| HS Code | 513790 |
| Density | 0.950 g/cm³ |
| Meltflowrate | 0.06 g/10 min |
| Tensileyieldstrength | 23 MPa |
| Tensilestrengthatbreak | 35 MPa |
| Elongationatbreak | 700% |
| Flexuralmodulus | 1000 MPa |
| Notchedizodimpactstrength | 20 kJ/m² |
| Vicatsofteningpoint | 122 °C |
| Heatdeflectiontemperature | 70 °C |
| Shoredhardness | 60 |
| Environmentalstresscrackresistance | >1000 h |
| Brittlenesstemperature | -70 °C |
| Waterabsorption | <0.01% |
| Crystallinity | 70-80% |
| Molecularweightdistribution | Broad |
As an accredited Yanchang China Coal Yulin (Shaanxi) HDPE A5006FA1280 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Yanchang China Coal Yulin (Shaanxi) HDPE A5006FA1280 is supplied in 25 kg polyethylene-lined woven bags, palletized and shrink-wrapped. |
| Container Loading (20′ FCL) | 20′ FCL container loading of Yanchang China Coal Yulin (Shaanxi) HDPE A5006FA1280, securely packed and stowed for ocean export shipment. |
| Shipping | Yanchang China Coal Yulin (Shaanxi) HDPE A5006FA1280 is a non-hazardous thermoplastic resin. It is typically shipped in 25 kg bags or bulk bags, palletized and stretch-wrapped, in 20'GP/FCL containers by sea from Chinese ports. Store in a cool, dry, ventilated area, protected from moisture, sunlight, and contamination. |
| Storage | Store Yanchang China Coal Yulin (Shaanxi) HDPE A5006FA1280 in a cool, dry, well-ventilated warehouse, away from direct sunlight, rain, heat, sparks, and open flames. Keep original bags sealed, palletized, and off the floor to prevent moisture, dirt, and contamination. Avoid prolonged UV exposure, strong oxidizers, and incompatible materials. Use good housekeeping, safe stacking, and first-in-first-out rotation. |
| Shelf Life | Shelf life: 24 months when stored in dry, cool, ventilated area, away from direct sunlight and moisture, in original packaging. |
For converters evaluating Yanchang China Coal Yulin (Shaanxi) HDPE A5006FA1280 in high-output blown film extrusion, the resin class occupies the high-molecular-weight HDPE film envelope used for down-gauged industrial liners, freezer-grade food packaging, and high-speed bag conversion. Publicly available grade-specific data for A5006FA1280 is limited; the processing references below are therefore drawn from HDPE blown-film grades with similar density and melt flow characteristics and should be verified against the supplier datasheet before line qualification. The resin is processed on 45–90 mm grooved-feed extruders with L/D ratios not less than 25:1 and not more than 30:1, because the high-molecular-weight distribution generates shear heating and melt-temperature overshoot above 225 °C when screw speeds exceed 120 min⁻¹ on 65 mm barrels. Melt temperatures at the die are normally maintained between 190 °C and 210 °C, while the die is set 5–10 °C above the adapter to reduce surface melt fracture on 0.8–1.2 mm die gaps. Bubble geometry is not neutral: a high-stalk configuration with a blow-up ratio of 3.0:1–4.5:1 and a frost line height of 8–12 die diameters is preferred because HDPE film grades exhibit low melt tension relative to LDPE and require a longer cooling path to stabilize the bubble. Dual-lip air rings with internal bubble cooling are applied on high-output lines, but condensate removal must be maintained to avoid water marks. Film property testing follows ASTM D882 for tensile yield and elongation at break, ASTM D1709 for dart impact, ASTM D1922 for Elmendorf tear, and ASTM D1894 for coefficient of friction. Food-contact film structures require compliance with FDA 21 CFR 177.1520 for olefin polymers and with EU Regulation 10/2011 including overall migration limits and specific migration of additives. Pre-drying is not normally required unless pellets are stored in unheated warehouses with high humidity; surface condensation can be removed with 60–70 °C hopper drying for 2 h. Melt temperature must not exceed 230 °C to avoid oxidation and die-lip plate-out generated by degraded oligomers.
