| HS Code | 137934 |
| Polymer Type | High-Density Polyethylene (HDPE) |
| Pe Classification | PE100 |
| Density | 0.950 g/cm³ |
| Melt Flow Rate 190 C 5 Kg | 0.25 g/10 min |
| Tensile Yield Strength | ≥25 MPa |
| Elongation At Break | ≥600% |
| Flexural Modulus | ≥1000 MPa |
| Notched Izod Impact Strength | ≥20 kJ/m² |
| Vicat Softening Temperature | ≥120°C |
| Environmental Stress Cracking Resistance Escr | ≥1000 h |
| Oxidation Induction Time Oit | ≥20 min |
| Ash Content | ≤0.03% |
| Moisture Content | ≤0.03% |
| Melting Point | 130-135°C |
| Bulk Density | 0.55-0.60 g/cm³ |
| Particle Size | 2-4 mm |
| Form | Pellets |
| Color | Natural |
As an accredited Yanchang China Coal Yulin (Shaanxi) HDPE HP50-25-153 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packed in 25 kg PP woven bags, labeled Yanchang China Coal Yulin (Shaanxi) HDPE HP50-25-153, suitable for industrial storage. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): Yanchang China Coal Yulin (Shaanxi) HDPE HP50-25-153, 25 kg bags, palletized or floor-loaded, stretch-wrapped, strapped; approx. 18–22 MT. |
| Shipping | Yanchang China Coal Yulin (Shaanxi) HDPE HP50-25-153 ships as non-hazardous polyethylene pellets. Standard export packing: 25 kg woven bags or 1 MT jumbo bags, palletized and stretch-wrapped. Keep dry, ventilated, away from moisture, sunlight, and heat. Transport by sea, rail, or truck in clean containers. |
| Storage | Store in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers sealed to prevent moisture, dust, and contamination. Use clean pallets, avoid sharp objects, and stack safely to prevent package damage. Protect from prolonged UV exposure. Maintain good housekeeping and follow local regulations and the supplier’s SDS. |
| Shelf Life | Approximately two years when stored in original unopened packaging, dry, at ambient temperature, away from direct sunlight, heat, and moisture. |
Municipal potable water piping produced from Yanchang China Coal Yulin (Shaanxi) HDPE HP50-25-153 is governed by the PE100 compound requirements of ISO 4427-2:2019, EN 12201-2:2011+A1:2013, NSF/ANSI/CAN 61, and GB/T 13663.2-2018. The material class must demonstrate a lower confidence limit of hydrostatic strength of not less than 10 MPa at 50 years and 20°C under ISO 9080:2012 and ISO 12162:2009. Extrusion formulations for blue potable water pipe are compounded from 100 phr HP50-25-153, 2.0–4.0 phr of blue HDPE carrier masterbatch yielding 0.2–0.5 wt% phthalocyanine pigment, and 0.1–0.3 phr of hindered phenolic/phosphite antioxidant masterbatch; black service pipe variants use 2.0–2.5 wt% carbon black per ISO 6964. Downstream production on a single-screw extruder with a grooved feed section and L/D 33:1 uses barrel zone settings from 190°C to 220°C, adapter temperature 210–225°C, and die head pressure 12–22 MPa, followed by vacuum calibration at −0.15 to −0.35 bar and ultrasonic wall-thickness inspection. Terminal products include SDR11 and SDR17 pipe in diameters from 25 mm to 1,200 mm for potable water mains, service laterals, and distribution branches. Batch-to-batch melt flow rate variation should be held within ±5% by the converter; regrind addition above 5 wt% is not recommended because notched pipe test performance under ISO 13479 degrades with repeated thermal history.
In buried natural gas distribution, resistance to slow crack growth and rapid crack propagation is inseparable from the bimodal molecular weight distribution of HP50-25-153. The governing standards include ISO 4437-2:2014, EN 1555-2:2021, ASTM D2513, and CSA B137.4. Compounding for gas service uses 100 phr resin, 2.0–2.5 wt% carbon black masterbatch to achieve uniform UV protection, and 0.2–0.4 phr antioxidant masterbatch; yellow stripe compounds are co-extruded at 3–5 wt% masterbatch in the stripe layer only, not mixed into the pressure-bearing core. Production of SDR11 and SDR17 gas pipe is performed on a barrier screw extruder with barrel zones 190–230°C and a spiral mandrel die at 220–230°C. The decisive processing conflict is residual thermal stress: excessively rapid cooling in the first calibration tank increases retained hoop stress and lowers ISO 13479 notched pipe lifetime; cooling water is therefore staged from 40°C to 20°C across 6–10 m of spray calibration. Terminal products are black or black-with-yellow-stripes HDPE gas mains and service lines from 20 mm to 630 mm, including coiled lengths up to 200 m for small diameters.
