Yanchang China Coal Yulin Shaanxi Hdpe A60 70 162

Yanchang China Coal Yulin (Shaanxi) HDPE A60-70-162

    • Product Name: Yanchang China Coal Yulin (Shaanxi) HDPE A60-70-162
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 354195
    Density 0.960 g/cm³
    Melt Flow Rate 0.07 g/10 min (190°C/2.16 kg)
    Tensile Yield Strength 23 MPa
    Elongation At Break >600%
    Flexural Modulus 1100 MPa
    Notched Izod Impact Strength 20 kJ/m²
    Vicat Softening Temperature 125°C
    Melting Point 130-135°C
    Shore D Hardness 60
    Thermal Conductivity 0.45 W/m·K
    Water Absorption <0.01%
    Dielectric Constant 2.3
    Volume Resistivity >10^16 Ω·cm
    Environmental Stress Cracking Resistance >1000 h
    Oxidation Induction Time >20 min
    Crystallinity 70-80%

    As an accredited Yanchang China Coal Yulin (Shaanxi) HDPE A60-70-162 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Yanchang China Coal Yulin (Shaanxi) HDPE A60-70-162 is packed in 25 kg PP woven bags, 40 bags per pallet, 1,000 kg total.
    Container Loading (20′ FCL) 20′ FCL loading: Yanchang China Coal Yulin (Shaanxi) HDPE A60-70-162, 25 kg bags, approx. 18 MT, securely stowed.
    Shipping Yanchang China Coal Yulin (Shaanxi) HDPE A60-70-162 is shipped as non-hazardous polyethylene pellets in 25 kg woven bags or 1,000 kg jumbo bags, palletized and stretch-wrapped. Transport in clean, dry containers or trucks; protect from moisture, heat, sunlight, and contamination. No special dangerous-goods documentation required.
    Storage Store Yanchang China Coal Yulin (Shaanxi) HDPE A60-70-162 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and oxidizing agents. Keep bags sealed and off the floor on pallets to prevent moisture and contamination. Avoid static buildup, excessive stacking, and prolonged outdoor exposure. Protect from impact damage. Use first-in, first-out inventory and follow local safety regulations.
    Shelf Life Typically 24 months when stored unopened in original packaging in a cool, dry, ventilated area, away from sunlight and moisture.
    Application of Yanchang China Coal Yulin (Shaanxi) HDPE A60-70-162

    Extrusion Blow Moulding of UN-Certified Open-Head Drums

    Accumulator-head blow moulding of large open-head drums demands parison sag control that is only partly captured by melt flow rate data. Qualification of the Yanchang China Coal Yulin HDPE A60-70-162 resin on a production line should begin with melt mass-flow rate determination under ISO 1133-1:2022 at 190 °C and 2.16 kg; a reading in the band of 0.20–0.60 g/10 min places the melt within the rheological window used on accumulator-head machines fitted with 80–120 mm single-screw extruders and 24:1–30:1 L/D barrels. Published data for the specific Yanchang grade in UN drum qualification is limited, so the starting melt temperature is set between 180 °C and 210 °C, with the die head held independently at 190–205 °C. A diverging die gap of 2–4 mm and an accumulator displacement of 5–10 L are typical; blow air pressure is controlled between 0.6 MPa and 0.8 MPa with mould cooling water at 10–40 °C. For 220 L open-head drums, cycle time may extend from 120 s to 300 s depending on wall-section distribution. The formulation for outdoor industrial packaging typically incorporates 2.0–2.5 wt% carbon black masterbatch with 40–50 wt% carbon black loading, a hindered phenolic/phosphite antioxidant package at 0.08–0.15 wt%, and a fluoropolymer processing aid at 0.02–0.05 wt% when die-lip build-up is observed. Tensile yield stress measured under ASTM D638-22 Type IV and environmental stress-cracking resistance under ASTM D1693-15 Condition B are the two material properties most relevant to UN drop testing. The finished open-head drum is evaluated under UN Model Regulations Chapter 6.1, with a 1.2 m drop for Packing Group II liquids of specific gravity not exceeding 1.2, plus stack and leakproofness tests. Failure of the parison-sag checkpoint—typically a parison length reduction beyond 15–20% before mould closing—requires raising melt strength through lower melt temperature, not through uncontrolled regrind addition.

