| HS Code | 784956 |
| Density | 0.954 g/cm³ |
| Melt Flow Rate | 0.4 g/10 min |
| Tensile Strength At Yield | 22 MPa |
| Elongation At Break | 500% |
| Flexural Modulus | 1000 MPa |
| Vicat Softening Temperature | 125 °C |
| Brittleness Temperature | -70 °C |
| Shore D Hardness | 60 |
| Water Absorption | <0.01% |
| Dielectric Constant | 2.3 |
| Volume Resistivity | >10^16 Ω·cm |
| Thermal Conductivity | 0.4 W/m·K |
As an accredited Yanchang China Coal Yulin (Shaanxi) HDPE 6094 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Yanchang China Coal Yulin (Shaanxi) HDPE 6094 is packed in 25 kg PP woven bags with PE liners, palletized and stretch-wrapped. |
| Container Loading (20′ FCL) | Yanchang China Coal Yulin (Shaanxi) HDPE 6094: 20′ FCL container loading, 25kg bags, securely stowed for safe ocean transport. |
| Shipping | Yanchang China Coal Yulin (Shaanxi) HDPE 6094 ships as non-hazardous polyethylene resin pellets in 25 kg PP bags or 1,000 kg jumbo bags, palletized and stretch-wrapped. Transport in clean, dry containers by sea/land. Keep dry, away from direct sunlight and heat; store in a cool, ventilated warehouse. |
| Storage | Store Yanchang China Coal Yulin (Shaanxi) HDPE 6094 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, moisture, and strong oxidizers. Keep in original sealed bags on pallets, avoiding punctures, contamination, and dust. Protect from UV, physical damage, and excessive stacking. Maintain clean handling areas; follow local fire, safety, and environmental regulations. Use FIFO inventory to prevent aging. |
| Shelf Life | Yanchang China Coal Yulin (Shaanxi) HDPE 6094 shelf life: typically 24 months if stored cool, dry, away from direct sunlight. |
In blown film conversion, HDPE 6094 from Yanchang China Coal Yulin (Shaanxi) is processed on extruders with L/D ratio between 30:1 and 38:1, barrier screws and spiral mandrel dies; grooved-feed sections are used to stabilise the feed zone when the extrudate is a high-viscosity melt. Screen pack configurations of 40/60/100 mesh reduce gel contamination and die-lip carbonization, while a rise in head pressure of more than 10% at constant screw speed indicates polymer degradation or additive dispersion failure. The temperature profile from feed to die is maintained between 180 °C and 230 °C, with die temperature no more than 20 °C above the adapter, to control melt strength and frost line height. Die gap 0.8 mm to 1.5 mm and blow-up ratio 3.5:1 to 5.0:1 produce film gauges from 8 μm to 35 μm. The frost line is positioned at 6 to 10 die diameters above the die face; a higher frost line raises dart drop impact but lowers machine-direction tear. Extruder output is set in proportion to die circumference at 0.6 kg/h to 1.2 kg/h per millimetre of die diameter, with bubble stability monitored by internal pressure and air ring temperature. Mechanical properties are measured under ASTM D882-18 for tensile, ASTM D1922-15 for Elmendorf tear, and ASTM D1709-16a for dart impact. Stress crack resistance is measured by ASTM D1693-15 Condition B in 10% Igepal CO-630 at 50 °C. Lightweight produce bags, industrial liners and heavy-duty sacks are the principal blown film articles. A process boundary appears at film thickness below 5 μm, where bubble stability declines and pinhole frequency increases because the melt is too stiff to support rapid necking.
