| HS Code | 591550 |
| Density | 0.944 g/cm³ |
| Melt Flow Rate | 11 g/10 min (190°C/2.16 kg) |
| Tensile Strength At Yield | 27 MPa |
| Elongation At Break | >500% |
| Flexural Modulus | 1100 MPa |
| Notched Izod Impact Strength | 50 J/m (23°C) |
| Vicat Softening Temperature | 120°C |
| Heat Deflection Temperature | 75°C (0.45 MPa) |
| Shore D Hardness | 65 |
| Melting Point | 130°C |
| Water Absorption | <0.01% |
| Volume Resistivity | >10^16 Ω·cm |
| Dielectric Constant | 2.3 |
| Form | Pellets |
| Color | Natural |
| Odor | Odorless |
As an accredited Yanchang China Coal Yulin (Shaanxi) HDPE K44-11-128 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Yanchang China Coal Yulin (Shaanxi) HDPE K44-11-128 is packaged in 25 kg polyethylene-lined woven bags on pallets. |
| Container Loading (20′ FCL) | 20′ FCL container loading of Yanchang China Coal Yulin (Shaanxi) HDPE K44-11-128, bagged, palletized, and securely sealed for standard export. |
| Shipping | Yanchang China Coal Yulin (Shaanxi) HDPE K44-11-128 is a non-hazardous polyethylene resin. It is shipped in 25 kg bags or 500–1000 kg jumbo bags, palletized and stretch-wrapped. Transport in dry containers, trucks, or rail at ambient temperature. Keep dry, cool, ventilated, away from sunlight and contamination. |
| Storage | Store Yanchang China Coal Yulin (Shaanxi) HDPE K44-11-128 in a cool, dry, well-ventilated warehouse at ambient temperature, away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags sealed and palletized; prevent moisture, dust, oil, and chemical contamination. Avoid excessive stacking to prevent deformation. Follow first-in-first-out rotation and good housekeeping. |
| Shelf Life | Shelf life is generally 24 months when stored cool, dry, ventilated, away from direct sunlight, in unopened original packaging. |
For extrusion blow moulding of 25 L to 200 L tight-head and open-top HDPE drums, the parison formation stage imposes the primary processing boundary rather than downstream filling or stacking performance. A low-melt-index HDPE resin in the 0.944 g/cm³ to 0.950 g/cm³ density band and melt index between 0.10 g/10 min and 0.35 g/10 min at 2.16 kg and 190 °C according to ASTM D1238-20 prolongs parison hang time and improves wall distribution in tall containers. During machine start-up on an accumulator-head blow moulder with 24:1 to 30:1 L/D barrier screw and grooved feed, die head pressure typically stabilises between 15 MPa and 35 MPa when the die gap is held at 1.5 mm to 2.8 mm. Parison swell of 18% to 40% at the die exit requires the mould parting-line flash pocket depth to be maintained at 0.3 mm to 0.8 mm; otherwise pinch-off weld tailing produces weak bottom corners and base-channel failure under stacking load. Drum pinch-off weld integrity is evaluated destructively by sectioning the weld and measuring minimum wall thickness after trimming, with acceptance based on absence of visible porosity at 10× magnification. Mould temperature is controlled between 10 °C and 40 °C, and cooling time for a 200 L drum with nominal wall 1.5 mm to 2.0 mm ranges from 60 s to 120 s. Finished drums in dangerous-goods service are subjected to the UN Model Regulations Chapter 6.1 drop test after conditioning at -18 °C for 24 h, and hydraulic pressure testing at 100 kPa for 30 min. Environmental stress-crack resistance is measured by ASTM D1693-15ε1 in 100% Igepal CO-630 at 50 °C; industrial chemical drums routinely require an F50 value above 100 h to avoid premature base-channel cracking. The use of post-industrial regrind beyond 30 wt% is not recommended without validating ESCR retention because low-molecular-weight fractions from degraded scrap reduce tie-molecule density and promote brittle failure. Pre-drying is not normally required at ambient relative humidity below 60%, but surface condensation on pellets stored in unheated silos should be managed by hopper preheat at 60 °C to 70 °C to prevent micro-void defects at the parison surface.
