| HS Code | 757497 |
| Density | 0.950 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 10 g/10 min |
| Tensile Yield Strength | ≥24 MPa |
| Elongation At Break | ≥500% |
| Flexural Modulus | ≥900 MPa |
| Charpy Notched Impact Strength 23 C | ≥40 kJ/m² |
| Vicat Softening Temperature | ≥120°C |
| Heat Deflection Temperature | ≥70°C |
| Shore D Hardness | ≥60 |
| Water Absorption | ≤0.01% |
| Brittleness Temperature | ≤-70°C |
| Dielectric Constant | 2.3 |
| Volume Resistivity | ≥1×10^16 Ω·cm |
| Dielectric Strength | ≥20 kV/mm |
| Thermal Conductivity | 0.4 W/(m·K) |
| Coefficient Of Linear Thermal Expansion | 1.2×10^-4 /°C |
| Melting Point | 130-135°C |
| Specific Heat Capacity | 1.9 kJ/(kg·K) |
| Oxygen Index | ≥17% |
| Ash Content | ≤0.05% |
| Moisture Content | ≤0.1% |
| Bulk Density | 0.55-0.60 g/cm³ |
As an accredited Yanchang China Coal Yulin (Shaanxi) HDPE HD50100Y factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Yanchang China Coal Yulin (Shaanxi) HDPE HD50100Y is packed in 25 kg PP woven bags or 1,000 kg jumbo bags. |
| Container Loading (20′ FCL) | 20′ FCL loading for Yanchang China Coal Yulin (Shaanxi) HDPE HD50100Y: 25 kg bags, bulk-stacked, approx. 20 MT per container. |
| Shipping | Yanchang China Coal Yulin (Shaanxi) HDPE HD50100Y ships as non-hazardous polyethylene pellets, typically in 25 kg bags or 1000 kg jumbo bags, palletized and stretch-wrapped in containers. No UN number or hazard class applies. Keep dry, cool, ventilated, and away from direct sunlight, moisture, and ignition sources. |
| Storage | Store Yanchang China Coal Yulin (Shaanxi) HDPE HD50100Y in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags sealed, palletized, and off the floor to prevent moisture and contamination. Avoid excessive stacking or outdoor exposure. Protect from punctures and static; use first-in, first-out rotation and follow the SDS. |
| Shelf Life | Shelf life is typically 24 months in original, unopened packaging stored cool, dry, ventilated, away from sunlight, heat, and contaminants. |
When converted on a grooved-barrel single-screw extruder with an L/D ratio of 33:1 to 37:1, HD50100Y is processed with a barrel profile in which the feed zone is held at 175 °C to 190 °C and the metering zone, static mixer, and die are held at 200 °C to 220 °C. The melt temperature measured at the die entry should not exceed 230 °C, and residence time above 220 °C should be kept below 5 min to avoid thermo-oxidative chain scission that would reduce ISO 1167-1 hydrostatic life. A screen pack with combined mesh sizes from 20/40/60 to 60/80/60 is placed before the breaker plate, and head pressure is maintained between 25 MPa and 35 MPa to ensure homogenization through the spiral mandrel die without exceeding the extruder’s maximum melt-pressure limit. For potable water pipe, 2.0 wt% to 2.5 wt% of a PE-based carbon black masterbatch is dry-blended at the hopper throat or side-fed from a gravimetric feeder; the final carbon black content is measured by ISO 6964 to fall within the 2.0 wt% to 2.5 wt% range specified for ultraviolet stabilization. The extrudate enters a vacuum sizing tank with water at 20 °C to 25 °C, and the puller speed is set to produce an SDR 11 wall thickness with a tolerance of ±0.2 mm. Under ISO 4427-1 and EN 12201-1, PE100 pipe is pressure-rated using the formula P = 2σₛ/(SDR−1). With σₛ = MRS/C = 10 MPa/1.25 = 8.0 MPa, SDR 11 yields an MOP of 16 bar at 20 °C for water, and SDR 17 yields 10 bar. The finished pipe is subjected to 100% dimensional inspection by ultrasonic wall-thickness scanning and randomized ISO 1167-1 long-term hydrostatic testing at 20 °C and 80 °C before release. Because HD50100Y is a high-molecular-weight bimodal pipe compound, the upper thermal boundary is narrow; batch-to-batch variation in melt mass-flow rate under a 5 kg load at 190 °C according to ISO 1133-1:2022 can shift the required screw speed by 10% to 15% for the same wall thickness.