When blown film lines add 3 wt% to 7 wt% LDPE or LLDPE to improve bubble stability and tear strength, the blend changes the density of the finished film by 0.001 g/cm³ to 0.003 g/cm³ and alters the seal initiation temperature. Sealability is therefore checked on a hot-tack tester per ASTM F1921-12, and film producers must reset the sealing temperature after every lot change. A known incompatibility is the combination with high levels of metal stearate lubricants, which can deposit on the die lip and generate speck defects. During extended runs, the high molecular weight fraction tends to accumulate at the die lip; the die is purged with a commercial polyolefin purge compound before the lip gap is mechanically cleaned. Melt pressure at the screen pack is commonly held between 150 bar and 250 bar, and a pressure drop of more than 15% across the screen pack indicates channeling or screen blinding. If the ambient relative humidity exceeds 60%, pre-drying is required at 70 °C to 80 °C for 2 to 4 hours to prevent surface splay and micro-voids.
Flat-die extrusion for geomembrane and industrial liner from HDPE 6094 operates with a gear pump between the extruder and a flexible-lip die to suppress pressure pulsations and transverse thickness variation. Melt temperatures of 220 °C to 250 °C are applied, with die gap 1.5 mm to 2.5 mm. The sheet is calendered between a mirror-finish roll at 70 °C to 95 °C and a cooling roll at 40 °C to 70 °C to control curl and shrinkage. Thickness from 0.5 mm to 2.5 mm is monitored by a traversing beta gauge; thickness variation is maintained within ±5% at all points across the web. The relevant property set includes density per ASTM D1505-18, tensile at break per ASTM D6693-16, tear resistance per ASTM D1004-13, puncture resistance per ASTM D4833-07, ESCR per ASTM D1693-15 and oxidative induction time per ASTM D3895-19. High-density polyethylene geomembrane liners frequently require carbon black dispersion per ASTM D5596-94 to prevent UV degradation and oxidative embrittlement. Flat-die processing of a sub-1.0 g/10 min melt index resin demands higher head pressure, typically 150 bar to 250 bar before the screen pack; this pressure increases the risk of melt inhomogeneity if the screw lacks a shear mixer. The extrudate swell is also stronger than with injection-grade HDPE, so die lip opening must be set narrower than the target sheet thickness to prevent over-thick edges. For landfill pond liners and tank farm secondary containment, the finished liner is evaluated under GRI GM13 and GRI GM17 for HDPE geomembranes. A processing boundary appears when the sheet is stretched too rapidly at the roll stack: surface haze and thickness banding occur if the draw ratio exceeds 1.2:1.
Seam tensile strength of field-fabricated liners is measured per ASTM D6392-12; weld shear strength and peel strength are recorded at 25 °C and 0 °C. If the liner is in contact with aggressive leachate, chemical resistance is screened by immersion in 10% HCl, 10% NaOH, and methanol for 30 days at 23 °C; tensile retention values below 80% after immersion signal a formulation conflict and require project-specific approval. There is a known boundary with high levels of recycled geomembrane flake: post-consumer reclaim at more than 15 wt% reduces ESCR sharply and can produce pinholes during flat-die extrusion due to volatile contaminants. The converter typically pre-dries reclaim at 70 °C to 80 °C for 3 hours and uses a vacuum vent on the extruder to strip moisture and residual odour. Because the melt index remains low, the flat-die line is not operated with a narrow lip opening and high draw speed; this would impose excessive orientation and reduce environmental stress crack resistance in the finished liner.
Because high-molecular-weight HDPE exhibits pronounced post-extrusion swell and sag, extrusion blow moulding of HDPE 6094 into 120 L to 220 L L-ring drums and 20 L to 30 L jerry cans uses accumulator-head machines with shot volumes from 2 L to 10 L and clamp force from 500 kN to 8,000 kN. The melt temperature measured at the die exit is maintained at 180 °C to 210 °C; die head tooling is sized 45% to 65% smaller in diameter than the finished parison diameter to compensate for swell. Blow air is delivered at 0.6 MPa to 0.9 MPa, and the mould is held at 8 °C to 20 °C to freeze the pinch-off weld and shorten cycle times. Wall thickness distribution is controlled by a 32-point or 64-point axial parison programmer; the portion of the parison corresponding to the top and bottom chime is programmed 20% to 30% heavier than the sidewall. In the pinch-off zone, low molecular orientation can cause stress cracks, so the length of the pinch is set to 8 mm to 12 mm and the final flash removal is done after part cooling. Critical tests include drop impact at -18 °C per ASTM D2463-15, stack loading per ASTM D642-21, and ESCR per ASTM D1693-15 Condition B. For UN-certified packaging, performance tests are conducted according to the applicable UN Model Regulations for dangerous goods packaging, including hydraulic pressure and leakproofness for 1H1 drums. Food-contact grades must satisfy FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011 as amended. A boundary condition appears with mould temperatures above 25 °C: thick-walled sections fail to freeze before ejection and exhibit post-mould shrinkage.
