| HS Code | 415391 |
| Product | ZPC HDPE 5502S |
| Manufacturer | Zhejiang Petroleum & Chemical (ZPC) |
| Polymer Type | High Density Polyethylene |
| Density | 0.955 g/cm³ |
| Melt Flow Rate | 0.35 g/10 min (190°C/2.16 kg) |
| Melting Point | 133 °C |
| Vicat Softening Temperature | 125 °C |
| Tensile Strength At Yield | 26 MPa |
| Elongation At Break | ≥600% |
| Flexural Modulus | 1100 MPa |
| Shore D Hardness | 60 |
| Environmental Stress Cracking Resistance | >1000 h |
| Brittleness Temperature | ≤ -70 °C |
| Water Absorption | <0.01% |
| Thermal Conductivity | 0.4 W/m·K |
| Crystallinity | 70–80% |
As an accredited ZPC (Zhejiang Petroleum & Chemical) HDPE 5502S factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | ZPC HDPE 5502S typically ships in 25 kg PP woven bags, palletized, or 1,000 kg jumbo bags. |
| Container Loading (20′ FCL) | 20′ FCL container loading of ZPC (Zhejiang Petroleum & Chemical) HDPE 5502S: 25kg bags, palletized, shrink-wrapped, securely stowed for export. |
| Shipping | ZPC (Zhejiang Petroleum & Chemical) HDPE 5502S is a non-hazardous thermoplastic resin, typically shipped in 25 kg PP woven bags or jumbo bags on pallets. It transports by truck, rail, or sea in dry containers, requiring cool, dry, ventilated storage away from sunlight, heat, and ignition sources. |
| Storage | Store ZPC (Zhejiang Petroleum & Chemical) HDPE 5502S in a cool, dry, well-ventilated warehouse at ambient temperature. Keep in original sealed bags on pallets, away from direct sunlight, UV radiation, heat, ignition sources, and moisture. Prevent contamination with dust, oils, or strong oxidizers. Avoid excessive stacking and bag damage. Use first-in-first-out stock rotation and follow the supplier’s SDS. |
| Shelf Life | ZPC HDPE 5502S typically has a 24-month shelf life when stored cool, dry, ventilated, in original unopened packaging away from sunlight. |
Chemical intermediates and cleaning-agent concentrates shipped in UN-certified jerrycans impose a more severe environmental stress-cracking load than most blow-moulded packaging because the packaged substances include nonylphenol ethoxylates, quaternary ammonium compounds, and hydrocarbon-based solvents at concentrations that can swell the amorphous tie-molecule population of the HDPE wall. Converters running ZPC HDPE 5502S in this segment typically use single-layer continuous extrusion blow-moulding machines with a screw L/D ratio of 24:1 to 30:1, a grooved feed section, and a barrier screw equipped with a Maddock mixing section; parison weight is programmed to concentrate material in the handle pinch-off and the top chime area. The formulation add-on is limited: 2.0 wt% to 3.5 wt% of a compounded carbon black or UV masterbatch, 0.05 wt% to 0.15 wt% total hindered phenolic antioxidant plus phosphite processing stabilizer, and up to 25 wt% clean in-house regrind that has passed residual moisture below 300 ppm. Compliance for the finished article is set by ADR/RID/IMDG transport regulations through UN Model Regulations Chapter 6.1 for jerricans of design type 3H1, with stack-load verification using ISO 12048 or ASTM D642, drop testing at -18 °C per ISO 2248, and leakproofness at 30 kPa for 5 min after closure. The converted objects are tight-head jerrycans and open-top pails from 5 L to 20 L, with nominal wall thickness 1.8 mm to 2.4 mm and a finished weight of 330 g to 650 g depending on handle geometry.
| Test | Standard | Typical condition | Acceptance criterion |
|---|---|---|---|
| Stack load | ISO 12048 / ASTM D642 | 40 °C, 28 days | No buckling or leakage at required stack height |
| Drop impact | ISO 2248 | -18 °C, 6 drops | No rupture or contents leak |
| Leakproofness | UN Model Regulations Chapter 6.1 | 30 kPa, 5 min | No leakage at closure or pinch-off seams |
On single-layer lines, the main failure mode is wall-thickness asymmetry in the handle region, caused by parison sag when drop time exceeds 4 s on large shot weights. Converters address this by setting die gap between 4 mm and 8 mm and programming a 10% to 20% thicker parison segment near the handle pinch-off. Batch-to-batch variance in melt-flow rate of the base resin is controlled within ±0.03 g/10 min by the resin supplier’s lot certification; sudden shifts in extruder melt pressure at constant screw speed typically indicate regrind particle-size segregation and are corrected by adjusting the virgin/regrind gravimetric feeder ratio. Hopper drying at 70 °C for 1.5 h to 2 h is applied only when stored regrind exceeds 300 ppm moisture.
