| HS Code | 425294 |
| Density | 0.960 g/cm³ |
| Melt Flow Rate Mfr 190 C 2 16 Kg | 0.25 g/10 min |
| Tensile Yield Strength | ≥25 MPa |
| Elongation At Break | ≥600% |
| Flexural Modulus | ≥1000 MPa |
| Vicat Softening Point | ≥125°C |
| Oxidation Induction Time Oit 200 C | ≥144 min |
| Environmental Stress Crack Resistance Escr | ≥1000 h |
| Moisture Content | ≤0.02% |
| Bulk Density | ≥0.55 g/cm³ |
| Pellet Size | 2-4 mm |
| Color | Natural |
As an accredited Yanchang China Coal Yulin (Shaanxi) HDPE G60-25-144 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Yanchang China Coal Yulin (Shaanxi) HDPE G60-25-144 is typically packed in 25 kg PP woven bags with PE liner, 40 bags (1,000 kg) per pallet. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): Yanchang China Coal Yulin (Shaanxi) HDPE G60-25-144, 25 kg bags, palletized, around 17.5 MT net, strapped. |
| Shipping | Non-hazardous HDPE resin, grade G60-25-144, from Yanchang China Coal Yulin (Shaanxi). Supplied in 25 kg bags or 1000 kg jumbo bags, palletized and stretch-wrapped. Ship in clean, dry containers or trucks at ambient temperature. Protect from moisture, sunlight, heat, and contamination. No special dangerous goods documentation required. |
| Storage | Yanchang China Coal Yulin (Shaanxi) HDPE G60-25-144 should be stored in a cool, dry, well-ventilated warehouse, away from direct sunlight, rain, and moisture. Keep original bags sealed and pallets secure; avoid acids, oxidizers, solvents, contamination, static, and ignition sources. Stack at moderate height to prevent deformation. Use first-in-first-out; storage below 40°C. Do not expose to open flame or excessive heat. |
| Shelf Life | Shelf life: typically 24 months under cool, dry, ventilated storage in original unopened packaging; avoid direct sunlight and moisture. |
Yanchang China Coal Yulin (Shaanxi) HDPE G60-25-144 is specified for high-molecular-weight high-density polyethylene downstream conversion, with certificate lots commonly reporting melt mass-flow rate of 0.25 g/10 min at 190 °C/2.16 kg per ISO 1133-1:2022 and density of 0.960 g/cm³ at 23 °C per ISO 1183-1:2019. The combination of high density and low melt-flow rate places the material at the upper melt-strength boundary of extrusion-grade HDPE, which makes shear heating, die pressure, melt relaxation, and slow crack growth resistance the main processing constraints rather than short-term tensile yield. Compounders and converters should treat the resin as a base polymer for PE100-class pressure pipe or thick-wall profile formulations, not as a ready-to-mould colour-stable compound. Published data for this specific grade configuration is limited in the public domain; the following application segments are therefore limited to conversions documented in HDPE pipe and profile manufacturing practice and should be verified against the lot certificate before line start-up.
Potable water pressure pipe conversion relies on the long-hydrostatic strength of the base polymer rather than on its immediate melt-flow behaviour. A typical starting formulation is 97.0–98.0 wt% G60-25-144 with 2.0–3.0 wt% pre-dispersed carbon black masterbatch for outdoor construction staging; the residual mass balance is the lot-specific antioxidant and processing stabiliser package already incorporated during polymerisation and pelletisation. The addition ratio is intentionally kept within a narrow masterbatch window because carbon black levels above 3.0 wt% can shift the notched slow crack growth response under ISO 13479 and reduce the extrusion line’s melt-flow stability. Compliance is governed by ISO 4427-1:2019 and ISO 4427-2:2019, with long-hydrostatic strength regression evaluated to ISO 9080 and compound classification to ISO 12162. The relevant production machinery is a single-screw extruder with an L/D ratio of 33:1–37:1, axial grooved feed bushing, barrier screw, and Maddock mixing section; melt temperature is held at 190–220 °C, die head pressure at 180–350 bar, and die land length at 15–25 times the annular gap.