| Test method / standard | Property evaluated | Acceptance value or tolerance |
|---|---|---|
| ISO 1183-1:2019 | Compound density | 0.949–0.953 g/cm³ |
| ISO 1133-1:2022 | Melt flow rate at 190°C, 5 kg | 0.23–0.30 g/10 min |
| ASTM D638-14 | Tensile yield strength | ≥ 23 MPa |
| ISO 9080:2012 / ISO 12162:2009 | Long-term hydrostatic strength | LCL ≥ 10 MPa at 50 years, 20°C |
| ISO 13479 | Notched pipe test for slow crack growth | No brittle failure below 500 h at 80°C |
Structured-wall corrugated polyethylene pipe for stormwater retention and culvert use places less demand on hydrostatic strength than on flexural modulus, corrugator forming stability, and resistance to environmental stress cracking in acidic soil conditions. Compliance is set by EN 13476-3:2018, ASTM F2648, AASHTO M294, and GB/T 19472.1-2019. The compounding recipe uses 100 phr HP50-25-153, 2.5 phr carbon black masterbatch for the outer corrugated wall, and 0.5–1.0 phr fluoropolymer processing aid where die lip deposit or melt fracture appears at corrugator speeds above 8 m/min. In the manufacturing process, a grooved-barrel extruder feeds a corrugator with vacuum forming at −0.2 to −0.5 bar; melt temperature is held between 205°C and 225°C to maintain elongational viscosity sufficient for rib filling while limiting continuous parison sag. If melt temperature falls below 205°C, incomplete rib formation produces thin roots that fail ring stiffness testing under ASTM D2412. Three-layer co-extrusion is common when a pale inner wall is specified, with the inner layer containing 3–5 phr white masterbatch and the middle structural layer maintained as virgin HP50-25-153. Terminal products range from DN100 to DN1000, including perforated underdrain configurations and heavy-duty culvert classes with annular corrugated exteriors.
Geomembrane liner extrusion is not the primary design target for pipe-grade HDPE, but converters running HP50-25-153 in flat-die sheet lines benefit from high melt strength and environmental stress crack resistance. The relevant compliance endpoints are GRI-GM13, ASTM D6693 tensile properties, ASTM D1004 tear resistance, ASTM D5397 notched constant tensile load, and ASTM D5885 oxidative induction time. The formulation is maintained at 100 phr resin, 2.0–2.5 wt% carbon black, 0.3–0.6 phr antioxidant masterbatch, and in some cases 0.5–1.0 phr processing aid to control melt fracture at high line speeds. Extrusion uses a flat die with adjustable lips set to 2.0–3.5 mm sheet thickness, polished chill rolls at 60–80°C, and haul-off tension limited to avoid gauge variation above ±5%; resin receiving at relative humidity above 60% requires hopper drying at 80°C for 2–4 h to prevent extrudate surface splay. The key limitation is that published data for this grade in textured-surface geomembrane configurations is limited, so surface co-extrusion pre-qualification is required before full-scale runs. Terminal products are smooth HDPE geomembranes in rolls of 1.0–2.5 mm thickness, applied as landfill liners, pond liners, and mining heap-leach pads.
When tailings and mineral slurry lines replace steel, the wall thickness design of HP50-25-153 pipe must simultaneously account for internal pressure, abrasive particle wear, and slow crack growth from notches initiated by sharp particles. Governing references include ISO 15494:2015, AS 4130 for Australian mining water services, and material cell classification under ASTM D3350; slurry abrasion comparisons are anchored to ASTM D4060 Taber wear or ISO 15527 if a standardized slurry test is specified. The compounding ratio typically uses 100 phr virgin resin without regrind exceeding 10 wt%, because regrind from pipe cutting lowers notched pipe test performance; carbon black masterbatch is held at 2.0–2.5 wt%. Production of thick-wall slurry pipe on a single-screw extruder with L/D 38:1 and downstream water-ring calibration must address sag risk for wall thickness above 40 mm: melt temperature is lowered to 195–210°C, die gap is offset to compensate parison draw-down, and internal air pressure is regulated to keep the inner diameter round during cooling. Terminal products include flanged or butt-fused tailings pipelines from 90 mm to 1,600 mm, frequently in 12 m or 20 m straight lengths for long-distance slurry transport and in-plant process lines.