Parison programming must be linked to the rheological character of the resin, not a generic curve. The 64-point axial wall thickness controller accumulates shot volume data; transients in the accumulator during shot transfer produce temperature differences of 5 °C to 15 °C across the parison if the transfer pot is not heated uniformly. Such temperature differences cause uneven swell and result in thick-thin bands in the sidewall. The pinch-off weld is the weakest zone in a drum; flash thickness and mould trench geometry are adjusted to generate a compressive yield in the weld. On 220 L drums, the pinch weld length is 10 mm to 12 mm, and the mould closing speed is slowed in the final 5 mm to avoid excessive material squeeze-out. Moisture in the resin at levels above 0.02 wt% can cause pinholes or splay marks at the bottom flash. Conveying and drying of the resin in a desiccant hopper at 70 °C for 2 hours is required when ambient humidity exceeds 60%. Inside the drum body, wall thickness is checked with an ultrasonic thickness gauge; variation of ±10% is accepted only outside the chime and pinch zones. Processors should not substitute this grade with a low-molecular-weight injection grade to increase output, because the drop in melt strength and ESCR causes pin-hole leaks at the pinch weld after 30 days of stacked storage.
Quench-bath cast film and tape lines running HDPE 6094 produce oriented tapes for woven sacks and monofilaments for ropes and nets. The resin is melted at 200 °C to 230 °C, extruded through a slit die, and quenched in a water bath at 30 °C to 55 °C with an air gap of 10 mm to 30 mm. The quenched sheet is slit into tapes 1.2 mm to 3.0 mm wide and drawn through a hot-air oven or hot roll system at 95 °C to 120 °C. The draw ratio is maintained between 6:1 and 9:1; below 6:1 the tape has low tenacity and high elongation, while above 9:1 fibrillation and web breaks increase sharply. Annealing after stretching at 100 °C to 110 °C under 3% to 5% relaxation reduces residual shrinkage to less than 2%. Finished tape tenacity is evaluated under ISO 2062:2009 or ASTM D2256-21, with conditioning at 23 ±2 °C and 50 ±5% relative humidity according to ISO 139. The coefficient of friction and slit-edge quality are controlled with calcium carbonate masterbatch additions of 2 wt% to 5 wt%, which reduce blocking on the loom. A process limitation occurs if the water bath temperature drops below 25 °C: the quench is too rapid, causing internal voids and poor drawability.
Monofilament orientation requires careful control of draw resonance. If the draw ratio is raised too quickly, the cross-section becomes oval and the filament drifts from the drawing rolls. The draw gap between the first and second godet rolls is set at 1,000 mm to 1,500 mm for tapes to allow necking at a stable point. In monofilament dies, the holes are arranged in circular patterns, and the hole diameter is 1.8 mm to 2.5 mm for finished diameters of 0.15 mm to 0.60 mm after drawing. The draw bath temperature around the godet rolls is maintained at 90 °C to 98 °C. When water quench is replaced by air quench, the tape thickness is limited to 0.8 mm; above this thickness, crystallinity in the core remains high and the tape splits during orientation. Additive packages for monofilament should avoid primary antioxidants with high colour contribution if the final product is used in visible netting; discoloration is measured under ASTM D6290-19 yellow colour index. Reclaim from edge trim during tape production is incorporated at up to 10 wt% only after granulation and blending, because higher reclaim levels lower the melt strength required for stable necking and increase tape break frequency.
