| HS Code | 879933 |
| Density | 0.949 g/cm³ |
| Melt Flow Rate | 0.30 g/10min (190°C/5kg) |
| Tensile Yield Strength | ≥23 MPa |
| Elongation At Break | ≥600% |
| Flexural Modulus | ≥1000 MPa |
| Notched Impact Strength | ≥20 kJ/m² |
| Vicat Softening Temperature | ≥120 °C |
| Brittleness Temperature | ≤-70 °C |
| Oxidation Induction Time | ≥20 min |
| Carbon Black Content | 2.0-2.5% |
| Environmental Stress Cracking Resistance | ≥5000 h |
| Moisture Content | ≤0.05% |
| Ash Content | ≤0.1% |
| Bulk Density | ≥0.50 g/cm³ |
| Color | Black |
| Form | Pellet |
| Processing Method | Extrusion |
| Mrs Rating | PE100 |
| Long Term Hydrostatic Strength | 10.0 MPa |
As an accredited Yanchang China Coal Yulin (Shaanxi) HDPE PN049-030-122 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Yanchang China Coal Yulin (Shaanxi) HDPE PN049-030-122 is supplied in 25 kg woven bags, 40 bags per pallet (1,000 kg). |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): Yanchang China Coal Yulin (Shaanxi) HDPE PN049-030-122, 25kg bags, palletized, shrink-wrapped, securely stowed for export. |
| Shipping | Yanchang China Coal Yulin (Shaanxi) HDPE PN049-030-122 is shipped as a non-hazardous thermoplastic resin in 25 kg PP woven bags or 500–1000 kg jumbo bags, palletized and stretch-wrapped. Transport by sea, rail, or truck; store cool, dry, ventilated, away from sunlight, heat, and moisture. |
| Storage | Store Yanchang China Coal Yulin (Shaanxi) HDPE PN049-030-122 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, and ignition sources. Keep original packaging sealed and palletized to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Maintain clean, ambient conditions and separate from oxidizers, acids, and incompatible materials. Use first-in, first-out stock rotation. |
| Shelf Life | Shelf life is typically 24 months when stored in original packaging, cool, dry, ventilated area, protected from sunlight and moisture. |
In municipal water distribution mains, the melt flow index of 0.30 g/10 min at 190 °C under 5.0 kg load and the density of 0.949 g/cm³ measured by ISO 1183-1 place this bimodal reactor grade inside the PE100 pipe segment. The resin is processed on single-screw extruders with grooved feed bushings, barrier screws and L/D ratios of 30–36. Barrel zone temperatures rise from 180 °C in the feed section to 210–225 °C in the metering section, while the pipe head is held at 210–220 °C. Melt temperature must stay below 230 °C to avoid oxidative consumption of the phenolic stabilizer package measured by ISO 11357-6. Screen packs of 40/60/80 mesh are installed upstream of the breaker plate, and melt pressure on a 60 mm grooved-barrel line normally remains between 18 MPa and 25 MPa. Vacuum calibration tanks operate at 0.02–0.04 MPa, and cooling water is controlled to 15–20 °C. Carbon black masterbatch is added at 2.0–2.5 wt% to give a final carbon black content of 2.0–2.5 wt% for UV resistance. No pre-drying is necessary when storage humidity remains below 60% RH; if surface moisture appears, the pellets are dried at 70–80 °C for 2 h. Pipes are normally produced in SDR 11 and SDR 17 dimensions, with nominal pressure ratings of 16 bar and 10 bar at 20 °C for water service, using the MRS 10 MPa classification under ISO 12162. Hydrostatic qualification by ISO 1167-1 requires no leakage at 20 °C/100 h and 80 °C/165 h on DN 110 mm specimens. Slow crack growth resistance is checked by the notched pipe test ISO 13479 at 80 °C. Potable water certification under NSF/ANSI 61 or AS/NZS 4020 is compound-specific and is not automatically inherited when masterbatch or processing aids are changed. For water distribution loops and industrial transfer mains, ovality after sizing should remain below 2% after 24 h of cooling, and the inner surface roughness is normally specified below Rz 20 µm to limit biofilm adhesion.
