Yanchang China Coal Yulin Shaanxi Hdpe Hd6007xa

Yanchang China Coal Yulin (Shaanxi) HDPE HD6007XA

    • Product Name: Yanchang China Coal Yulin (Shaanxi) HDPE HD6007XA
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 713076
    Density 0.960 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 7.0 g/10 min
    Melting Point 130-135 °C
    Vicat Softening Temperature 125 °C
    Heat Deflection Temperature 0 45 Mpa 75 °C
    Tensile Yield Strength 29 MPa
    Elongation At Break >500%
    Flexural Modulus 1200 MPa
    Notched Izod Impact Strength 23 C 50 J/m
    Shore D Hardness 65
    Crystallinity 70-80%
    Glass Transition Temperature -120 °C
    Thermal Conductivity 0.4 W/m·K
    Coefficient Of Linear Thermal Expansion 1.2e-4 /°C
    Water Absorption <0.01%
    Dielectric Constant 1 Mhz 2.3
    Volume Resistivity >10^16 Ω·cm

    As an accredited Yanchang China Coal Yulin (Shaanxi) HDPE HD6007XA factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Yanchang China Coal Yulin (Shaanxi) HDPE HD6007XA is packed in 25 kg PP woven bags with PE inner liners.
    Container Loading (20′ FCL) 20′ FCL: Yanchang China Coal Yulin (Shaanxi) HDPE HD6007XA, floor-loaded 25 kg bags, approx. 25 MT net per container.
    Shipping Yanchang China Coal Yulin (Shaanxi) HDPE HD6007XA is a non-hazardous high-density polyethylene resin. It is normally shipped in 25 kg woven bags or 500–1000 kg jumbo bags, palletized and stretch-wrapped. Transport is by truck/rail to Chinese ports, then sea freight in 20'/40' containers. No special dangerous goods handling required.
    Storage Store Yanchang China Coal Yulin (Shaanxi) HDPE HD6007XA in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, moisture, and ignition sources. Keep original bags sealed, palletized, and stacked safely to avoid deformation. Prevent contamination, UV exposure, and static buildup. Maintain ambient temperature, preferably below 50°C, and observe good housekeeping and fire precautions. Use first-in, first-out stock rotation.
    Shelf Life Shelf Life: 24 months when stored in original, unopened packaging in a cool, dry, well-ventilated area, protected from direct sunlight.
    Application of Yanchang China Coal Yulin (Shaanxi) HDPE HD6007XA

    Yanchang China Coal Yulin (Shaanxi) HDPE HD6007XA is an extrusion blow molding grade high-density polyethylene with a nominal melt flow rate of 0.7 g/10 min at 190 °C under 2.16 kg load (ASTM D1238) and a nominal density of 0.960 g/cm³ (ASTM D1505). The resin is supplied as pellet for hollow-body conversion and is specified only for downstream segments in which parison melt strength, die swell, pinch-off weld integrity, and environmental stress-crack resistance determine container fitness. The following application scenarios are limited to actual extrusion blow molding routes for rigid bottles and small-to-medium containers: dairy and fresh beverage, household and industrial chemical, personal care surfactant, pharmaceutical solid-dose, edible oil and liquid food service, and automotive aftermarket fluid packaging. Injection molded closures, blown film, pipe, and rotational molded parts are excluded from this resin scope because the 0.7 g/10 min melt flow rate and molecular weight distribution do not match the shear and cooling requirements of those processes.

    Single-layer extrusion blow molding of milk and fresh juice containers places HD6007XA as the 100 wt% virgin food-contact resin; white TiO₂ masterbatch is metered at 1.0–2.5 wt% to provide light blocking and to separate dairy lots. Calcium carbonate and optical brightener masterbatches are not used in this segment because they alter parison sag and complicate food-contact declarations under double-jurisdiction audits. Compliance for the finished container is evaluated under FDA 21 CFR 177.1520(c) for olefin polymers in contact with food, and under EU Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm² in dairy and fruit juice simulants; Chinese domestic shipments require GB 4806.7-2016. On production-scale shuttle machines with grooved-barrel extruder length-to-diameter ratio 24:1, melt temperature is maintained at 190–210 °C at adapter and die, with parison die gap profiled between 1.2–1.8 mm to achieve sidewall thickness 0.35–0.65 mm. Mold cooling water is held at 10–15 °C, blow pressure at 0.60–0.80 MPa, and cooling time below 4–6 s per 500 mL bottle produces pinch-weld hinge cracking in 0 °C drop impact. Terminal products include 200 mL–2 L pasteurized milk, fresh juice, drinkable yogurt, and cream bottles with blow-molded neck finishes; cap sealing surfaces are not injection molded from this grade.

