| HS Code | 251234 |
| Productname | Zhongtian Hechuang LLDPE 35B |
| Polymertype | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene-1 |
| Physicalform | Pellets |
| Color | Natural |
| Density | 0.925 g/cm³ |
| Meltflowrate | 35 g/10 min (190°C/2.16 kg) |
| Tensileyieldstrength | ≥8 MPa |
| Tensilestrengthatbreak | ≥10 MPa |
| Elongationatbreak | ≥100% |
| Vicatsofteningtemperature | ≥85°C |
| Brittlenesstemperature | ≤-70°C |
| Meltingpoint | 120-125°C |
| Hardness | Shore D 50-55 |
| Waterabsorption | <0.01% |
| Dielectricconstant | 2.3 (1 MHz) |
| Volumeresistivity | ≥1×10^16 Ω·cm |
| Ashcontent | ≤0.03% |
| Moisturecontent | ≤0.1% |
As an accredited Zhongtian Hechuang LLDPE 35B factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Zhongtian Hechuang LLDPE 35B is packaged in 25 kg bags or 1,000 kg jumbo bags for bulk handling. |
| Container Loading (20′ FCL) | Zhongtian Hechuang LLDPE 35B is supplied in 25 kg bags, typically loading about 28 MT per 20′ FCL container. |
| Shipping | Zhongtian Hechuang LLDPE 35B is usually shipped in 25 kg woven bags or 500–1000 kg jumbo bags, palletized and stretch-wrapped. Transport in clean, dry containers or trucks. Store in a cool, dry, ventilated place, away from direct sunlight, heat, moisture, and sharp objects. Handle carefully to prevent package damage and contamination. |
| Storage | Store Zhongtian Hechuang LLDPE 35B in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and open flames. Keep original packaging tightly closed, palletized off the floor, and protected from moisture, dust, oils, and other contaminants. Avoid prolonged UV exposure. Maintain clean handling areas and follow the manufacturer’s safety data sheet for detailed precautions. |
| Shelf Life | Store cool, dry, ventilated, away from direct sunlight; typical shelf life is 12 months from manufacture in unopened original packaging. |
In three-layer blown film structures used for frozen food pouches and form-fill-seal overwrap, Zhongtian Hechuang LLDPE 35B is typically introduced into the sealant layer at 20–35 wt% of total sealant formulation, with the balance comprising LDPE or metallocene LLDPE selected to maintain bubble stability and seal-through-contamination performance. The grade is processed on grooved-feed extruders with 25:1–30:1 L/D ratios, screw diameters of 60–90 mm, die gaps of 1.8–2.4 mm, blow-up ratios of 2.0–2.7, and melt temperatures of 190–210 °C. Pellets with surface moisture above 0.05 wt% should be pre-dried at 70–80 °C for 2–4 h before processing; otherwise bubble instability and microvoids can occur. Seal initiation temperature is evaluated under ASTM F1921-18, tensile properties under ISO 527-2:2021, dart impact under ISO 7765-1:2015 or ASTM D1709-22, and hot-tack strength under ASTM F1921-18 as applicable. Food-contact compliance for olefin polymers is referenced to FDA 21 CFR 177.1520 and Commission Regulation (EU) No 10/2011 Annex I, with overall migration below 10 mg/dm² for the olefin polymer fraction. Finished product types include frozen vegetable pouches, bakery bread bags, liquid liner bags, and horizontal form-fill-seal side-weld packs where low seal initiation and broadened hot-tack behaviour reduce missed-seal frequency at line speeds above 40 m/min.
On five-layer cast stretch film lines with working widths of 1,600–2,500 mm and throughput demands between 700–1,200 kg/h, LLDPE 35B is metered into the core and sub-skin layers at 65–85 wt% of total film, while the skin layers receive polyisobutylene tackifier at 0.5–2.0 wt% to adjust cling. The extrusion temperature profile from hopper to die is typically maintained between 230–275 °C; the melt curtain is quenched on a 600–1,200 mm diameter chill roll at 18–24 °C, with an air gap of 60–120 mm. Physical properties are quantified under ASTM D5458-13 for cling, ASTM D5748-19 for puncture resistance, ISO 527-2:2021 for tensile elongation at break, and ASTM D1894 for coefficient of friction. Regulatory conformity relies on REACH Annex XVII restrictions and Directive 2011/65/EU RoHS heavy-metal limits for non-food industrial films; where food-contact stretch is required, the film must separately satisfy EU No 10/2011 and FDA 21 CFR 177.1520. Terminal articles include machine pallet wrap, hand pallet wrap, pre-stretched film at 200–300% pre-stretch ratios, and industrial bundling films, with edge trim and film scrap recycled into the core at up to 15 wt% where optical haze is not critical.
