5831D is not sold as a dedicated food-contact grade unless the lot-specific certificate states compliance with Commission Regulation (EU) No 10/2011, converters should avoid direct food or oral-care applications without migration testing. The terminal parts in this segment are non-food detergent bottles, soap dispensers, and household chemical containers; their lot acceptance tests typically include density by ISO 1183-1, melt-flow rate by ISO 1133-1:2022, and drop impact resistance of the empty bottle at -18 °C by ASTM D2463-15.
For industrial jerrycans and cubitainers in the 10 L to 25 L range, HDPE 5831D is extruded on accumulator-head machines with clamp force usually between 300 kN and 800 kN and shot capacity above 3 kg. The governing specification is the UN Model Regulations for dangerous goods packaging; design-type testing imposes a drop height of 1.2 m for Packing Group II or 1.8 m for Packing Group I, a hydraulic pressure test of 100 kPa for 30 min, and a leakproofness test at 20 kPa internal air pressure for 5 min. Stacking strength is evaluated for 28 days at 40 °C at a load equivalent to 1.8 m of stacking height. These requirements translate into a minimum pinch-off weld thickness at the base and top seams of 1.2 mm to 1.8 mm, with no cold-weld channel visible under 20× optical inspection. The extrusion profile for 20 L jerrycans usually holds barrel zones from 170 °C to 210 °C and a die head at 190 °C to 210 °C; melt temperature below 185 °C raises weld-line notch sensitivity, while operation above 225 °C can induce low-boiling volatiles from recycled post-industrial content and generate pinholes at the pinch-off. Regrind levels in UN-certified packaging are normally limited to 20 wt% to 25 wt% of internal clean flash and tailings, because higher recycled fractions reduce environmental stress-crack resistance under the ASTM D1693 condition B constant-strain test. Masterbatch addition for carbon black or UN orange is capped at 3 wt%, and carrier resins should be HDPE-based so that the 0.958 g/cm³ density class is not shifted below 0.940 g/cm³. Compliance is documented with a batch-specific certificate of analysis covering density, melt-flow rate, tensile yield at 50 mm/min by ISO 527-2, flexural modulus by ISO 178, and notched Izod by ISO 180. Terminal products are UN-marked jerrycans for solvents, lubricant additives, adhesive components, and agrochemical intermediates; the plastic packaging must resist the filled product for 90 days without stress whitening greater than 2 mm penetration at the shoulder weld line.
| Test | Condition | Pass limit | Reference |
|---|---|---|---|
| Drop impact | Packing Group II, 1.2 m, 20 °C | No leakage after impact | UN Model Regulations 6.1.5.3 |
| Leakproofness | 20 kPa internal air pressure, 5 min | No leakage | UN Model Regulations 6.1.5.5 |
| Hydraulic pressure | 100 kPa internal water pressure, 30 min | No leakage or rupture | UN Model Regulations 6.1.5.6 |
| Stacking | 40 °C, 28 days | No rupture or deformation that compromises closure | UN Model Regulations 6.1.5.7 |
Suction blow moulding of automotive under-bonnet reservoirs often selects a medium-molecular-weight HDPE with an MFR below 0.5 g/10 min to maintain parison stability across a 1.2 m vertical drop. HDPE 5831D is processed on three-axis machines with part weights from 350 g to 1.5 kg, where the parison is manipulated into complex shapes and blow air enters through a needle at 0.6 MPa to 0.9 MPa. The main design constraint is cold impact at -30 °C after heat-ageing at 100 °C for 168 h; accepted parts are leak tested at 20 kPa to 30 kPa and subjected to burst pressure of 200 kPa minimum. In washer reservoir production, the melt temperature is maintained between 195 °C and 215 °C, with tool temperature held at 15 °C to 25 °C; ejector pin marks and blow-pin orifices are welded closed by spin welding or hot-plate welding after demoulding. The material must remain compatible with glycol-based and methanol-based washer fluids, which means the converter should run immersion tests at 60 °C for 21 days with the actual fluid mixture and reject parts showing mass change above 1.5 % or volume swell above 2 %. The terminal parts are windshield washer reservoirs, coolant overflow tanks, and auxiliary fluid vessels; the grade is not recommended for pressurised cooling-system components above 90 kPa continuous operating pressure unless hot-plate welded seams are destructively tested for burst failure.
