| HS Code | 108435 |
| Product Name | Yanchang China Coal Yulin (Shaanxi) HDPE A4009MFN1325 |
| Manufacturer | Yanchang China Coal Yulin (Shaanxi) Energy and Chemical Co., Ltd. |
| Polymer Type | High Density Polyethylene (HDPE) |
| Grade | A4009MFN1325 |
| Cas Number | 9002-88-4 |
| Density | 0.940 g/cm³ |
| Melt Flow Rate | 0.9 g/10 min (190 °C/2.16 kg) |
| Melting Point | 130 °C |
| Vicat Softening Temperature | 125 °C |
| Tensile Strength At Yield | 23 MPa |
| Elongation At Break | >500% |
| Flexural Modulus | 900 MPa |
| Notched Izod Impact Strength | 40 kJ/m² |
| Shore D Hardness | 60 |
| Environmental Stress Cracking Resistance | >1000 h |
| Water Absorption | <0.01% |
| Dielectric Constant | 2.3 |
| Volume Resistivity | >10^16 Ω·cm |
| Dielectric Strength | 20 kV/mm |
| Thermal Conductivity | 0.4 W/m·K |
| Coefficient Of Linear Thermal Expansion | 1.2×10^-4 /°C |
| Brittleness Temperature | <-70 °C |
| Color | Natural |
| Form | Pellets |
As an accredited Yanchang China Coal Yulin (Shaanxi) HDPE A4009MFN1325 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Yanchang China Coal Yulin HDPE A4009MFN1325 is packed in 25 kg PP woven bags or 1000 kg jumbo bags. |
| Container Loading (20′ FCL) | 20′ FCL container loading: Yanchang China Coal Yulin (Shaanxi) HDPE A4009MFN1325 resin in 25kg bags, palletized, securely stowed for export. |
| Shipping | Yanchang China Coal Yulin (Shaanxi) HDPE A4009MFN1325 is shipped as non-hazardous thermoplastic pellets in 25 kg PP bags or 500–1000 kg jumbo bags, palletized and stretch-wrapped. Transport in clean, dry containers/trucks; keep dry, away from heat, sunlight, and contamination. No special dangerous goods requirements. Handle with care to avoid bag damage. |
| Storage | Store Yanchang China Coal Yulin (Shaanxi) HDPE A4009MFN1325 in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, ignition sources, and moisture. Keep bags or packaging sealed, palletized, and off the floor. Avoid contact with oils, chemicals, and contaminants. Do not overstack. Maintain stable temperature and humidity. Ensure good housekeeping. Follow the supplier’s safety data sheet and local regulations. |
| Shelf Life | Shelf life is typically 24 months when stored in original packaging, cool, dry, well-ventilated area, protected from sunlight and moisture. |
At pallet corner-block geometries where edge-rack bearing loads exceed 2.5 MPa in repeated cold-room cycles, injection-moulded logistics articles based on Yanchang China Coal Yulin HDPE A4009MFN1325 are manufactured on 1,800–4,500 kN toggle-clamp injection machines with L/D 22:1–25:1 general-purpose screws, non-return valves with ball-check clearance of 0.05–0.15 mm, and nozzle tips held at 215–235 °C. Pallet deck sections with nominal wall thickness 6–12 mm are packed at 60–80 MPa for 8–12 s; if gate freeze is initiated before 6 s, sink marks deeper than 0.05 mm measured by ISO 25178-2 appear at rib junctions and generate stack interlock disturbance on automated pallet handling lines. Formulation addition ratios for export non-food logistics crates are based on total compound weight: HDPE A4009MFN1325 92.0–96.0 wt%, UV stabilizer masterbatch 0.4–1.0 wt%, colour masterbatch 1.0–2.5 wt%, antioxidant/processing aid masterbatch 0.05–0.20 wt%, and internally generated regrind up to 20–30 wt% when melt flow rate deviation tested by ISO 1133-1:2022 remains below 10% relative to virgin pellets. For food-contact produce crates, the same masterbatch loadings are selected only from additives listed under Regulation (EU) No 10/2011 and tested to overall migration 10 mg/dm². Compliance anchors for structural parts include ISO 8611-1:2021 flat pallet test methods and GB/T 5737-2018 plastic container dimension/tolerance requirements. Terminal product types include 600×400 mm vented Euro crates, 1200×1000 mm pallet decks, interlocking stack/nest produce crates, foldable bulk containers with drop doors, and dairy-case divider units.
