| HS Code | 136233 |
| Tensile Yield Strength Mpa | >=25 |
| Elongation At Break Percent | >=600 |
| Flexural Modulus Mpa | >=1000 |
| Vicat Softening Temperature C | >=125 |
| Oxidation Induction Time Min | >=20 |
| Carbon Black Content Percent | 2.0-2.5 |
| Environmental Stress Cracking Resistance H | >=5000 |
| Slow Crack Growth Resistance H | >=5000 |
| Hydrostatic Strength Class | PE100 |
| Color | Black |
| Form | Pellets |
As an accredited Yanchang China Coal Yulin (Shaanxi) HDPE TR571Y factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied in 25 kg polyethylene-lined woven bags, 40 bags per 1,000 kg pallet, labeled Yanchang China Coal Yulin HDPE TR571Y. |
| Container Loading (20′ FCL) | 20′ FCL container loading of Yanchang China Coal Yulin (Shaanxi) HDPE TR571Y in 25kg bags, palletized and shrink-wrapped, securely stuffed. |
| Shipping | Yanchang China Coal Yulin (Shaanxi) HDPE TR571Y is shipped as non-hazardous HDPE resin pellets. Typical packaging: 25 kg woven bags or 500–1000 kg jumbo bags, palletized. Transport by sea in 20-ft/40-ft containers. Store cool, dry, ventilated; avoid moisture, sunlight, and ignition sources. No special dangerous goods requirements. |
| Storage | Store Yanchang China Coal Yulin (Shaanxi) HDPE TR571Y in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, ignition sources, and strong oxidizers. Keep original bags sealed and palletized; prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking pressure. Maintain moderate temperatures, good housekeeping, and first-in, first-out stock rotation. |
| Shelf Life | Yanchang China Coal Yulin (Shaanxi) HDPE TR571Y typically has a 12-month shelf life when stored cool, dry, sealed, and away from direct sunlight. |
The Yanchang China Coal Yulin (Shaanxi) HDPE TR571Y resin is a PE100-class high-density polyethylene supplied as natural pellet for pressure-pipe extrusion; it should be converted into finished pipe with carbon black or pigment masterbatch added at the converter unless the application is indoor and ultraviolet exposure is absent. The six downstream sectors selected below are limited to installed PE100 pressure-pipe applications where the resin’s long-term hydrostatic strength, slow crack growth resistance, and chemical resistance are exercised in production environments. Each section states the governing compliance standard, the formulation addition ratio for the pipe compound, the downstream manufacturing route, and the terminal product form. Processing temperatures, pressures, and dimension ranges are typical for PE100-grade HDPE; the TR571Y mill certificate must be checked for melt mass-flow rate per ISO 1133-1, density per ISO 1183-1, and oxidation induction time per ISO 11357-6 before extrusion parameters are fixed.
Municipal potable water specifications for TR571Y are dominated by slow crack growth resistance over a 50-year service life, because the pipe operates under internal pressure at temperatures that fluctuate between 4°C and 25°C and at hoop stresses below the short-term yield point. Under ISO 12162 and ISO 9080 regression analysis, the resin is classified as PE100 with minimum required strength 10.0 MPa at 20°C; ISO 4427-1 and ISO 4427-2 reduce this by a service coefficient of 1.25 to a design stress of 8.0 MPa for water at 20°C. Conformance testing therefore includes hydrostatic pressure testing per ISO 1167 at 20°C and 80°C, slow crack growth evaluation on notched pipe per ISO 13479, and oxidation induction time retention per ISO 11357-6, rather than reliance on tensile yield or hardness. Where North American approvals are required, potable-water contact is verified under NSF/ANSI/CAN 61; Chinese municipal projects typically reference GB/T 13663.2, while European tenders reference EN 12201. The formulation addition ratio for black potable-water pipe introduces carbon black masterbatch into TR571Y natural pellet to achieve 2.0–2.5 wt% carbon black in the finished pipe compound; clean in-house regrind may be used only in quantities permitted by the drinking-water listing and never from external reclaim. Downstream extrusion on a grooved-feed single-screw extruder with L/D 30:1–36:1 and a barrier screw is carried out at melt temperatures of 200–230°C, with vacuum tank calibration, spray cooling at 10–25°C, laser diameter scanning, and cut-to-length sawing or coiling for small diameters. Terminal products are black or blue PE100 water pipes in dimensions 20–1600 mm, SDR 11/13.6/17/21/26, installed as municipal mains, service connections, and distribution laterals.