In agricultural chemical packaging, HDPE 5831D is converted on single-layer extrusion blow moulding lines with die gap oscillation at 0.8 mm to 1.5 mm for bottle volumes from 500 mL to 5 L. The governing framework includes the FAO guidelines for pesticide packaging and the same UN design-type tests for liquids in Packing Group III at 0.8 m drop height. Because many pesticide formulations include xylene, cyclohexanone, or n-methyl-2-pyrrolidone as co-solvents, the bottle wall may show environmental stress cracking at the shoulder and base radius within 30 days if those solvents exceed 20 wt% in the liquid formulation; in such cases monolayer HDPE must be verified by 90-day storage tests with the actual formulation, or fluorination or coextruded polyamide barrier layers are introduced. The base resin is compounded with hindered-amine light stabilizers and a carbon black or titanium dioxide masterbatch at 2 wt% to 4 wt% to meet 24-month outdoor storage under direct sunlight; UV resistance is commonly evaluated by ISO 4892-2 accelerated weathering with retention of tensile elongation above 50 %. Extrusion temperatures for pigmented agricultural bottles are held between 190 °C and 220 °C, and the melt is filtered through screen packs of 60 mesh to 80 mesh to remove carbon agglomerates. The terminal products are pesticide bottles, plant growth regulator containers, and foliar fertiliser bottles; they require a production-lot drop test at 0 °C with 95 % fill of the actual formulation, not water, because solvent attack changes the yield stress at the weld line and can misrepresent real-world drop performance.
When twin-sheet thermoforming replaces injection-moulded logistics trays, HDPE 5831D is first extruded through a flat die with width up to 1 200 mm at melt temperatures from 210 °C to 240 °C. The two sheets are transferred to aluminium forming tools maintained at 70 °C to 90 °C, vacuum-formed around spacers, and fused at the perimeter by hot-plate or direct-contact welding under 0.3 MPa to 0.6 MPa clamping pressure. The terminal tray weighs between 2 kg and 8 kg and is used for automotive components, battery modules, or industrial work-in-process transport. Compliance for these applications is not governed by UN dangerous-goods packaging unless the tray contains a leak-tight top shell; however, load-bearing performance is validated by static compression at 23 °C for 24 h by ASTM D642 and dynamic drop at -20 °C with a 50 kg payload by ASTM D2463. The main process conflict is thermoforming temperature versus melt memory: if the sheet surface drops below 165 °C before plug assistance, the hinge points form microcracks; if the tool temperature exceeds 95 °C, the HDPE surface can stick and require excessive release agent. Pinch-off weld strength in twin-sheet edges should exceed 40 N per 25 mm width when tested by ISO 527-3 on cut specimens. HDPE 5831D in this segment competes with HDPE sheet grades that carry a broader molecular weight distribution; the lower MFR improves melt integrity but narrows the maximum draw ratio before webbing occurs on plug-assisted forming lines.
Thick-sheet extrusion from HDPE 5831D is performed on single-screw extruders with L/D ratios of 30:1 to 36:1 and a melt pump to dampen pressure fluctuations below 0.1 MPa; sheet thicknesses between 4 mm and 20 mm are used for chemical storage tank sidewalls, duct sections, and scrubber liners. The melt enters a three-roll stack at 190 °C to 215 °C, and roll temperatures are set at 60 °C, 80 °C, and 70 °C from top to bottom to avoid warpage. Welding is done by hot-gas extrusion welding using HDPE 5831D rod of the same melt classification, with wedge heating at 220 °C to 260 °C and inert-gas shielding when high weld strength is required. The weld tensile strength should meet 80 % of parent material yield when tested by ISO 527-2, and the structure should be subjected to a 24 h water fill test at 23 °C for leaking. The chemical resistance of HDPE in this application depends on the storage liquid: continuous contact with strong oxidizers or chlorinated solvents is outside the recommended service range unless specific immersion data are available. Terminal products include modular chemical storage cells, air pollution control ducting, and secondary containment liners; glass-fibre-reinforced HDPE may be specified for roof spans exceeding 1.2 m.
Post-industrial regrind insertion is a continuous downstream stream for 5831D scrap generated in pinch-off flash, top and tail sections, start-up purge, and off-spec bottles. The clean regrind is granulated to 6 mm to 8 mm flake and blended with virgin resin at 15 wt% to 30 wt% for non-UN containers and below 20 wt% for UN-certified jerrycans. The limit is governed by ESCR loss after multiple heat histories: published data for this specific configuration is limited, but converters usually measure melt-flow rate after each heat history and adjust regrind level if the high-load MFR at 21.6 kg shifts by more than 5 % from the virgin lot value. Converters typically install 80 mesh screen packs in the reclaim stream to remove char and paper fibre contamination; for high-gloss personal care bottles, the recycled stream is limited to 10 wt% and passed through a melt filter at 20 MPa maximum differential pressure. The terminal product of the regrind stream is not a separate public-facing article but a moulding compound that re-enters the blow moulder and must be traceable by batch. In multi-layer articles, regrind is used in the core of a three-layer structure with virgin skin layers at 10 wt% to 15 wt% each side; this configuration is common when the outer surface requires exact colour and the inner surface requires chemical resistance. The operational boundary is clear: if the regrind fraction exceeds 30 wt% and the melt temperature drops below 190 °C, surface pitting on the pinch-off weld increases, and the bottles may fail leakproofness at 20 kPa.