| Application segment | Critical standard / method | Measured parameter |
|---|---|---|
| Blown film | ASTM D882-18, ASTM D1709-16a, ASTM D1922-15 | Thickness 8 μm to 35 μm; dart drop and tear retained by end-use |
| Geomembrane | ASTM D6693-16, ASTM D1693-15, ASTM D3895-19 | Thickness 0.5 mm to 2.5 mm; weld peel and shear strengths per project specification |
| Extrusion blow moulding | ASTM D2463-15, ASTM D1693-15, UN Model Regulations 6.1 | Drop impact at -18 °C; ESCR Condition B |
| Oriented tape / monofilament | ISO 2062:2009, ASTM D2256-21 | Draw ratio 6:1 to 9:1; residual shrinkage <2% |
| Cast sheet / thermoforming | ISO 527-2:2012, ISO 178:2019, ASTM D543-21 | Sheet thickness 2 mm to 10 mm; tensile retention after immersion |
| Corrugated pipe / conduit | EN ISO 9969, ASTM F2306-22, ASTM F2160-22 | Ring stiffness SN2 to SN8; wall thickness per DN-series dimension |
For industrial dunnage and thermoformed tote inserts, HDPE 6094 is run on single-screw extruders with L/D ratio 30:1 to 38:1 and a gear-pump-assisted flexible-lip die. Melt temperature 210 °C to 240 °C is maintained, and the die gap is set 15% to 25% above target sheet thickness because high-viscosity melt exhibits die swell. The polished roll stack is operated at 75 °C to 95 °C top roll and 60 °C to 80 °C bottom roll to balance surface gloss and residual stress. Sheet thickness from 2 mm to 10 mm is produced; thicker sheet above 10 mm can develop vacuum voids unless the resin is pre-dried at 70 °C to 80 °C for 2 to 4 hours when ambient relative humidity exceeds 60%. Thermoforming of HDPE 6094 sheet requires surface temperature 160 °C to 180 °C; below this range the sheet does not conform uniformly; above it, plug marks and thinning at corners occur. The formed part is tested for tensile properties per ASTM D638-14 or ISO 527-2:2012, and flexural modulus per ASTM D790-17 or ISO 178:2019. Chemical resistance is screened in immersion per ASTM D543-21, with reportable changes in mass and tensile retention after 7 days at 23 °C. Large thermformed parts replace glass-reinforced thermoset laminates in moderate chemical exposure trays; structural loading must account for the lower modulus of unfilled HDPE, which is in the range of 800 MPa to 1,400 MPa depending on crystallinity and test rate. A processing boundary exists when the extruder back pressure is below 100 bar: melt homogeneity declines, leading to specks and thickness variation.
Thermoforming moulds for HDPE 6094 are usually blanketed with 10 °C to 20 °C water lines to extract heat from thick sections. The sag resistance of the melt is high, which permits male plug forming of deep-draw totes with draw ratios up to 1.5:1. When the sheet is heated to 170 °C, high molecular weight causes it to resist thinning near the clamp frame; however, sheet thickness in the corner region can still fall below 50% of the initial gauge if the plug speed is too low or the plug temperature exceeds 80 °C. In cutting boards, the sheet is stress-relieved by annealing at 90 °C for 30 minutes after extrusion to reduce curl. Fabricated parts are tested for tensile at yield per ISO 527-2:2012, notched impact per ISO 180:2019 at -20 °C, and Vicat softening temperature per ISO 306:2022 Method A50. There is a property cliff at processing melt temperatures above 245 °C: chain scission begins and the material turns yellow, with a drop in notched impact strength of more than 20% compared with 230 °C processing. This limits sheet temperature settings and excludes hot-runner injection-type thermal histories for this resin class.