The limiting variable is rarely the extruder itself; it is the bubble geometry and the crystalline orientation that develops between the die lip and the frost line. When A5006FA1280 is down-gauged to 10–15 μm on a die gap of 1.0 mm, the draw ratio exceeds 70:1–100:1, and the low melt tension of HDPE causes bubble breathing and edge flutter unless the blow-up ratio is reduced to 3.0:1–3.5:1 and the frost line is raised to 10–12 die diameters. The frost line is the functional quench point: below it, the film is still molten enough to stretch and reduce thickness, while above it the crystalline network is fixed. High-stalk processing deliberately moves the frost line upward to increase machine-direction orientation, which raises modulus and reduces elongation at break but creates severe tear anisotropy. When measured by ASTM D1922, machine-direction Elmendorf tear values are typically only 15–40% of transverse-direction values, and this imbalance becomes a critical failure mode in perforated bag applications. Dart impact measured by ASTM D1709A also shows a non-linear cliff: a 25 μm film may fall above 120 g, while a 12 μm film often falls below 60 g, because impact resistance depends on the plastic deformation volume and thickness cubed. Gel formation and die-lip plate-out become magnified at thin gauge because a 200 μm gel is invisible in 50 μm film but becomes a failure point in 12 μm film. Melt filtration through 40/80 mesh screen packs protects the die lip but raises melt temperature by 5–10 °C; therefore barrel temperatures are trimmed accordingly. On production-scale lines, gauge variation is monitored with capacitance thickness sensors and must be held within ±4% of nominal, because downstream bag machines amplify thickness error into seal and perforation defects. Published data for A5006FA1280 under all these conditions is limited; these ranges are representative of the high-molecular-weight HDPE film envelope and require confirmation on the target line.
In three-layer coextruded structures for dry-mix pouches, cereal liners, and pet food bags, A5006FA1280 is assigned as the 20–35 μm core or outer moisture-barrier layer between metallocene LLDPE skins. The outer skins provide low seal initiation temperature and high hot tack, while the HDPE layer contributes stiffness, deadfold, and water-vapour resistance. The HDPE core is processed on a dedicated 65 mm grooved-feed extruder with barrel temperatures of 180–200 °C and adapter/die temperatures of 200–215 °C, while the LLDPE skins are run at 150–180 °C to avoid seal-layer degradation. Layer ratios of 30/40/30 or 20/60/20 are common, but the barrier layer must remain continuous; a layer-thickness variation above ±5% creates local water-vapour transmission spikes. Moisture vapour transmission rate is measured by ASTM F1249 at 38 °C and 90% RH; a 70 μm three-layer film with a continuous HDPE core typically falls below 6 g/(m²·day), although published data for this specific grade in a finished coextrusion is limited. Seal performance is tested by ASTM F88 for seal strength and ASTM F1921 for hot tack; the HDPE core shifts the overall seal initiation temperature upward by 5–10 °C compared with an all-LLDPE film. Food-contact compliance for the finished pouch must be evaluated under EU Regulation 10/2011 with worst-case food simulants, and the HDPE layer must meet FDA 21 CFR 177.1520 if the structure is intended for the North American market. The main incompatibility is physical rather than chemical: blending the HDPE layer with recycled LLDPE containing amine-based antifog additives can generate odour at high melt temperatures and should be avoided without prior additive screening.
High-output bag conversion is sensitive to gauge variation because rotary sealing bars and perforation knives operate on a fixed dwell-time basis; even a ±5% thickness drift can cause thin spots to over-seal and thick spots to produce weak cold seams. The seal window for HDPE blown film of this class normally falls between 115 °C and 135 °C, and the actual seal bar temperature must be set 10–15 °C above the film surface temperature because residence time is below 0.1 s on 250–350 cycles/min servo-driven bag machines. Seal initiation and hot tack are measured by ASTM F1921, and final seal strength is measured by ASTM F88 after 24 h crystallisation. Coefficient of friction is controlled by a slip/antiblock package and measured by ASTM D1894; kinetic film-to-metal values below 0.35 are typically required for V-board folding and wicket punching. The additive package must be selected before conversion because excessive erucamide slip migration into the seal area can reduce seal strength by more than 20% after 7 days of storage. Static decay is measured by MIL-PRF-81705D, and a decay time below 0.5 s is required for automatic bag stacking and counting sensors. The terminal product range includes T-shirt grocery bags, produce roll bags, and side-weld garbage liners, but the same film can be used for industrial liners if the gauge is increased to 25–30 μm and the dart impact is verified by ASTM D1709A.