    In high-cavitation closure moulding, the limiting constraint is not melt temperature but gate solidification. Short-cycle injection moulding of tamper-evident caps from the same high-density ethylene matrix proceeds only after melt-flow-rate confirmation under ASTM D1238-20 at 190 °C/2.16 kg. Because closures are thin-walled, a melt flow rate below 1.0 g/10 min may restrict filling beyond a nominal wall thickness of 0.6 mm; typical high-density polyethylene closure grades fall within 2.0–8.0 g/10 min. If the measured value for A60-70-162 is lower, gate diameter and cycle time cannot compensate indefinitely; published data for this specific configuration is limited. Machines are commonly 150–300 ton hydraulic or hybrid presses with 24–32 cavities; clamp force is configured at 5–10 tonnes per cavity, injection speed at 20–60 mm/s, hold pressure at 40–60 MPa, and screw back pressure below 0.5 MPa to avoid excessive shear heating. Melt temperature is held between 200 °C and 220 °C, while mould temperature is maintained at 10–30 °C. Hot-runner tips are set at 240–260 °C to prevent premature gate freeze. The formulation for caps includes 0.05–0.15 wt% nucleating agent to increase crystallisation temperature, 0.05–0.10 wt% erucamide slip, and 0.05–0.10 wt% antistatic glycerol monostearate where dust attraction is a filling-line issue. Shrinkage after 48 h is controlled by observed data from ISO 294-4:2018; typical HDPE cap resin linear mould shrinkage is between 1.5% and 2.5%. The finished tamper-evident cap is tested for environmental stress-cracking in surfactant solution per ASTM D1693-15 and for food-contact compliance under FDA 21 CFR §177.1520(c) and EU 10/2011/EC where the application is food packaging.

    What Constrains Film Stability in High-Stalk HDPE Liners?

    A high-stalk blown film line processing high-density ethylene polymer encounters the primary process conflict between blow-up ratio and frost-line height. High-density polyethylene liner film requires a stalk bubble geometry to balance transverse direction tear resistance and output rate. On a typical line with a 100–300 mm die diameter, the die gap is set at 1.2–2.0 mm, the blow-up ratio between 3:1 and 5:1, and the frost-line height between 6 and 12 die diameters. Melt temperature leaving the adapter is held at 190–220 °C; screen packs of 60/80/100 mesh are used to filter degraded gel particles. Internal bubble cooling stabilises the stalk and raises specific output; without it, output per unit die circumference is limited by bubble-couple instability. Film-grade formulations for HDPE liners incorporate 0.10–0.30 wt% synthetic silica antiblock, 0.05–0.15 wt% erucamide slip, and 0.02–0.05 wt% fluoropolymer processing aid. Compliance testing for food-contact liner applications follows FDA 21 CFR §177.1520(c), EU 10/2011/EC, and, where the liner contacts aqueous foods, extraction testing under GB 4806.7-2023. Mechanical properties are assessed by ASTM D882-22 for thin film tensile and ASTM D1922-23 for Elmendorf tear. Finished film thickness usually falls between 10 µm and 50 µm for industrial liners; for coextruded structures, the HDPE layer functions as the load-bearing stratum while a tie layer and barrier polymer provide oxygen transmission resistance below 50 cm³/(m²·d) when measured at 23 °C and 0% RH by ASTM D3985-24. Instability in the stalk—visible as periodic bubble diameter variation exceeding ±3%—is corrected by lowering extruder rear-barrel temperature, not by increasing blow-up ratio above the validated range.

