Yanchang China Coal Yulin Shaanxi Hdpe Tb5610y

Yanchang China Coal Yulin (Shaanxi) HDPE TB5610Y

    • Product Name: Yanchang China Coal Yulin (Shaanxi) HDPE TB5610Y
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 744668
    Polymer Type High-Density Polyethylene (HDPE)
    Grade TB5610Y
    Density 0.956 g/cm³
    Melt Flow Rate Mfr 10 g/10 min
    Tensile Yield Strength ≥26 MPa
    Elongation At Break ≥600%
    Flexural Modulus ≥1100 MPa
    Vicat Softening Temperature ≥120 °C
    Brittleness Temperature ≤-60 °C
    Shore D Hardness ≥60
    Ash Content ≤0.04%
    Moisture Content ≤0.1%
    Bulk Density ≥0.56 g/cm³

    As an accredited Yanchang China Coal Yulin (Shaanxi) HDPE TB5610Y factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Yanchang China Coal Yulin (Shaanxi) HDPE TB5610Y is packed in 25 kg PP woven bags, palletized, 1000 kg per pallet.
    Container Loading (20′ FCL) Container loading (20′ FCL) for Yanchang China Coal Yulin (Shaanxi) HDPE TB5610Y: 25 kg bags, palletized, securely stowed; about 16–17 MT net.
    Shipping Yanchang China Coal Yulin (Shaanxi) HDPE TB5610Y is a non-hazardous high-density polyethylene resin. It is normally shipped in 25 kg bags or 1,000 kg jumbo bags, palletized and containerized, or in bulk trucks. Transport as general cargo; keep dry, cool, away from direct sunlight. No dangerous goods documentation required.
    Storage Store Yanchang China Coal Yulin (Shaanxi) HDPE TB5610Y in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, moisture, and ignition sources. Keep original packaging sealed on pallets, off the floor, and stacked safely to prevent bag deformation. Protect from UV, dust, oils, acids, oxidizers, and other contaminants. Use first-in, first-out rotation and follow local regulations.
    Shelf Life Typically 12–24 months when stored dry, cool, ventilated, away from sunlight, in original unopened packaging; confirm with supplier.
    Application of Yanchang China Coal Yulin (Shaanxi) HDPE TB5610Y

    Extrusion blow moulding of 20 L–30 L industrial chemical jerrycans from Yanchang China Coal Yulin (Shaanxi) HDPE TB5610Y is run on an accumulator-head machine with an extruder L/D ratio of 24:1–30:1. The parison must be programmed in at least 10 axial points; a constant-thickness parison produces a sidewall that thins to 1.0–1.4 mm at the shoulder and thickens to 5–7 mm at the corner weld, which creates bending stiffness but consumes excess resin. The die gap is set between 2.0 mm and 3.5 mm for a 25 L container, with die swell in the range 30–50 %; the blow ratio at the widest panel is limited to 2.0:1–2.5:1 to avoid excessive orientation and environmental stress-crack resistance loss. Melt temperature is maintained at 175–205 °C. The lower limit is constrained by melt fracture and poor parison knit at the pinch-off; the upper limit is constrained by volatile formation that condenses on the mould surface and increases part odour. Mould cooling uses glycol at 8–15 °C and turbulent flow through beryllium-copper pinch-off inserts; the mould face adjacent to the pinch-off is held below 15 °C to prevent post-ejection dimensional recovery. For dangerous goods packaging, the finished jerrycan is filled to 95 % capacity and subjected to UN 6.1.5 drop testing from 1.2 m after conditioning at −18 °C, followed by a 28-day stacking test at 40 °C. The top-load force on an empty jerrycan measured by ISO 12048 is monitored; a drop below 1.5 kN triggers a wall-thickness audit and a parison-programmer reset. Because aromatic hydrocarbons swell HDPE, compatibility with the filled product must be established by ASTM D543-21 using the actual formulation; when the mass gain exceeds the end-user limit, surface fluorination or a barrier layer is introduced.

    Comparative extrusion blow moulding boundaries for HDPE TB5610Y across four rigid-packaging scenarios
    ParameterIndustrial 20–30 L jerrycanThin-wall 250 mL–1 L bottleAutomotive 1–5 L reservoir6-layer barrier bottle
    Extruder L/D ratio24:1–30:124:1–28:124:1–28:124:1–30:1
    Melt temperature175–205 °C180–195 °C175–200 °C190–220 °C
    Die gap2.0–3.5 mm0.8–1.5 mm1.5–2.5 mm1.0–2.0 mm
    Mould temperature8–15 °C10–12 °C10–15 °C8–12 °C
    Blow pressure0.8–1.2 MPa0.6–0.9 MPa0.8–1.2 MPa0.6–1.0 MPa
    Cycle time90–150 s9–14 s60–100 s30–70 s

    What Limits Ambient Temperature Drop Resistance in Thin-Wall Detergent Bottles?