    Which Validation Controls Apply to Sodium Hypochlorite and Detergent Bottles?

    Sodium hypochlorite and detergent container validation is driven by environmental stress cracking at the pinch weld and sidewall flex zones, not by tensile yield. By weight, HD6007XA is run at 90–100 wt% virgin pellet; clean post-industrial regrind from edge trim and rejected bottles is added up to 10 wt% only when lot-specific environmental stress-crack resistance remains above finished-container acceptance thresholds. Bleach containers filled with 5–12 wt% sodium hypochlorite should not exceed 15 wt% regrind without long-term storage testing, because oxidized regrind reduces molecular weight and accelerates crack propagation at the pinch-off. Packaging compliance is assessed under REACH Annex XVII restrictions for substances in articles, UN Model Regulations Chapter 6.1 design-type tests for dangerous goods packaging, and ADR 6.1 when the filled container exceeds 3 L or carries a dangerous goods classification. Production equipment includes reciprocating screw blow molders and continuous shuttle machines with parison programming; melt temperatures are limited to 190–215 °C because sodium hypochlorite exposure increases sensitivity to frozen-in stress. Mold temperatures 15–25 °C and post-cooling fixtures for 8–12 s control paneling on flat sidewalls, while pinch-off die land length is increased relative to food bottle tooling to keep weld thickness above 0.25 mm. Terminal products are 500 mL–5 L bottles and small jerrycans for liquid bleach, hard-surface cleaners, laundry detergent, and diluted agrochemical adjuvants; containers above 5 L are not assigned to this grade unless the lot certificate confirms a high-molecular-weight tail appropriate for large-part parison hang.

    When packaging anionic surfactant systems such as sodium laureth sulfate and cocamidopropyl betaine, the neck and handle pinch-off regions of HD6007XA bottles are subjected to stress cracking that is not predicted by melt flow ratio alone; batch-to-batch variance in comonomer distribution will shift ESCR performance more than a 0.05 g/10 min MFI drift. The packaging component is assessed against REACH Annex XVII restrictions for phthalates and heavy metals in colorants, and against EU Regulation (EU) No 1223/2009 by the filler for the finished cosmetic product; the HDPE container itself is not a cosmetic formula. Addition ratio in this segment is 100 wt% HD6007XA with color masterbatch limited to 0.5–2.0 wt%; pearlescent or metallic masterbatches above 2 wt% narrow the processing window because plate-like pigments increase low-shear viscosity and reduce parison uniformity on shuttle machines. Silicone-based external processing aids above 0.05 wt% are not used in neck-bearing containers because they lower weld strength at the pinch-off. Reciprocating screw machines are operated with melt temperatures 185–205 °C, converging die gap 1.0–1.5 mm, and mold cooling 8–12 °C to maintain surface gloss on polished cavities. The terminal types include 150–750 mL bottles for shampoo, body wash, hand soap, and conditioner; oval and cylindrical formats use thread or snap-cap neck finishes, with closures supplied from polypropylene rather than HD6007XA.

    USP <661.1> Packaging Systems and the Limits of HDPE Solid-Dose Bottles

    Pharmaceutical solid-dose packaging converts HD6007XA under a qualification regime that treats the polymer as a packaging system component rather than as a standalone approved excipient. Compliance is assessed against USP <661.1> plastic packaging system requirements, Ph. Eur. 3.1.3 polyethylene for containers, FDA 21 CFR 177.1520 for the base olefin polymer, and ICH Q3D elemental impurity risk assessment where the filler’s finished-pack stability studies require it. The resin is processed at 100 wt% virgin pellet; regrind is excluded from the product-contact layer unless explicitly permitted by the pharmaceutical packaging supplier’s change-control procedure, and color masterbatch for amber or opaque bottles is restricted to 0–1.5 wt% with extractables and leachables data supporting USP <661.1>. Blow molding is performed on dedicated or validated campaign equipment with melt temperatures 180–205 °C, cavity cooling at 10–15 °C, and post-mold trimming under filtered airflow; mold release is not used on the product-contact surface. Process validation includes extractables testing, leak testing under USP <1207> or equivalent, and wall thickness distribution mapping at the neck, shoulder, and base. Terminal product scope covers 30–500 mL round and oblong bottles for tablets, capsules, powders, and desiccant canisters; child-resistant closures are supplied separately from polypropylene, not from HD6007XA.