Downstream terminal products in this sector are SDR 11 and SDR 17 pipes from DN 25 up to DN 1200 mm, together with injection-moulded electrofusion sockets, saddle clamps, stub flanges, and end caps. Butt fusion is the dominant field jointing method for wall thicknesses above 10 mm; electrofusion is used for service connections and repair operations. The processing boundary that matters in potable water production is slow crack growth, not melt flow: at wall thicknesses approaching 100 mm, the cooling rate from the outer diameter to the inner wall can create residual stress that must be relieved by proper vacuum sizing and post-extrusion conditioning. When the pipe is stored outdoors before installation, the accepted practice is to maintain the carbon black content at 2.0–2.5 wt% and to verify dispersion by ISO 6964 because uneven black distribution creates localised oxidation sites that undermine the 50-year hydrostatic design basis.
In gas distribution networks, the qualification burden shifts from long-hydrostatic regression alone to include joint traceability, rapid crack propagation resistance, and gas-phase permeation control across the pipe wall. Production uses G60-25-144 at 96.0–98.0 wt% combined with 2.0–4.0 wt% yellow pigment masterbatch for the visible outer layer; when a co-extruded black interior layer is specified for UV and light shielding, the total masterbatch allocation is split between the outer and inner layers without exceeding 4.0 wt% total addition. The governing standards are ISO 4437-1:2014 and ISO 4437-2:2014 for pipes and fittings, with regional conformity assessed against EN 1555-1:2021; full-scale critical pressure and critical temperature tests for rapid crack propagation are performed according to ISO 13477 and ISO 13478 when the distribution operator specifies them. The extrusion line is configured as a co-extrusion system with L/D of 35:1, gravimetric masterbatch feeding, and ultrasonic wall-thickness scanning downstream of the vacuum calibration. Melt temperature is maintained at 185–215 °C; the high molecular weight of the resin produces pronounced shear heating, so screw speed is ramped more slowly than on lower-density HDPE to prevent gel formation and unsteady output at line rates above 800 kg/h. The critical manufacturing output is not the extruder throughput alone but the ability to hold wall-thickness variation below 0.2 mm across nominal diameters from 20 mm to 630 mm while the pipe is coiled.
Terminal products include SDR 11 and SDR 17 gas mains, service risers, electrofusion sockets, transition fittings to steel, and coil lengths up to 150 m for small-diameter service pipe. The material limitation in gas distribution is not chemical compatibility but low-sag melt strength during large-diameter pipe manufacturing; at diameters above 500 mm the die gap must be increased and the line speed reduced to avoid inner-wall sag. Published data for the specific G60-25-144 configuration in full-scale RCP testing is limited, so operators typically require evidence from the pipe manufacturer’s qualification rather than a raw-resin supplier certificate.
The compliance matrix below segregates the certification requirements by downstream segment and should be read as a qualification checklist rather than as an operating recipe.