    Shuttle blow moulding lines that convert TB5610Y into 250 mL–1 L household cleaning product bottles operate with a twin-station clamping system and a continuously rotating grooved-barrel extruder. The critical conflict is between cooling time and low-temperature impact. A melt temperature of 180–195 °C and a mould temperature of 10–12 °C allow a cycle time of 9–14 s, but fast cooling freezes orientation into the sidewall and can reduce the −20 °C drop height to below 1.2 m in thinner panels. The bottle is blow moulded with a programmed parison that places 0.6–0.8 mm of material at the label panel and 1.0–1.4 mm at the bottom radius. Drop testing follows ASTM D2463 with a 500 mL bottle filled to 98 % capacity with water; a brittle crack at the base hinge or below the neck is unacceptable. The neck finish is reamed to 24/410 or 28/410 dimensions with an ovality tolerance of 0.20 mm; cap back-off torque after 24 h at 40 °C must remain within 1.0–1.8 N·m. For bleach-containing products, the resin package is checked against ASTM D1693 Condition B after contact with 5.0 wt % sodium hypochlorite at 60 °C for 500 h; a shortened failure time indicates oxidative degradation at the weld line and requires a peroxide-resistant stabilizer package.

    Windshield washer reservoirs and coolant overflow tanks are blow moulded in 1 L–5 L formats from TB5610Y on single-station accumulator machines. The part design includes blow-pins that form hose barbs and sensor bosses; the pinch-off weld is the failure origin in underhood thermal cycling. The accumulator head is run with a parison drop time of 2–4 s, a blow pressure of 0.8–1.2 MPa, and a mould temperature of 10–15 °C. The finished part is pressure-cycled between −40 °C and 100 °C for 1,000 h according to OEM coolant-system specifications; leakage at 1.5 bar internal air pressure through the pinch-off or insert area fails the component. Low-velocity puncture testing is performed by ISO 6603-2 at −30 °C; the weld line must show ductile yielding rather than cleavage. The continuous-use limit of standard HDPE in dry underhood environments is approximately 60–80 °C, so coolant reservoirs are not used as pressure vessels and the wall thickness is designed to compensate for modulus loss at 80 °C relative to 23 °C flexural modulus. Insert bosses are fabricated from the same HDPE family to prevent weld-line contamination; use of glass-filled PP inserts is avoided because differential shrinkage creates a leak path at the seal ring.

    Solvent Permeation in Agricultural Chemical Bottles Drives a Six-Layer Barrier Strategy

    Monolayer HDPE bottles holding xylene, cyclohexanone, or mixed aromatic-aliphatic pesticide formulations exhibit solvent migration that can soften the outer surface and distort the label panel within storage periods shorter than the required 24-month shelf life. A six-layer continuous coextrusion blow moulding process places TB5610Y as the inner and outer structural layers, with a maleic anhydride-grafted polyolefin tie layer on each side of an EVOH or polyamide barrier layer. The EVOH layer is held at 60–120 µm in the flat wall, while the combined HDPE layers provide 80–90 % of the 1.0–2.0 mm total wall. The die head temperature for the HDPE stream is 200–220 °C; the barrier stream is kept at 190–210 °C to avoid EVOH gel formation and is fed through a separate manifold to the feedblock. Layer stability depends on the viscosity ratio between the HDPE and EVOH streams; a ratio of 2:1–3:1 at the respective shear rates prevents layer encapsulation and wave instability. Edge trim and rejected preforms are reground at 20–30 wt % into the outer HDPE layer only; incorporating barrier regrind into the structural layer creates gels and pinholes because EVOH domains do not re-disperse in the HDPE matrix. Permeation is measured by ASTM D2684 with the intended solvent model at 40 °C; the container is accepted when the mass loss rate remains below the formulator’s limit, typically 0.5–1.0 % per year. Because published data for this specific TB5610Y/tie-layer/EVOH combination is limited, the converter must run a designed experiment with three layer-ratio levels and confirm sidewall delamination resistance before commercial launch.