    When Edible Oil Fillers Require Top-Load Strength but Not Oxygen Barrier

    Ambient-filled cooking oil and liquid food service packaging selects HD6007XA for top-load strength, handle integrity, and consistent wall-thickness distribution rather than gas barrier; monolayer HDPE is not an oxygen barrier and should not be specified for oxygen-sensitive oils without nitrogen flushing or foil induction sealing. Food contact compliance follows FDA 21 CFR 177.1520(c), EU Regulation (EU) No 10/2011 overall migration limit 10 mg/dm², and GB 4806.7-2016 for Chinese domestic distribution. Use ratio is 100 wt% HD6007XA with optional oil-compatible colorant masterbatch at 0–1 wt%; regrind from the same production lot is accepted up to 20 wt% only when the blow molder can document source control and lot traceability, and when finished-container migration remains below the overall limit. Antioxidant masterbatches are not added beyond the resin supplier’s stabilization package, because migration into oil must remain below the overall migration limit. Extrusion blow molding with handled containers uses parison programs that thicken the handle pinch area to 1.0–1.5 mm; melt temperature is held at 190–210 °C, mold temperature at 10–20 °C, and blow pressure at 0.60–0.80 MPa. Screw speed is reduced relative to smaller bottle production to avoid melt temperature overshoot above 215 °C, which produces pinholes at the pinch weld. Terminal products designated for this segment include 500 mL–5 L cooking oil, vinegar, syrup, and food service sauce bottles with handles; seed oils requiring shelf life beyond 6–9 months without modified atmosphere packaging are not placed in monolayer HDPE.

    Diesel exhaust fluid (AUS 32) and automotive aftermarket fluid packs use HD6007XA only as a monolayer container for non-flammable fills; the segment imposes ultraviolet resistance, stack loading, and label adhesion constraints that differ from household chemical fills. Packaging for diesel exhaust fluid is governed by ISO 22241-1:2019 for automotive urea solution quality and ISO 22241-3:2019 for handling, transportation, and storage; container materials must not introduce aldehydes or metals that degrade AUS 32. HD6007XA is formulated at 100 wt% virgin pellet; UV-stabilizer masterbatch is added at 0.5–2.0 wt% depending on intended outdoor storage, carbon black at 0.3–1.0 wt% for opaque black packs, and same-family regrind up to 15 wt% where scrap control is demonstrated. Extrusion blow molding on shuttle machines runs with melt temperatures 190–210 °C, die gap 1.5–2.0 mm, and mold cooling 12–18 °C; wall thickness is increased to 0.8–1.2 mm at the bottom chime and handle to resist stack load. Screw and head are purged between color changes to avoid black speck contamination in natural or white retail packs. Terminal products include 1–5 L diesel exhaust fluid packs, windshield washer fluid bottles, and automotive coolant overflow reservoirs; containers for petroleum-based brake fluids are excluded because ester-based brake fluids demand barrier materials or surface treatment.

    Free Quote

    Competitive Yanchang China Coal Yulin (Shaanxi) HDPE HD6007XA prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Yanchang China Coal Yulin (Shaanxi) HDPE HD6007XA is a pelletized high-density polyethylene resin supplied by the Yanchang China Coal production site in Yulin, Shaanxi. In the producer’s nomenclature, the HD segment denotes high-density polyethylene, the 6007 segment is associated with a nominal density class of 0.960 g/cm³ and a nominal melt flow rate class of 0.7 g/10 min under 190 °C and 2.16 kg load, and the XA suffix denotes an extrusion-grade additive package. The grade is intended primarily for blown-film extrusion, high-stiffness packaging, and selected thin-wall injection-moulded articles. Published data for this specific Yanchang grade is limited; the supplier certificate of analysis and lot-specific data should therefore be treated as controlling. Density should be measured according to ISO 1183-1, while melt flow rate should be determined according to ISO 1133-1. In commercial practice, HD6007XA is positioned for applications requiring moderate melt flow, elevated crystalline density, higher tensile yield strength, and lower water-vapour transmission than low-density or linear low-density polyethylene films.