Power and telecom cable protection conduit made from HP50-25-153 is produced to ASTM F2160, NEMA TC 7, UL 651A, and IEC 61386-24 where buried non-metallic conduit is specified. The formulation uses 100 phr resin, 2.0–2.5 wt% carbon black for UV-stabilized black conduit, and 0.3–0.5 phr antioxidant masterbatch; for ribbed or corrugated conduit, the same masterbatch is used in the outer layer while the inner wall may remain unpigmented to reduce additive cost. In production, a single-screw extruder with a grooved feed and L/D 30:1 feeds a die with internal mandrel cooling; vacuum sizing slots maintain outer diameter tolerance to ±0.5% at line speeds of 3–10 m/min. The critical process parameter is melt temperature: melt temperature above 230°C reduces melt strength and promotes inner wall sag, while melt temperature below 180°C increases head pressure and reduces output. Low-temperature impact resistance of the finished conduit is evaluated by impact testing after conditioning at −25°C for 24 h, with failure defined as any crack or split in the wall. Terminal products are straight or coiled HDPE conduits from 16 mm to 200 mm, including smooth inner wall types for cable blowing and pre-installed pull tape configurations.
Competitive Yanchang China Coal Yulin (Shaanxi) HDPE HP50-25-153 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Yanchang China Coal Yulin (Shaanxi) HDPE HP50-25-153 is a pelletized high-density polyethylene resin produced by Shaanxi Yanchang China Coal Yulin Energy Chemical Co., Ltd. The material falls within the ethylene polymer family controlled by ISO 17855-1; the suffix HP50-25-153 is a producer-specific trade designation rather than an ISO 1043-1 standardized designation. Supplier documentation typically associates the resin with a nominal density of 0.953 g/cm³ determined by ISO 1183-1 method A and a nominal melt mass-flow rate of 25 g/10 min at 190 °C under a 2.16 kg load determined by ISO 1133-1:2022 condition D. This flow class is intended for high-flow injection molding conversions in which rapid filling of multi-cavity tools, thin-wall penetration, and short cycle times are primary processing criteria. Published data for this specific configuration in open literature is limited; therefore the producer certificate of analysis remains the authoritative specification source.
Incoming quality assurance should include melt mass-flow rate, density, tensile yield stress, elongation at break, flexural modulus, notched impact resistance, Vicat softening temperature, and ash content. The test matrix is normally defined by the producer’s release specification and should be verified against the actual lot certificate. The following reference ranges apply to the high-flow 0.953 g/cm³ HDPE class and are not a substitute for lot-specific certification:
| Parameter | Test method | Unit | Reference range for the 0.953 g/cm³ / 25 g/10 min class |
|---|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 condition D | g/10 min | 20–30 |
| Density at 23 °C | ISO 1183-1 method A | g/cm³ | 0.950–0.956 |
| Tensile yield stress | ISO 527-2, Type 1A, 50 mm/min | MPa | 24–30 |
| Nominal tensile strain at break | ISO 527-2, Type 1A, 50 mm/min | % | ≥100 |
| Flexural modulus | ISO 178 | MPa | 1000–1500 |
| Notched Izod impact at 23 °C | ISO 180/A | kJ/m² | 3.0–6.0 |
| Vicat softening temperature | ISO 306/A50 | °C | 122–130 |
| Ash content | ISO 3451-1 | % | ≤0.05 |
Visual pellet inspection for contamination, gel specks, black specks, or crosslinked fractions should be performed at incoming receiving. HDPE lot contamination with polypropylene or other incompatible polymers can produce localized viscosity defects in thin ribs, hot-runner channels, and small gate geometries. Bulk density, pellet size distribution, and color are also checked for automatic material handling systems. Storage should be in clean, closed, UV-shielded silos or hoppers at ambient temperature below 40 °C. Prolonged storage above 45 °C can accelerate antioxidant depletion and shift the oxidation induction time measured by ISO 11357-6.
HDPE absorbs very little water; equilibrium moisture uptake at 23 °C and 50% relative humidity is typically below 0.01%. Surface condensation remains the dominant moisture-related defect source. For pellets stored in unheated warehouses or transferred from cold silos during humid weather, pre-drying with a desiccant dryer at 80 °C for 2–4 h or a hot-air hopper dryer at 85 °C for 3–4 h is sufficient to eliminate splay and surface streaking. The use of low-speed, high-torque reciprocating-screw machines with L/D ratios between 20:1 and 25:1 and compression ratios of 2.5:1 to 4.0:1 allows homogeneous melt quality without excessive shear overheating. Melt temperature measured by an immersion probe should be maintained at 220–250 °C, with nozzle temperature not exceeding 260 °C. Back pressure between 0.3 MPa and 0.7 MPa and screw surface speeds of 0.3–0.6 m/s are common for this flow class, but high-speed thin-wall molding may require injection velocities of 150–300 mm/s and packing pressures of 60–100 MPa on hydraulic or electric machines with adequate clamp force. Extended melt residence time above 250 °C beyond 15 min should be avoided; if a machine stops, barrel temperatures should be reduced to 160 °C or the material purged to reduce oxidative chain scission.
