Yanchang China Coal Yulin Shaanxi Hdpe B50 35h 111

Yanchang China Coal Yulin (Shaanxi) HDPE B50-35H-111

    • Product Name: Yanchang China Coal Yulin (Shaanxi) HDPE B50-35H-111
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 677735
    Product Name Yanchang China Coal Yulin (Shaanxi) HDPE B50-35H-111
    Polymer Type High Density Polyethylene (HDPE)
    Density 0.950 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.35 g/10 min
    Tensile Yield Strength 26 MPa
    Tensile Break Strength 30 MPa
    Elongation At Break 600%
    Flexural Modulus 1100 MPa
    Notched Izod Impact Strength 60 kJ/m²
    Vicat Softening Point 125°C
    Heat Deflection Temperature 75°C
    Shore D Hardness 65
    Environmental Stress Crack Resistance >1000 h
    Brittleness Temperature -70°C
    Water Absorption <0.01%
    Melt Temperature 190-210°C
    Mold Shrinkage 1.5-3.0%
    Color Natural
    Form Pellets

    As an accredited Yanchang China Coal Yulin (Shaanxi) HDPE B50-35H-111 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Yanchang China Coal Yulin (Shaanxi) HDPE B50-35H-111 comes in 25 kg net PP woven bags, palletized, or 1000 kg jumbo bags.
    Container Loading (20′ FCL) Loaded in 20′ FCL with 25kg bags, 22MT per container, unpalletized, for Yanchang China Coal Yulin (Shaanxi) HDPE B50-35H-111.
    Shipping Yanchang China Coal Yulin (Shaanxi) HDPE B50-35H-111 is a non-hazardous high-density polyethylene resin. It is typically shipped in 25 kg PP woven bags or 500–1000 kg jumbo bags, palletized and stretch-wrapped. Store in a cool, dry, ventilated area, away from direct sunlight, heat, and moisture. Standard truck, rail, or sea freight applies.
    Storage Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and oxidizing agents. Keep original packaging sealed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and extreme temperatures. Stack pallets securely, observe safe load limits, and follow first-in, first-out inventory. Use appropriate handling equipment and comply with the manufacturer's SDS and local regulations.
    Shelf Life Shelf life: typically 24 months in original unopened packaging, stored cool, dry, ventilated, away from direct sunlight, heat, and contaminants.
    Application of Yanchang China Coal Yulin (Shaanxi) HDPE B50-35H-111

    Extrusion blow-molded HDPE B50-35H-111 is assigned to UN-certified industrial jerrycans in the 5–25 L segment when the lot is qualified with an MFR of 0.35 dg/min at 190 °C/2.16 kg under ISO 1133-1:2022 and with a density near 0.950 g/cm³ under ISO 1183-1:2019. On shuttle machines fitted with 24:1 L/D barrier screws and accumulator heads, the resin is processed at die-exit melt temperatures between 190 °C and 215 °C. Wall-thickness control is assigned to 100-point parison programming, with thickened sections at the chime, handle, and bottom pinch area. The dominant failure mode in 49 CFR 178.603 drop impact is not sidewall burst but stress-whitened fracture along the pinch-off weld, particularly after conditioning at −18 °C. The tail-flash mass fraction is controlled below 25 wt%, and regrind content above that level requires re-qualification under ASTM D1693-15 Condition B in 100% Igepal CO-630. Mold coolant inlet temperatures are maintained at 12–18 °C to balance cycle time against outer-skin crystallinity. Surface moisture from storage at relative humidity above 60% is removed by drying at 80 °C for 2–4 h before extrusion; otherwise splay and pinhole defects appear on the inner wall.

    What Limits Parison Hang-Time When Molding 200 L Open-Head Drums?

    Open-head 200 L drums consume parison weights from 8 kg to 14 kg depending on specified wall thickness. The limiting variable between die exit and mold close is melt strength, not extruder throughput. Single-station accumulator machines with 120 mm grooved-feed extruders and 30:1 L/D are operated with barrel profiles from 170 °C in the feed zone to 205–210 °C at the head. Published data for HDPE B50-35H-111 in this exact configuration is limited, so hang-time targets are typically established on a fixed parison length and mass. Industrial practice accepts less than 10% length change over the first 20 s at melt temperature. If parison sag exceeds this threshold, the parison programmer adds a thicker bottom band and a narrower top curl zone. Blow air is introduced in two stages at 0.8–1.0 MPa to avoid bubble oscillation. Cooling time for a 6 mm sidewall is observed in the 180–240 s range because heat removal scales with wall thickness squared. Deflashing leaves a tail weight of 15–25% of parison mass; the regrind is dried and screened before letdown into virgin resin.