Extrusion blow moulding with A5006FA1280 is evaluated primarily for small to medium containers where moisture barrier, drop impact, and stress-crack resistance are non-negotiable because the high-molecular-weight portion of the resin increases parison melt strength and improves environmental stress-cracking resistance under ASTM D1693 condition B. The target product range includes 5–25 L jerrycans, agrochemical bottles, and UN 3H1/Y-rated containers when the grade is compounded with carbon black or UV stabiliser. Processing is carried out on single-station shuttle or long-stroke blow moulders with 80 mm extruders and accumulator heads; the parison die gap is programmed to 2–4 mm, and the melt temperature is kept at 190–200 °C at the die. High-density polyethylene of this melt flow class shows parison swell of 30–50%, which must be offset through die geometry and wall-thickness programming to avoid pinch-off weld defects and uneven sidewalls. Blow air pressure is set at 0.6–0.8 MPa, and mould temperature is held at 10–30 °C with chiller water to control crystallinity and minimise post-mould shrinkage. Drop impact is tested by ASTM D2463 at -18 °C for UN packaging, and top-load resistance is measured by ASTM D2659. The grade is not recommended for thin-wall injection-moulded caps or closures because the low melt flow rate increases injection pressure and may produce short shots in multi-cavity hot-runner tools; closures are better produced from HDPE grades with higher melt flow rates, while A5006FA1280 is reserved for the container body. Pre-drying is not normally required, but pellets stored at relative humidity above 60% can carry surface moisture that produces splay in the parison and should be dried at 60–70 °C for 2 h. Contamination with polypropylene or PET flakes must be controlled below visible fraction because melt flow separation causes hard spots at the pinch-off weld.
A 2.0 mm geomembrane line requires a flat die with a restrictive die gap if the resin is to achieve the yield stress and elongation values demanded by GRI-GM13. In this segment, A5006FA1280 is converted as a natural resin compounded with 2.0–3.0 wt% carbon black masterbatch, and the carbon black content is verified by ASTM D1603 because carbon black is the primary UV stabilisation mechanism in buried and exposed lining systems. Sheet extrusion is performed on 120 mm or 150 mm single-screw extruders with flat dies up to 7 m wide, melt temperatures of 200–220 °C, and polished chill rolls at 60–90 °C to control cooling rate and reduce internal stress. Thickness uniformity is measured by ASTM D5199, and the minimum average thickness must be maintained; individual readings below -10% of nominal are cause for rejection. Tensile properties are measured by ASTM D638 Type IV specimens at 50 mm/min, and stress-crack resistance is evaluated by the notched constant tensile load test under ASTM D5397; oxidative induction time is measured by ASTM D3895 at 200 °C. A standard OIT below 100 min indicates insufficient stabiliser for long-term service and requires formulation adjustment before the sheet is shipped. The resin must not be extruded above 240 °C because carbon black-filled HDPE can generate oxidative crosslinking and die-lip oxidation product accumulation. The terminal products include landfill caps, canal liners, and secondary containment sheets, but published data for A5006FA1280 in geomembrane-grade testing is limited; therefore each compound formulation must be qualified against GRI-GM13 on the target flat-die line.
Competitive Yanchang China Coal Yulin (Shaanxi) HDPE A5006FA1280 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Yanchang China Coal Yulin (Shaanxi) HDPE A5006FA1280 appears in procurement and extrusion documentation as a high-density polyethylene resin grade produced at the Yulin, Shaanxi complex. The complete technical data sheet for this exact designation is not currently indexed in accessible English-language public literature; therefore, the following discussion separates the general HDPE classification from the product-specific values that must be obtained through the supplier certificate of analysis. HDPE is defined by a density from 0.941 g/cm³ to 0.965 g/cm³ when tested according to ASTM D1505-18 or ISO 1183-1:2019. This density band separates high-density polyethylene from low-density polyethylene and linear low-density polyethylene, but it does not establish the density of A5006FA1280. The suffix FA1280 is treated as a controlled formulation and finishing identifier; its exact meaning is not decoded in the available public literature.
Model-level specification data that require supplier confirmation include melt flow rate at 190 °C/2.16 kg and 190 °C/21.6 kg under ISO 1133-1:2022, density, tensile yield stress, elongation at break, notched impact strength, Vicat softening temperature, and additive loading. Absence of these values prevents any substantiated claim about processability, end-use suitability, or grade equivalence. The grade should not be treated as interchangeable with another HDPE simply because both fall within the density range of 0.941–0.965 g/cm³.