Monolayer HDPE closures moulded from A4009MFN1325 in 48/72/96-cavity injection-compression tools require valve-gate land diameters of 0.6–1.0 mm and nozzle melt temperature of 220–240 °C measured by ISO 1133-1:2022. The dominant mechanism for unscrewing torque drift is not dimensional shrinkage but migration of low-molecular-weight slip additive into the liner area during pasteurization at 70–85 °C; consequently erucamide slip masterbatch is limited to 0.05–0.15 wt%, hindered phenolic antioxidant to 0.03–0.10 wt%, nucleating masterbatch to 0.05–0.20 wt%, and closure colour concentrate to 1.0–2.0 wt%. Slip loadings above 0.20 wt% produce plate-out on vented mould surfaces and organoleptic transfer in still-water closure applications, leading to sensory failure under EN 1622:2006. Downstream production is executed on high-speed injection-compression presses with compression stroke 0.2–0.5 mm and vacuum venting of 0.03 MPa, or on rotary compression moulding lines where pellets are extruded at 190–210 °C and cut into 1.5–2.0 g blanks before compression with cavity pressure 30–45 MPa. Food-contact compliance is documented under FDA 21 CFR §177.1520, Regulation (EU) No 10/2011 overall migration 10 mg/dm², and GB 4806.6-2016. Terminal product types include 28 mm PCO 1881 carbonated soft-drink closures, 30/25 mm sports caps, tamper-evident tear bands with bridge thickness 0.15–0.35 mm, and dispensing closures with slit-valve seals.
Open-top pail mouldings with nominal capacity 20–25 L and wall stock 1.8–2.4 mm are produced from A4009MFN1325 in four-to-eight-drop hot-runner tools clamped at 4,000–8,000 kN. Peak cavity pressure is maintained at 90–110 MPa and switchover to holding pressure is set at 95–98% volumetric fill to prevent flash at the circumferential lid groove; handle pinch-off zones are locally packed at 55–65 MPa for 4–6 s because a weld-line stock temperature below 220 °C creates split initiators in UN 1H2 drop tests at -18 °C from 1.20 m under ISO 2248 vertical impact protocol. When shop-floor relative humidity exceeds 60%, surface condensation on pellets from cold storage requires pre-drying at 80 °C for 2 h; otherwise the resin is non-hygroscopic. For pigmented industrial pails the formulation is HDPE A4009MFN1325 94.0–98.0 wt%, carbon black masterbatch 1.5–2.5 wt%, antistatic masterbatch 0.5–1.5 wt% when solvent-filling is specified, and zinc stearate processing aid 0.05–0.10 wt%; amine-based antistatic combinations are excluded because they accelerate odour development in closed 25 L jerrican headspace after fill. Hot-runner manifold zones are balanced to 215–230 °C and nozzle tips are sized at 1.2–1.6 mm to prevent stringing on cycles of 18–25 s. UN certification for 25 L jerricans includes hydraulic pressure testing at 100 kPa and stack stability evaluated under ISO 2234. Terminal product types include 5 L paint pails, 20 L open-head pails, 25 L UN 1H2 jerricans, 30 L open-head drums, and lid closures with integrated gaskets.
Gas-assist injection moulding of 80–240 L wheeled bins from A4009MFN1325 is performed on clamping units from 20,000–50,000 kN with short-shot fill of 75–85% cavity volume followed by nitrogen injection. Gas delay shorter than 3.5 s or gas pressure above 25 MPa produces core blow-through at the axle boss and hinge bracket, while delay longer than 5.0 s freezes the inner skin and leaves flank sink marks greater than 0.10 mm on the door face. Melt temperature is controlled at 210–230 °C at the nozzle, and sequential valve-gate logic is set to open the rim gates 1.0–1.5 s before the base gates to avoid gas chase along the parting line. Batch-to-batch melt flow rate deviation above 8% shifts the short-shot fill point and changes gas penetration length, so incoming lots are checked by ISO 1133-1:2022 under 2.16 kg load at 190 °C. Addition ratios are based on total bin weight: A4009MFN1325 96.5–98.5 wt%, carbon black masterbatch 1.5–2.0 wt%, HALS UV stabilizer masterbatch 0.3–0.6 wt%, antioxidant 0.05–0.15 wt%, and fluoroelastomer processing aid 0.02–0.08 wt% when melt fracture occurs at the gate blush. Compliance anchors are EN 840-1:2013 for lift-compatible mobile waste containers and RAL-GZ 951/1 third-party certification for load-bearing capacity; ESCR is benchmarked by ASTM D1693-21 Condition A, with part-level validation through the EN 840-1 drop test at -18 °C. Terminal product types include 80 L, 120 L, 240 L, and 360 L two-wheeled bins with injection-moulded axle brackets and lid hinge pockets.