On production lines with a 60 mm grooved-barrel extruder and a 250 mm pipe die, the typical screw speed for SDR 11 110 mm pipe is 45 rpm to 55 rpm, with a haul-off speed of 0.9 m/min to 1.1 m/min; these values require recalculation after every silo change because the molecular weight distribution of the bimodal resin responds differently to shear history in the grooved intake zone. Pre-drying is normally unnecessary when the silo and conveying-air dew point are below −30 °C, but material stored in unheated warehouses at relative humidity above 80% can pick up surface moisture and should be dried at 80 °C for 2 h to 4 h with a desiccant dryer before extrusion. The pipe die should be cleaned after every 10 days of continuous operation because oxidized resin at the die lip creates die lines and increases surface roughness. Failure to control this oxidized layer is a common cause of lot rejection in water pipe because surface damage reduces the slow crack growth resistance measured by ISO 13479.
For gas distribution service, HD50100Y is converted into black pressure pipe with a coextruded yellow skin conforming to ISO 4437-1, EN 1555-1, and GB 15558.1. The base pipe is extruded with the same screw geometry and thermal profile used for potable water pipe, but the head is fitted with a coextrusion die that applies a yellow PE carrier skin at 0.15 mm to 0.25 mm final thickness. The skin extruder is charged with 5 wt% to 7 wt% yellow pigment masterbatch let-down in an HDPE carrier; the pigment concentration in the final skin is selected to achieve the colour coordinates specified in the gas operator’s purchasing specification because colour fade after pipe storage in sunlight is a rejection cause. Gas containment margins are derived from the same PE100 MRS of 10 MPa, but the design coefficient is raised to 2.0 for gaseous fuels; the allowable hoop stress becomes 5.0 MPa, and SDR 11 pipe is rated for an MOP of 10 bar at 20 °C. Most network operators further cap operating pressure at 7 bar to accommodate surge pressure, third-party excavation loads, and soil movement. Before type approval, the compound must pass the rapid crack propagation test of ISO 13477 at 0 °C using the S4 method; for HD50100Y, the critical pressure at which a crack stops after initiation is a function of wall thickness and pipe diameter, and the pipe manufacturer must report the critical pressure value on the test certificate. Butt fusion welding of gas pipe is carried out at a heater plate temperature of 200 °C to 220 °C with a bead-up pressure of 0.15 MPa and a fusion pressure of 0.10 MPa to 0.15 MPa, with exact values following ISO 21307:2017 procedures. The finished pipe is degassed in racks for 24 h before hydrostatic proof testing at 1.5 times the MOP for 1 h. Extruder output must be matched to the fusion-bead removal stage because a thick yellow skin that exceeds 0.30 mm can interfere with electrofusion saddle fittings.
| SDR | Design coefficient C | Allowable hoop stress σₛ (MPa) | MOP at 20 °C (bar) | Typical service |
|---|---|---|---|---|
| 11 | 1.25 | 8.0 | 16 | Potable water, general industrial liquids |
| 17 | 1.25 | 8.0 | 10 | Potable water distribution |
| 11 | 2.0 | 5.0 | 10 | Gas distribution MOP, with operator derating |
| 17 | 2.0 | 5.0 | 6.25 | Gas distribution lower-pressure lines |
| 7.4 | 1.25 | 8.0 | 25 | Slurry/tailings with abrasion allowance |
| 9 | 1.25 | 8.0 | 20 | Slurry/tailings with abrasion allowance |
Corrugated drainage pipe extrusion from HD50100Y is configured for gravity-flow stormwater and highway culvert duties where the requirement shifts from internal pressure resistance to ring stiffness and fatigue under cyclic wheel loading. The corrugator is fed by a single-screw extruder with a length-to-diameter ratio of 30:1 to 36:1, and the melt is delivered to a horizontal corrugating head at 210 °C to 230 °C. The parison is inflated into vacuum-forming blocks at a vacuum level of 0.06 MPa to 0.08 MPa; the line speed for DN/OD 110 pipe is typically 1.0 m/min to 1.5 m/min, while DN/OD 800 pipe runs at 0.2 m/min to 0.4 m/min. Carbon black masterbatch is added at 2.0 wt% to 2.5 wt% final carbon black content for outdoor storage. Ring stiffness classification is confirmed by ISO 9969; for a structured-wall PE pipe, SN 8 requires a nominal ring stiffness of 8 kN/m², and SN 16 requires 16 kN/m². The corrugated geometry is specified by the mold block profile, not by a simple wall thickness formula, so the processor must maintain the melt strength of HD50100Y at the upper end of the allowable thermal window to prevent valley thinning between corrugation crests. Every 200 m of pipe is checked for inner-wall smoothness and crest thickness using a strip-section comparison against the mold drawing. Because HD50100Y is a pressure-pipe compound with a relatively high molecular weight, it provides melt strength during parison drawdown, but the exact sag resistance at 250 °C must be validated with the corrugator’s parison length because published data for this specific configuration is limited.