Differentiation from other HDPE products in the same production portfolio is performed through measured rheological and thermal properties rather than code proximity. A change from a blow-moulding HDPE, film-grade HDPE, or pipe-grade HDPE to A5006FA1280 cannot be justified by density class alone. The primary comparative parameters are melt flow rate at 190 °C/2.16 kg and high-load melt flow rate at 190 °C/21.6 kg determined under ISO 1133-1:2022, the resulting melt flow ratio, molecular weight distribution shape, and short-chain branching distribution. A narrow molecular weight distribution typically reduces die swell and increases surface smoothness, but it also raises extrusion pressure and can lower the critical shear rate for melt fracture. A broad molecular weight distribution improves shear thinning and is commonly preferred for large-part blow moulding and thick sheet. If A5006FA1280 contains a slip or antiblock additive package, it may differ from other HDPE grades in coefficient of friction and sealing behaviour; any difference must be verified by ISO 8295:1995 or the relevant packaging standard. Published data for this specific configuration is limited, so the producer’s certificate of analysis is the only valid source for grade-to-grade substitution.
Analytical differentiation is supported by gel permeation chromatography in 1,2,4-trichlorobenzene at 150 °C to determine number-average molecular weight, weight-average molecular weight, and the polydispersity index Mw/Mn. Extrusion-grade HDPE commonly exhibits a polydispersity index from 3 to 25 depending on catalyst technology and reactor conditions. Short-chain branching is inferred from density and comonomer analysis; higher comonomer content lowers density and crystallinity, reducing flexural modulus while increasing environmental stress crack resistance. Without product-specific gel permeation chromatography or comonomer data for A5006FA1280, the exact molecular architecture cannot be stated.
Initial extrusion trials on a grooved-feed single-screw extruder with L/D 30:1 typically begin with a barrel profile from 180 °C in the feed zone to 220–240 °C at the die. Because no public melt flow curve exists for A5006FA1280, start-up should use the lower temperature boundary and rely on melt pressure and motor load data rather than temperature adjustment alone. Feed-throat cooling is maintained at 20–40 °C to prevent resin bridging. Melt filtration through a 60/80/100 mesh screen pack is standard for extrusion-grade HDPE; a pressure rise greater than 0.5 MPa over a single production shift indicates gel accumulation or external contamination and requires screen replacement. HDPE is not hygroscopic, but surface condensation at relative humidity above 60% can produce surface defects; hopper drying at 60–80 °C for 4–6 h is applied when visual moisture is present. Residence time above 240 °C should not exceed 10 min to limit thermo-oxidative chain scission and gel formation. For laboratory additive dilution, a co-rotating twin-screw extruder with L/D 40:1 is used; torque, melt temperature, and die pressure are recorded against the qualified reference resin. Batch-to-batch variance is monitored by trending melt pressure at constant screw speed; a variation greater than ±5% may indicate lot-to-lot rheology drift and requires laboratory confirmation.
Production-scale failure modes associated with HDPE grade substitution include melt fracture, surging, parison instability, die lip build-up, and plate-out. Melt fracture appears as sharkskin or cyclic surface roughness when the critical wall shear stress is exceeded. For general HDPE, critical shear rates are commonly between 100 s⁻¹ and 1000 s⁻¹ at 190 °C, but the exact limit for A5006FA1280 must be measured. Surging is often caused by unstable solids conveying or inadequate barrel temperature; it is observed as periodic variation in die pressure and product thickness. On a grooved-feed extruder, insufficient feed-throat cooling can cause melt film formation in the feed section and reduce output by 10–20%. Parison instability in blow moulding is linked to molecular weight distribution; a narrow distribution can reduce sag resistance, while a broad distribution can improve hang strength. Die lip build-up results from additive migration and low-molecular-weight species; it is controlled by die design, purge procedures, and the stabilizer package. Published data for this specific configuration is limited.
Process conflicts arise when a substitute HDPE is accepted on the basis of a generic density range and the FA1280 suffix is omitted from procurement verification. If A5006FA1280 replaces a previously qualified HDPE without a documented change-control, melt pressure at constant screw speed can shift by more than 10%, parison sag can increase or decrease in blow moulding, and die lip build-up can change because of additive migration differences. These effects are not predictable from density alone. The practical re-validation threshold is a melt flow rate difference greater than 0.5 g/10 min at 190 °C/2.16 kg or a density difference greater than 0.003 g/cm³ relative to the qualified grade. For film extrusion, the critical shear rate for melt fracture should be measured by capillary rheometry at 190 °C, 210 °C, and 230 °C; a shift of more than 15% requires adjustment of die temperature or die gap before stable production can be established.
Additive interactions also constitute a process conflict. If the FA1280 suffix denotes a higher loading of erucamide or oleamide slip additive, surface migration can alter lamination bond strength and printing ink adhesion. Compliance with EU Regulation 10/2011 for food-contact plastics or FDA 21 CFR 177.1520 for olefin polymers must be re-verified when the additive package changes. External antistatic or acid scavenger additives can affect colour stability and plate-out on downstream calibrators. Without the product-specific formulation, the only safe procedure is a laboratory extrusion trial followed by full physical property testing against the current production grade.