In gas distribution networks, the controlling variable shifts from hydrostatic creep to rapid crack propagation arrest, because a longitudinal crack in a pressurised polyethylene main can propagate faster than gas decompression waves and extend beyond the fusion joint. The governing compliance framework for TR571Y in this application is ISO 4437 and EN 1555 in international and European gas distribution; ASTM D2513 and 49 CFR Part 192 apply where US federal gas pipeline regulations are invoked. Pipe manufactured from TR571Y must satisfy the ISO 13477 small-scale steady-state test at 0°C, and full-scale ISO 13478 testing may be required for larger diameters or colder installation conditions. The design stress for natural gas is derived from the PE100 MRS of 10.0 MPa using a service coefficient of 2.0, yielding 5.0 MPa at 20°C; SDR 11 pipe therefore carries a maximum operating pressure near 10 bar, while SDR 17.6 is assigned lower pressure classes. Formulation addition ratio for buried gas pipe is 2.0–2.5 wt% carbon black in the final compound, with the yellow identification stripe or outer layer produced by coextrusion using a separate pigmented PE100 skin; no recycled or filled material is introduced because rework can reduce rapid crack propagation arrest fracture energy. Downstream conversion uses the same grooved-feed extrusion line as potable-water pipe, but the melt temperature band is often narrowed to 190–220°C to limit oxidative thermomechanical degradation during long runs; post-extrusion cooling is staged to reduce frozen-in stress before hydrostatic proof testing. Terminal products are black PE100 gas mains and service pipes in 20–630 mm diameters, joined by butt fusion or electrofusion fittings, with installation temperatures specified by the gas utility and limited by the pipe’s RCP resistance rather than by general low-temperature impact strength.
Abrasive tailings service subjects the pipe wall to simultaneous internal pressure, moving solid particles, and occasional full vacuum during shutdown drainage; for TR571Y there is no single ISO product standard covering slurry abrasion, so pressure rating is derived from ISO 9080 long-term hydrostatic strength and ISO 12162 PE100 classification, while wear allowance is based on site-specific slurry pot tests using the mine’s solids size distribution. The formulation addition ratio remains 2.0–2.5 wt% carbon black for outdoor storage and ultraviolet resistance; mineral fillers such as silica, calcium carbonate, or ceramic powder are not used because hard particulate fillers create stress-concentration sites that reduce slow crack growth resistance without improving the polyethylene matrix’s ability to absorb solid-particle impact energy. TR571Y processed into heavy-wall tailings pipe is extruded on large grooved-feed single-screw machines with outputs scaled to diameters from 250 mm to 1200 mm and wall thicknesses exceeding 50 mm; the downstream line must include multiple vacuum calibration tanks and long spray-cooling zones with water temperatures rising no higher than 25°C, otherwise the low thermal conductivity of HDPE produces core voids and residual stress that shorten hydrostatic life. Terminal products are solid-wall PE100 tailings and dredge lines in 12–20 m straight lengths, joined by butt fusion, and often fitted with wear-resistant steel or ceramic elbows at high-velocity direction changes. Published slurry-abrasion data for this specific TR571Y grade is limited; a plant trial under actual slurry velocity, particle size distribution, and temperature is required before wall-thickness reduction from the pressure rating is accepted.
Landfill leachate is a chemically aggressive aqueous mixture containing volatile fatty acids, ammonia, chlorides, and trace organics, so the specification of TR571Y for collection and transfer pipe rests on chemical resistance under long-term exposure rather than on ultraviolet ageing alone. The compliance framework uses ISO/TR 10358 chemical-resistance classifications for polyethylene after immersion in representative leachate constituents at 23°C and 40°C; solid-wall pressure sections above the landfill liner are specified under ISO 4427 or ASTM F714, while slotted collection pipe is treated as a perforated pressure pipe and hydrostatically tested before slotting. Formulation addition ratio for leachate pipe is 2.0–2.5 wt% carbon black in the final compound; no plasticiser, filler, or external regrind is added because leachate extraction tests can detect releases from unsuitable rework streams. Downstream manufacturing involves standard PE100 pipe extrusion followed by mechanical slotting with water-jet or CNC router equipment; slot dimensions and spacing are cut perpendicular to the pipe axis, with tool speed and coolant controlled to avoid microcracking at slot ends that could propagate under hoop stress. Terminal products are slotted HDPE collection pipes and unperforated transfer pipes in diameters commonly between 160 mm and 630 mm, joined by butt fusion or flex coupling, with risers and manhole connections produced from the same PE100 material to preserve compatibility at the connection.