Non-pressure corrugated drainage pipe and cable conduit from HDPE 6094 are produced on corrugators where the melt is drawn into moving mould blocks under vacuum. Melt temperature is set at 200 °C to 230 °C; pipe head pressure at the die is 150 bar to 250 bar. Mould block vacuum is set at 0.4 bar to 0.8 bar negative pressure to pull the melt into corrugation valleys. The corrugated product is formed at speeds of 0.5 m/min to 8 m/min depending on diameter and corrugation pitch. For drainage pipe, outside diameter ranges from 75 mm to 800 mm in DN-series dimensions; ring stiffness is tested under EN ISO 9969 and is classified as SN2, SN4 or SN8, where the number after SN denotes kilonewtons per square metre at 3% circumferential deflection. Pipe wall thickness and weld line at the block pinch are inspected under ASTM F2306-22 for HDPE corrugated drainage pipe and ASTM F2160-22 for conduit. Impact resistance is evaluated at -20 °C to 0 °C by the falling-weight method. The low melt flow of HDPE 6094 improves melt strength, which reduces sidewall collapse on large-diameter profiles; however, the high molecular weight also increases extruder current draw and requires barrel cooling in the feed zone to avoid premature melting and rat-holing. A limitation appears in the conduit jacket application if operating temperature exceeds 60 °C, because creep and load-deflection increase; the end-use design must include derating factors per ISO 178 or long-term hydrostatic data for pressure-rated variants.
Corrugated pipe from HDPE 6094 is often coextruded with a black outer layer containing 2.0 wt% to 2.5 wt% carbon black to satisfy outdoor UV resistance. The inner layer may be unfilled natural HDPE; the melt streams are combined in a spiral distribution coextrusion die and then drawn into the corrugator. If the two melts differ by more than 30 °C at the die entry, interface instability creates wrinkles in the corrugation valleys. Vacuum calibration is critical on the downstream side; insufficient vacuum below 0.3 bar leads to incomplete block fill and flat spots on the pipe crown. Pipe stiffness is checked at 3% deflection to classify SN2, SN4 or SN8; the relationship between ring stiffness and wall thickness depends on diameter but generally follows cubic thickness dependence. In cable conduit, the internal surface roughness is kept below 10 μm to ease cable pulling; the die mandrel is polished to Ra below 0.4 μm. A processing boundary exists when line speed is pushed above 8 m/min for 110 mm diameter pipe: cooling water at 10 °C to 20 °C and vacuum residence time become insufficient to set the corrugations before the mould blocks open, resulting in spring-back and dimensional instability.
Competitive Yanchang China Coal Yulin (Shaanxi) HDPE 6094 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Yanchang China Coal Yulin (Shaanxi) HDPE 6094 is a high-density polyethylene grade produced by Shaanxi Yanchang China Coal Yulin Energy Chemical Co., Ltd. on the coal-to-olefin methanol-to-olefin platform. The resin is positioned for extrusion blow molding of industrial hollow parts rather than thin-wall injection molding. Nominal values published for this product class include a melt flow rate of 0.9 g/10 min at 190 °C under a 2.16 kg load according to ASTM D1238-23 and a density of 0.949 g/cm³ according to ASTM D1505-18. These figures are drawn from standard HDPE 6094-class documentation and should be verified against the producer’s current certificate of analysis; published data for this specific configuration is limited because coal-derived ethylene can vary in comonomer distribution, residual catalyst content, and additive package stability.
Industrial applications are concentrated in 20 L to 200 L extrusion blow molded containers, automotive fluid reservoirs, intermediate bulk container liners, and thick-section industrial packaging where high-flow HDPE cannot maintain parison or melt integrity. The following sections define the material’s boundaries against injection-molding, pipe, and film grades, and the processing conditions that affect surface finish, environmental stress-crack resistance, and layer stability.