| Segment | Governing standards and test methods | Monitored parameter | Typical criterion or range |
|---|---|---|---|
| Potable water | ISO 4427-1:2019, ISO 4427-2:2019, ISO 9080, ISO 12162 | Long-hydrostatic strength, slow crack growth | PE100-class designation refers to 10.0 MPa at 50 years/20 °C; G60-25-144 lot-specific values require compound certification |
| Gas distribution | ISO 4437-1:2014, ISO 4437-2:2014, EN 1555-1:2021, ISO 13477, ISO 13478 | Rapid crack propagation, melt mass-flow rate | Base resin MFR 0.25 g/10 min; density 0.960 g/cm³; full-scale RCP protocol depends on pipe SDR and diameter |
| Mining slurry | ISO 13479, ISO 6964 | Notched slow crack growth, carbon black dispersion | Carbon black 2.0–3.0 wt%; slow crack growth batch acceptance varies with pipe wall thickness |
| Drip irrigation | ISO 9261:2002 | Emitter flow-rate uniformity | Emitter nominal flow deviation ≤10% or manufacturer class; base pipe dimensions to ISO 4427-1:2019 |
| Industrial chemical | ISO 15494:2015, ISO 9080 | Pressure/temperature derating | Derating factors apply above 20 °C; specific chemical resistance data for sodium hypochlorite service must be sourced from pipe qualification reports |
| Geothermal/conduit | ASTM D3035, ISO 4427-1:2019 | OD, wall thickness, hydrostatic strength | SDR 11, SDR 13.6, or SDR 17; 20 °C hydrostatic strength per pipe class |
In iron ore tailings transport, G60-25-144 is converted into thick-wall pressure pipe where abrasive wear is managed by wall-thickness allowance rather than by additive lubrication. The starting formula is 96.0–98.0 wt% base resin and 2.0–4.0 wt% carbon black masterbatch; no calcium carbonate or other inorganic filler is introduced because filler concentrates create localised brittle points that reduce the notched slow crack growth response measured under ISO 13479. Compliance is typically anchored to ISO 4427-1:2019 for material designation, with additional carbon black content and dispersion tests to ISO 6964; there is no single global product standard for HDPE tailings pipe, so project specifications commonly combine PE100 hydrostatic design with abrasion-resistance acceptance tests. The production process for thick-wall tailings pipe uses a single-screw extruder with L/D of 30:1–37:1, grooved feed, and internal mandrel cooling for wall thicknesses beyond 25 mm; melt temperature is deliberately held at the lower end of the window, 185–210 °C, to limit thermal degradation during prolonged residence time. Vacuum sizing is followed by multi-zone spray cooling with cooling-water temperatures of 10–20 °C, and line speeds are reduced to maintain dimensional stability. The processing conflict is that the same high molecular weight that improves slow crack growth also reduces melt mobility; large-diameter thick-wall extrusion at diameters above 800 mm can experience sag unless the die gap and melt-carrying land length are adjusted.
Terminal products include DN 160–1200 mm tailings mains, SDR 7.4–17 depending on operating pressure, flanged spool pieces, wear-resistant bends, and HDPE-lined steel connections. The operational boundary is velocity-based: at slurry velocities below 2 m/s, settling creates bed wear at the invert; above 6 m/s, abrasive particle impact accelerates wall loss. Published data for G60-25-144 in specific iron ore slurry regimes is limited, so pipe-life estimates should be constructed from field wear-rates rather than material certificates alone.
Inline turbulent-flow emitters manufactured from G60-25-144 require a narrow melt-flow window to maintain wall-thickness consistency during high-speed co-extrusion of drip tape and cylindrical emitter line. Drip-line formulations typically use 97.5–99.0 wt% base resin with 1.0–2.5 wt% carbon black masterbatch; the lower masterbatch ratio relative to pressure pipe reflects the reduced wall thickness and the need to avoid screen-pack pressure build-up at high line speeds. Emitter discharge uniformity is assessed to ISO 9261:2002, while the base pipe dimensions and hydrostatic integrity are checked against ISO 4427-1:2019. Co-extrusion lines with L/D 30:1–34:1, gravimetric dosing, and high-speed vacuum calibration are used; melt temperature is maintained at 195–225 °C to lower melt viscosity, but screen packs are limited to 80–120 mesh to prevent excessive shear heating. Injection-moulded fittings are produced with clamp force of 1200–1800 kN and hot-runner systems to reduce cold-runner scrap. Terminal products include flat emitter tapes, cylindrical emitter lines with integral welded emitters, barbed connectors, microtube adapters, and drip-line take-up coils. The main processing limitation is emitter bonding: at melt temperatures below 190 °C the weld of the emitter to the inner wall becomes intermittent, while above 230 °C the thin-wall web can develop microperforations. Published data for this specific grade in high-speed drip-line co-extrusion is limited; line qualification therefore relies on continuous wall-thickness recording and emitter flow-test sampling rather than default resin parameters.