Where irrigation mainlines are laid in shallow trenches and exposed to ultraviolet radiation, the formulation and extrusion controls differ from indoor industrial pipe because the pipe must withstand daily thermal expansion cycles, soil loading, and occasional water hammer from pump starts. TR571Y irrigation mains are specified under ISO 4427 for pressure rating, with hydrostatic acceptance testing per ISO 1167 at 20°C and 80°C; in North American irrigation districts, ASTM F714 is often referenced for larger-diameter gated pipe systems. The formulation addition ratio for a black irrigation pipe is 2.0–2.5 wt% carbon black in the final compound; if a coextruded white exterior skin is specified to reduce solar heat absorption, the skin layer is compounded with a titanium dioxide masterbatch at 2–5 wt% addition ratio to the skin resin, while the core remains carbon black-filled PE100. Downstream production uses high-output pipe extrusion lines with grooved-feed barrels and internally cooled pipe dies; for diameters below 110 mm, the finished pipe may be coiled in 50–200 m lengths after cooling, while larger diameters are cut to 6–12 m sticks. Terminal products are irrigation mains, submains, gated pipes, and hydrant risers with SDRs selected from 17 to 26 according to design pressure; joints are typically butt-fused for permanent mains and mechanical compression couplings for removable field laterals.
Industrial process water and dilute chemical transfer pipe made from TR571Y is selected for its resistance to acidic and caustic aqueous streams at temperatures below 40°C, with the pressure envelope based on the PE100 MRS of 10.0 MPa and a service coefficient selected by the plant safety review, commonly between 1.25 and 2.0. The compliance basis is ISO/TR 10358 chemical-resistance classification and ISO 12162/ISO 9080 long-term pressure strength; where potable-water listing is not required, the pipe is commonly supplied as natural PE100 with 0% carbon black for indoor installations, while outdoor chemical lines use 2.0–2.5 wt% carbon black in the final compound. Downstream extrusion for industrial pipe follows the same grooved-feed single-screw route, but melt temperature is held between 200°C and 220°C because chemical-transfer pipe often operates in secondary containment where long-term stress-cracking resistance under aggressive media is the critical failure mode. Butt fusion welding on site uses heater-plate temperatures of 210±10°C, with bead-up pressure and soak time adjusted to wall thickness; the resulting joints are hydrostatically tested at 1.5 times the design pressure before commissioning. Terminal products are solid-wall industrial pipe in diameters from 20 mm to 630 mm, used for bleach dosing lines, acid brine transfer, demineralised water loops, and cooling-water headers. Published data for TR571Y in concentrated oxidising acids above 40°C is limited, and service under such conditions must be validated by immersion testing using the actual plant stream.
Competitive Yanchang China Coal Yulin (Shaanxi) HDPE TR571Y prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Yanchang China Coal Yulin (Shaanxi) HDPE TR571Y is a high-density polyethylene extrusion resin supplied as pellets from the coal-to-olefins complex in Jingbian, Shaanxi. The model designation TR571Y identifies a medium-molecular-weight blown-film grade positioned between high-load melt-index blow-moulding resins and high-flow injection-moulding grades. Its nominal melt flow rate is 0.50 g/10 min when measured at 190°C under 2.16 kg load in accordance with ISO 1133-1:2022 or ASTM D1238-20, and its nominal density is 0.951 g/cm³ under ISO 1183-1:2019. Because the polymer is produced from coal-derived ethylene via a low-pressure slurry polymerization train, the base resin is an ethylene-rich polyolefin; the producer does not routinely disclose exact comonomer type or amount in standard technical literature. The primary design target is blown-film packaging where stiffness, thin-gauge drawdown, and consistent bubble geometry are required. Lot-specific certificates of analysis should be obtained from the producer for actual melt flow rate, density, ash content, gel count, and additive package identification.
Film-grade high-density polyethylene is often specified by two parameters only; however, conversion behavior is also controlled by molecular weight distribution, comonomer distribution, and additive package. TR571Y is not a fractional-melt film resin; the 0.50 g/10 min MFR allows lower extruder torque than a 0.30 g/10 min high-molecular-weight film grade and reduces back-pressure in spiral mandrel dies. The density of 0.951 g/cm³ yields a balance between stiffness and impact resistance; at this density level the crystalline fraction is high enough to provide load-bearing capacity but not so high that thin-gauge film loses all dart drop resistance. Processors selecting the grade for T-shirt bags, refuse sacks, and secondary packaging generally use melt temperatures of 200–215°C and blow-up ratios between 3:1 and 5:1; the frost line is placed at 6–9 die diameters above the die face to stabilize the bubble and control orientation balance.