Competitive ZPC (Zhejiang Petroleum & Chemical) HDPE 5831D prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
ZPC (Zhejiang Petroleum & Chemical) HDPE 5831D is a high-density polyethylene pellet grade supplied for blown film conversion in industrial packaging and related rigid-stiffness film applications. The resin is built around a nominal density of 0.958 g/cm³ determined according to ISO 1183-1 and a nominal melt flow rate of 0.30 g/10 min under 2.16 kg load at 190 °C according to ISO 1133-1:2022. Those two values place the grade in the low-melt-flow HDPE film segment, where melt pressure, bubble stability and directional stiffness dominate conversion behaviour. Typical downstream uses include industrial liners, carrier films, overwrap constructions and high-strength bags in thicknesses generally bounded between 15 μm and 100 μm. Film converters verify tensile behaviour according to ISO 527-3, dart impact according to ISO 7765-1 or ASTM D1709, and tear resistance according to ISO 6383-2 or ASTM D1922. Published film property data for this specific grade across every gauge, die gap and blow-up-ratio combination is limited; lot-specific certificates of analysis are the controlling reference.
Differences from other polyethylene grades arise first from density and melt flow rate. A standard LLDPE film resin at 0.918 g/cm³ and MFR 1.0 g/10 min normally runs with lower extruder head pressure and produces higher puncture-energy absorption than an HDPE film of equal thickness. An HDPE blow-moulding resin may sit near the same density but is optimised for high swell and parison hang strength rather than bubble stability and film orientation. The low MFR of HDPE 5831D reduces melt sag and supports high-stalk bubble geometry on suitable blown film lines, but it also increases torque demand and lowers the shear rate at which shark-skin melt fracture appears. The product is not a linear low-density polyethylene and should not be substituted at equal thickness in applications requiring LLDPE-level dart impact unless the converter rebalances stiffness, down-gauging and tear behaviour.
Process records from production-scale lines using grooved-barrel extruders with 25:1 to 30:1 L/D indicate that the resin behaves as a stiff, fast-crystallising high-density polyethylene. Barrel temperatures are held between 180 °C and 210 °C, while adapter and die zones are set from 190 °C to 220 °C. Melt temperature at the die is normally maintained below 230 °C to limit thermo-oxidative gel formation and surface defects. Die gaps between 1.2 mm and 1.8 mm are used with blow-up ratios from 3:1 to 5:1; when internal bubble cooling is active, exchanger air temperature is adjusted to keep the frost line at 3 to 5 die diameters. Higher frost lines destabilise the stalk because the resin crystallises early, while lower frost lines reduce machine-direction orientation and may raise haze. Output is constrained by die shear rate; if transverse ridges appear on the stalk, die temperature should be increased within the allowed range or screw speed reduced by 10% to 15%. Fluoropolymer processing aid masterbatch at 200 ppm to 800 ppm active fluoropolymer can reduce melt fracture, but contaminated screens or damaged screw elements invalidate the aid.
Moisture above 0.05 wt% produces surface pitting and bubble instability. When ambient relative humidity exceeds 60%, the pellets should be dried at 70 °C for 2 h in a desiccant dryer before extrusion. The resin is incompatible with PVC or PET contamination; mixed scrap raises melt viscosity heterogeneity and creates visible gelling, die-lip build-up and thickness variation. Feed-throat plugging is more likely if fines generation is high, so pellet conveying should be checked and dedusted when regrind content exceeds 20%. The grade does not contain an intentionally added slip or antiblock package in base form; converter-added masterbatches are required for controlled slip, blocking resistance or antistatic performance.
Gauge uniformity in HDPE 5831D film is strongly dependent on die lip geometry and air-ring performance. The low melt flow rate reduces bubble self-levelling compared with LLDPE, so even minor die eccentricity produces persistent thick-thin bands. On lines with segmented die lips, thickness variation should be corrected through die bolts rather than by air flow adjustment alone. Beta-gauge feedback and oscillating haul-off are standard on film lines, but the absolute gauge variability is machine-specific; a nominal tolerance of ±6% at 30 μm may be optimised on new equipment, while older flat dies with worn lips can exceed that. No universal winder tension can be specified because layflat width, core diameter and roll hardness differ by line configuration. Blocking risk increases with roll hardness above 30 Shore D on high-density surfaces in warm warehouses.