    How Does the Density–Melt Flow Pairing of HD6007XA Compare With Other HDPE Film Grades?

    The combination of density and melt flow rate gives HD6007XA a different processing window from lower-melt-flow blow-moulding grades such as the 0.955 g/cm³ class HD5502W. The higher 0.7 g/10 min melt flow rate class permits lower extruder head pressure in high-output film lines but reduces melt strength. In high-stalk blown-film geometries, this means the bubble support air, frost-line height, and die-face air cooling must be maintained within a narrower operating envelope than for a 0.2 g/10 min HDPE. The comparative table below summarizes typical class data; the figures are reference values for general high-density polyethylene classes and do not replace lot-specific certificates for HD6007XA.

    Material class Density (g/cm³) Melt flow rate 190 °C/2.16 kg (g/10 min) Typical processing behaviour
    HD6007XA class 0.958–0.961 0.60–0.80 High-stalk blown film; higher throughput potential; narrower bubble stability window
    HD5502W class 0.953–0.956 0.15–0.30 Large-part blow moulding; higher melt strength; lower film-line pressure efficiency
    LLDPE butene film grade 0.918–0.922 0.80–1.20 Low-stalk bubble; higher dart impact; lower modulus and lower moisture barrier

    For film converters, the most important difference is not only the density but the molecular weight distribution. A 0.960 g/cm³ HDPE with a 0.7 g/10 min melt flow rate typically exhibits stronger crystallization-driven stiffness than LLDPE, but lower dart drop resistance and lower Elmendorf tear resistance. When downgauging a film from 30 µm to 20 µm, the smaller bubble window of the 0.960 g/cm³ class must be offset by higher stalk height, typically 6 to 8 die diameters, and lower melt temperature relative to LLDPE.

    On lines configured for high-stalk HDPE bubble geometries, HD6007XA-class resin is commonly processed through a single-screw extruder with a grooved feed section, L/D ratio between 30:1 and 33:1, and a compression ratio between 3.0:1 and 4.0:1. Typical barrel temperature programmes start at 180 °C in the feed zone and rise to 210–220 °C in the metering zone, with die zones held at 210–230 °C. Melt temperature should be kept below 260 °C to reduce gel formation and to avoid oxidative degradation of the stabiliser package. Die gap settings from 1.8 mm to 2.4 mm are commonly reported for HDPE film lines; exact die geometry should be matched to blow-up ratio, which is typically 3.5:1 to 4.5:1 for high-density film. Bubble cooling with dual-lip air rings and internal bubble cooling is generally required when output exceeds 300 kg/h on a 90 mm extruder. Although HDPE does not normally require desiccant drying, pellets stored in uncontrolled humidity can carry surface moisture. If moisture exceeds 0.1 % by weight, hopper drying at 60–80 °C for 1–2 h is applied to prevent bubble instability and surface defects.

    When converted into 25 µm film, a 0.960 g/cm³ high-density polyethylene of this class typically exhibits tensile yield strength in the machine direction of 26–32 MPa and transverse direction of 24–30 MPa when tested according to ISO 527-3. Elongation at break commonly exceeds 600 % in both directions, although film orientation and extrusion conditions strongly influence the result. Dart impact measured according to ASTM D1709 Method A generally ranges from 100 g to 180 g for 25 µm HDPE film, whereas LLDPE of the same thickness may exceed 300 g. Elmendorf tear resistance determined under ISO 6383-2 is typically lower in HDPE, particularly in the machine direction, because molecular orientation increases splitting tendency. The practical trade-off is that HD6007XA-class film provides a secant modulus of roughly 800–1200 MPa according to ISO 527-2, which is about 2.5 to 3 times higher than a typical 0.920 g/cm³ LLDPE film. Water-vapour transmission rate measured under 38 °C and 90 % relative humidity according to ISO 15106-3 is reported in polymer packaging literature to be approximately 40–60 % lower for high-density polyethylene than for LLDPE at equivalent thickness.