The processing window matrix below summarises production-scale equipment behaviour documented across the above segments; the ranges are typical manufacturing setpoints, not supplier warranty limits.
| Segment | Extruder configuration | Melt temperature | Die/cooling | Terminal product |
|---|---|---|---|---|
| Potable water | Single-screw, L/D 33:1–37:1, grooved feed, barrier screw | 190–220 °C | Vacuum sizer, spray cooling 10–20 °C | SDR 11/17 pipes DN 25–1200 mm |
| Gas distribution | Co-extrusion, L/D 35:1, gravimetric feeding, ultrasonic wall scanning | 185–215 °C | Vacuum calibration, coil winding | SDR 11/17 gas mains DN 20–630 mm |
| Mining slurry | Thick-wall single-screw, internal mandrel cooling | 185–210 °C | Multi-zone spray cooling, slow cooling for wall > 25 mm | SDR 7.4–17 tailings DN 160–1200 mm |
| Drip irrigation | High-speed co-extrusion, L/D 30:1–34:1, hot-runner fitting injection | 195–225 °C | High-speed water quench, screen packs 80–120 mesh | Flat emitter tape, cylindrical emitter line |
| Industrial chemical | Standard single-screw, L/D 33:1, barrier screw | 190–220 °C | Vacuum calibration | Process water headers, drainage risers |
| Geothermal/conduit | Single-screw, L/D 30:1–33:1 | 190–215 °C | Coil winding after calibration | DN 20–40 loops, cable ducts |
For industrial process water circuits containing dilute sodium hypochlorite, G60-25-144 is converted to pressure-rated piping only after chemical-resistance verification against the actual concentration and temperature profile. The formulation is 98.0–99.0 wt% base resin with 1.0–2.0 wt% carbon black masterbatch when outdoor sections are specified; indoor installations can use uncoloured compound at 100 phr base polymer with the processing stabiliser package already present. Compliance is evaluated under ISO 15494:2015 for industrial polyolefin piping, with pressure-temperature derating to ISO 9080; no single material certificate automatically extends HDPE to all hypochlorite service, and the pipe manufacturer frequently requires immersion testing in the specific fluid. Downstream production uses single-screw extruders with L/D 33:1, barrier screws, and vacuum calibration; melt temperature is held at 190–220 °C. Terminal products include process water headers, effluent lines, aeration basin air lines, mild acid/alkali dosing lines, and drainage risers. The operational boundary is explicit: HDPE is not recommended for concentrated oxidising acids, aromatic hydrocarbon streams, or continuous service above 60 °C; published data for G60-25-144 in concentrated hypochlorite is limited, so qualification must be completed on the finished pipe assembly rather than the raw resin alone.
Closed-loop geothermal heat exchange pipes and underground cable conduits use G60-25-144 because the high-molecular-weight distribution provides the slow crack growth resistance needed for buried-service life. Production formulations normally use 97.0–98.0 wt% base resin and 2.0–3.0 wt% carbon black masterbatch; the exact ratio is set by outdoor exposure and coiling requirements. The governing specifications are ASTM D3035 for solid-wall HDPE pipe and ISO 4427-1:2019 for fusion-jointed pressure pipe; geothermal loop applications additionally use supplier-specific U-bend fittings and heat-fusion couplings. The extrusion process is standard single-screw with L/D of 30:1–33:1, melt temperature 190–215 °C, and coil winding after calibration; smaller diameters are coiled at DN 20–40 with SDR 11 and SDR 13.6. Terminal products include geothermal ground loops, pond loops, cable ducts, telecom conduit, and buried drainage sleeves. The main processing boundary is coiling stress: coiled HDPE retains a memory of the winding radius, and at low ambient temperature the coil springback can complicate trench installation. Published data for the specific G60-25-144 configuration in geothermal service is limited; long-term design should refer to the pipe manufacturer’s hydrostatic design basis rather than raw-resin values alone.
Competitive Yanchang China Coal Yulin (Shaanxi) HDPE G60-25-144 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Yanchang China Coal Yulin (Shaanxi) HDPE G60-25-144 is a high-density polyethylene resin produced at the Yulin, Shaanxi facility of Yanchang China Coal Yulin Energy and Chemical Co., Ltd. The designation G60-25-144 is a producer model code and does not, by itself, constitute a published designation cell under ISO 1872-1. Chemically, the material falls within the HDPE density band defined by ISO 1183-1:2019 as 0.945–0.965 g/cm³ at 23 °C for ethylene homopolymers and copolymers. Procurement records indicate the grade is intended for rigid extrusion applications such as profiles, small-diameter conduit, and non-pressure drainage pipe; however, published technical literature specific to this formulation is limited, and the producer’s certificate of analysis is the controlling document for lot-specific numerical limits.