Typical converter evaluations for high-flow HDPE include multicavity caps and closures, thin-wall food containers, housewares, crates, toys, and technical components with wall sections below 1.2 mm. The flow length-to-thickness ratio at 25 g/10 min permits filling of long thin ribs with lower injection pressure than a 0.7 g/10 min blow-molding grade. For food-contact articles, the finished part must comply with EU Regulation (EU) No 10/2011 as amended or FDA 21 CFR 177.1520 for olefin polymers, and the supplier’s food-contact certification should cover the specific additive package and production campaign. A generic HDPE class approval does not automatically extend to this grade.
Direct substitution of this high-flow injection grade for a low-MFR pipe grade is not appropriate in pressure piping because the molecular architecture differs. PE100 pipe grades typically have MFR in the range of 0.20–0.50 g/10 min at 190 °C/5 kg and a bimodal molecular weight distribution that combines high stiffness with slow crack growth resistance under ISO 9080 and ISO 12162. The high-flow class represented by HP50-25-153 has lower melt viscosity and improved spiral flow, but it is not classified as PE100 and lacks the hydrostatic design basis required for pressure pipe. In rigid packaging, the high-flow resin reduces cycle time and improves replication of fine mold texture relative to a blow-molding grade, while giving up some environmental stress-cracking resistance as measured by ASTM D1693. The difference is primarily due to lower weight-average molecular weight and reduced tie-molecule density, which decreases ductile fracture resistance under constant load. Converters should therefore use this grade only in non-pressure, non-load-bearing applications unless specific certified data support otherwise.
Comparative property values for high-flow HDPE, general-purpose LDPE, and PP homopolymer are given in the following matrix. The values are class-level reference data from standardized measurements and should not be read as grade-specific release limits.
| Property | Test method | High-flow HDPE class | General-purpose LDPE | PP homopolymer |
|---|---|---|---|---|
| Density | ISO 1183-1 | 0.950–0.956 g/cm³ | 0.915–0.925 g/cm³ | 0.900–0.910 g/cm³ |
| Tensile yield stress | ISO 527-2 | 24–30 MPa | 9–14 MPa | 30–38 MPa |
| Flexural modulus | ISO 178 | 1000–1500 MPa | 150–300 MPa | 1200–1700 MPa |
| Vicat softening temperature | ISO 306/A50 | 122–130 °C | 85–95 °C | 150–155 °C |
| Notched Izod impact at 23 °C | ISO 180/A | 3.0–6.0 kJ/m² | No break | 2.5–5.0 kJ/m² |
| Water absorption after 24 h | ISO 62 | ≤0.01% | ≤0.015% | ≤0.02% |
The producer-specific code HP50-25-153 should not be interpreted using global standard designations. The numeric portion is normally decoded through the producer’s technical data sheet and lot certificate. A certificate of analysis should list lot-level melt mass-flow rate, density, tensile properties, ash, and any additive levels. For food-contact or pharmaceutical packaging, the certificate should also identify the production campaign and confirm that the grade was manufactured under the relevant hygiene management system. If the application requires accelerated weathering, the UV stabilizer package must be specified at the time of order, because standard HDPE grades without carbon black or hindered amine light stabilizers will lose surface integrity under ISO 4892-2 exposure.
Operational boundaries include sustained service above 60–80 °C under mechanical load, where creep and stress relaxation become significant. The resin should not be used in prolonged contact with strong oxidizing acids, aromatic hydrocarbons, or chlorinated solvents without verification by environmental stress-cracking testing under ISO 22088-1. Copper compounds and certain heavy-metal pigments can accelerate oxidation at elevated processing temperatures and should be excluded unless the stabilizer package is specifically formulated for metal deactivation.
On production-scale machines, a frequent defect with high-flow HDPE is flash in worn molds because the low melt viscosity penetrates clearances below 0.03 mm. Mold maintenance should confirm parting-line flatness and clamp force distribution; injection velocity should be reduced if flash cannot be controlled without dropping holding pressure. Part weight, melt cushion, and cushion stability measured on each cycle provide a practical lot-to-lot viscosity check. A lot that requires a cushion change greater than 5% to maintain part weight should be checked by ISO 1133-1:2022 and compared with the supplier certificate of analysis.