    When Solid-Wall Gravity Pipe Replaces Concrete in Aggressive Soils

    For solid-wall gravity pipe, the governing requirement is ring stiffness and environmental stress-cracking resistance rather than tensile yield alone. Extrusion of solid-wall gravity pipe from the Yanchang HDPE A60-70-162 grade is governed by ISO 4427 and EN 12201 for pressure service, but gravity drainage pipe is additionally classified under ASTM D3350-24 and tested for resistance to slow crack growth by ISO 16770:2019 or ASTM F1473-22. Pipe lines typically use a 60–90 mm grooved-feed single-screw extruder with 30:1–33:1 L/D, a 20/40/60 mesh screen pack, and a spiral mandrel die. Melt temperature is controlled at 200–220 °C; measured melt pressure before the screen changer should remain below 35 MPa to avoid excessive shear work. The pipe exits the die into a calibrator under vacuum of -0.03 MPa to -0.06 MPa, followed by spray cooling tanks with water at 15–25 °C and haul-off speed synchronised to produce wall thicknesses between 5 mm and 20 mm for outer diameters of 110–400 mm. Formulation for black pipe requires 2.0–2.5 wt% carbon black masterbatch with particle dispersion ≤3 on ISO 18553:2002, an antioxidant package at 0.10–0.30 wt%, and an acid scavenger such as calcium stearate at 0.02–0.05 wt%. The finished pipe is used in culverts, land drainage, and sewer gravity lines where soil pH is below 5 or where sulphate and chloride exposure would corrode concrete. Published data for this specific configuration is limited, so hydrostatic design basis for the specific Yanchang grade should be established before pressure service is claimed.

    TestMethodValidation window
    Carbon black contentISO 6964:20192.0–2.5 wt%
    Carbon black dispersionISO 18553:2002Rating ≤ 3
    Oxidative induction timeISO 11357-6:2018≥ 20 min at 200 °C
    Melt flow rateISO 1133-1:2022Grade-specific; report 190 °C/2.16 kg
    Ring stiffnessISO 9969:2016SN8 or SN16 as designed

    Cut-sheet thermoforming lines fed with high-density polyethylene sheet expose a separate set of thermal-history constraints. HDPE sheet lines typically run a 75–150 mm single-screw extruder with 30:1–36:1 L/D, a barrier screw with a Maddock mixing section, and a flexible-lip sheet die from 800 mm to 2000 mm width. Melt temperature is set at 200–230 °C; the polished three-roll stack is held at 70–100 °C to control gloss and minimise crystallinity-induced warpage. Sheet thickness ranges from 0.8 mm to 6.0 mm; thinner sheet below 1.2 mm can suffer edge-necking unless die bolt adjustment is monitored every 15 min. Thermoforming is performed in a shuttle or rotary machine with oven surface temperatures of 160–180 °C and plug assist using syntactic foam plugs at 90–110 °C. Draw ratios are limited to 1.5:1–3:1; beyond 3:1, corner thinning exceeds 25% of nominal sheet thickness and lowers top-load resistance. Formulation for reusable transport dunnage includes 10–25 wt% in-house regrind, a hindered phenolic antioxidant at 0.05–0.10 wt%, and carbon black masterbatch at 0.5–2.0 wt% for grey or black products. Compliance is governed by REACH 1907/2006/EC, RoHS 2011/65/EU, and durability is verified by ASTM D790-17 flexural modulus and ISO 179-1:2023 Charpy impact. Published data for this specific configuration is limited, so pre-production runs must establish actual sag and sidewall thickness distribution before serial output.