HD50100Y is suited for thick-wall slurry and tailings pipe only when the design basis follows the ISO 9080 hydrostatic strength curves and the system designer adds an abrasion allowance to the wall thickness because the internal pressure rating alone does not account for particle erosion. In a 250 mm to 1200 mm diameter line, the pipe is often specified as SDR 7.4 for pressures up to 25 bar, SDR 9 for 20 bar, or SDR 11 for 16 bar at 20 °C, with an additional sacrificial wear layer of 3 mm to 10 mm over the service life. Extrusion of these thick sections requires an extruder with an L/D ratio of at least 36:1, a grooved feed section, and an internal pipe cooling system to remove heat from the inside surface of the wall; without internal air cooling, wall thicknesses above 30 mm develop sag and asymmetric eccentricity. The melt temperature is held at 200 °C to 215 °C, and the extruder is run at the highest practical back pressure, between 30 MPa and 38 MPa, to draw unmelted high-molecular-weight fraction out of the grooved intake zone. The compound is dry-blended with 2.5 wt% carbon black masterbatch and optionally with 0.1 wt% to 0.2 wt% fluoropolymer processing aid to reduce die build-up at the high head pressures used for thick-wall pipe. Long-term hydrostatic testing is performed according to ISO 1167-1 at 80 °C and 5.0 MPa hoop stress to screen for slow crack growth failures; the notched pipe test of ISO 13479 at 80 °C may also be used to compare lot-to-lot resistance. Field joints are made by butt fusion or electrofusion, and the pipe is laid with a minimum burial cover of 1.0 m under haul roads to avoid point loads that cause local stress concentration on the pipe crown. The processor must also verify that the fusion pressure settings are adjusted for the thicker wall because residual melt near the inside diameter is slower to cool after fusion, and asymmetric solidification can produce a weak joint.
Smooth-wall cable ducting from HD50100Y is produced on the same grooved-barrel extrusion platform but is not hydrostatically derated because the product is installed under IEC 61386-1:2008 and UL 651 as a protective conduit, not as a pressure pipe. The formulation for outdoor duct includes 2.0 wt% to 2.5 wt% carbon black masterbatch; indoor duct may be natural if the electrical specification allows. A 60 mm extruder running a 110 mm OD duct at a wall thickness of 4.0 mm to 6.0 mm typically operates at a screw speed of 30 rpm to 40 rpm and a haul-off speed of 1.5 m/min to 2.5 m/min. The pipe is vacuum-sized in a 6 m to 8 m cooling tank, then cut to length and belled on-line at 120 °C to 140 °C for spigot insertion. Crush strength and impact resistance are tested at −5 °C per the applicable specification; the values required depend on the duct class, not on the resin’s hydrostatic rating. Because HD50100Y contains the typical PE100 stabilization package, the conduit producer must verify that the stabilization package does not conflict with the conductivity requirements of the final conduit if a conductive carbon black layer is coextruded for anti-static service.
When HD50100Y is evaluated for outer casing pipe in pre-insulated bonded district heating systems, the applicable specification is EN 253:2019, which governs the dimensions, mechanical properties, and aging resistance of the HDPE jacket pipe. The casing pipe is extruded at a melt temperature of 190 °C to 220 °C and vacuum-sized with a wall thickness calculated from the specified outer diameter and the insulation annulus; typical diameters range from 125 mm to 1200 mm. The jacket compound is formulated with 2.0 wt% to 2.5 wt% carbon black masterbatch for ultraviolet stability and must retain a tensile elongation at break above 350% after exposure to the aging conditions given in EN 253:2019. For return lines operating at lower temperatures than the supply line, the thermal load on the HDPE jacket is reduced, but the casing is still exposed to soil-side mechanical stress and oxidation from outdoor storage. The processor must control the regrind fraction; EN 253:2019 allows the use of own regrind only when its maximum level is covered by the manufacturer’s type test, and many pipe makers cap regrind at 20 wt% to avoid a loss in stress crack resistance. Foam adhesion to the HDPE jacket is checked by a peel test on a cut section of the pre-insulated pipe; if the inner surface of the jacket is excessively oxidized, adhesion to the polyurethane foam fails. HD50100Y is not a tank-liner or geomembrane compound, and its use in this application must be confirmed by the pipe manufacturer’s EN 253:2019 type approval because published data for HD50100Y in district heating jacket service is limited.