Greenhouse and mulch film compounds built around LLDPE 35B commonly use a base resin content of 78–88 wt%, with 10–20 wt% LDPE introduced to increase bubble stability during extrusion, and additive loadings of 0.10–0.25 wt% phenolic antioxidant, 0.20–0.50 wt% hindered amine light stabilizer, 0.10–0.30 wt% UV absorber, and 0.5–1.5 wt% anti-drip concentrate. The compound is processed on mono-layer or three-layer blown film lines with die diameters of 350–600 mm, die gaps of 1.8–2.4 mm, blow-up ratios of 2.0–3.0, and melt temperatures of 190–215 °C; frost-line height is maintained between 500–800 mm to balance machine-direction and transverse-direction tear orientation. Weathering resistance is tested under ISO 4892-2:2013 for artificial UV exposure and rated by retained tensile elongation under ISO 527-2:2021, while greenhouse film durability claims reference EN 13206:2017. Black mulch film incorporates carbon black masterbatch at 2.0–3.5 wt% and is assessed for opacity at 150–250 µm thickness. Sulphur-containing pesticide exposure can deactivate hindered amine stabilizers, so films destined for sulphur-fumigated greenhouses require stabilizer package reformulation rather than increased loading alone. Finished product categories include anti-drip greenhouse covers, low tunnel films, silage sheets, and black/white coextruded mulching films.
Where polypropylene homopolymer food containers exhibit stress-whitening and notch sensitivity in cold-chain distribution, LLDPE 35B is compounded at 8–20 wt% into the PP matrix using a co-rotating twin-screw extruder with 40:1 L/D ratio, 10–12 barrel zones, and screw speeds of 350–600 rpm; the melt is strand-pelletized after vacuum devolatilization at -0.08 MPa or lower to remove low-volatile contaminants. Injection moulding is performed with barrel temperatures of 190–230 °C, nozzle temperature 200–230 °C, mould temperatures of 15–30 °C, injection pressures of 60–100 MPa, and hold pressures of 40–70 MPa. Impact performance is measured under ISO 180:2023 Charpy notched and ASTM D256-23 Izod notched; tensile modulus and yield stress under ISO 527-2:2021; and melt volume-flow rate under ISO 1133-1:2022. Because LLDPE lowers flexural modulus more than ethylene-propylene copolymer modifiers, the addition rate is limited to 20 wt% where top-load stiffness is specified. Conformity for food-contact thin-wall packaging is established under FDA 21 CFR 177.1520 and EU No 10/2011, with overall migration below 10 mg/dm² under EN 1186-1:2002 and specific migration testing under EN 1186-13:2002. Terminal moulded articles include thin-wall dairy packaging, freezer-safe food containers, and textured lids where the seal surface requires non-tearing removal after conditioning at -20 °C.
Compounding low-smoke zero-halogen cable jackets with LLDPE 35B requires addition rates of 10–25 wt% of total compound to improve environmental stress crack resistance and filler wetting when aluminium trihydrate loadings reach 55–65 wt%. Compounding is executed on a co-rotating twin-screw extruder with 44:1 L/D and liquid injection ports; barrel temperatures are limited to 150–180 °C to avoid premature release of flame-retardant water of hydration, and the melt is screened through 80–120 mesh breaker plates before underwater pelletizing. Jacket extrusion onto copper or aluminium conductors uses a crosshead die temperature of 150–180 °C, screw speed adjusted for 50–400 m/min line speed, and a water trough temperature of 40–60 °C to reduce internal stress. Peroxide crosslinking is not recommended for this compound class because the coexisting metal hydroxide fillers and LLDPE phases produce uneven gel fraction unless a dedicated XLPE carrier is used; gel content should be verified via ASTM D2765-16 extraction before running crosslinked specifications. Finished jacket tests include tensile elongation at break under IEC 60811-501:2012, acid gas evolution under IEC 60754-1:2011, smoke density under IEC 61034-2:2019, and vertical flame propagation under IEC 60332-1-2:2015; RoHS compliance is assessed under Directive 2011/65/EU. Terminal product types include LSZH sheathing for control cables, optical fibre distribution cable jackets, and industrial instrumentation cables where 70 °C continuous conductor temperature is the design limit.