Long-stroke blow moulding of enclosed technical reservoirs such as windshield washer tanks, coolant overflow bottles and diesel exhaust fluid containers requires a melt index low enough to resist parison sag but high enough to avoid excessive backpressure during accumulator discharge. The operating window is defined by parison length, which can exceed 1.0 m for large under-hood reservoirs, and by pinch-off weld thickness at the mould parting line. When the melt index falls below 0.20 g/10 min at 2.16 kg and 190 °C per ASTM D1238-20, accumulator pressure requirement rises because of higher extensional viscosity; when it rises above 0.40 g/10 min, parison sag creates wall thinning below 1.2 mm in vertical sections. Parison programming with 80-point to 120-point wall thickness control is applied along the stroke, with die gap modulation between 0.8 mm and 2.2 mm. The pinch-off land angle is specified between 15° and 30°, and the flash pocket is vented to avoid trapped air that causes burn marks at the weld. For diesel exhaust fluid reservoirs, continuous exposure to 32.5 wt% urea solution at temperatures up to 60 °C requires high environmental stress-crack resistance; testing under ASTM D1693-15ε1 in 100% Igepal CO-630 at 50 °C is used as a screening surrogate, with acceptance thresholds above 300 h in some automotive tier-1 supply chains. Low-temperature ductility is assessed by drop impact testing at -30 °C after 24 h conditioning; absence of complete fracture at 3 J to 6 J impact energy is commonly specified for windshield washer reservoirs. Mould temperature is maintained at 15 °C to 35 °C using closed-loop chillers, and blow air pressure is set between 0.6 MPa and 0.9 MPa to force the parison into sharp radii without inducing blowout. Because aqueous urea systems can promote stress cracking in HDPE with low tie-molecule density, regrind content is limited to 20 wt% unless batch-specific ASTM D1693-15ε1 data confirm otherwise. Published data for K44-11-128 in this specific application configuration is limited; production validation must include a full mould trial to map wall thickness distribution and pinch-off strength under production-scale accumulator discharge speeds.
Under sustained internal pressure at 20 °C and 60 °C, the long-term hydrostatic strength of an HDPE pipe material is determined by extrapolating tube failure data according to ISO 9080:2012, but published data for K44-11-128 in PE100 or PE4710 certification is limited. Consequently the grade is more conservatively assessed in non-pressure gravity sewer, land drainage, cable ducting and corrugated culvert applications where hoop stress remains below 2 MPa and long-term pressure creep is not the governing design limit. Pipe extrusion on a 30:1 L/D grooved-feed extruder with barrier screw is run at melt temperatures of 190 °C to 210 °C; die head pressures between 20 MPa and 30 MPa are typical for low-melt-index HDPE at screw speeds of 40 min⁻¹ to 80 min⁻¹. The critical wall shear stress for sharkskin melt fracture in HDPE is generally observed between 0.14 MPa and 0.25 MPa; therefore the die land length and mandrel exit gap are selected so that local shear stress remains below 0.14 MPa if a smooth inner surface is required. Vacuum calibration is operated at 20 kPa to 60 kPa negative pressure with water-spray cooling at 15 °C to 25 °C; the resulting crystallinity distribution affects circumferential shrinkage and must be controlled to maintain outside diameter tolerance of 0.3 mm to 0.5 mm for small-diameter conduits. Oxidation induction time measured by ASTM D3895-19 at 200 °C is commonly required above 20 min for pipe formulations containing hindered phenolic and phosphite stabilisers, while carbon black dispersion in black pipe is assessed according to ISO 18553 to prevent agglomerate-induced cracks. Short-term burst testing under ASTM D1598-15 and long-term hydrostatic design basis calculation according to ASTM D2837-13ε1 are required for any pressure application; without a resin-specific hydrostatic database, assigning a pressure rating to K44-11-128 is not technically defensible. Weldability in butt fusion is assessed through bead appearance and bend-back tests after joining at 220 °C to 230 °C and 0.15 MPa interfacial pressure; low-melt-index HDPE generally produces a stable melt bead, but excessive molecular weight can increase insertion force and reduce melt flow into the joint gap.