    Fluorination and Permeation Control in Blow-Molded Diesel Filler Necks

    For automotive evaporative emission systems, blow-molded HDPE B50-35H-111 filler necks and shells are selected for low-temperature drop impact resistance under ASTM D2463-15 at −40 °C. The main process conflict is the combination of thin-wall geometry with a fully fused pinch-off at each end. In automotive fuel systems, evaporative emission limits are set by the applicable EPA or CARB category, and permeation tests are usually conducted according to OEM-specific procedures; published data for this grade in continuous fuel contact is limited. Where neat HDPE is approved, post-molding surface fluorination is performed in a reactor at 0.1–1.0% fluorine in nitrogen. The treatment creates a barrier layer without changing the base resin mechanical properties. Multi-layer parison with EVOH is an alternative but requires a tie-layer channel and a die-head window controlled within ±5 °C to prevent interfacial instability. Leak testing after full assembly is run at 0.05 MPa internal air pressure for 30 s. The pinch-off tail width is held between 4 mm and 7 mm; narrower tails produce microvoids that become permeation paths, while wider tails increase deflashing energy and regrind load.

    In pesticide and herbicide packaging in the 0.5–10 L range, HDPE B50-35H-111 is judged primarily by environmental stress crack resistance rather than short-term tensile yield. Concentrates based on aromatic solvents, ketones, or nonionic surfactants attack the pinch-off weld and the label-panel flex zone. Candidate containers are therefore qualified with drop impact per 49 CFR 178.603 after conditioning at −18 °C, hydrostatic pressure retention per 49 CFR 178.605, and ESCR per ASTM D1693-15 Condition B. The extrusion blow-molding line uses a 55–65 mm extruder with 24:1 L/D and a low-shear screw, with melt temperature limited to 195–210 °C. The die gap is set from 1.5 mm to 2.2 mm because narrower gaps increase shear stress at the die land and promote melt fracture. Regrind from tail flash and trimmings is restricted to ≤25 wt%; higher fractions shift die swell and reduce ESCR. Amine-based antistatic additives are used only after a separate compatibility trial under ASTM D1693-15 because ethoxylated amines can depress stress-crack resistance. Outdoor-stored containers are assessed for UV embrittlement under ASTM D2565-21 when the exposure period exceeds 6 months.

    Qualification targetReferenceMeasured property
    UN-certified drop impact49 CFR 178.603Fracture or leakage after drop
    Hydrostatic pressure retention49 CFR 178.605Container deformation or bursting
    Environmental stress crack resistanceASTM D1693-15 Condition BFailure time in 100% Igepal CO-630
    Melt mass-flow rateISO 1133-1:2022Flow at 190 °C/2.16 kg
    DensityISO 1183-1:2019Mass per unit volume at 23 °C
    Oxidative induction timeISO 11357-6:2022Time to oxidation onset at 200 °C

    When Large Intermediate Bulk Container Liners Require High Melt Strength

    IBC inner liners of 1000 L nominal capacity and 4–8 mm wall thickness demand a high-molecular-weight HDPE with sufficient melt strength to avoid parison draw-down during the long extrusion cycle. The mold closes on the parison before significant thinning occurs, but the extruder must deliver a large shot from the accumulator head without excessive residence time. On 150 mm grooved-feed machines with 30:1 L/D, melt temperature is held between 190 °C and 215 °C; higher temperatures reduce sag resistance but improve surface finish. A 100-point parison programmer is required to redistribute wall thickness around the top lip, sidewall, valve boss, and bottom pallet support. Mold cooling water enters at 10–15 °C, and poorly cooled valve-boss areas show sink marks and dimensional drift. The pinch-off zone is reinforced during programming because it carries the entire hydrostatic load when the IBC is filled. Pressure retention is confirmed by an internal test at 20 kPa for 10 min; the applicable dangerous-goods design qualification is verified under the relevant ADR/RID/IMDG or 49 CFR requirements for the complete IBC assembly. Regrind from thick flash is ground to uniform particle size and limited to 30 wt%; higher addition levels create pinholes at the pinch-off and increase leakage rates.

    Household and institutional chemical packaging lines running HDPE B50-35H-111 produce handleware bottles for laundry detergents, acid cleaners, and diluted bleach formulations. The processing window is wider than in large-part blow molding, but the main technical restriction is residual stress at the handle weld and injection-molded neck finish. In rotary wheel and shuttle lines, melt temperature is set from 185 °C to 205 °C, and blow pressure is held at 0.6–0.8 MPa. The pinch-off is cut hot and conveyed to granulators; grind particle size is controlled with a 6 mm screen to avoid melt-temperature fluctuations during regrind feeding. For bleach and acid-based cleaners, ESCR is re-evaluated under ASTM D1693-15 Condition B because oxidative formulation components accelerate crack initiation at the handle weld. Light-blocking color concentrates are added at 1–3 wt%, but the carrier resin must be selected for stress-crack compatibility. Dimensional checks after molding include top-load testing at 50 mm/min compression speed and bottle-volume verification by water-fill displacement.