    Monofilament Yarn and Oriented Geogrid Structures

    When high-density ethylene monofilament is run on a multi-stage godet line, the first process conflict is spinneret blockage. Monofilament production from the Yanchang HDPE A60-70-162 grade requires melt filtration that is more severe than in film or sheet because spinneret holes of 0.8–1.2 mm diameter can be blocked by degraded gel. The extruder is typically 45–65 mm with 30:1 L/D, equipped with a static mixer and a gear pump to maintain volumetric output within ±1%. Melt temperature is held at 190–220 °C; filtered melt is distributed through a spinneret and quenched in a water bath at 30–40 °C. The resulting filaments are drawn through a series of godets: first-stage draw temperature 90–100 °C, total draw ratio 6:1–10:1, followed by relaxation of 5–10% at 100–120 °C. Finished monofilament diameter is typically 0.20–0.40 mm; tensile strength measured by ISO 2062:2009 or ASTM D2256-21 depends on draw ratio and molecular orientation. The formulation for outdoor geogrid or agricultural netting requires 0.20–0.50 wt% hindered amine light stabilizer and 2.0–2.5 wt% carbon black masterbatch; for coloured nets, non-black pigments must be UV-stable. The oriented monofilaments are converted into geogrids or nets and tested under ISO 10319-1:2015 for wide-width tensile strength and EN 13249:2016 for road construction applications. Long-term installation in soil environments requires a creep-limited strength determined by ISO 13431:1999 or ASTM D6992-16 at 20 °C. The primary process failure is filament fibrillation at draw ratios above 8:1, which cannot be corrected by increasing melt temperature alone; lowering the quench water temperature to 25 °C and increasing the first godet speed are typically required.

    Free Quote

    Competitive Yanchang China Coal Yulin (Shaanxi) HDPE A60-70-162 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Yanchang China Coal Yulin (Shaanxi) HDPE A60-70-162: Technical Introduction for Converters

    The high-density polyethylene resin Yanchang China Coal Yulin (Shaanxi) HDPE A60-70-162 is identified in commercial documentation as an injection-grade high-density polyethylene. The material specification is controlled under the manufacturer’s certificate of analysis and should be compared against ASTM D1505, ISO 1183-1, ASTM D1238, ISO 1133-1, ASTM D638, ISO 527-2, ASTM D790, ISO 178, ASTM D1693, and ISO 11357-6 before it is introduced to a production-scale conversion line. The grade designation does not encode a universal property set; the converter must therefore obtain lot-specific numerical values for density, melt mass-flow rate, and mechanical properties before setting process parameters.

    Defining the Material Class and Commercial Positioning of A60-70-162

    Commercial literature describes the grade as a rigid high-density polyethylene intended for injection moulding of thin-wall packaging, closures, crates, and appliance components. The positioning is distinguished from blow moulding and blown film HDPE by a narrower molecular-weight distribution and a higher melt-flow rate at equivalent density, which reduces filling pressure and improves melt-front reproducibility in multi-cavity tools. Published converter guidance commonly places injection-grade HDPE within a density band of 0.941–0.965 g/cm³ and a melt mass-flow rate range of 0.2–80 g/10 min at 190 °C under 2.16 kg load when tested to ASTM D1238 or ISO 1133-1. A specific lot of A60-70-162 may occupy a narrower portion of this space; lot-specific values remain controlling.

    Molecular architecture in this resin class is dominated by ethylene sequences with a controlled concentration of short-chain branches. The comonomer type, when present, is typically 1-butene or 1-hexene. The resulting crystallinity influences density, modulus, barrier, and stress-crack resistance. Because A60-70-162 is positioned as an injection moulding grade, the manufacturer generally targets a balance among melt-flow rate, stiffness, and environmental stress-cracking resistance. However, published data for this specific configuration is limited and must not be inferred from unrelated HDPE grades.

    Property Test method Specimen and condition Process-control significance
    Density ISO 1183-1 / ASTM D1505 Compression-moulded plaque or pellets, 23 °C Crystallinity, rigidity, and barrier balance
    Melt mass-flow rate ISO 1133-1 / ASTM D1238 190 °C, 2.16 kg or 5.0 kg Molecular weight and mould-filling behaviour
    Tensile yield stress and elongation at break ISO 527-2 / ASTM D638 Type 1B or Type IV specimen, 50 mm/min Short-term load resistance and part toughness
    Flexural modulus ISO 178 / ASTM D790 Bar specimen, 2 mm/min test speed Part rigidity and dimensional stability
    Charpy notched impact strength ISO 179-1/1eA / ASTM D6110 Notched bar, 23 °C and -30 °C Impact resistance in service and during assembly
    Vicat softening temperature ISO 306 / ASTM D1525 A50 or B50 condition Thermal stability under short-term load
    Environmental stress-cracking resistance ASTM D1693 Bent strip, 10% Igepal CO-630, 50 °C Resistance to detergent and aggressive media
    Oxidative induction time ISO 11357-6 / ASTM D3895 Isothermal at 200 °C in oxygen Stabilizer effectiveness and melt life