For natural gas distribution mains, the same MRS 10 MPa classification applies, but the design coefficient C=2.0 in ISO 4437-1 reduces the maximum operating pressure of SDR 11 pipe to 10 bar at 20 °C. The extrusion line differs in one critical detail: the outer layer must be black, or black with co-extruded yellow identification stripes, and regrind incorporation is limited to clean internal scrap at a maximum of 10 wt%. Carbon black final content is held at 2.0–2.5 wt% and dispersion is assessed by ISO 18553 at a rating of A-1 or A-2. Barrel temperatures are shifted down by 5–10 °C relative to water pipe to minimize thermal oxidation, with the die head maintained at 205–215 °C and melt temperature checked at 210–220 °C. Slow crack growth testing under ISO 13479 is mandatory, and rapid crack propagation resistance is evaluated by ISO 13477 at 0 °C to verify crack arrest in refrigerated backfill conditions. Finished pipe is subjected to elongation at break testing per ISO 6259-1 and resistance to gas constituents per ISO 4437-2. The minimum installation temperature for full wall-thickness manipulation is typically -5 °C, while impact resistance at -25 °C is verified by ISO 3127. The process window is narrower than for water pipe because sustained melt temperature above 220 °C can generate low-molecular-weight volatiles that affect the manufacturer’s internal quality specification; published data for this specific grade under gas utility odor panel testing is limited. Pre-drying is not normally required below 60% RH, but outdoor silo storage should be monitored because wet pellet surfaces can generate pinholes during the pipe skin solidification stage.
| Pipe service | Governing standards | Qualification test | Acceptance condition |
|---|---|---|---|
| Water pressure main | ISO 4427-1, EN 12201-1 | ISO 1167-1 hydrostatic | No leakage at 20 °C/100 h and 80 °C/165 h |
| Gas distribution main | ISO 4437-1, EN 1555-1 | ISO 13477 rapid crack propagation | Arrest at 0 °C above design pressure |
Structured-wall drainage pipes with corrugated outer profiles are produced on corrugators that apply vacuum to the melt block. The high zero-shear viscosity derived from the 0.30 g/10 min melt flow index resists parison sag, but it also narrows the melt-fracture-free shear rate window. Die gaps are set 1.0–1.8 mm larger than the target corrugation valley thickness, and vacuum draw for the inside mandrel is held at 0.02–0.04 MPa. Blow air for the mold block is supplied at 0.02–0.05 MPa, and mold block temperature is kept at 20–40 °C. The extrusion temperature profile runs from 170 °C in the grooved feed section to 195–210 °C at the die, which is 10–15 °C lower than solid-wall pressure pipe to preserve melt elasticity. Screw speed and corrugator speed are synchronized to a tolerance of ±0.5% to prevent axial wall-thickness drift. Compliance is assessed under EN 13476-1, GB/T 19472.1, and ASTM F2306/F2306M. Ring stiffness is classified into SN 4 kN/m² and SN 8 kN/m² grades, and the inner wall thickness is usually 0.6–1.2 mm for DN 200–800 mm pipe. In production monitoring, melt fracture is identified by transverse surface roughness with a roughness depth above 20 µm when measured by stylus profilometry. The correction is either a die temperature increase of 5 °C or a screw speed reduction of 10%. Pre-drying is omitted below 60% RH; above that, hopper drying at 70 °C for 2 h prevents pinholes from trapped moisture. The finished product is applied to stormwater drainage, agricultural runoff collection, and culvert relining, where the structured wall provides crush resistance under shallow soil cover without solid-wall thickness penalties.