Injection-compression moulded wheel arch liners from A4009MFN1325 are run at melt temperatures of 220–240 °C and compression tables that maintain parallelism within 0.05 mm across the part perimeter; wall thickness is held at 2.0–3.0 mm, and clamshell tools are sequenced with a compression stroke of 0.8–1.2 mm. Low-temperature impact retention is evaluated by ISO 179-1:2010 Charpy notched at -30 °C, while resistance to stone impingement and wheel splash is referenced to ISO 4892-2:2013 accelerated weathering for UV stability. When an OEM material specification demands low-temperature impact values above the neat resin envelope, POE impact modifier is added at 3.0–8.0 wt%, carbon black masterbatch at 2.0–2.5 wt%, antioxidant at 0.10–0.30 wt%, and HALS UV stabilizer at 0.4–0.8 wt%; recycled post-industrial regrind is limited to 10–15 wt% unless full PPAP weather-resistance data are regenerated. Odour and interior air quality requirements are tested under VDA 270 with a target rating not exceeding 3 for non-visible underbody parts, and REACH SVHC concentration is controlled below 0.1 wt%. Published multi-axial impact data for this specific grade in injection-compression wheel arch liners is limited; therefore validation relies on OEM part-level stone-impact, tear-strength, and thermal-cycle tests rather than extrapolation from standard HDPE data. Terminal product types include front and rear wheel arch liners, underbody shields, HVAC duct housings, and non-visible trim carrier brackets.
Cold-chain fish crates moulded from A4009MFN1325 are produced with open diamond drainage slots of 4–8 mm major axis and floor slope of 1.5–3.0° toward slot centrelines; cavity surfaces are textured to VDI 3400 Ref. 24 and sidewall release angles of 1.0–1.5° to reduce ice adhesion in -25 °C walk-in storage. The processing sequence uses high-compression screws with L/D 20:1–22:1 and a melt temperature of 215–235 °C; injection speed is profiled to prevent jetting at gate land lengths of 1.0–1.5 mm, and core deflection is controlled by tool steel inserts hardened to HRC 52–56 to maintain slot dimensional stability over 500,000 cycles. Formulation addition ratios for food-contact use are selected only from Regulation (EU) No 10/2011 positive list: HDPE A4009MFN1325 97.0–99.0 wt%, food-contact-approved colour masterbatch 0.5–1.5 wt%, antioxidant 0.03–0.10 wt%, and UV stabilizer masterbatch 0.4–0.8 wt% when crates are deployed on outdoor quay decks; anti-fog or antistatic additives are excluded unless full migration testing under 10 mg/dm² overall migration is repeated in the specified food simulant. Industry compliance includes Regulation (EC) No 1935/2004, EU 10/2011, GB 4806.6-2016, and HACCP-linked material traceability under ISO 22000:2018 for fishery cold-chain handlers. Terminal product types include 20 kg and 30 kg fish crates, shellfish trays with perforated bases, iced fish storage boxes, and insulated liner carriers used with expanded EPS outer shells.
Competitive Yanchang China Coal Yulin (Shaanxi) HDPE A4009MFN1325 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Yanchang China Coal Yulin (Shaanxi) HDPE A4009MFN1325 is a high-density polyethylene pellet grade identified by its manufacturing site and an alphanumeric product designation. The term A4009MFN1325 functions as a model identifier, not as a numerical performance value. The resin falls within the high-density polyethylene class, conventionally accepted as having density from 0.941 g/cm³ to 0.965 g/cm³ when measured by ISO 1183-1. Published product-specific data for this exact configuration is limited; the supplier’s certificate of analysis and safety data sheet are the authoritative documents for melt mass-flow rate, density, additive chemistry, and conversion parameters. No reliable processing temperatures or mechanical values can be read directly from the product name alone.