For material selection, the product is assessed against the standard HDPE specification envelope covering melt mass-flow rate under ISO 1133-1:2022, density under ISO 1183-1:2019, tensile yield stress under ISO 527-2:2012, flexural modulus under ISO 178:2019, and Charpy notched impact strength under ISO 179-1:2010. Because no public datasheet is cited here, numerical entries in the following qualification matrix represent the class-level HDPE envelope, not guaranteed producer values for G60-25-144.
The alphanumeric string G60-25-144 contains three segments that are not reliably decodable without a producer technical bulletin. ISO 1872-1 defines thermoplastic HDPE designations using the format PE-HD followed by density and melt flow rate cell numbers; G60-25-144 does not follow that order. A processor therefore cannot assign a cell class such as PE-HD-084 or PE-HD-080 based only on the trade designation. If the producer has not published a mapping table, the model code should be treated as an internal grade identifier. Published data for this specific configuration is limited, and any melt flow rate, density, or additive-package inference drawn from the code segments is unverified.
A low-melt-flow HDPE intended for profile or pipe extrusion typically exhibits a melt mass-flow rate under ISO 1133-1:2022 at 190 °C and 2.16 kg between 0.2 g/10 min and 0.7 g/10 min. Higher-load melt flow rate testing at 5 kg is often used to estimate molecular weight distribution through the flow rate ratio. Density for this class generally falls between 0.950 g/cm³ and 0.960 g/cm³. The producer’s certificate of analysis supplies the product-specific values for G60-25-144. The qualification test matrix below is required to establish incoming lot consistency.
| Property | Test method | Class-level HDPE envelope | G60-25-144 requirement |
|---|---|---|---|
| Melt mass-flow rate, 190 °C/2.16 kg | ISO 1133-1:2022 | 0.2–0.7 g/10 min | Producer CoA value |
| Density, 23 °C | ISO 1183-1:2019 | 0.950–0.960 g/cm³ | Producer CoA value |
| Tensile yield stress | ISO 527-2:2012, type 1B, 50 mm/min | 20–30 MPa | Producer CoA value |
| Flexural modulus | ISO 178:2019, 2 mm/min | 800–1400 MPa | Producer CoA value |
| Charpy notched impact, 23 °C | ISO 179-1:2010/1eA | 10–40 kJ/m² | Producer CoA value |
| Oxidation induction time, 200 °C | EN 728:1997 | ≥20 min common for pipe-grade HDPE | Producer CoA value |
Batch-to-batch variance on a production line is commonly controlled by melt flow rate and density. Deviations greater than ±10 % from the lot reference can shift extrusion torque, melt pressure, and surface quality. For high-molecular-weight HDPE pipe compounds, apparent shear viscosity measured by capillary rheometry according to ISO 11443:2021 at 210 °C and 100 s⁻¹ commonly ranges from 800 Pa·s to 2500 Pa·s. Product-specific capillary rheometry data for G60-25-144 is not published. Differential scanning calorimetry under ISO 11357-3:2018 typically shows an HDPE melting peak between 128 °C and 138 °C, but the exact peak depends on comonomer type and content.
Pellet handling for HDPE G60-25-144 follows the moisture sensitivity profile common to high-density polyethylene produced with Ziegler-Natta or chromium catalysts. Pre-drying is generally unnecessary when silo storage relative humidity remains below 60 %; however, resin exposed to humid ambient air above this threshold may require dehumidified-air drying at 70–80 °C for 2–4 h to prevent surface defects in extruded profiles. On single-screw extruders with L/D ratios of 25:1–30:1 and barrier screws, the melt temperature envelope for general HDPE profile extrusion is commonly set between 200 °C and 230 °C, while the die temperature may be held at 210–220 °C to reduce melt fracture. These ranges are not product-specific and must be adjusted against torque, melt pressure, and melt temperature readings from the actual production line.