    Personal care and cosmetic bottles produced from TB5610Y are typically extrusion blow moulded on high-cavity shuttle machines in 50 mL–500 mL formats. The failure modes are not primarily mechanical so much as aesthetic: sink marks above closures, non-uniform pearlisation after silk-screen or sleeve labelling, and orange-peel on the shoulder where the parison is stretched at high blow-up ratio. The melt temperature is reduced to 175–190 °C to retain surface gloss; the mould is polished to an SPI A-2 finish and maintained at 12–15 °C. A blow-up ratio above 3.0:1 at the shoulder is avoided because strain-induced whitening becomes visible in dark colours. Neck finishes for pumps and sprayers are normally 24/410 or 28/410 with a neck I.D. tolerance of ±0.1 mm to prevent lotion pump gasket leakage. Because cosmetic formulations often contain ester-based fragrances, the bottle is tested by ASTM D543-21 for weight change after 30 days at 40 °C; a weight gain above the packager’s established limit indicates that the grade should be swapped or the interior fluorinated. Odor transfer from the resin to the product is minimised by keeping the melt temperature below 200 °C and by purging the extruder with a dedicated HDPE purge compound after pigment changes.

    Regulatory Exclusion Criteria for Monolayer HDPE Food-Contact Articles

    TB5610Y extruded into monolayer bottles for dry food, confectionery, or solid pharmaceutical intermediates is assessed under EU Regulation (EC) No 1935/2004 and EU 10/2011 as amended, GB 4806.7-2016 in China, and FDA 21 CFR 177.1520 in the United States. The overall migration limit is 10 mg dm−2 of food-contact surface area when tested with the prescribed simulants; for aqueous foods the simulant is distilled water or 3 % acetic acid, and for fatty foods it is 95 % ethanol or an equivalent. The resin compliance depends on the antioxidant and catalyst-neutraliser additives used during pelletisation, so the converter must request the lot-specific food-contact declaration from the manufacturer; a generic HDPE compliance statement is not sufficient under EU 10/2011 Article 15. The continuous hot-fill temperature for monolayer HDPE is limited to approximately 60–70 °C; above 80 °C the bottle body can distort under capping top load, and migration of low-molecular-weight species accelerates. For acidic liquids with pH below 2.5, long-term storage is validated by immersion in the actual food simulant for 10 days at 40 °C using ASTM D543-21; the container must not show blushing or cracking, and the percent elongation change is measured by ISO 527-2 against the unexposed control. Post-consumer regrind is not permitted in monolayer food-contact layers unless the source is a closed-loop process approved under the relevant food-contact regulation; edge trim and injection flash from the same food-grade lot may be reintroduced at up to 15 wt % only if migration testing is repeated on the finished article.

    Compliance verification matrix for HDPE TB5610Y downstream applications
    End-use segmentPrimary standardTest parameterTypical threshold
    Dangerous goods packagingUN 6.1.5Drop, stacking, leakproofnessPass at designated drop height
    Food-contact dry foodEU 10/2011, GB 4806.7-2016, FDA 21 CFR 177.1520Overall migration10 mg dm−2
    Agricultural chemical barrierASTM D2684Permeation mass loss0.5–1.0 % per year at 40 °C
    Household detergent bottleASTM D2463Drop impact at −20 °C1.2 m, no brittle fracture
    Automotive underhood reservoirISO 6603-2Puncture impactNo brittle weld-line failure
    ESCR lot acceptanceASTM D1693Condition BFailure rate below 10 % at 48 h
    Free Quote

    Competitive Yanchang China Coal Yulin (Shaanxi) HDPE TB5610Y prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Yanchang China Coal Yulin (Shaanxi) HDPE TB5610Y is a high-density polyethylene blow moulding resin produced at the Yulin coal-to-olefins complex. The grade is a medium-molecular-weight ethylene copolymer with a nominal density of 0.956 g/cm³ when measured according to ISO 1183-1 or ASTM D1505 and a melt mass-flow rate of 1.0 g/10 min at 190 °C under 2.16 kg load when tested under ISO 1133-1:2022 or ASTM D1238. These two indices place TB5610Y in the extrusion blow moulding window in which parison melt strength is sufficient for continuous shuttle and reciprocating screw equipment but the viscosity is not so high that melt fracture becomes the limiting defect at standard die gaps. The resin is supplied as white cylindrical pellets and is typically stabilised with a phenolic antioxidant/phosphite package and an acid scavenger to limit oxidative degradation during extrusion. The grade is not intended for injection moulding of thin-wall articles, cast film, or pressure piping; its design basis is the production of rigid containers and technical parts where wall-thickness distribution, surface quality, and stress-crack resistance are controlled on blow moulding tools.