Processing limits for TR571Y are defined by oxidation, melt fracture, and bubble instability rather than by moisture uptake. Virgin high-density polyethylene is not hygroscopic; surface condensation from cold storage is more relevant than internal moisture. When the pellet surface is allowed to reach 25°C before extrusion, no drying is normally required. A single-screw extruder with L/D ≥ 30:1 and a grooved feed bushing is adequate. Barrel profiles from feed throat to adapter are typically set from 170°C to 205°C, with the die and adapter at 200–215°C. The melt temperature should be kept below 240°C; above this threshold, thermo-oxidative degradation accelerates and produces gel flecks, fish eyes, and discoloration in film. Below 170°C, the melt may not homogenize sufficiently, causing pressure fluctuations and melt fracture at the die lip. If die head pressure rises above 450 bar on a spiral mandrel die, the most common causes are insufficient melt temperature, excessive screen-pack pressure drop, or accumulations of degraded gel in the die lips. The die gap should be maintained between 1.2 mm and 2.0 mm for thin-gauge HDPE film; narrower gaps can increase shear heating and reduce throughput stability. Screw speed should not exceed 80% of the extruder drive maximum unless the drive and screw design have been specifically matched for high-throughput film lines.
Bubble stability is governed by the ratio of frost line height to die diameter and by air ring control. For TR571Y, a blow-up ratio of 3:1 to 5:1 is commonly used; at blow-up ratios below 2.8:1, transverse orientation may be insufficient and film can split along the machine direction under puncture. At blow-up ratios above 5.5:1, the bubble becomes sensitive to ambient air currents and gauge variation increases. Frost line height is typically set at 6–9 die diameters; a lower frost line increases machine-direction orientation and produces higher machine-direction tensile strength but lower transverse tear resistance. The specific frost line position depends on air ring velocity, melt temperature, and line speed, not on resin alone. The grade is intended for gauges from 15 µm to 80 µm; below 12 µm, published data for this specific configuration is limited and film toughness becomes highly dependent on die design and cooling geometry.
The shear viscosity of TR571Y is not characterized solely by the 0.50 g/10 min melt flow rate because the MFR test applies a low shear rate. In spiral mandrel dies, the melt experiences apparent shear rates on the order of 100–1000 s⁻¹, where the distinction between narrow and broad molecular weight distribution becomes controlling. A narrow molecular weight distribution reduces die swell and permits lower die gaps; however, it also lowers melt elasticity and may make the bubble more sensitive to ambient air movement. Therefore, air ring design and bubble-stabilization calipers are more important for this grade than for a broad-distribution blow-moulding resin. Published capillary rheometry data for this specific product is limited; processors should map viscosity versus apparent shear rate on a dual-bore capillary rheometer at 190°C, 210°C, and 230°C before changing die geometry.
Mechanical property expectations for extruded film are thickness-dependent; the values below are bulk resin values from producer technical literature and are not guarantees for finished film. For film made at 25 µm gauge on a monolayer line, tensile properties and dart drop resistance will vary with blow-up ratio, frost line height, and die gap.
| Property | Nominal Value | Test Method |
|---|---|---|
| Melt flow rate, 190°C/2.16 kg | 0.50 g/10 min | ISO 1133-1:2022 / ASTM D1238-20 |
| Density | 0.951 g/cm³ | ISO 1183-1:2019 |
| Tensile yield stress | 24 MPa | ISO 527-2:2012 |
| Tensile elongation at break | >600% | ISO 527-2:2012 |
| Flexural modulus | 900 MPa | ISO 178:2019 |
| Vicat softening temperature, 10 N | 124°C | ISO 306:2022 |
| Shore D hardness | 63 | ISO 868:2003 |
The reported 24 MPa tensile yield stress and 900 MPa flexural modulus place TR571Y in the medium-stiffness segment of high-density polyethylene film grades. These values are lower than a 0.956 g/cm³ fractional-melt film resin, which may show yield stresses above 26 MPa and flexural moduli above 1000 MPa, but higher than a 0.945 g/cm³ medium-density grade with flexural modulus below 800 MPa. The balance is relevant when stiffness-driven packaging is specified but film impact resistance cannot be sacrificed. Published data for this specific configuration is limited; comparative performance should always be generated on the target blown-film line rather than inferred from bulk resin values alone.