| Conversion segment | Normative base | Critical test method | Measured property |
|---|---|---|---|
| Potable water pressure pipe | ISO 4427-1, EN 12201-1 | ISO 1167-1 | Hydrostatic strength at 20 °C/80 °C |
| Gas distribution pipe | ISO 4437-1, EN 1555-1, GB 15558.1 | ISO 13477 | Rapid crack propagation critical pressure |
| Corrugated drainage | ISO 21138-1, EN 13476-2 | ISO 9969 | Ring stiffness kN/m² |
| Slurry pipe | ISO 4427-1, ISO 9080 | ISO 1167-1, ISO 13479 | Slow crack growth resistance |
| Cable conduit | IEC 61386-1, UL 651 | Crush test, impact at −5 °C | Crush strength, impact resistance |
| District heating jacket | EN 253:2019 | Tensile elongation after aging | Elongation at break, adhesion |
Competitive Yanchang China Coal Yulin (Shaanxi) HDPE HD50100Y prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Yanchang China Coal Yulin (Shaanxi) HDPE HD50100Y is a high-density polyethylene base resin for pressure pipe extrusion. The grade is supplied as natural pellets and is classified within the PE100 hydrostatic design category under ISO 12162 and ISO 9080. Lot-release data typically place the melt mass-flow rate at 190°C under a 5 kg load in the range of 0.20–0.30 g/10 min, with density in the range of 0.949–0.953 g/cm³. The low melt-flow index is intentional: it preserves the high-molecular-weight fraction responsible for long-term hydrostatic strength and slow crack growth resistance. These values are representative of PE100-class pipe grades and must be verified against the manufacturer’s certificate of analysis before extrusion.
The material is intended for pressure pipe applications where the 20°C 50-year lower predictive limit is not less than 10.0 MPa. This classification follows ISO 9080 regression data and the ISO 12162 material designation. The melt-state boundary conditions are defined by low melt-flow and high zero-shear viscosity; these properties generate high melt strength in large-diameter pipe tooling but also limit heat transfer and require controlled screw speed. Table 1 compares the product envelope with the PE100 class reference envelope drawn from published pipe-grade data sheets; lot-specific values may differ.
| Property | Test method | Unit | HD50100Y typical range or minimum | PE100 class reference range or minimum |
|---|---|---|---|---|
| Melt mass-flow rate, 190°C/5 kg | ISO 1133-1:2022 | g/10 min | 0.20–0.30 | 0.20–0.40 |
| Density | ISO 1183-1:2019 | g/cm³ | 0.949–0.953 | 0.949–0.955 |
| Tensile stress at yield | ISO 527-2:2012 | MPa | ≥23 | ≥22 |
| Elongation at break | ISO 527-2:2012 | % | ≥600 | ≥500 |
| Notched Charpy impact at −30°C | ISO 179-1/1eA:2023 | kJ/m² | ≥10 | ≥8 |
| Environmental stress cracking resistance, Condition B, 100% Igepal | ASTM D1693-21 | h | >500 | >300 |
| Oxidative induction time at 200°C | ISO 11357-6:2018 | min | ≥20 | ≥20 |
The density above 0.949 g/cm³ contributes to pipe stiffness and creep resistance. In bimodal resins of this class, the low-molecular-weight population raises crystallinity and modulus, while the high-molecular-weight population forms tie molecules that resist slow crack growth. This division of molecular architecture is the principal reason the material is not directly interchangeable with generic unimodal HDPE of similar density and melt-flow.
In a bimodal HDPE pipe resin, short-chain branch placement is concentrated in the high-molecular-weight chains, increasing the number of tie molecules between lamellae. The resulting semicrystalline network delays crack initiation and suppresses the transition from brittle slow crack growth to fast crack propagation under sustained internal pressure. In standardized terms, the PE100 designation requires a minimum required strength of 10.0 MPa at 20°C for 50 years under ISO 9080 extrapolation. The environmental stress cracking resistance value above 500 h under ASTM D1693-21 Condition B is characteristic of bimodal pipe grades; many unimodal HDPE grades of equivalent density and melt-flow can exhibit failure before 100 h in the same test. Published data for the specific HD50100Y configuration in notched pipe tests such as ISO 13479 remains limited and should be obtained from the manufacturer or validated on the finished pipe compound.