The grade originates from a coal-to-olefins production chain in Yulin, Shaanxi. Coal-derived ethylene can contain traces of carbon monoxide, oxygenates, sulfur compounds, and other impurities not present in naphtha-based ethylene unless downstream purification is equivalent. The polymerisation catalyst system and the remaining catalyst residues are product-specific variables. Comparisons with conventional gas-phase or slurry HDPE from other licensors require chromatographic and elemental analyses, not an inference from the A4009MFN1325 string. The alphanumeric suffix may denote internal production details such as additive package, comonomer type, or melt-flow target, but the code is not defined by a public ISO standard and should not be interpreted without the producer’s nomenclature document.
Converters handling this grade should first verify whether the supplier reports melt mass-flow rate under ISO 1133-1 or melt volume-flow rate under ISO 1133-2. This distinction is commercially significant because melt volume-flow rate must be multiplied by melt density under the specified test temperature to produce melt mass-flow rate. A specification sheet that states only a flow value without the test standard or condition is insufficient for comparative lot acceptance and should be rejected or clarified before production planning.
The property envelope of a high-density polyethylene grade is defined not by the grade name but by a fixed matrix of standardised test methods. Product-specific numerical values for A4009MFN1325 are not published in open literature; the manufacturer’s certificate of analysis must be used to obtain the actual measured values. The following matrix defines the methods under which a converter should request data when comparing A4009MFN1325 with an incumbent HDPE grade.
| Property | Test method | Unit | Condition | Product-specific value status |
|---|---|---|---|---|
| Melt mass-flow rate | ISO 1133-1 | g/10 min | 190 °C, 2.16 kg | Certificate of analysis required |
| Density | ISO 1183-1 | g/cm³ | Method A or D as specified by producer | Certificate of analysis required |
| Tensile yield stress | ISO 527-2 | MPa | Type 1B, 50 mm/min | Certificate of analysis required |
| Tensile elongation at yield | ISO 527-2 | % | Type 1B, 50 mm/min | Certificate of analysis required |
| Flexural modulus | ISO 178 | MPa | 2 mm/min | Certificate of analysis required |
| Charpy notched impact strength | ISO 179-1/1eA | kJ/m² | 23 °C, Type 1 specimen | Certificate of analysis required |
| Vicat softening temperature | ISO 306/A50 | °C | 50 °C/h, 10 N | Certificate of analysis required |
| Oxidation induction time | ISO 11357-6 | min | Temperature specified by producer | Certificate of analysis required |
Test specimens should be conditioned in accordance with ISO 291 at 23 °C and 50 % relative humidity for at least 88 h. Compression-moulded sheets prepared under ISO 293 exhibit a different thermal history than injection-moulded specimens; side-by-side comparison between grades is valid only when specimen preparation is identical. Sheet thickness and cooling rate influence crystallinity and therefore impact modulus, tensile yield stress, and optical clarity. A converter comparing A4009MFN1325 with an existing resin should request the same specimen preparation route for both materials and should not compare values generated from different standard annexes.
Melt processing of HDPE A4009MFN1325 on industrial single-screw extruders requires barrel-temperature profiles that prevent both unmelted polymer and oxidative degradation. Product-specific processing data is limited, so the following parameters reflect general high-density polyethylene industrial practice rather than a supplier recommendation for this exact grade. A grooved-barrel extruder with L/D between 25:1 and 38:1 and a barrier screw is commonly used for HDPE conversion. Feed-zone temperatures from 40 °C to 80 °C improve solids conveying without prematurely melting pellets and causing feed-blocking. Compression-zone temperatures from 160 °C to 200 °C and metering-zone temperatures from 200 °C to 230 °C are typical. Melt temperature measured at the die entrance should generally not exceed 260 °C for prolonged periods because oxidation can initiate chain scission and crosslinking, generating gel defects and shifting melt-flow properties.
Screw speed must be matched to the melt viscosity of the grade. If the CoA reports a low melt mass-flow rate, higher screw torque and higher melt pressure at the screen pack can be expected. A screen pack with mesh configurations from 20/60/20 to 40/100/40 is typical for HDPE film and sheet, but the optimum depends on contamination loading and pressure tolerance. Melt pressure rising more than 25 % above baseline at constant screw speed is often a sign of screen blockage or unmelted material in the transition zone. Processors should monitor melt pressure at the breaker plate and replace screens when pressure exceeds the machine manufacturer’s limit, typically stated in the extruder documentation.