    Typical extrusion blow-molding process window for HDPE B50-35H-111 class
    ParameterOperating rangeMeasurement method
    Melt temperature at die exit185–215 °CInfrared pyrometer
    Mold coolant inlet10–18 °CChiller setpoint
    Blow pressure0.6–1.0 MPaCalibrated transducer
    Die gap1.5–3.0 mmFeeler gauge
    Free Quote

    Competitive Yanchang China Coal Yulin (Shaanxi) HDPE B50-35H-111 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Yanchang China Coal Yulin (Shaanxi) HDPE B50-35H-111 is a high-density polyethylene resin produced at the Yulin, Shaanxi coal-to-olefins complex of Shaanxi Yanchang ChinaCoal Yulin Energy and Chemical Co., Ltd. The grade code indicates a nominal density of 0.950 g/cm³ by ISO 1183-1:2019 or ASTM D1505-18 and a nominal melt flow rate of 0.35 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022 or ASTM D1238-20. These are class identifiers and not acceptance values; the producer’s lot certificate remains the only authoritative source for density, melt flow rate, additive package, and molecular weight distribution. The resin is classified as an extrusion blow moulding grade for small-to-medium containers; the low melt flow rate increases melt strength and reduces parison sag during open-mould production. It differs structurally from injection moulding HDPE and bimodal pipe grades in molecular weight distribution, die swell, and stress crack resistance. Published English-language engineering datasheets for this specific grade are limited, so all processing and specification values must be verified against the current certificate of analysis before production release.

    What Extrusion Blow Moulding Parameters Are Required to Prevent Parison Instability?

    Parison instability in low-melt-flow HDPE arises from two competing effects. Insufficient melt temperature increases melt fracture and uneven die swell, while excessive melt temperature reduces melt strength and increases draw-down sag. The extrusion blow moulding window for a 0.35 g/10 min HDPE homopolymer typically lies between 180 °C and 210 °C at the die head, but grade-specific additives or molecular weight distribution may narrow this range. Accumulator-head machines with a 24:1 to 25:1 L/D barrier screw and a grooved feed section are preferred for this melt index class. Continuous extrusion machines with axial screw movement require tighter parison programming because the lower melt flow index increases back pressure and reduces plasticating capacity. Die swell is expected to be higher than that of a 0.8 g/10 min blow moulding grade; therefore, die tooling must be sized with a lower blow-up ratio or an adjustable die gap. Blow-up ratios of 1.5:1 to 3.0:1 and parison programming with die gap variation of 25 % to 40 % can maintain wall thickness uniformity in jerry can geometries. Melt pressure at the die head should be monitored. A sustained pressure above 35 MPa may indicate excessive shear heating or restrictive tooling, while pressure fluctuation greater than ±1.5 MPa can cause visible weld-line thinning. Pre-drying is generally minimal because HDPE is not hygroscopic; however, condensation on cold resin transferred from outdoor silos at relative humidity above 60 % should be removed by hopper heating at 60–70 °C for 2 h before extrusion. Published capillary rheometry data for this specific lot are limited; shear viscosity should be established at 190 °C across 10 s⁻¹ to 1,000 s⁻¹ before tooling is cut.

    In production of intermediate bulk containers and automotive washer fluid bottles, the resin is conveyed from rail hopper cars to day silos and then gravimetrically fed into a shuttle blow moulder. The low melt flow index reduces flash thinning at the pinch-off and helps retain parison shape when the mould is open for insert loading. Tooling should maintain clamp force from 300 kN to 800 kN depending on mould area; smaller machines with 15–20 MPa hydraulic pressure may require lower extrusion output to avoid parison swell-induced flash. The material’s low melt flow index increases cycle time relative to medium-melt-flow grades because longer screw recovery time is required to plasticate the resin. Screw speed should be set so that recovery completes before mould open time without exceeding a melt temperature of 210 °C. These processing characteristics are observed on production-scale shuttle machines, not from laboratory data alone.