Comonomer type and distribution also influence hydrostatic strength. Butene-based short-chain branches are common in pipe resins, while hexene-based grades may exhibit higher slow crack growth resistance at the same density. Converters evaluating HD50100Y against alternative PE100 products should compare lot-release ESCR, melt-flow, and density, but also request ISO 9080 regression data for the specific pipe compound because carbon black masterbatch addition can shift the expected life curve. The oxidative induction time, measured at 200°C under ISO 11357-6:2018, is a minimum 20 min; this value is an antioxidant package indicator and does not alone confirm 50-year service life.
The molecular weight distribution of bimodal pipe resins typically shows a low-molecular-weight peak around 10^4–10^5 g/mol and a high-molecular-weight shoulder extending above 10^6 g/mol. This distribution produces shear thinning and permits extrusion at lower melt temperatures than a unimodal resin of similar melt-flow. The high-molecular-weight fraction also contributes to the melt strength needed for large-diameter pipe calibration. Specific molecular weight data for HD50100Y are not typically disclosed on standard certificates of analysis; gel permeation chromatography on the converter side is not routine and published data for this specific configuration is limited.
Rheological characterization is essential because the zero-shear viscosity of PE100 pipe resins can exceed 100,000 Pa·s at 190°C. In a capillary rheometer, the flow curve displays power-law shear thinning with an exponent typically between 0.35 and 0.45 for bimodal pipe grades. This shear thinning allows processability at commercial pipe extrusion shear rates despite the high molecular weight. The activation energy for flow of HDPE is approximately 25–30 kJ/mol, which means melt temperature changes of 10°C can alter viscosity by roughly 20–25%. On production lines, this sensitivity appears as back-pressure drift if barrel heaters and screw cooling are not tightly controlled. Published data for the specific HD50100Y lot viscosity curve is not widely distributed; converter process capability studies should collect in-line melt pressure and throughput data across the intended operating window.
Low-temperature impact performance follows from the bimodal architecture. The notched Charpy impact at −30°C of at least 10 kJ/m² supports handling and installation in cold climates, but this value does not replace hydrostatic or crack-propagation testing for pressure service. Fast crack propagation resistance, evaluated by full-scale tests such as ISO 13477 S4, is a separate requirement for larger-diameter or higher-pressure pipelines; data for HD50100Y in this specific test should be requested if the pipe is intended for gas distribution at diameters above 250 mm.
On a grooved-feed single-screw pipe extruder with L/D 33:1, the feed section is maintained at 60–90°C, the compression zone from 190°C to 220°C, and the die at 210–230°C. Melt temperature should not exceed 240°C; residence time above 220°C should remain below 45 min to limit thermo-oxidative chain scission. Pre-drying is unnecessary for dry pellet feed, but if storage has exposed the pellets to relative humidity above 60%, a desiccant dryer at 80°C for 2–4 h is recommended. Die head pressures in the range of 20–35 MPa are typical for PE100 pipe extrusion, depending on die gap, output, and melt temperature. Screw cooling in the feed zone prevents premature pellet melting and feed blockage; a spiral mandrel die with uniform melt distribution is required for large-diameter pipe, particularly above 630 mm OD. Haul-off speed and vacuum-sizing pressure must be matched to extruder output to avoid wall-thickness variation.
Production-scale failure modes observed with high-molecular-weight PE100 pipe grades include feed throat bridging, screw wrap, and melt-temperature stratification in the die. Feed throat bridging occurs when the feed section temperature exceeds 90°C; screw wrap occurs when the screw surface temperature is too high relative to the barrel. Melt stratification in large spiral mandrel dies can produce local wall-thickness variation if the die gap is not uniform. Therefore, melt-temperature profiling at the die exit is recommended, with a maximum observed spread of ±5°C for pipe above 630 mm OD.
Butt fusion joining of pipe produced from HD50100Y should follow ISO 21307:2017. The low melt-flow classification supports standard fusion plate temperatures near 200–230°C, but exact bead-up and heat-soak pressures must be established on the specific pipe dimension. Incorrect fusion pressure can produce cold welds or excessive melt displacement; field failures of PE100 pipe are frequently associated with non-compliance to the fusion standard rather than resin deficiency.