Geomembrane liners produced with LLDPE 35B as the primary polyolefin typically use 85–94 wt% base resin, 2.0–3.5 wt% carbon black masterbatch with average primary particle size below 50 nm, and 0.2–0.5 wt% antioxidant/processing stabilizer; the compound is mixed in a gravimetric batch blender and fed to a single-screw flat-die extruder with 30:1–34:1 L/D, die width 2,000–4,000 mm, melt temperatures of 200–230 °C, and polished chill rolls at 60–90 °C. Sheet thickness is controlled within 0.75–2.00 mm using a traversing beta gauge, and surface defects are monitored by camera systems at line speeds of 3–10 m/min. Durability is measured under ASTM D638-14 for tensile break properties, ASTM D4833-07 for puncture resistance, ASTM D5397-20 for single-point notched constant tensile load stress crack resistance, and ASTM D3895-19 for oxidative induction time by differential scanning calorimetry. Published OIT values for this specific grade under site-specific leachate conditions are limited; therefore long-term design requires site-specific accelerated ageing rather than reliance on unstressed laboratory OIT alone. Regulatory conformance for landfill and water containment applications references EN 13493:2018, with carbon black dispersion assessed under ISO 18553:2018 and density under ASTM D1505-18. Terminal geomembrane products include landfill base liners, heap-leach pad liners, evaporation pond liners, and secondary containment panels where seam peel and shear tests are specified under ASTM D6392-12.
Competitive Zhongtian Hechuang LLDPE 35B prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Zhongtian Hechuang LLDPE 35B is supplied as a pelletized linear low-density polyethylene film resin. The grade is classified in public trade literature as a narrow molecular weight distribution, butene-comonomer LLDPE intended primarily for blown film extrusion. Distributor data sheets commonly quote a nominal melt flow rate of 1.9–2.1 g/10 min at 190 °C under 2.16 kg load when tested to ISO 1133-1:2022, and a nominal density of 0.918–0.922 g/cm³ at 23 °C according to ISO 1183-1:2019. These values place 35B within the conventional C4-LLDPE film envelope, but the certificate of analysis remains the only traceable release document because distributor summaries may omit additive package and comonomer details.
The 35B designation does not encode comonomer type or stabilizer formulation. Public trade sources identify the grade as a butene-comonomer film resin; if a downstream application depends on hexene or octene toughness, that distinction must be verified before substitution. The molecular architecture consists of linear polyethylene chains with short-chain branches and no long-chain branching. This absence of long-chain branching separates 35B from autoclave or tubular LDPE and explains several processing differences observed on blown film lines.
Principal conversion is blown film extrusion for general packaging, agricultural film, lamination substrates, and heavy-duty sacks. The resin is selected where moderate stiffness, high elongation, and seal integrity are required in film thicknesses of 25–50 µm. Typical conversion uses a BUR between 2.0:1 and 2.5:1 and a die gap of 1.8–2.3 mm to limit bubble sag. Published data for 35B specifically under high-stalk film conditions is limited; converters should map bubble temperature, frost line, and air-ring pressure before committing the grade to ultrathin film below 20 µm.
High-stalk bubble stability is generally the limiting processing variable for 35B-type C4-LLDPE. The short-chain branch distribution produces less pronounced shear thinning than high-pressure LDPE, so the melt retains higher viscosity inside the die while displaying lower melt strength in the bubble. This combination raises extruder torque and increases sensitivity to air-ring turbulence. Processors commonly compensate with low-pressure spiral dies, dual-lip air rings, and internal bubble stabilization when BUR exceeds 2.5:1. On a 65 mm grooved-feed extruder with L/D 30:1, barrel set points are typically 170–210 °C, die zones 200–220 °C, and melt temperature 195–225 °C. Melt temperatures above 240 °C are not recommended because oxidative chain scission can generate gel particles and reduce dart impact under ASTM D1709.
The melt flow ratio I21/I2 is frequently absent from broker data sheets, but where it is reported it provides an indirect measure of molecular weight distribution. For C4-LLDPE film resins with nominal melt flow rate near 2.0 g/10 min, the I21/I2 ratio is typically 24–30, whereas autoclave LDPE may fall between 40 and 80. The narrower distribution reduces draw resonance but lowers bubble stability, so the same frost line setting cannot be transferred unchanged from an LDPE product. Frost line height for 35B-type film is normally 250–500 mm above the die and must be established on the actual tower.