    On production-scale equipment, the most frequently observed failures with injection-grade HDPE are not melt instability but variability in lot-to-lot melt mass-flow rate and additive package concentration. In twin-screw compounding or masterbatch dilution, feed throat bridging and screw slippage can occur when regrind ratio exceeds 20–25 wt% without adjustment of feed screw speed. Incoming inspection should include melt-flow verification and, where possible, differential scanning calorimetry. A shift in melt-flow rate outside the manufacturer’s accepted band alters fill time, gate pressure, and part weight even when machine temperatures remain unchanged.

    What Processing Limits Emerge During Injection Moulding of This Grade?

    Injection moulding of high-density polyethylene requires the screw, barrel, and tooling to be selected against the material’s viscosity and thermal stability. For general-purpose HDPE injection grades, barrel set points from feed to nozzle are commonly established in the range of 190–260 °C, with melt temperature measured at the nozzle. A flat or slightly rising temperature profile is preferred to avoid overheating at the compression zone. Back pressure is maintained between 5–20 bar hydraulic in many converter settings, but actual values depend on screw diameter and length-to-diameter ratio. A general-purpose screw with an L/D of 20:1–24:1 and compression ratio of 2.5:1–3.5:1 is typical. Drying is generally not required when the package is sealed and storage relative humidity is below 60%; however, surface moisture from condensation must be avoided in pneumatic conveying.

    Tool temperature controls surface finish, shrinkage, and warpage. Mold temperatures in the range of 20–60 °C are used for fast-cycle packaging, whereas 60–90 °C may be required for parts with tight dimensional tolerances or high visual-quality requirements. Higher mold temperature increases crystallinity and mold shrinkage; uneven cooling across thick-to-thin transitions causes differential shrinkage and part distortion. Gate geometry should be sized according to the part wall thickness and flow length. For thin-wall containers with wall thickness below 1.2 mm, a high-flow injection grade allows lower injection pressure, but gate freeze time shortens. On presses with clamp force below 1200 kN, filling thin-wall multi-cavity tools may be limited if the projected area exceeds machine capacity.

    Holding pressure decay and cushion control must be validated on the actual machine. Short cushions and spool decomposition cause silver streaks and reduced Charpy impact strength. The melt residence time should be minimized above 260 °C because chain scission and oxidative gel formation can occur. If screw recovery time is excessive or the material is stored beyond the manufacturer’s stated shelf life, oxidation induction time should be re-tested before production approval.

    On production-scale equipment, the observed failure modes include gate-stringing, warpage at the transition from thick to thin sections, and inconsistent part weight when the screw cushion is not maintained. In multi-cavity tools, cavity-to-cavity filling variation is often more dependent on runner balance and venting than on small shifts in melt-flow rate. Process boundaries for A60-70-162 are determined by the certificate of analysis, the tool geometry, and the condition of the machine; published data for this specific configuration is limited, so trial validation on the target production line remains necessary.

    When A60-70-162 Replaces a Fractional-Melt Pipe or Blow Molding Grade in Rigid Part Production

    Substitution of a fractional-melt HDPE pipe grade by an injection-grade A60-70-162 is not a drop-in change. The pipe-grade resin is designed for long-term hydrostatic strength and slow crack growth resistance under ISO 9080 and ISO 13479; its melt mass-flow rate is typically low, and its molecular-weight distribution is broad or bimodal. An injection-grade resin with higher flow reduces processing pressure but may exhibit lower long-term hydrostatic strength if used in pressurized pipe applications. Therefore, any replacement must be evaluated according to the application’s relevant standard, such as ISO 4427 for polyethylene piping systems or equivalent national specifications.