    Environmental Stress Crack Resistance, Oxidation Induction Time, and Chemical Resistance Boundaries

    For HDPE containers exposed to surfactants, alcohols, or agricultural chemicals, environmental stress crack resistance is the controlling property. ESCR testing by ASTM D1693, condition A or B, with 10 % Igepal CO-630 at 50 °C, is the standard laboratory method for lot acceptance. Blow moulding grades with a density near 0.950 g/cm³ frequently show ESCR values between 30 h and 100 h, but published data for this specific grade configuration are limited. Containers subjected to UN/DOT hazardous materials certification should be tested on the finished article under ASTM D5571 or ASTM D2561. Oxidation induction time measured by ISO 11357-6:2018 at 200 °C should be reported in the producer’s certificate; values below 20 min for virgin HDPE may indicate insufficient stabilizer dispersion, but this is a quality indicator rather than a specification. Strong oxidizing acids, hydrocarbons, and high-aromatic-content solvents can permeate or stress-crack HDPE. The resin should not be used with aromatic or chlorinated solvents at elevated temperature unless migration and finished-container stress crack testing is performed. Contact with ketones and ethyl acetate can soften the amorphous phase; for UN/DOT packaging of such substances, compatibility testing under 49 CFR 178 or ADR 6.1 governs.

    During colour masterbatch addition, the low melt flow matrix can resist distributive mixing. A single-screw extruder with a vented 25:1 barrel and a Maddock mixer may be needed to disperse 4 % to 6 % masterbatch without unmelted agglomerates. Adding low-viscosity liquid colour or slip additives can lower melt strength and cause parison folding; such additives should be limited to 0.5 wt% unless validated on the specific blow moulder. This processing boundary is observed on production machines with open parison drop times exceeding 8 s.

    When Grade B50-35H-111 Replaces Injection Moulding or Bimodal Pipe Grades

    Direct substitution is not recommended without tooling and screw changes. Injection moulding HDPE typically has a melt flow rate of 4–20 g/10 min, more than one order of magnitude higher than this blow moulding grade. Using B50-35H-111 in an injection mould with long flow paths or wall sections below 1.5 mm will produce short shots, excessive injection pressure, and gate blush. The melt flow index of 0.35 g/10 min is outside the capability envelope of most standard injection presses. Compared with bimodal pipe grades such as PE100, B50-35H-111 is not designed for sustained hydrostatic stress at 20 °C as measured by ISO 9080:2012 or ASTM D2837; its molecular weight distribution is narrower, and its long-term hydrostatic strength class may not meet PE100. The grade also differs from film-grade HDPE through lower melt flow and higher die swell, which improves parison shape stability but is unsuitable for blown film bubble formation. Against other blow moulding HDPE grades with melt flow indexes of 0.2 g/10 min or 0.8 g/10 min, B50-35H-111 occupies an intermediate range: likely better ESCR than 0.8 g/10 min grades and easier parison extrusion than 0.2 g/10 min grades, but exact ranking must be established by lot-specific testing.

    Mechanical Property Verification and Acceptance Test Matrix

    Because published English-language engineering data for this specific product are limited, mechanical property verification should use producer lot certificates and finished-article testing. The following test method matrix defines the standard bounding conditions used for HDPE blow moulding grades; it does not replace the producer’s specification.

    PropertyTest methodConditionVerification role
    DensityISO 1183-1:2019/ASTM D1505-1823 °C, compression moulded plaqueClass identification
    Melt flow rateISO 1133-1:2022/ASTM D1238-20190 °C, 2.16 kgGrade identification
    Tensile yield stressISO 527-2:2012/ASTM D638-1450 mm/min, Type IV specimenProducer lot data
    Flexural modulusISO 178:2019/ASTM D790-172 mm/minProducer lot data
    Notched Izod impactISO 180:2019/ASTM D256-1023 °C, Method AProducer lot data
    Environmental stress crack resistanceASTM D169350 °C, 10 % Igepal CO-630Container-specific
    Oxidation induction timeISO 11357-6:2018200 °CProducer certificate

    Acceptance testing for blow moulded containers under ASTM D4509 or ISO 16101:2004 is performed on the finished article; tensile bars cut from compression moulded plaques do not capture weld-line or pinch-off effects. The wall of a 25 L jerry can may show thickness from 1.2 mm to 2.0 mm, and the pinch-off tail must be tested separately for impact and ESCR. Lot release values should be compared against the producer’s current certificate of analysis.

    Under food-contact requirements, HDPE produced in coal-to-olefins facilities must be evaluated for residual catalyst and hydrocarbon migration. No claim of FDA 21 CFR 177.1520 or EU 10/2011 compliance is made without a producer statement. REACH and RoHS declarations should be obtained from the supplier; the base HDPE molecule is not a hazardous substance under REACH registration, but additives and processing aids may impose exposure limits. Operational boundaries include avoiding long residence times above 230 °C, which can initiate oxidative chain scission and odour formation in the finished container.

    Top