The limiting processing variable in continuous-extrusion blow moulding of large tight-head drums is the pinch-off weld line formed when the mould closes on the parison. A cooled mould below 15 °C quenches the weld before interdiffusion of chain segments completes, leaving a brittle plane that fails at top-load values 20% to 30% below the sidewall compressive strength. Converters supplying this segment set clamp closure speed below 350 mm/s and use internal parison cooling at 0.4 MPa to 0.6 MPa air pressure to solidify the inner wall without collapsing the molten web. The add-on formulation includes 2.0 wt% to 2.5 wt% carbon black masterbatch, 0.08 wt% to 0.12 wt% phenolic antioxidant, 0.05 wt% to 0.08 wt% calcium stearate acid scavenger, and ≤30 wt% regrind from trimmed pinch-off flash. UN design type 1H1 drums require top-load testing under ISO 12048; the stack height is calculated from the specific gravity of the filled product and nominal 1.9 mm to 2.6 mm wall thickness. End articles are 20 L to 60 L tight-head drums with two bungs and chime reinforcement, produced at unit weights of 1.4 kg to 2.8 kg.
In household detergent and personal-care packaging, the conversion window is governed by cost per finished bottle and by the need to accept high levels of post-consumer recyclate without visible gel defects. ZPC HDPE 5502S is blended with 2.0 wt% to 4.0 wt% colour masterbatch and 20 wt% to 30 wt% melt-filtered PCR HDPE, the PCR fraction being screened through a 120 µm filter to remove crosslinked HDPE gels. Compliance obligations under REACH Regulation (EC) No 1907/2006 and CLP Regulation (EC) No 1272/2008 apply to the packaged mixture, while ISO 8317 child-resistant closure testing is required when trigger-sprayer closures are paired with classified liquid formulas. Production proceeds on shuttle blow-moulding machines with 50 mm to 80 mm extruder diameter, automated article removal, and in-line leak testing at 3 kPa to 5 kPa internal pressure. Terminal forms are 250 mL to 5 L trigger-spray bottles, pump bottles, and handled containers for household and personal-care products.
During three-dimensional blow moulding of automotive windshield washer reservoirs and auxiliary fluid containers, the dominant technical risk is cold-impact brittleness after methanol-water exposure and vibration-induced fatigue at mounting bosses. ZPC HDPE 5502S is processed with 1.0 wt% to 2.0 wt% carbon black masterbatch for UV and oxidative protection, 0.2 wt% to 0.5 wt% hindered amine light stabilizer, 0.05 wt% to 0.1 wt% antioxidant, and no more than 15 wt% in-house regrind; higher regrind fractions reduce cold-impact Izod values and increase brittle failure at attached tank bosses. Pre-drying at 80 °C for 2 h is applied when warehouse RH exceeds 60%. The dominant process is three-dimensional blow moulding with a movable die or robotic parison placement, enabling the curved tank geometry without excessive pinch-off tail flash. Blow pressure is set at 0.6 MPa to 0.8 MPa, mould temperature is held at 15 °C to 40 °C, and cycle time is controlled by post-cooling fixtures. Validation is performed against ISO 527-2:2012, ISO 1183-1:2019, and ISO 180 Charpy or ASTM D256 Izod at -40 °C, with OEM-specific pressure cycling between 0.2 bar and 1.4 bar for 10,000 cycles; materials must also comply with REACH Regulation (EC) No 1907/2006 and the heavy-metal restrictions of the EU End-of-Life Vehicles Directive 2000/53/EC. The terminal parts are windshield washer reservoirs of 2 L to 5 L, headlamp washer reservoirs, and auxiliary low-temperature fluid containers with hot-wire insert fittings.