When flat-die extrusion is run beyond 2.0 mm nominal thickness for HDPE geomembrane, edge waviness and transverse gauge uniformity become the critical process limits because the melt curtain is sensitive to draw resonance and roll-stack temperature gradients. A 120 mm to 200 mm single-screw extruder with 30:1 L/D barrier screw feeds a coat-hanger or fishtail die of 2.4 m to 8.0 m width, with die gap set between 2.0 mm and 3.0 mm. Melt temperature is controlled at 210 °C to 230 °C, and the melt curtain is drawn down through a three-roll stack with a draw ratio of 1.2 to 1.6; increasing the draw ratio tightens thickness tolerance but raises orientation anisotropy. Exact gauge control is required by GRI-GM13, with average thickness tolerance of ±10% and minimum individual readings not below -10% of nominal. Textured surface asperity height is specified between 0.25 mm and 0.75 mm by embossed rolls, and the sheet is quenched to 70 °C to 100 °C before pulling through a cooling conveyor. Environmental stress-crack resistance of geomembrane formulations is evaluated by notched constant tensile load testing under ASTM D5397-19; typical HDPE geomembrane acceptance values exceed 300 h in 10% Igepal CO-630 at 50 °C, although higher-performance specifications can require above 500 h. Oxidative induction time determined by ASTM D5885/D5885M-20 at 200 °C is required above 100 min for standard geomembranes, while high-pressure oxidative induction time above 400 min may be required for exposed liner applications. Carbon black loading between 2 wt% and 3 wt% with good dispersion according to ISO 18553 is maintained to suppress ultraviolet degradation, but the exact K44-11-128 stabiliser package should be confirmed because insufficient carbon black dispersion creates stress concentrations at film crystallite boundaries. Weld windows for hot-wedge and extrusion fillet welding are established on production seams using shear and peel tests per ASTM D6392 and ASTM D4437; seam strength must exceed 80% of parent-sheet yield strength.
| Application | Standard/Code | Test method or clause | Typical acceptance value |
|---|---|---|---|
| Industrial drums, dangerous goods | UN Model Regulations Chapter 6.1 | Drop test at -18 °C, hydraulic pressure | 1.2 m drop; 100 kPa/30 min |
| Industrial drums, ESCR | ASTM D1693-15ε1 | 100% Igepal CO-630, 50 °C | F50 > 100 h |
| Food-contact olefin polymers | FDA 21 CFR 177.1520 | Olefin polymer specification | Per 21 CFR 177.1520(c) 3.1a |
| Pipe long-term hydrostatic strength | ISO 9080:2012 | 20 °C / 60 °C extrapolation | Requires grade-specific hydrostatic database |
| Geomembrane stress cracking | ASTM D5397-19 | Notched constant tensile load, 10% Igepal | > 300 h |
| Oxidative induction time | ASTM D5885/D5885M-20 | DSC at 200 °C | > 100 min |
| Injection moulding shrinkage | ASTM D955-08 | 24 h after demoulding | 1.5%–2.5% MD |
Where low-melt-index HDPE is pushed into thick-wall injection moulding, the processing envelope narrows around short-shot prevention and internal void formation rather than cycle time alone. HDPE K44-11-128 may be processed in industrial crates, pallets, machine housings and dunnage components with nominal wall thickness above 4.0 mm because low melt flow increases filling resistance but also reduces flash formation at the parting line. The barrel temperature profile is set from rear 200 °C, centre 220 °C, front 230 °C to nozzle 240 °C, and the mould is controlled between 20 °C and 50 °C. Injection pressure required for thick-section flow typically falls between 80 MPa and 140 MPa, while hold pressure is maintained at 50 MPa to 80 MPa for 15 s to 40 s depending on gate freeze-off time. Full-round runner diameters of 8 mm to 12 mm and tab or edge gates with thickness 50% to 75% of the part wall are used to reduce shear heating; vent depth is held between 0.015 mm and 0.030 mm to allow gas escape without flash. Mould shrinkage after 24 h according to ASTM D955-08 is expected in the range of 1.5% to 2.5% in the flow direction and 1.0% to 2.0% transverse; thick sections exhibit greater volumetric shrinkage and sink marks if hold pressure is terminated before gate freeze. Long residence times above 10 min at 240 °C can initiate chain scission and increase yellowness; processing should be interrupted and purged if machine faults extend beyond that window. Notched Izod impact strength measured by ASTM D256-10(2018) is generally ductile at 23 °C, but low-temperature impact at -30 °C must be confirmed on moulded plaques because specimen geometry and weld-line location influence failure mode. Injection moulding of parts below 2.5 mm wall thickness with this low-melt-index resin is not recommended, and published moulding data for the K44-11-128 configuration is limited to general HDPE grades unless a production-scale trial is documented.