The primary difference is melt viscosity. A melt flow rate of 0.9 g/10 min places 6094 in a high-molecular-weight class relative to injection-molding HDPE grades with 20 g/10 min or higher at 190 °C/2.16 kg. In multicavity thin-wall molds with wall sections below 2 mm and flow-length-to-thickness ratios above 120:1, the higher viscosity increases injection pressure and cycle time. The material is therefore not a suitable drop-in for high-flow thin-wall packaging, closures, or disposable food containers. However, the same viscosity supports parison wall uniformity in extrusion blow molding and reduces draw-down on vertical tooling. If melt temperature exceeds 240 °C for prolonged residence, oxidative chain scission can reduce average molecular weight and lower environmental stress-crack resistance, thereby erasing the primary processing advantage of 6094 over high-flow grades.
Product-class data for this melt-flow bracket indicate die swell in accumulator-head processing of 25–35% at shear rates typical for large-part extrusion. Actual die swell must be measured on the production line because die geometry, melt temperature, and regrind content all modify parison diameter growth. A flow-analysis simulation using capillary viscosity data under ISO 11443:2021 from the actual lot should be used for tooling design; single-point melt flow rate measurements do not quantify die swell or extensional hardening.
| Property | HDPE 6094 class | High-flow injection HDPE | PE100 pipe HDPE | Test method |
|---|---|---|---|---|
| Melt flow rate at 190 °C/2.16 kg | 0.9 g/10 min | 20–50 g/10 min | 0.2–0.4 g/10 min | ASTM D1238-23 / ISO 1133-1:2022 |
| Density | 0.949 g/cm³ | 0.952–0.960 g/cm³ | 0.950–0.959 g/cm³ | ASTM D1505-18 / ISO 1183-1:2019 |
| Tensile yield strength | ≥21 MPa | ≥24 MPa | ≥21 MPa | ASTM D638-14 / ISO 527-2:2012 |
| Elongation at break | ≥600% | ≥200% | ≥600% | ASTM D638-14 / ISO 527-2:2012 |
| Application boundary | Extrusion blow molded containers | Thin-wall packaging, caps | Pressure pipe | — |
These are class-level values and do not constitute a substitution matrix. PE100 pipe grades are bimodal resins engineered for slow crack growth under sustained hydrostatic stress; HDPE 6094 should not be used as a pipe-grade substitute without hydrostatic testing under ISO 9080 or ASTM D2837-22. Similarly, the low melt flow rate of 6094 is not an advantage in injection molds with high-shear gates and runners below 1 mm.
Container drop impact is not controlled by tensile yield alone. For blow molded industrial containers, drop testing at -20 °C must be performed on the actual part. A resin with elongation at break above 600% at 23 °C may still exhibit brittle fracture at the pinch-off seam if the tooling produces an excessively thick weld. Fabrication should therefore be qualified by ASTM D2463-15 drop impact and, for stacked containers, by column crush testing at the maximum intended stacking height.
Accumulator-head blow molding of HDPE 6094 generally uses single-screw extruders with 24:1 to 30:1 length-to-diameter ratios. Grooved feed sections improve solids conveying above 50 kg/h. Melt temperature measured at the die should be maintained between 180 °C and 210 °C, with die head zones between 185 °C and 200 °C. Mold cooling water is normally controlled at 10–25 °C. Lower mold temperatures reduce post-demold warpage in flat panels but can increase surface haze and reduce pinch-off weld strength at container seams.
Pre-drying is required when storage relative humidity exceeds 60% or when regrind shows condensed moisture. Standard practice for this density and molecular weight class is desiccant drying for 2 hours at 80 °C with a dew point below -30 °C. Without drying, moisture can volatilize at the die land and produce splay or blow-pin sticking. In intermittent extrusion, parison sag should be evaluated at production cycle time. For a parison length-to-diameter ratio above 4:1, sag of 10–15% over 1.5 s is typical for this melt-strength class; sag above 20% should be corrected by lowering die head temperature in 5 °C increments rather than adding external lubricant, which can alter heat sealing and contaminate mold surfaces.