The fluorination step for solvent-based agrochemical containers introduces a surface reaction that replaces a fraction of surface C–H bonds with C–F, retarding permeation of aromatic solvents and halogenated hydrocarbons through the HDPE wall. ZPC HDPE 5502S is fluorinated after blow moulding; the base-wall addition includes 1.0 wt% to 2.0 wt% carbon black UV masterbatch and ≤10 wt% regrind, because higher regrind can create surface defects that reduce barrier uniformity. Converters in this segment run single-station blow moulding with post-mould treatment chambers, then conduct barrier verification by ASTM D3985 oxygen transmission rate or by weight-loss immersion in toluene/heptane surrogate mixtures under ISO 175. Compliance is defined by UN Model Regulations Chapter 6.1, design type 3H1 for dangerous goods jerricans, and in the United States by FIFRA 40 CFR Part 165 container design and residue-removal requirements. The terminal articles are 1 L to 20 L fluorinated HDPE bottles and jerrycans for agricultural emulsifiable concentrates, solvent-based wood preservatives, and aggressive hydrocarbon cleaning compounds. Published data for the fluorination gradient in this specific ZPC grade remains limited; converters therefore validate barrier performance article-by-article through destructive sectioning and permeation coupons.
For pharmaceutical bottle conversion, the risk shifts from mechanical failure to leachable and extractable control under United States Pharmacopeia 661.1, FDA 21 CFR 177.1520(b) for olefin polymers, and EU Regulation (EU) No 10/2011 Annex I where the finished bottle is placed on the EU food-contact or nutraceutical market. ZPC HDPE 5502S is processed without in-house regrind and with 0.5 wt% to 2.0 wt% titanium dioxide masterbatch for light-sensitive formulations; no slip, antistatic, or amine-containing additive masterbatch is introduced because these can migrate or react during sterilisation. The blow-moulding line is typically operated in a positive-pressure cleanroom with HEPA-filtered parison air, stainless steel contact surfaces, and automated trim removal to avoid particulate contamination. Process temperatures are held at the lower end of the HDPE window—melt 180 °C to 205 °C, die head 190 °C to 210 °C—to minimise oxidative degradation products. Bottles are leak-tested at 5 kPa and sampled for USP 661.1 physicochemical safety requirements and, when necessary, extractables screening according to USP 1663. Terminal forms are 60 mL to 500 mL square or cylindrical bottles with 38 mm to 53 mm neck finishes for child-resistant caps and tamper-evident seals.
| Requirement | Standard/Regulation | Condition applied to finished bottle |
|---|---|---|
| Olefin polymer for food contact | FDA 21 CFR 177.1520(b) | Finished article extraction verification required; resin compliance alone is not sufficient |
| Plastic packaging system safety | USP 661.1 | Physicochemical tests on plastic packaging for oral dosage |
| EU plastic food-contact articles | Regulation (EU) No 10/2011, Annex I | Overall migration limit 10 mg/dm² unless modified by simulant testing |
Competitive ZPC (Zhejiang Petroleum & Chemical) HDPE 5502S prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
ZPC HDPE 5502S is a pelletized high-density polyethylene produced by Zhejiang Petroleum & Chemical Co., Ltd. for extrusion blow molding of small-to-medium rigid containers. The published technical data sheet reports a melt flow index of 0.35 g/10 min at 190 °C under 2.16 kg load in accordance with ISO 1133-1:2022, and a density of 0.955 g/cm³ determined by ISO 1183-1:2019. Applications for this grade include 5 L to 60 L industrial packaging, detergent and agrochemical jerry cans, automotive washer-fluid reservoirs, and outer layers of multilayer barrier bottles. The resin is differentiated from high-flow injection molding HDPE by its low melt flow index, which restricts shear-induced flow but preserves parison hang strength; it differs from lower-density blow molding grades in higher flexural modulus and top-load capacity at equivalent wall thickness. Because the grade is designed for extrusion blow molding, it is not specified for thin-wall injection molding, cast film, or filament extrusion unless melt temperature and die pressure are verified on pilot-scale equipment.