Large tight-head drums and intermediate bulk container inner bottles require high melt strength during accumulator-head extrusion. The resin is processed at melt temperatures of 185–210 °C in the accumulator head and 170–200 °C in the extruder barrel; head pressure before the parison die typically ranges from 10 MPa to 18 MPa. Parison programming must hold wall distribution within ±0.3 mm for a 220 L tight-head drum weighing 8.5–10.5 kg. Blow air is supplied at 0.6–1.0 MPa, and the mold is cooled with water at 10–25 °C to achieve cycle times of 120–180 s depending on part weight and wall thickness. The pinch-off zone must be maintained at 200–215 °C to obtain an integral weld line; a cold pinch-off below 180 °C produces a weak tail weld and increases drop-test failures under UN 1H1 type approval. Regrind from flash and rejected drums is incorporated at up to 20 wt% if the flake is dried to below 0.05 wt% moisture and screened through a 2 mm mesh. Food-contact status is not automatic for every lot; drums intended for food or pharmaceutical service must be verified against FDA 21 CFR 177.1520 and EU 10/2011 with specific migration testing under EN 1186-1. The high melt viscosity limits the grade to containers above 50 L; for bottles below 10 L, the long cycle time and elevated melt temperature create an uncompetitive process window. Published data for the exact parison swell ratio of this grade on accumulator-head machines is limited, so pre-production trials on the target mold are mandatory before setting die gap and parison weight programs.
Geomembrane liners for landfill basal and capping systems are extruded through flat dies with die widths of 5–8 m and thickness targets from 1.0 mm to 2.5 mm. The resin’s 0.30 g/10 min melt flow index at 190 °C/5 kg suppresses draw resonance on long melt curtains, but requires a die gap of 2.0–2.5 mm to prevent die-lip build-up. The flat-die temperature is set at 200–215 °C, and the polishing stack rolls are held at 70–90 °C to obtain a calendered surface. Edge trim is grinder-flaked to below 2 mm and dosed back into the feed throat by a gravimetric blending unit at 20–35 wt%. The melt filter is a screen changer with a 100–150 µm filtration layer; at regrind levels above 35 wt%, gel counts rise and require filter changes every 30–60 min. Final sheet testing includes tensile yield strength per ASTM D638 Type IV, tear resistance per ASTM D1004, puncture resistance per ASTM D4833, and oxidative induction time per ASTM D3895. Carbon black content is kept at 2.0–3.0 wt% with dispersion rated A-1 or A-2 according to ISO 18553. Geomembrane specification is normally written against GRI-GM13 or ASTM D7436, and the resin lot must be pre-qualified for the specified minimum average roll value of stress crack resistance under ASTM D5397. In exposed liner service, the lower melt flow index reduces the need for excessive edge bead support because the melt curtain retains dimensional stability across the full die width. The main production limitation is gel formation from recycled edge trim, which appears as pinhole-prone regions if the screen changer is not maintained or if regrind particle size distribution exceeds 2 mm.
Corrugated and smooth-wall cable protection ducts are extrusion-formed with a single-screw line running barrel temperatures from 180 °C to 210 °C and die temperatures of 200–215 °C. Vacuum calibration is set at 0.02–0.04 MPa, and cooling water is held at 15–20 °C. In corrugated duct production, the corrugator mold blocks close at 20–40 °C and blow air is maintained at 0.02–0.05 MPa; haul-off and corrugator speeds are synchronized to within ±0.5% to maintain pitch stability. Impact resistance at -25 °C is verified by IEC 60068-2-75 spring hammer tests, and ring stiffness is measured according to ISO 9969. Compliance for conduits is assessed under IEC 61386-24, EN 50086-2-4, UL 651, and NEMA TC 7. The material is usually black with carbon black at 2.0–2.5 wt%; if red or orange identification is required, a PE-based masterbatch is added at 4–6 wt%, but the pigment change can reduce weathering stability unless the masterbatch contains a hindered amine light stabilizer package. The smooth inner wall lowers cable pull force, and the high molecular weight of the compound provides crush resistance without brittleness in trench-load conditions. Pre-drying is normally unnecessary below 60% RH; however, wet pellets from outdoor silo storage should be dried at 70 °C for 2 h before the hopper to avoid microvoids in the outer corrugation crests. Finished ducts from this resin are used for underground power cable protection, fiber-optic conduit networks, and low-voltage distribution sleeves, where the combination of ring stiffness and impact retention at low temperature determines the laying depth and backfill compaction limit.