Extruded HDPE sheet in the 2 mm to 8 mm thickness range is subsequently vacuum formed into dunnage trays, material handling liners and protective panel covers, where the low-sag character of a low-melt-index resin permits wider sheet spans. Sheet extrusion is conducted at melt temperature 200 °C to 220 °C through a flat die with gap 2 mm to 6 mm; the roll stack is held at 80 °C to 100 °C to prevent rapid surface quenching before gauge is set. During forming, the sheet core temperature is brought to 150 °C to 170 °C, which is above the crystalline melting region of HDPE but below oxidative degradation onset for unstabilised surfaces. The mould temperature is maintained between 30 °C and 60 °C, and vacuum is applied at 60 kPa to 80 kPa; plug assist speed is limited to 0.5 m/s to 1.5 m/s to avoid local plug marks and wall thinning below 1.5 mm. Post-form shrinkage measured after 48 h at ambient temperature commonly ranges from 1.2% to 2.0%, and annealing at 100 °C for 30 min reduces subsequent distortion in service. Tensile properties of formed sheet are tested according to ISO 527-2:2012, while flexural modulus is measured under ISO 178:2019; typical HDPE sheet values for flexural modulus fall between 800 MPa and 1,200 MPa, but K44-11-128-specific data must be drawn from the producer certificate or an independent laboratory report. Incompatibility with flame treatment should be considered when adhesive bonding is required, because excessive surface oxidation above 44 mN/m wetting tension can create a weak boundary layer; corona or plasma treatment is preferred for adhesion promotion on HDPE sheet. Recycled sheet trim can be reintroduced at up to 25 wt% if the regrind is dust-free and the melt filter screen stack includes screens of 80 mesh to 120 mesh to remove gels.
Competitive Yanchang China Coal Yulin (Shaanxi) HDPE K44-11-128 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
The high-density polyethylene grade K44-11-128 is supplied by Yanchang China Coal Yulin Energy & Chemical Co., Ltd. as a pipe-extrusion resin. The designation is associated in trade literature with a bimodal high-density polyethylene in the PE100 class, but independently published values for the exact K44-11-128 formulation are limited outside the producer’s controlled documents. The supplier’s certificate of analysis therefore governs lot-specific density, melt flow rate, tensile properties, oxidative induction time, and hydrostatic design basis. Pipe processors typically evaluate the material against ISO 9080, ISO 1167, ISO 4427-2, and ISO 13479; the resin is not intended for injection moulding or blown film operations. The principal end uses are pressure water mains, gas distribution lines, industrial process water, and mining slurry or dredge pipelines operated at derated pressures. Black pipes produced from this grade normally contain 2.0–2.5% carbon black by mass according to ISO 4427-1 requirements for ultraviolet resistance.