    Compared with film-grade HDPE, the resin’s melt strength and extensional rheology are usually lower. Film grades are formulated with broader molecular-weight distribution or moderate long-chain branching to stabilize the bubble and withstand gauge variation in blown film lines. Injection-grade A60-70-162 is optimized for mould filling and rapid dimensional stabilization; therefore, bubble stability in blown film extrusion would likely be insufficient. Converters should not infer film performance from injection moulding property sheets. If a trial is intended, minimum blow-up ratio and frost-line height must be established on the specific line and compared with the film grade’s data.

    The differentiation among HDPE grades is therefore not primarily one of chemical resistance or thermal stability, but of molecular-weight distribution, comonomer distribution, and stabilization. A60-70-162 should be selected when the application requires fast filling, consistent part mass, and moderate stiffness. It should not be selected for slow crack growth–limited pressure piping, high melt-strength blown film, or thick-wall blow moulded containers without additional validation.

    Vicat Softening, Slow Crack Growth, and Oxidative Stability Data Review

    For rigid injection mouldings, heat deflection temperature and Vicat softening temperature are usually reported according to ISO 306 / ASTM D1525 and ISO 75-2 / ASTM D648. The measured value depends on load, heating rate, and specimen conditioning. The Vicat softening temperature of general-purpose HDPE typically ranges from 110–135 °C under A50 conditions, but the grade-specific value of A60-70-162 must be taken from the manufacturer’s lot certificate. Fluctuations in comonomer content and cooling rate alter these results by several degrees.

    Slow crack growth resistance in HDPE is assessed through ASTM D1693 bent-strip environmental stress-cracking resistance, notched pipe testing under ISO 13479, or full notch creep testing under ISO 16770. Injection moulding grades often have lower environmental stress-cracking resistance values than pipe grades because of lower molecular weight and narrower molecular-weight distribution. When A60-70-162 is used in parts exposed to detergents, lubricants, or polar organic species, the application must be validated under the service environment. No property sheet value can substitute for environmental stress-crack testing on the actual moulded part.

    Oxidative stability is checked through oxidation induction time or oxidation onset temperature. The stabilizer package is designed for the intended processing temperature and end-use lifetime. Overdrying or excessive regrind can deplete phenolic and phosphate antioxidants, causing melt-flow drift and discoloration. If storage exceeds the manufacturer’s stated shelf life, oxidative induction time should be re-tested before use.

    Regulatory or standard reference Scope Condition for converter evaluation
    FDA 21 CFR 177.1520 Olefin polymers for food contact Grade-specific food-contact statement required
    EU Regulation (EU) No 10/2011 Plastic materials intended for food contact Migration testing under intended conditions
    REACH Regulation (EC) No 1907/2006 Registration, evaluation, authorization of chemicals SVHC declaration from manufacturer required
    RoHS Directive 2011/65/EU Lead, cadmium, mercury, chromium VI, PBB, PBDE Concentration verification in finished part
    ISO 9080 Hydrostatic design basis for pressure pipe Applicable only if converted into pressure pipe
    GB 4806.6 China food-contact plastic resin standard Compliance certificate from supplier required

    The manufacturer’s regulatory declaration should be consulted before using A60-70-162 in food-contact or medical applications. The presence of residual catalyst components, slip agents, antistatic agents, or nucleating agents is not identifiable from the grade name alone. Lot-to-lot variations in additive systems are possible; therefore, the converter must maintain incoming inspection records and match each production lot to the correct certificate of analysis.

    Avoid combining A60-70-162 with copper-based heat stabilizers or amine-bearing additives that may accelerate discoloration. Avoid prolonged melt residence times above 260 °C because chain scission and oxidative gel formation can occur. In pneumatic conveying, ensure grounding to prevent static discharge. Ventilation must be available during melt processing to remove decomposition products. When the material is run at high screw speed with deep-channel feed, monitor melt quality and feed stability because screw slippage can shift throughput and melt temperature without a corresponding change in barrel set points.

    Top