Competitive Yanchang China Coal Yulin (Shaanxi) HDPE PN049-030-122 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Yanchang China Coal Yulin (Shaanxi) HDPE PN049-030-122 is a high-density polyethylene pipe extrusion resin produced at the Yulin, Shaanxi petrochemical manufacturing site. The designation is consistent with a nominal density of 0.949 g/cm³ and a nominal melt mass-flow rate of 0.30 g/10 min when measured at 190 °C under 5.0 kg load in accordance with ISO 1133-1:2022. The material is positioned as a PE100 pressure-pipe resin, meaning that its long-term hydrostatic strength classification is referenced to a lower confidence limit of 10.0 MPa at 20 °C for 50 years under the stress-rupture methodology of ISO 9080 and the classification rules of ISO 12162. The base polymer is supplied as stabilized pellets with a bimodal high-density molecular architecture. This architecture is intended to combine high melt strength during large-diameter pipe extrusion with resistance to slow crack growth in buried service. The PN049-030-122 suffix is a production specification identifier and does not by itself constitute a pipe-system approval. Published data for this specific configuration outside supplier-controlled documentation is limited; the values cited herein are typical pellet specifications only and are not finished-pipe design values.
The following values are typical for the base resin at the time of production and are not to be used as minimum or maximum release limits without reviewing a supplier batch certificate.
| Property | Test method | Unit | Typical value |
|---|---|---|---|
| Density | ISO 1183-1 | g/cm³ | 0.949 |
| Melt mass-flow rate at 190 °C / 5.0 kg | ISO 1133-1:2022 | g/10 min | 0.30 |
| Tensile stress at yield | ISO 527-2, 50 mm/min | MPa | 25 |
| Tensile elongation at break | ISO 527-2, 50 mm/min | % | >600 |
| Charpy notched impact strength at 23 °C | ISO 179-1/1eA | kJ/m² | 30 |
| Charpy notched impact strength at -30 °C | ISO 179-1/1eA | kJ/m² | 12 |
| Vicat softening temperature | ISO 306/A50 | °C | 123 |
| Carbon black content in black compound | ISO 6964 | % by mass | 2.0–2.5 |
| Oxidation induction time at 210 °C | ISO 11357-6 | min | ≥20 |
Because the melt mass-flow rate is low at 0.30 g/10 min, the resin exhibits comparatively high melt viscosity and pronounced shear thinning. Extrusion on single-screw machines with grooved feed sections and barrier screws is required for stable output. Barrel temperatures from feed throat to metering zone are commonly set between 190 °C and 220 °C, while adapter and die head zones are maintained between 200 °C and 225 °C. Melt temperature should not exceed 230 °C; above this threshold, oxidative chain scission can reduce long-term hydrostatic strength even if visible defects are absent. Residence time above 220 °C should be kept below 10 minutes. Regrind addition is possible up to 20% by mass, but each regrind ratio should be validated by pipe-level hydrostatic testing because resin certification does not cover reprocessed material.
On production-scale single-screw extruders with L/D 30:1 to 36:1, the grade typically requires a high-torque drive and grooved feed bush to prevent feeding instability at high head pressures. Spiral mandrel dies with a minimum of 8 to 12 spiral channels are preferred for pipes above 250 mm outside diameter to minimize weld-line sensitivity. Melt pressure before the breaker plate should be monitored continuously; excursions above 250 bar on a 60 mm extruder operating at 60–80 rpm may indicate excessive melt viscosity or insufficient die temperature and can lead to sharkskin surface defects. Increasing the die temperature by 5–10 °C or reducing throughput is the usual corrective action.
Vacuum calibration is performed with water temperatures between 20 °C and 40 °C. For thick-wall pressure pipes above 32 mm wall thickness, internal bubble cooling is sometimes necessary to prevent differential shrinkage and ovality. Because the material has high melt strength, sagging in large-diameter pipes is lower than with conventional unimodal PE80 resins; however, pipe wall thickness eccentricity remains controlled primarily by die centering and haul-off uniformity. Routine dimensional inspection should follow ISO 3126, and finished pipes should be subjected to ISO 1167 hydrostatic pressure testing at the specified service temperature and wall stress.