The measured properties that define K44-11-128 for pressure-pipe service include density, melt flow rate, yield stress, and resistance to slow crack growth. For bimodal PE100 pipe resins, density is generally controlled between 0.958 g/cm³ and 0.962 g/cm³ at 23 °C when tested by ISO 1183-1. The melt flow rate at 190 °C under 5 kg is typically 0.20–0.30 g/10 min, while the high-load melt flow rate under 21.6 kg may be reported to characterize processability. A low-load melt flow rate in this range is associated with high molecular weight and high melt strength, which are necessary for large-diameter thick-wall pipe extrusion.
The exact molecular weight distribution of K44-11-128 is not disclosed in independent public data. Bimodal pipe grades achieve a balance between processability and toughness by combining a low-molecular-weight fraction with a high-molecular-weight fraction; the latter contains short-chain branching introduced by a comonomer, but the specific comonomer type used in K44-11-128 should be confirmed from the producer’s technical datasheet. This bimodal architecture differs from unimodal high-density polyethylene grades, which generally show either lower extrusion output or lower long-term creep resistance at equivalent melt flow rate.
| Property | Test method | Typical range |
|---|---|---|
| Density at 23 °C | ISO 1183-1 | 0.958–0.962 g/cm³ |
| Melt flow rate at 190 °C, 5 kg | ISO 1133-1 | 0.20–0.30 g/10 min |
| Tensile stress at yield | ISO 527-2 | 23–27 MPa |
| Elongation at break | ISO 527-2 | >600% |
| Flexural modulus | ISO 178 | 900–1200 MPa |
| Notched Charpy impact at 23 °C | ISO 179-1 | >20 kJ/m² |
| Thermal oxidative induction time at 210 °C | ISO 11357-6 | >20 min |
On grooved-feed single-screw pipe extrusion lines, K44-11-128 is processed with barrel temperatures from 180 °C to 220 °C. The grooved feed throat provides positive solids conveying and reduces the dependence of output on backpressure; screws with 30:1 to 36:1 length-to-diameter ratios are standard. The melt temperature at the die entry is maintained between 190 °C and 230 °C. Operation above 240 °C for prolonged residence times can reduce oxidative induction time, generate gels, and shift the long-term hydrostatic strength regression line. Barrel purge procedures after shutdown are therefore part of standard operation, particularly for diameter changes or color changes.
Die head temperatures are commonly set at 200–220 °C to balance wall-thickness control against die drool. Head pressure in grooved-feed extrusion of high-viscosity high-density polyethylene is frequently observed in the range 20–35 MPa, depending on die land length, melt temperature, and output rate. Vacuum sizing pressures of -0.02 MPa to -0.06 MPa and water-bath temperatures from 10 °C to 20 °C are used to fix outside diameter and wall thickness. Wall-thickness variation in thick-wall pipe is often caused by non-uniform melt temperature at the crosshead die; a melt pump is recommended when wall-thickness tolerances below ±0.2 mm are required for SDR 17 and higher SDR classes. Pre-drying is not required for normal ambient storage at relative humidity below 60%; if surface condensation occurs after outside storage or abrupt temperature changes, 80 °C for 4 h is applied before extrusion.
When hydrostatic design stress controls wall-thickness selection, the governing classification method is ISO 9080. Internal pressure tests under ISO 1167 are conducted at multiple temperatures, commonly 20 °C, 40 °C, 60 °C, and 80 °C, with hoop stresses selected to produce ductile and brittle failures. Regression of the log stress–log time data yields the lower prediction limit σ_LPL at 20 °C and 50 years. A PE100 classification requires σ_LPL ≥ 10.0 MPa, using the 97.5% lower prediction limit. The design stress for water at 20 °C is obtained by dividing the minimum required strength by a service coefficient C of 1.25, giving 8.0 MPa. This lower confidence limit is not a simple tensile value; it is derived from long-term hydrostatic failure data and therefore reflects creep rupture, slow crack growth, and processing history.