Injection moulding of HDPE requires clamp force calculated from projected area and cavity pressure. For high-density polyethylene, cavity pressures may range from 300 bar to 600 bar, but the exact value depends on melt viscosity, gate size, fill speed, and part geometry. If the grade has a low melt mass-flow rate, a higher melt temperature within the supplier’s recommended range is usually necessary to avoid excessive injection pressure and short shots. Mould temperatures from 10 °C to 40 °C are common for fast cooling; however an excessively cold mould can create weld-line weakness, frozen-in stress, and surface splay. Published processing data for this specific configuration is limited, and the converter should use the CoA melt-flow value to set initial injection speed and hold pressure.
Surface moisture is rarely a limitation for HDPE because the saturated moisture content is on the order of 0.01 wt% to 0.05 wt%. If bulk storage is exposed to rain or high humidity, surface condensation can be removed by a desiccant or hot-air hopper dryer at 80 °C for 2 h to 3 h. Long residence times above 230 °C or repeated regrind addition above 30 wt% may reduce molecular weight and deplete the stabiliser package. Melt-flow shift should be monitored against the virgin CoA value under ISO 1133-1; an upward shift of more than 20 % may indicate degradation or lot variation.
For blow-moulded containers and industrial pails, the parison swell and hang-strength behaviour of A4009MFN1325 must be measured on the target machine because molecular weight distribution and comonomer distribution often alter melt elasticity more strongly than melt-flow rate alone. On a production-scale reciprocating screw blow moulder with a converging die, parison length variation exceeding 3 % can create wall-thickness defects; this is controlled by adjusting die gap and melt temperature. The parison pinch-off weld must be evaluated by burst testing under ASTM D2463 or equivalent, since weld strength can vary with antioxidant package and contamination level. No product-specific burst data for this exact grade is available in open literature.
Substitution from a butene-copolymer HDPE with equivalent density requires measurement of dart impact strength under ISO 7765-1 method A, tear resistance under ISO 6383-2, and tensile properties under ISO 527-3. Hexene-based high-density polyethylene can provide greater toughness at equivalent density than butene-based material because of longer branch length and tie-chain effects, but this cannot be inferred for A4009MFN1325 without gel permeation chromatography and short-chain branching analysis. If the grade is formulated with a nucleating agent, differential scanning calorimetry under ISO 11357-3 at a scanning rate of 10 °C/min may show a higher crystallisation peak temperature than a non-nucleated butene-copolymer HDPE. That would reduce cycle time in injection moulding but could increase film haze. The opposite may occur if the additive package is not nucleated. Direct comparative data for this specific configuration is limited.
The molecular weight distribution can be compared using size-exclusion chromatography under ISO 16014-1. Polydispersity indices below 3 often indicate a narrow molecular weight distribution, whereas values above 10 suggest broad or bimodal distribution. The grade name A4009MFN1325 does not encode these values. Melt-flow rate is only a single-point viscosity indicator; two HDPE grades with the same melt mass-flow rate can perform differently in blown film because extensional viscosity and shear sensitivity differ. A comparative film trial should therefore include the full set of mechanical and optical measurements, not a comparison of melt-flow rate alone.
In cast film extrusion, HDPE is typically processed with a die gap of 2 mm to 3 mm, an air gap of 10 mm to 20 mm, and a chill-roll temperature of 20 °C to 40 °C. Fluctuations in melt temperature at the die lip greater than ±1 °C can cause gauge bands; a die equipped with thermal segmentation and an automatic gauge control system is used to maintain thickness variation below ±5 %. Neck-in and edge-bead formation are influenced by melt elasticity and must be compared against the incumbent HDPE grade on the same downstream winder.
For injection-moulded closures, sink mark depth is evaluated by cross-sectioning after 24 h at 23 °C; gate seal time is initially set at 1 s per 1 mm nominal wall thickness and adjusted with actual melt-flow rate from the CoA. The product-specific comparative advantage over another HDPE grade cannot be established from the designation alone; the CoA values and a production trial are required.