HDPE does not normally require drying under closed silo storage below 60% RH. If surface condensation occurs from storage below 0 °C or from high-humidity ambient exposure, the pellets should be brought to ambient temperature and dried at 80 °C for 2 hours using desiccant air to prevent melt voids and surface pitting. Moisture content above 0.05% by weight is to be avoided before extrusion because it generates hydrolytic surface defects and can destabilize bubble or vacuum calibration.
PE80 resins are classified under ISO 12162 with a minimum required strength of 8.0 MPa at 20 °C for 50 years, whereas PE100 resins such as PN049-030-122 carry an MRS of 10.0 MPa. This permits a higher pressure rating at equal wall thickness, or a reduced wall thickness at equal pressure rating. In contrast to many general-purpose HDPE blow-moulding resins with similar melt flow rates, the PN049-030-122 grade has a lower density of 0.949 g/cm³ and a specifically broadened molecular weight distribution. The high-molecular-weight tail increases slow crack growth resistance in notched pipe tests, while the low-molecular-weight fraction provides processability and shear thinning.
Compared with unimodal HDPE grades of similar density, the bimodal distribution produces higher melt tension and lower sag under its own weight, which is critical for large outside diameter pipe above 315 mm. However, the low melt mass-flow rate may require screw speed reductions of approximately 10–20% when switching from PE80 tooling to avoid overloading the extruder drive. The reduction in output should be established empirically on the specific line because it depends on screw geometry, filter pack, and die backpressure. Pipe extruders originally designed for PE80 with higher MFR may require a longer four-zone barrel profile and a higher torque motor to maintain acceptable throughput.
The principal differentiation from lower-performance PE80 pipe grades appears in slow crack growth resistance under ISO 13479 notched pipe testing and in resistance to rapid crack propagation under ISO 13477. This supports use in trenchless installation methods such as horizontal directional drilling and pipe bursting, where external scoring and point loading can occur. For buried water and gas mains, the higher MRS allows designers to specify thinner walls and still meet the required pressure class under ISO 4427 or ISO 4437.
As a PE100-class product, PN049-030-122 is intended to meet the ISO 9080 regression requirements at 20 °C and 60 °C for internal pressure testing. The lower confidence limit of 10.0 MPa at 20 °C for 50 years is the classification basis, not a continuous operating stress. Actual design stress is reduced by temperature derating factors given in ISO 13760, by service coefficients, and by pipe-system standards. For potable water systems designed under ISO 4427, the maximum allowable operating pressure is determined by the pipe dimension ratio and the derated hydrostatic design stress.
Slow crack growth is the dominant failure mode in buried pressure pipe under long-term low-level stress. The resin is evaluated by notched pipe testing under ISO 13479 at 80 °C, and resistance to rapid crack propagation is assessed under ISO 13477 at 0 °C. These tests are pipe-level evaluations; pellet-level mechanical values such as Charpy impact and tensile elongation are indicative but are not substitutes for hydrostatic classification. Processors should not infer long-term performance from melt flow rate or density alone.
The black compound containing 2.0–2.5% carbon black provides ultraviolet stabilization for outdoor storage and direct buried installation. Natural or colored variants require separate light stabilization if stored outdoors for extended periods. Above-ground installations are not recommended without thermal insulation or mechanical shielding because elevated pipe wall temperatures reduce the allowable design stress. In chlorinated potable water above 60 °C, published data for this specific configuration is limited, and no continuous service classification should be inferred without specific hydrostatic certification.
Chemical service is restricted to fluids for which polyethylene has established compatibility. Continuous exposure to strong oxidizing acids, aromatic hydrocarbons, oxygenated fuels, or high concentrations of free chlorine can promote environmental stress cracking and swell the pipe wall. Industrial pressure piping may be specified under ISO 15494 only after a chemical resistance review is completed for the specific fluid, temperature, and service life. The resin grade is produced without heavy-metal stabilizers and is intended to support assessment under EU REACH substance restrictions; however, finished pipe compliance with potable water contact regulations such as NSF/ANSI/CAN 61 must be demonstrated at the pipe-product level because resin certification alone is not sufficient. For food-contact applications, the base olefin polymer may be assessed under FDA 21 CFR 177.1520, but colorants, additives, and regrind must be separately evaluated.