Residence time in the accumulator should be limited. At 210 °C melt temperature, average residence time should remain below 8 min; at 200 °C, below 12 min. Extended hold times increase oxidation probability and may produce yellowing or surface gels. If injection molding is attempted in thick sections above 5 mm, published data for this specific configuration is limited. Tools should use generous gates and runners, and hot-runner residence time should remain below 10 min at 210 °C to reduce molecular-weight loss.
Regrind ratio above 20 wt% may shift melt flow rate upward if the regrind has experienced repeated heat history. Each pass through an accumulator-head extruder at 210 °C can promote molecular-weight degradation, especially if the regrind stream contains fine dust or label fragments. The regrind feed should be metered gravimetrically to avoid melt surge and parison length variation.
Color concentrates used with 6094 should employ a polyethylene carrier and should be dried to the same dew point as the base resin. Inorganic pigments above 2–3 wt% can raise density and reduce impact; organic pigments may shift low-shear viscosity. The final blended compound should be recharacterized for melt flow rate and tensile yield after color addition, because automotive and industrial container specifications commonly require lot-to-lot appearance control.
In multi-layer blow molding, HDPE 6094 can serve as a core or outer layer. If an EVOH or polyamide barrier layer is used, the tie layer must be selected for viscosity compatibility with the HDPE layer; otherwise layer thickness oscillation can appear at throughput ratios above 4:1. Avoid compounding with amine-based antistatic packages, because extended hold times above 210 °C may produce yellowing and reduce environmental stress-crack resistance. For outdoor service, unpigmented 6094 will undergo surface microcracking and chalking unless compounded with carbon black at 2–3 wt% or a hindered amine light stabilizer system. Accelerated weathering can be screened using ASTM G154-23; outdoor failure modes should be confirmed by natural exposure.
Storage should be below 40 °C in a dry environment away from direct sunlight to protect the stabilization package. Regrind from post-industrial blow molding scrap may be added up to 20 wt% when clean, dry, and of identical grade. Post-consumer recyclate is not automatically suitable for food-contact layers unless the recycling process has a favorable opinion under EU 2022/1616 or FDA.
Food-contact use is not conferred by the pellet specification alone. As an olefin polymer, HDPE 6094 may be evaluated against FDA 21 CFR 177.1520(c) 1.1, which covers polyolefin homopolymers and copolymers with density not less than 0.94 g/cm³ and specified extractable fraction limits. EU market articles require end-article testing under EU 10/2011; the overall migration limit is 10 mg/dm² for plastic materials and articles. In China, GB 4806.6-2016 regulates food-contact polyethylene and includes migration and sensory requirements.
| Reference | Scope | Numerical condition or limit |
|---|---|---|
| FDA 21 CFR 177.1520(c) 1.1 | Olefin polymers for food contact | Density not less than 0.94 g/cm³; extractables per clause |
| EU 10/2011 | Plastic food-contact materials | Overall migration ≤ 10 mg/dm² |
| GB 4806.6-2016 | Food-contact polyethylene | Migration and sensory requirements per standard |
| REACH 1907/2006 | SVHC declaration | 0.1 wt% threshold per article |
| RoHS 2011/65/EU | Homogeneous material heavy metals | Lead 1000 mg/kg; cadmium 100 mg/kg |
Environmental stress-crack resistance in 6094 is generally quantified by ASTM D1693-15e1 condition B, but the test is a bent-strip method and does not replicate all molded-in stresses. Service testing in the intended filled liquid is required for agricultural chemicals, surfactant-based cleaners, and ethanol blends above 10 vol%. Early failure below 300 h may indicate unsuitability for polar organic liquids above 50 °C. Long-term creep under load should be measured by ISO 899-1:2017 when service temperature exceeds 40 °C. No compatibility claim is made here for strong oxidizers, aromatic hydrocarbons, or chlorinated solvents; filled-liquid exposure must be tested on the final part under ASTM D543-21 or equivalent immersion protocols at the maximum service temperature.