For the same SDR 11 dimension at 110 mm outside diameter, the maximum allowable operating pressure at 20 °C is 1.6 MPa for PE100 and 1.28 MPa for PE80. The wall thickness at SDR 11 is 10.0 mm. At temperatures above 20 °C, pressure derating factors in ISO 4427-1 must be applied; chlorinated water distribution may require additional project-specific validation because chlorine can reduce slow crack growth resistance. The low melt flow rate of K44-11-128 supports thick-wall processing but reduces line speed relative to lower-molecular-weight pipe grades. Pipe diameter changes and long-term shutdowns require purging with a lower-viscosity high-density polyethylene to avoid stagnant material accumulation in the die head.
For pressure-pipe service in poorly compacted embedment, rock impingement, or trenchless installation, long-term brittle failure is governed by slow crack growth rather than homogeneous creep rupture. The notched pipe test ISO 13479 applies hydrostatic pressure to a pipe containing an external longitudinal notch at 80 °C. The time to failure is used as a comparative measure of slow crack growth resistance; the notch depth is defined in the standard and must be reproduced to avoid invalid data. The Pennsylvania notch tensile test ASTM F1473 uses a notched bar under constant tensile stress at 80 °C and provides a plane-strain measurement of slow crack growth. The full-notch creep test ISO 16770 and strain hardening modulus ISO 18488 are used to differentiate standard PE100 materials from PE100-RC grades. K44-11-128 should not be considered a PE100-RC material unless the producer’s datasheet and third-party listing explicitly confirm the additional requirements for rapid crack propagation and slow crack growth.
Slow crack growth resistance is controlled by tie molecule density and comonomer distribution in the high-molecular-weight fraction. Bimodal polymerization routes improve tie molecule connectivity between lamellae, which is why bimodal PE100 grades are preferred over unimodal PE80 grades for higher-pressure or notched service. The rapid crack propagation test ISO 13477 uses an S4 specimen at low temperature and reports critical pressure and critical temperature; gas distribution projects often require this test under ISO 4437. Notched-pipe failure time is not universally codified across standards, so project specifications must state the required minimum ISO 13479 time at 80 °C and the applicable hoop stress.
The primary difference between K44-11-128 and a PE80 pipe grade is the minimum required strength and the resulting pressure rating for a given wall thickness. PE80 resin has an MRS of 8.0 MPa; PE100 resin has 10.0 MPa. For a 110 mm outside-diameter pipe at a nominal pressure of 1.0 MPa, the calculated SDR is 13.8 for PE80 and 17 for PE100, using the formula SDR = 2σ_s/P + 1. This corresponds to a wall-thickness reduction from approximately 8.0 mm to 6.5 mm. K44-11-128 therefore permits thinner-wall pressure pipe at equal pressure rating when its PE100 classification is confirmed.
| Parameter | PE80 | PE100 | PE100-RC |
|---|---|---|---|
| Minimum required strength by ISO 9080 | 8.0 MPa | 10.0 MPa | 10.0 MPa |
| Design stress for water at 20 °C, C=1.25 | 6.4 MPa | 8.0 MPa | 8.0 MPa |
| SDR 11 pressure rating at 110 mm OD | 1.28 MPa | 1.60 MPa | 1.60 MPa |
| Slow crack growth assessment | ISO 13479 baseline | ISO 13479 intermediate | ISO 13479 plus ISO 16770 or ISO 18488 elevated threshold |
| Rapid crack propagation evaluation | Project-specific | ISO 13477 where specified | ISO 13477 critical criteria commonly required |
Compared with low-molecular-weight high-density polyethylene blow-moulding or film grades, K44-11-128 has a lower 5 kg melt flow rate and higher melt strength. These characteristics are necessary for thick-wall pressure pipe but reduce extruder output per screw revolution and make the grade unsuitable for high-speed thin-wall injection moulding or film casting. Compared with PE100-RC resins, the standard PE100 classification of K44-11-128 may not include the additional slow crack growth and rapid crack propagation performance thresholds demanded for trenchless installation, no-dig rehabilitation, or rough-embedment projects. The producer’s technical datasheet should be consulted for the declared ISO 13479 failure time, ISO 16770 results, ISO 13477 critical pressure and temperature, and any PE100+ association listing.