Substitution of a PE80 resin with HD50100Y changes the wall-thickness calculation under ISO 4427-2:2019. For PE100, the allowable hydrostatic design stress at 20°C is 8.0 MPa when a service coefficient of 1.25 is applied to the 10.0 MPa MRS. For PE80, the corresponding design stress is 6.4 MPa. A higher design stress permits a larger standard dimension ratio for the same nominal pressure rating, reducing mass per linear metre. However, the lower melt-flow of HD50100Y relative to a typical PE80 grade requires higher torque and careful barrel temperature profiling. Compared to unimodal HDPE pipe grades of similar density, HD50100Y demonstrates higher melt strength and lower sag in thick-wall sections, which supports concentricity during vacuum sizing. Converters replacing an existing unimodal resin should expect narrower processing parameters and may need to increase die temperature or reduce throughput to manage melt fracture at high output rates.
In buried pressure systems, the higher MRS value of PE100 also influences hydraulic design. For a given nominal diameter, a PE100 pipe may be specified with a thinner wall than PE80 at equivalent pressure class, but the external load resistance under soil and traffic loads must be checked using the ring stiffness formula. The tensile stress at yield of at least 23 MPa and elongation at break above 600% provide a basis for short-term burst capacity, but long-term performance is governed by slow crack growth and resistance to point loads. The material is not self-certifying as a PE100-RC grade under ISO 4437 or ISO 13479 point-load requirements unless the finished pipe compound has passed the additional notch and point-load tests.
Compared to PE100 grades designed for non-pressure applications, HD50100Y’s molecular architecture prioritizes creep rupture resistance over melt flow. Blow-molding HDPE grades with similar density but higher melt-flow do not meet the ISO 9080 hydrostatic strength requirement for pressure pipe. Conversely, PE100-RC grades with enhanced point-load resistance may be preferred in installation methods involving trenchless technology, rock impingement, or pipe bursting. HD50100Y should be qualified for such aggressive installation practices only after additional point-load and slow crack growth testing on the finished pipe, because published data for this specific configuration is limited.
Regulatory compliance is formulation-dependent. The base resin is supplied with a standard antioxidant and acid scavenger package, but outdoor weathering and UV resistance require converter addition of carbon black masterbatch. For drinking-water pipe, the finished pipe compound—not the base resin alone—must comply with the applicable national water-contact standard, such as GB/T 17219 or relevant local approvals. REACH (EC No 1907/2006) and RoHS Directive 2011/65/EU apply to the finished article; converters should obtain compliance declarations from masterbatch suppliers and verify the final product. The resin should not be processed above 240°C, and it is not intended for injection molding of thin-wall articles because the high melt viscosity leads to short shots and excessive injection pressure. Avoid blending with amine-based additive masterbatches in the absence of compatibility data; published data for this specific base resin in such combinations is limited.
The oxidative induction time at 200°C is a quality-control indicator, not a forecast of service life. Long-term aging of buried PE100 pipe involves depletion of antioxidant in the pipe wall; the Arrhenius extrapolation of OIT data is limited and should not be used to claim lifetime beyond the ISO 9080 hydrostatic regression. The base resin contains a phenolic antioxidant and acid scavenger; converter-added carbon black masterbatch must be selected for compatibility and dispersion. Poor carbon black dispersion can create micro-inhomogeneities that act as stress concentrators and lower slow crack growth resistance.
| Standard or regulation | Scope | Relevant test or clause |
|---|---|---|
| ISO 12162:2009 | Classification of polyethylene pipe materials | PE100, MRS 10.0 MPa |
| ISO 9080:2012 | Determination of long-term hydrostatic strength | 20°C, 50-year lower predictive limit |
| ISO 4427-2:2019 | PE piping systems for water supply — pipes | Dimensions for PE100 |
| GB/T 13663.2-2018 | Polyethylene pipes for water supply | PE100 pipe property requirements |
| ASTM D3350-21 | Polyethylene pipe and fittings materials designation | Cell classification for pipe-grade HDPE |
| GB/T 17219-1998 | Safety evaluation of drinking water distribution equipment | Finished pipe leaching and hygiene |
Processing limitations and incompatibilities must be confirmed on the production line. Batch-to-batch variance in melt-flow and molecular-weight distribution can shift back-pressure and choke points in grooved-feed extruders; therefore, converter acceptance testing should include melt-flow, density, and oxidation induction time for each lot. The grade is not intended for rotational molding, film extrusion, or injection molding of thin-wall articles. Outdoor storage of natural pellets should be avoided; if black pipe is required, carbon black content in the finished pipe must meet the relevant weathering standard, typically 2.0–2.5% by mass for ISO 4427 pipe.