Processability comparison should be performed on a 25 mm single-screw laboratory extruder with L/D 25:1 and a rod die, recording output in kg/h, melt temperature, and die pressure at screw speeds of 20 rpm, 40 rpm, and 60 rpm. The data are used to construct a processability fingerprint. If the laboratory extruder is not available, a capillary rheometer with a 1 mm diameter die and 20:1 length-to-diameter ratio can provide shear viscosity data. The Bagley correction and Rabinowitsch correction should be applied to obtain true viscosity and true shear rate.
Mechanical screening of HDPE articles is performed using tensile yield stress per ISO 527-2:2012 or ASTM D638-14, elongation at break, flexural modulus per ASTM D790-17, notched Charpy impact per ISO 179-1:2010 at 23 °C, and Vicat softening temperature per ISO 306:2022 method A50. For the HDPE resin family, tensile yield stress commonly lies between 20 MPa and 32 MPa, and Vicat softening temperature often falls from 120 °C to 130 °C; these ranges describe the class and must not be reported as A5006FA1280 values. Stiffness and environmental stress crack resistance are inversely related: higher density raises flexural modulus but can reduce resistance to slow crack growth. Environmental stress crack resistance is evaluated by ASTM D1693-21 in a nonylphenol ethoxylate or other specified surfactant environment; no product-specific ESCR prediction can be made without the manufacturer’s density and molecular weight distribution data. Finished-part performance in pipe, sheet, film, or blow moulding must be confirmed by product-specific hydrostatic, tear, or drop-impact testing as defined by the end-use standard.
General HDPE category differentiation is useful as a screening reference only. The following table summarizes typical industrial ranges for HDPE sub-classes; it does not assign A5006FA1280 to any category. The ranges are drawn from general HDPE extrusion and moulding practice and are not a substitute for the supplier certificate of analysis.
| HDPE sub-class | Melt flow rate at 190 °C/2.16 kg | Density | Typical processing equipment |
|---|---|---|---|
| Blow moulding | 0.2–1.2 g/10 min | 0.949–0.960 g/cm³ | Accumulator blow moulder with parison programmer |
| Film | 0.3–2.0 g/10 min | 0.948–0.960 g/cm³ | Grooved-feed single-screw extruder with spiral die |
| Pipe | 0.2–0.8 g/10 min | 0.945–0.955 g/cm³ | Single-screw extruder with spiral mandrel die |
| Injection moulding | 4–20 g/10 min | 0.950–0.965 g/cm³ | Injection moulding machine with clamp force matched to part area |
Each incoming lot should be tested against the following matrix before release to production. The table lists applicable standard designations and general HDPE reference ranges; product-specific acceptance limits must be taken from the supplier certificate of analysis because published data for A5006FA1280 is limited.
| Property | Test method | General HDPE reference | Product-specific acceptance |
|---|---|---|---|
| Density | ASTM D1505-18 / ISO 1183-1:2019 | 0.941–0.965 g/cm³ | Supplier certificate of analysis |
| Melt flow rate | ISO 1133-1:2022 at 190 °C/2.16 kg | 0.1–20 g/10 min depending on grade | Supplier certificate of analysis |
| Tensile yield stress | ISO 527-2:2012 | 20–32 MPa | Supplier certificate of analysis |
| Notched Charpy impact | ISO 179-1:2010 at 23 °C | 4–20 kJ/m² | Supplier certificate of analysis |
| Vicat softening temperature | ISO 306:2022 method A50 | 120–130 °C | Supplier certificate of analysis |
| Environmental stress crack resistance | ASTM D1693-21 | > 10 h typical for HDPE | Supplier certificate of analysis |
Storage and handling boundaries apply. Resin should be stored in unopened or sealed containers below 40 °C, protected from direct ultraviolet exposure, and segregated from polypropylene, EVOH, and ionomer regrind. Cross-contamination with those materials can produce phase separation, delamination, and gel defects in finished articles. When A5006FA1280 is used in blow moulding or sheet extrusion, purging with a broad-molecular-weight HDPE before prolonged shutdown reduces die lip build-up and carbonized deposits. The operational limits for potable water, food-contact, and medical packaging must be confirmed under the relevant national or regional standard; published data for this specific configuration is limited. No equivalence with another HDPE grade should be inferred from the density class alone.