Surface moisture is an operational boundary. At ambient relative humidity above 60%, pellet condensation can produce bubble instability and surface defects; hopper drying at 70–80 °C for 2–4 h may be required. Contamination with polypropylene or acid-containing ethylene vinyl alcohol recycle is incompatible because viscosity mismatch can produce melt fracture and gel accumulation. Recycle streams should be segregated and evaluated for ash and gel count before reintroduction.
Differences from other product classes are primarily mechanical and rheological. Against an autoclave LDPE of equivalent melt index, 35B has higher tensile strength at break and higher dart impact but lower melt strength and less shear thinning. Against a hexene-LLDPE of similar density, the shorter butene branches in 35B are less effective at forming tie molecules, so dart impact and Elmendorf tear are typically lower under equivalent film-conversion conditions. Against an octene-LLDPE, the difference becomes more significant in low-temperature abuse. Against HDPE film grades, 35B has lower modulus and higher elongation but lower stiffness and lower water-vapour barrier.
The following comparison is qualitative but is anchored to the test methods used in film release testing.
| Property | Test method | 35B-class C4-LLDPE | Autoclave LDPE | C6-LLDPE |
|---|---|---|---|---|
| Long-chain branching | Rheological evaluation | Absent | Present | Absent |
| Dart impact at 25 µm | ASTM D1709 | Moderate | Lower | Higher |
| Elmendorf tear propagation | ASTM D1922 | Moderate, directional | Lower | Higher |
| Bubble stability in high-stalk | Processing evaluation | Moderate | High | Lower |
| Low-temperature seal initiation | Heat-seal profile | Comparable to LLDPE class | Higher seal initiation temperature | Comparable to LLDPE class |
Substitution of 35B for a hexene-LLDPE is not recommended in frozen-food packaging where dart impact at -20 °C is critical unless end-use testing under ASTM D1709 confirms acceptable performance. Conversely, replacing an autoclave LDPE with 35B may require a reduction in melt temperature and an increase in die gap to avoid melt fracture. The lower long-chain branching reduces bubble stability but increases tensile strength and puncture resistance under standard test conditions.
On production-scale grooved-feed blown film lines, the pressure profile is a useful diagnostic indicator. The grooved barrel generates high feed-zone pressure and requires water cooling to prevent premature melting. With 35B-class C4-LLDPE, die pressure is commonly observed in the range 200–350 bar at output rates of 150–220 kg/h on a 65 mm line running a 1.8 mm die gap. These values are class-level; exact pressure depends on die diameter, die design, and resin lot. A sudden pressure rise at constant screw speed can indicate gel accumulation or degraded regrind, while a pressure drop at constant speed may indicate feed bridging or screw wear.
Output and melt temperature must be balanced against optical quality. If the frost line is too low, film orientation decreases and tear anisotropy increases. If the frost line is too high, bubble stability declines. The use of a dual-lip air ring improves gauge uniformity; gauge variation should be held below ±5% for consistent tensile and barrier performance. Internal bubble stabilization is generally required when BUR exceeds 2.5:1, especially on lines without an adjustable upper nip.
Typical film property data obtained for C4-LLDPE of this melt index and density at 25 µm, BUR 2.5:1, and die gap 1.8 mm include tensile strength at break of 25–45 MPa in the machine direction and 20–40 MPa in the transverse direction when tested to ASTM D882-18, elongation at break of 500–800%, secant modulus of 150–250 MPa, dart impact of 50–120 g under ASTM D1709, and Elmendorf tear of 50–150 gf MD and 100–250 gf TD under ASTM D1922. These data are not a substitute for lot-specific values because comonomer content, additive package, and film cooling history shift the results.
Optical properties are controlled by film gauge, cooling rate, die cleanliness, and air-ring configuration. Haze for 35B-class film is typically 10–20% at 50 µm when measured under ASTM D1003. Gloss is moderate and generally lower than an equivalent LDPE film. Blending with up to 10 wt% of high-pressure LDPE can improve optical clarity, but such blending alters dart impact and tear balance and must be evaluated against the end-use specification.
For food-contact applications, the resin must be evaluated under the relevant polymer regulation. In the United States, compliance is assessed under 21 CFR 177.1520 for olefin polymers; in the European Union, the requirements of Commission Regulation (EU) No 10/2011 and its amendments apply. Ash content is typically below 0.05% when determined by ISO 3451-1:2019. Specific migration limits for additives should be confirmed with the masterbatch or compounding source. Pellets should be stored in closed containers at ambient temperature below 50 °C and protected from UV exposure to preserve the antioxidant package.