    What Distinguishes the Specification Profile of TB5610Y from Generic HDPE?

    The producer’s representative datasheet for TB5610Y lists the property profile in the table below. These values are typical lot averages and not maximum or minimum certification limits; a certificate of analysis governs individual batches.

    Representative TB5610Y property profile
    PropertyMethodTypical value
    Melt mass-flow rate (190 °C, 2.16 kg)ISO 1133-1:2022 / ASTM D12381.0 g/10 min
    Density (23 °C)ISO 1183-1 / ASTM D15050.956 g/cm³
    Tensile yield strength (50 mm/min)ISO 527-2 / ASTM D63824 MPa
    Elongation at breakISO 527-2 / ASTM D638600%
    Flexural modulus (2 mm/min)ISO 178 / ASTM D790900 MPa
    Notched Izod impact (23 °C)ISO 180 / ASTM D2568.0 kJ/m²
    Vicat softening temperature (A50)ISO 306 / ASTM D1525125 °C
    Shore D hardness (15 s)ISO 868 / ASTM D224063

    The combination of 0.956 g/cm³ density and 1.0 g/10 min melt mass-flow rate is significant because it balances container rigidity against parison stability. The flexural modulus of approximately 900 MPa supports stacking strength in rectangular and cylindrical bottles without requiring excessive wall thickness, while the tensile yield strength of 24 MPa provides resistance to burst deformation during pressurised filling. Elongation at break near 600% indicates ductile failure under tensile overload, which is relevant for drop-impact survival. The Vicat softening temperature of approximately 125 °C under ISO 306/ASTM D1525 means that continuous hot-fill above 60 °C is generally outside the safe processing envelope unless the converter redesigns the closure and headspace to relieve thermal deformation.

    The density of 0.956 g/cm³ reflects a linear polyethylene backbone with a low concentration of short-chain branches introduced by comonomer. This branch content is not specified by the producer but can be inferred from density depression relative to 0.965 g/cm³ homopolymer. The short-chain branch population affects slow crack growth resistance by increasing tie-molecule probability, while excessive comonomer reduces crystallinity and stiffness. TB5610Y occupies a mid-range position in which the crystalline fraction, estimated from density by the two-phase model, is approximately 65–70%. This crystalline fraction contributes to the Vicat softening temperature and flexural modulus. Environmental stress-cracking resistance under ASTM D1693 is frequently cited for this density/MFR class, but published numerical F50 data for TB5610Y can vary with comonomer lot and bottle geometry; critical detergent, surfactant, and agrochemical packaging should therefore be qualified on production-scale bottles rather than relying on a single resin property.

    On continuous shuttle blow moulding machines with 65 mm single-screw extruders and 25:1 L/D barrier screws, TB5610Y has been processed with melt temperatures of 180–210 °C, die head temperatures of 190–210 °C, and blow-air pressures of 0.4–0.8 MPa. Mould temperatures are commonly maintained at 10–30 °C to control cooling time and surface gloss. The grade exhibits moderate die swell in the range of 35–50% on diverging blow-pin tooling; programmed parison control must therefore compensate for swell and sag simultaneously. On a 5 L jerry can tool with a shot mass of 180 g, a hang time above 4 s can thin the bottom pinch-off region below the design minimum unless radial programming increases wall thickness at the lower segment. Conversely, at melt temperatures below 170 °C, sharkskin and die lines appear on the parison surface because the relaxation time of the melt exceeds the die transit time. These defects are not eliminated by increasing screw speed alone; they reflect insufficient melt temperature or excessive shear stress at the die lip.

    Extruder output stability is more important than absolute throughput for bottle weight consistency. Screw speed fluctuations greater than ±5% or feed-throat bridging cause visible weight variation in containers with wall thickness below 1 mm. The use of a grooved feed section is not required because the resin does not have the high slip tendency of bimodal pipe grades; however, feed throat temperature should be kept below 50 °C to prevent premature pellet softening and irregular solids conveying. Back pressure between 10–20 MPa is typical for adequate mixing of masterbatch, but excessive back pressure raises melt temperature and can generate gels if the residence time exceeds 3–5 min.