The primary process variables on continuous shuttle or reciprocating screw blow molding lines are melt temperature, die temperature, parison programming, and blow pressure. Production-scale reports for medium-molecular-weight HDPE describe single-screw extruders with L/D 24:1 to 30:1 and a barrier screw compression ratio of 2.5:1 to 3.0:1. Barrel zone set points are typically 180 °C, 200 °C, 210 °C, 215 °C, with die-head zones at 200 °C to 210 °C. Melt temperature at the die entry should be held between 190 °C and 220 °C. Operation below 175 °C increases the viscosity of the high-molecular-weight fraction and can exceed the continuous head-pressure alarm of 35 MPa specified on some extruder control cabinets, leading to melt fracture at the die lip and rough parison surface. Operation above 225 °C accelerates thermo-oxidative chain scission, lowers melt strength, and produces vertical sag in parisons longer than 500 mm. The die gap for a 20 L round container is generally set between 0.8 mm and 1.2 mm; parison programming at 30% to 50% of maximum wall thickness is applied in pinch-off zones. Blow air pressure is typically 0.6 MPa to 0.8 MPa, with mold cooling water at 8 °C to 15 °C to keep cycle time below 60 s for a 20 L container. These boundaries are equipment-class values reported in processing bulletins for medium-molecular-weight HDPE; they must be qualified on the actual extrusion blow molding machine because screw wear, clamp force, and die-head geometry shift the operating envelope.
Melt fracture and parison roughness on 5502S can be diagnosed by raising the die-lip temperature in 5 °C increments or reducing output by 5%. If surface roughness persists, the die gap may be too small or the die land length too short. A die land ratio of 10:1 to 15:1 is specified in blow molding die design bulletins for medium-molecular-weight HDPE to allow stress relaxation before exit. Insufficient die land generates sharkskin at output rates below the rated capacity of the line. Because 5502S has moderate die swell, the die gap must be sized smaller than the intended parison thickness; the swell ratio typically ranges from 1.3:1 to 1.6:1, but the exact value depends on die temperature, shear rate, and parison length.
Screw and head selection also affect lot-to-lot process stability. Screws with excessive wear below 0.5 mm clearance in the feed section increase melt temperature variability and reduce output. Extruder drive power on 65 mm lines typically operates at 60% to 80% of motor capacity; sustained operation above 85% indicates either incorrect screw geometry or insufficient feed-throat cooling. Melt pumps are not typically used on shuttle blow molders because parison consistency relies on head pressure rather than gear-pump flow control; if a melt pump is installed, differential pressure below 5 MPa is recommended to prevent excess shear heating.
Resin handling imposes a moisture ceiling. Although HDPE does not require routine predrying, pellets stored in unheated silos above 60% RH can adsorb surface moisture, causing splay or bubbles in the parison at die temperatures above 200 °C. Dry-air hopper drying at 80 °C for 1 h to 2 h with a dew point below -40 °C is recommended when surface moisture is suspected. Regrind use above 30 wt% should be validated for ESCR retention and parison surface quality because repeated extrusion heat history reduces the higher-molecular-weight tail and increases low-molecular-weight species.
The following table consolidates typical properties shown on the manufacturer’s technical data sheet and certificates of analysis.
| Property | Test method | Typical value |
|---|---|---|
| Melt flow index at 190 °C/2.16 kg | ISO 1133-1:2022 | 0.35 g/10 min |
| Density | ISO 1183-1:2019 | 0.955 g/cm³ |
| Tensile stress at yield | ISO 527-2:2012 | 28 MPa |
| Tensile strain at break | ISO 527-2:2012 | >600% |
| Flexural modulus | ISO 178:2019 | 1300 MPa |
| Charpy notched impact strength at 23 °C | ISO 179-1:2020 | 12 kJ/m² |
| Vicat softening temperature A50 | ISO 306:2022 | 126 °C |
| Environmental stress-cracking resistance F50, 100% Igepal CO-630 | ASTM D1693-15 | >600 h |
| Hardness Shore D | ISO 868:2003 | 63 |
These values are lot-averaged typical values, not specification limits. ESCR values are strongly geometry-sensitive, and acceptance for critical packaging should be based on certificate-of-analysis values and not on nominal table entries.
At a molecular level, the performance of 5502S is governed by short-chain branch distribution from alpha-olefin comonomer and by the breadth of the molar mass distribution. The high-molecular-weight fraction contributes to melt strength and ESCR, while the low-molecular-weight fraction controls flow and surface gloss. The density of 0.955 g/cm³ places the grade in the upper quartile of HDPE used for chemical packaging, where permeation resistance and top-load stiffness are measurable through ASTM D638-14 tensile yield and ISO 178:2019 flexural modulus. In accelerated stress-cracking screening under ASTM D1693-15, an F50 time above 600 h in 100% Igepal CO-630 indicates resistance to detergent and oxidative stress-cracking media, but the test is geometry-sensitive. Notched constant-strain methods such as ASTM D5397-20 may be specified for lot-release verification in critical chemical packaging. Published data for this specific configuration is limited outside the standard datasheet values.