    When Down-Gauging Requires Higher Melt Strength and Density

    On high-speed bag-making lines, downgauging from 25 µm to 18 µm shifts the failure mode from tensile yield to impact puncture and tear propagation. HD6007XA-class HDPE is selected when the converter can accept reduced dart impact for improved stiffness, lower extensional stretching under load, and lower moisture vapour transmission. In T-shirt bag production, the higher density provides better sheet separation and improved cutting behaviour on transverse sealing and perforation units, but the lower melt strength compared with a 0.2 g/10 min blow-moulding HDPE requires careful control of the frost-line position. If frost-line height varies by more than ±10 %, gauge bands and bubble chatter can occur. Processors operating Windmöller & Hölscher or Hosokawa Alpine lines with internal bubble cooling have reported that HDPE of this melt-flow class can be processed at die pressures lower than those observed with lower-melt-flow HDPE grades, but film blocking increases at roll temperatures above 35 °C. Anti-block additive levels should be specified by the resin supplier and verified by coefficient of friction testing under ASTM D1894 or ISO 8295.

    Compatibility with post-industrial reclaim is another operational boundary. HD6007XA can be blended with LLDPE or LDPE at low levels, typically below 20 % by weight, to modify stiffness without complete loss of impact strength. However, blends with polypropylene or polar barrier polymers should be avoided unless the line is configured for active homogenization. Polypropylene contamination above 5 % by weight in the melt may reduce film clarity and create delamination zones because of immiscibility and differences in crystallization kinetics. Furthermore, blends with amorphous polyamide or EVOH in barrier film structures require tie-layer adhesives and are outside the intended monolayer application range of HD6007XA.

    Regulatory evaluation of HD6007XA depends on the specific stabiliser package, catalyst residues, and additive formulation used in the lot. The base high-density polyethylene polymer may fall under FDA 21 CFR 177.1520 if the end-use extraction testing is completed for the specific food type and temperature condition. For food-contact films sold in the European market, compliance with EU Regulation No 10/2011 requires an overall migration limit of 10 mg/dm² under the intended food simulant and contact time. A supplier declaration of compliance should be obtained for each lot. For industrial applications, the resin should be assessed against REACH Article 33 and RoHS 2011/65/EU Annex II restricted substance thresholds, including lead 0.1 %, cadmium 0.01 %, mercury 0.1 %, hexavalent chromium 0.1 %, PBB 0.1 %, and PBDE 0.1 % by weight in homogeneous material. Unpigmented HDPE grades generally contain no intentionally added heavy-metal pigments, but a compliance matrix should be based on supplier analytical data rather than product-class assumptions.

    Regulatory requirement Test or reference Typical scope for HD6007XA-class HDPE
    US food-contact olefin polymers FDA 21 CFR 177.1520 Requires extraction testing and condition-of-use designation; lot-specific documentation required
    EU plastic food-contact migration EU 10/2011 Overall migration limit 10 mg/dm²; simulant and time/temperature dependent
    EU electrical and electronic restriction RoHS 2011/65/EU Annex II Restricted heavy metals and brominated flame retardants below threshold limits
    European chemical registration REACH Article 33 Substances of very high concern above 0.1 % w/w must be declared; supplier letter required

    Storage and handling constraints are often underestimated. HD6007XA pellets should be kept dry and covered, preferably below 60 % relative humidity, to minimize surface moisture pickup. Reclaimed pellet storage in external silos with temperature cycles can create condensation and increase film defects. Bags should not be stacked more than 10 high in warehouse conditions because creep deformation of lower bags can compact pellets and alter bulk-density feeding behaviour. When material is transferred pneumatically, conveying air should be dried to a dew point below −40 °C if ambient humidity exceeds 70 %. Dust and angel hair generated in conveying systems can build up in hopper magnets and cause feed bridging, so screen-pack and magnet inspection intervals should be shortened when high-speed lines exceed 500 kg/h. The resin is not inherently UV-stabilized for outdoor film exposure; if outdoor service beyond 6 months is required, an additional UV stabiliser masterbatch must be evaluated under ASTM D4329 or ISO 4892-2 for accelerated weathering.