When TR571Y is compared with other high-density film grades produced in the same coal-to-olefins complex, the positioning is typically based on MFR and density rather than on comonomer type. In the absence of producer-published full rheology curves, the most reliable differentiation is obtained by measuring the melt flow rate ratio between 21.6 kg and 2.16 kg loads under ISO 1133-1:2022. A higher flow rate ratio indicates a broader molecular weight distribution and usually greater melt strength; a lower ratio indicates a narrower distribution and better surface finish. This ratio is often more useful than a single MFR value for predicting film line behavior.
TR571Y differs from blow-moulding grades in the same density range primarily in melt flow rate and additive package. A large-part blow-moulding high-density polyethylene may have an MFR of 0.25–0.35 g/10 min and a broader molecular weight distribution to resist parison sag; TR571Y, at 0.50 g/10 min, is less viscous under typical extrusion shear rates and therefore generates less back-pressure in narrow die gaps. The distinction is exploited in film lines where 1.2 mm die gaps and 15–25 µm final gauges are required. A blow-moulding grade would trend toward higher melt pressure and may produce unacceptable gauge scatter in such thin film. Conversely, an injection-moulding high-density polyethylene with MFR above 10 g/10 min has insufficient melt strength to sustain a stable bubble at typical blow-up ratios of 3:1 to 5:1; it tends to draw down too fast and produce narrow gauge bands or bubble collapse.
Compared with a typical butene-LLDPE film resin of similar MFR, TR571Y has higher density and higher flexural modulus, but lower dart drop impact and lower elongation. The difference is directly related to the higher crystalline fraction in HDPE; the resultant film is stiffer but less forgiving to puncture and flex cracking. In multi-layer structures, TR571Y may be used in the core layer of a coextruded film to provide stiffness while LLDPE skins supply dart drop and seal initiation. This is a specific usage difference from other products: TR571Y is generally not selected for high-haze or high-gloss retail packaging requiring low seal initiation temperature; its sealing window is narrower than metallocene LLDPE. For monolayer HDPE film, heat-seal temperatures are commonly set at 145–170°C with dwell times of 0.3–0.8 s; published data for this specific grade is limited and must be confirmed on the production sealer.
Use in direct food contact requires verification of the finished film, not just the base resin. The base olefin polymer may be evaluated under GB 4806.6-2016, FDA 21 CFR 177.1520, and EU Regulation 10/2011. For EU compliance, total migration must not exceed 10 mg/dm² for a single-sided contact test using the simulants specified in Annex III; for high-fat foods, simulants such as D2 or E may be required. The converter must include contributions from any masterbatch, slip agent, antioxidant, or processing aid. A certificate of analysis for the base resin does not eliminate the need for finished-article testing. For FDA status, olefin polymers are listed in 21 CFR 177.1520; the finished substance must meet density and extraction limits in paragraph (c). For China, GB 4806.6-2016 applies to food-contact plastics; migration tests under GB 31604.1 and GB 31604.8 may be required depending on food type and contact time.
For non-food industrial packaging sold into electronics supply chains, the converter may be asked to demonstrate compliance with IEC 62321 test methods for restricted substances under the EU RoHS Directive 2011/65/EU. High-density polyethylene produced without heavy-metal pigments typically passes these screens, but antistatic or color masterbatches can introduce restricted metals and must be controlled. Importers should also manage SVHC communication duties under Article 33 of REACH when the packaged article contains substances above the applicable concentration threshold; the polymer itself is not subject to REACH registration.
Operational boundaries for TR571Y include additive compatibility and regrind control. The resin should not be combined with amine-based antistatic additives unless the specific stabilizer package is confirmed compatible; amine species can interfere with phenolic antioxidant systems and cause yellowing or odor generation at high processing temperatures. Post-industrial regrind from edge trim and start-up film is generally acceptable at 10–20 wt% when the trim is dry and free of print or adhesive. Levels above 30 wt% may increase gel counts and reduce dart drop impact because each heat history increases chain branching and crosslinking precursors. If regrind is generated from film that has been stored outdoors or in contact with organic vapors, it should be excluded from food-contact structures. Pellets should be stored below 50°C and protected from direct UV radiation; prolonged exposure to sunlight can create oxidized surface layers that produce gel specks and odor. Melt residence time at temperatures above 240°C should be kept below 5 min; if a line stops, the extruder should be purged with lower-viscosity polyethylene or operated at reduced temperature before restart. Die-lip buildup should be monitored at every shift; sudden increases in die pressure or appearance of oxidized gel flecks indicate the need to reduce melt temperature or replace the screen pack.