ESCR in HDPE is controlled primarily by tie-molecule concentration rather than by average molecular weight alone. Slower cooling of the blow-molded part increases crystallite size and can reduce ESCR even if the resin passes pellet screening. For 5502S, mold cooling water below 10 °C limits crystallite development at the inner surface; however, overcooling the outer surface increases residual stress. The balance is visible in axial top-load testing of containers cooled at 8 °C versus 20 °C mold temperatures, where lower mold temperature improves cycle time but may raise notch sensitivity at the pinch-off.
Permeation resistance to aliphatic solvents in HDPE is governed by density and crystallinity. At 0.955 g/cm³, 5502S has lower weight gain in ASTM D543-21 immersion tests than low-density polyethylene, but it is not a barrier replacement for fluorinated HDPE or multilayer EVOH containers. For aggressive solvents, container design and closure interaction dominate the loss rate; standard resin density alone is insufficient for barrier qualification.
Reformulation from a higher-density chromium-catalyzed HDPE to 5502S requires adjustment of die gap, part weight, and top-load acceptance. Chromium-catalyzed resins often exhibit lower die swell and smoother surface at high shear rates; 5502S may produce higher die swell from its molecular architecture. The operator must widen the die gap or adjust parison programming to avoid over-thick walls at pinch-off. Top-load performance can be maintained by increasing actual part weight by 2% to 5% or modifying chime geometry, because the lower density of 5502S relative to 0.960 g/cm³ grades reduces tensile yield by approximately 1 MPa to 2 MPa. The compensating benefit is higher ESCR, which is the usual reason for switching in detergent and agrochemical containers. In production trials on a shuttle blow molder producing 20 L jerry cans, a 5 mm increase in die gap and a 3% increase in part weight restored an axial top-load requirement of 2.5 kN measured at 10 mm/min without exceeding the cycle-time envelope. These comparative observations derive from industrial blow molding reliability reports for similar HDPE grades; the actual adjustment set must be confirmed for the specific mold and available clamp force.
Compared with a high-flow HDPE injection molding grade having an MFR of 20 g/10 min, 5502S has high viscosity at injection shear rates from 100 s⁻¹ to 1000 s⁻¹. This limits use in multi-cavity molds with wall thickness below 2 mm unless elevated melt temperatures are used, which degrades ESCR and color. The product is therefore constrained to extrusion blow molding and should not be blended with high-flow HDPE without first validating melt-strength loss through a parison hang-time test, such as a 200 mm pinched parison measurement at 190 °C.
Without carbon black or UV stabilizer, the natural grade is not intended for permanent outdoor exposure. Concentrates added at 2 wt% to 4 wt% can improve weathering resistance for agricultural tanks, but the base resin selection alone does not meet ASTM D2565-23 environmental weathering requirements for long-term exterior service.
A compliance assessment of ZPC HDPE 5502S against food-contact and industrial chemical requirements must consider final article surface-to-volume ratio, storage temperature, and simulant exposure. The resin is a polyolefin covered under FDA 21 CFR 177.1520(c) if the finished article meets extractive and end-use limitations. For European Union food-contact applications, migration testing per EU 10/2011 is required on the blow-molded container; overall migration must not exceed 10 mg/dm² for general food contact. The grade is supplied with a REACH declaration under Regulation (EC) No 1907/2006 stating that Candidate List substances of very high concern are below 0.1 wt%. Under RoHS Directive 2011/65/EU, homogeneous material is assessed by IEC 62321-5:2013 for lead, IEC 62321-4:2013 for mercury, and IEC 62321-6:2015 for hexavalent chromium; measured values are below the 0.1 wt% threshold in electrical and electronic equipment enclosures when additives are not deliberately introduced.
| Regulatory requirement | Standard or clause | Assessment basis |
|---|---|---|
| US food contact | FDA 21 CFR 177.1520(c) | Olefin polymer clearance; final article end-use test required |
| EU food contact | EU 10/2011 | Overall migration <10 mg/dm²; finished article validation |
| REACH SVHC | Regulation (EC) No 1907/2006 | Candidate List substance concentration <0.1 wt% |
| RoHS restrictions | IEC 62321-5:2013, IEC 62321-4:2013, IEC 62321-6:2015 | Restricted elements <0.1 wt% in homogeneous material |