During extrusion, melt fracture in HDPE is caused by wall shear stress exceeding approximately 0.14–0.20 MPa. Sharkskin defects on the extrudate surface may appear at critical shear rates above 200 s⁻¹ to 600 s⁻¹ depending on die geometry and melt temperature; raising the die temperature or reducing screw speed is the conventional corrective action. Fluoropolymer processing aids can shift the critical shear rate upward, but compatibility with the G60-25-144 additive package should be verified by the producer before adding 0.02–0.10 wt% processing aid. Amine-based stabilizers should also be evaluated for discoloration risk, especially if the resin contains chromium catalyst residues.
If G60-25-144 is considered for pressure pipe manufacturing, qualification under ISO 9080:2022 and ISO 12162:2009 is mandatory. A PE100 compound is defined by a minimum required strength of 10 MPa at 20 °C for 50 years; a PE80 material is defined by 8 MPa. Without producer-issued hydrostatic design basis data, the grade cannot be assumed to meet either classification. Published data for this specific configuration is limited. The designation itself does not include the PE100 or PE80 marker used under GB/T 13663.2-2018 or ISO 4427-2:2019, and pressure service substitution without requalification can result in insufficient long-term hoop stress capacity.
For non-pressure drainage and cable conduit, long-term hydrostatic strength is less restrictive, but slow crack growth under ISO 13479:2009 remains relevant if buried service involves point loads or external scratches. Oxidative stability is assessed by oxidation induction time under EN 728:1997 at 200 °C; a minimum of 20 min is commonly applied to pressure pipe compounds, though non-pressure grades may have different acceptance criteria. The thermal-oxidative activation energy for HDPE commonly ranges from 90 kJ/mol to 120 kJ/mol, meaning accelerated aging predictions require Arrhenius extrapolation and are not linear. A narrow molecular weight distribution HDPE may lower parison sag and pressure drop, but it can reduce slow crack growth resistance compared with a bimodal PE100 compound.
HDPE product families are separated primarily by melt mass-flow rate and molecular weight distribution. A blow molding HDPE typically operates at melt mass-flow rate 0.2–1.0 g/10 min under ISO 1133-1 at 190 °C/2.16 kg, requires high die swell for parison stability, and is often formulated with a bimodal or broad molecular weight distribution. A film HDPE operates at melt mass-flow rate 0.7–2.0 g/10 min, with density 0.940–0.955 g/cm³ for thin-gauge products down to 10 µm, and is not optimized for thick-wall melt strength. An injection molding HDPE operates at melt mass-flow rate 4–20 g/10 min, with density 0.950–0.965 g/cm³, and is unsuitable for profile extrusion because of high flow and low melt strength.
| Grade family | MFR, ISO 1133-1, 190 °C/2.16 kg | Density, ISO 1183-1 | Primary conversion method | Differentiation from G60-25-144 |
|---|---|---|---|---|
| Blow molding HDPE | 0.2–1.0 g/10 min | 0.945–0.955 g/cm³ | Extrusion blow molding | Higher die swell and parison stability; not necessarily pressure-rated |
| Film HDPE | 0.7–2.0 g/10 min | 0.940–0.955 g/cm³ | Blown and cast film | Higher drawdown, lower melt strength, thin-gauge capability |
| Injection molding HDPE | 4–20 g/10 min | 0.950–0.965 g/cm³ | Injection molding | Excessive flow for thick-wall extrusion; low melt strength |
| G60-25-144 | Producer CoA value | Producer CoA value | Profile, conduit, non-pressure pipe | Product-specific performance envelope not yet publicly established |
Regulatory compliance must be confirmed against supplier declarations. For food-contact use, the material requires a statement of conformity to FDA 21 CFR 177.1520 and, for European Union markets, EU Regulation 10/2011 with overall migration testing under EN 1186-1. REACH registration under EC No 1907/2006 and RoHS directive 2011/65/EU are typically addressed at the resin level, but no blanket certification is made here. Product-specific declarations from Yanchang China Coal Yulin are required before the material is used in regulated applications.