High-stalk orientation creates anisotropic mechanical response. Machine-direction tensile stress at yield is normally higher than transverse-direction stress at the same gauge, while elongation at break is lower in the machine direction because of preferential chain alignment. Test data should be generated on film specimens according to ISO 527-3, with specimen width, gauge length and crosshead speed reported. Dart impact measured by ISO 7765-1 or ASTM D1709 is directionally lower in HDPE films than in LLDPE films of equivalent thickness because the 0.958 g/cm³ density reduces energy absorption during high-speed puncture. The compensating property is water-vapour resistance. A higher-density crystalline HDPE transmits less water vapour per unit thickness than a lower-density LLDPE when compared under the same humidity gradient; comparative testing is normally performed according to ISO 15106-2 at 38 °C and 90% RH. A direct numerical WVTR for ZPC HDPE 5831D is not assignable without fixing gauge, BUR, frost-line height and film orientation, and published values for the grade across multiple downstream line configurations are limited.
Table 1 lists representative physical and film values for ZPC HDPE 5831D. Film-related values are indicative for a 30 μm film at a nominal blow-up ratio of 4:1; they are not guaranteed specifications for other gauges or line geometries. Base-resin density and melt flow rate are controlled by lot certificate, but film properties must be verified on the converter’s own line.
| Property | Unit | Representative value | Test method |
|---|---|---|---|
| Density | g/cm³ | 0.958 | ISO 1183-1 |
| Melt flow rate, 190 °C / 2.16 kg | g/10 min | 0.30 | ISO 1133-1:2022 |
| Tensile stress at yield, film | MPa | 27 | ISO 527-3 |
| Tensile strain at break, film | % | 650 | ISO 527-3 |
| Elmendorf tear resistance, MD | N | 18 | ISO 6383-2 |
| Dart impact, Type A | g | 120 | ISO 7765-1 |
The same dependence on processing geometry applies to tear resistance and dart impact. A lower frost line reduces machine-direction orientation and may raise dart impact at the cost of machine-direction tensile yield. A higher blow-up ratio increases transverse-direction orientation and may reduce dart impact further. Because the resin crystallises quickly, air-ring temperature and frost-line position influence haze, gloss and blocking more strongly than screw speed within the normal operating window. Processors converting the grade on long-stalk lines report that stable stalk length is the principal control variable for balancing these properties; published data for the specific grade under vacuum-box or internal bubble cooling is limited.
In stiffness-controlled industrial liners, replacement of an LLDPE-rich formulation with ZPC HDPE 5831D typically increases tensile yield stress and tensile modulus, which can permit thickness reduction when stiffness is the controlling failure mode. The conversion is not direct for high-puncture service. In waste-collection and construction films, LLDPE grades provide higher dart impact and tear energy absorption at equal thickness. If the switch is made, minimum film thickness should be confirmed by ISO 7765-1 dart drop and ISO 6383-2 tear testing before down-gauging. The lower melt flow rate of HDPE 5831D may require higher barrel and die settings than LLDPE; machines with 20:1 L/D general-purpose screws may not develop adequate melt pressure. Grooved-barrel extruders with 25:1 to 30:1 L/D are preferred. Gusset-section and weld-line performance should be checked by ISO 527-3 because HDPE can show lower transverse-direction elongation than LLDPE at the same frost-line height. Production-line trials report that stiffness-limited structures can sometimes be down-gauged by 20%, but this is not a transferable design limit; each film structure, gauge and destination must be tested on the actual line.
Class-level comparison between HDPE 5831D, LLDPE film resins and HDPE blow-moulding grades appears in Table 2. The table is intended for material selection only; it does not replace lot-specific certificates or downstream film testing.
| Attribute | ZPC HDPE 5831D film | LLDPE film class | HDPE blow-moulding class |
|---|---|---|---|
| Density, ISO 1183-1 | 0.958 g/cm³ | 0.918–0.925 g/cm³ | 0.952–0.960 g/cm³ |
| MFR, ISO 1133-1:2022 | 0.30 g/10 min | 0.8–1.2 g/10 min | 0.25–0.40 g/10 min |
| Primary conversion route | blown film | blown or cast film | extrusion blow moulding |
| Tensile modulus at equal gauge | high | low to medium | not applicable to film |
| Dart impact at equal gauge | lower than LLDPE | higher | not applicable to film |
| Water-vapour transmission at equal thickness | lower than LLDPE | higher | not applicable to film |
Food-contact suitability, heavy-metal compliance and storage stability are lot-specific matters. Polyethylene grades sold for industrial film may carry REACH and RoHS conformity for heavy metals, but food-contact documentation under FDA 21 CFR 177.1520 or EU 10/2011 must be obtained from the supplier’s product stewardship records for the specific lot. The base resin is not supplied with an intentionally added slip or antiblock package; additive loading is controlled by the converter. Storage beyond 6 months from production may increase oxidation risk if bags are opened in warm environments. Oxidation resistance of the finished film should be assessed by ISO 4577 or equivalent when film is intended for hot environments above 80 °C. The product is not recommended for continuous-use service above that temperature unless stabilisation is verified under the end-use oxidative environment.