    When High Ambient Humidity or Long Residence Time Becomes a Processing Constraint

    Polyethylene does not undergo hydrolytic degradation in the same manner as polyamides or polyesters, so predrying is not mandatory. However, when pellets are stored in outdoor silos or conveyed through humid plant air with relative humidity above 60%, surface condensation can be carried into the extruder feed throat. This moisture appears as splay, pinholes, or local streaks on the bottle surface. In such cases a hot-air hopper dryer or desiccant dryer at 80 °C for 2 h is applied before processing. Drying beyond 4 h does not improve surface quality and may oxidise the pellet surface if the dryer is not air-swept.

    Thermal degradation is the main processing risk. Above 220 °C, chain scission and oxygen-induced crosslinking proceed rapidly; the resulting gels are visible as pin-head specks in thin-walled containers and can cause failure at the pinch-off weld. Residence time at melt temperature should be held below 5 min. During production interruptions longer than 15 min, the extruder should be purged with a general-purpose HDPE or LDPE to displace the heat-stabilised melt from the die head. Restarting the screw without purge after a thermal soak can produce black specks and carbonised deposits at the mandrel tip. The product is incompatible with moisture-curing PUR systems, and high levels of free amine-based additives in colour concentrates should be avoided because they may interfere with the stabiliser package and reduce oxidative stability. Copper and brass components in hot runner and die assemblies should also be avoided because copper can catalyse polyethylene degradation at processing temperatures.

    Comparative Differentiation Against Film, Injection, and Pipe Resins

    TB5610Y is separated from other HDPE grades primarily by its 1.0 g/10 min melt mass-flow rate and its molecular weight distribution. Compared with a general-purpose injection-moulding HDPE with MFR in the 8–20 g/10 min range, TB5610Y has higher melt viscosity, lower spiral-flow length, and higher die swell. These features are advantageous in blow moulding but make the product unsuitable for thin-wall injection applications such as caps, closures, or housewares with wall thickness below 1.5 mm. Conversely, compared with a blow moulding grade with MFR below 0.3 g/10 min, TB5610Y gives lower melt strength and higher parison sag on large containers above 10 L, but it permits lower melt temperature and faster cycle time on small bottles.

    Against film-grade HDPE, which typically has a density near 0.952 g/cm³ and a melt mass-flow rate of 0.05–0.15 g/10 min, TB5610Y does not provide the bubble stability or melt strength required for high-stalk film extrusion. Its density also produces a stiffer container wall but lower dart impact in film form. Against PE100 pipe-grade HDPE, the difference is more categorical: TB5610Y is not classified under ISO 12162, has no hydrostatic design basis, and should not be used for pressure piping or buried pipe networks. Pipe-grade resins use bimodal molecular weight distributions with high slow-crack-growth resistance; TB5610Y is not formulated for that service.

    Within the same producer’s blow moulding portfolio, TB5610Y should be selected when the priority is a rigid wall at moderate container size and when the tool has limited parison programming. If the container exceeds 10 L or carries aggressive surfactant-based contents, a lower-MFR blow moulding resin with higher ESCR and melt strength is generally preferred. If the container is smaller than 200 mL with thin walls, an injection-blow moulding grade may offer better neck finish definition.

    Qualified applications on shuttle and reciprocating screw blow moulding lines include rigid bottles and jerry cans from 100 mL to 10 L, pharmaceutical and cosmetic containers, edible-oil bottles where the converter verifies fatty-food migration limits, industrial packaging for lubricants and detergents, and technical mouldings with moderate ESCR requirements. Food-contact conformity is assessed under FDA 21 CFR 177.1520 for olefin polymers, EU Regulation 10/2011 with its specific migration limits for monomers and additives, and China GB 4806.7 for food-contact plastics. The resin supplier’s regulatory statement should be requested for each batch, but final conformity depends on the complete formulation, including masterbatch, regrind ratio, and processing aid. For containers used with aggressive hydrocarbons, oxygenated cleaners, or essential oils, prequalification on production tooling is required because ESCR failure is geometry-dependent and cannot be predicted solely from resin density or melt index.

    Regrind addition up to 30% is often tolerated in non-critical containers when the regrind is clean, dry, and generated from the same lot; higher regrind ratios may reduce ESCR and impact performance and should be validated by drop testing and ASTM D1693 F50 comparison. Blending with LLDPE at 10–20% improves notched impact and pinch-off weld toughness but reduces flexural modulus and increases cycle time because of lower crystallisation rate. This trade-off is managed on production-scale equipment by adjusting blow pressure and mould cooling.

    Top