Yanchang China Coal Yulin Shaanxi Hdpe 5502

Yanchang China Coal Yulin (Shaanxi) HDPE 5502

    • Product Name: Yanchang China Coal Yulin (Shaanxi) HDPE 5502
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 445690
    Density 0.954 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.20 g/10 min
    Tensile Yield Strength 26 MPa
    Elongation At Break >500%
    Flexural Modulus 1100 MPa
    Vicat Softening Temperature 125 °C
    Brittleness Temperature < -70 °C
    Environmental Stress Cracking Resistance >1000 h
    Hardness 65 Shore D
    Melting Point 130-135 °C
    Crystallinity 70-80%
    Water Absorption <0.01%
    Form Pellets
    Color Natural
    Chemical Resistance Good against acids, bases, and salts; poor against strong oxidizing agents and some hydrocarbons

    As an accredited Yanchang China Coal Yulin (Shaanxi) HDPE 5502 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Yanchang China Coal Yulin (Shaanxi) HDPE 5502 is packaged in 25 kg PP woven bags with PE liners, palletized for transport.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Yanchang China Coal Yulin (Shaanxi) HDPE 5502, palletized bags, securely stuffed into 20-foot container and sealed.
    Shipping Yanchang China Coal Yulin (Shaanxi) HDPE 5502 ships as a non-hazardous polymer in 25 kg PP woven bags or 1000 kg jumbo bags, palletized and stretch-wrapped. It is loaded into 20-foot FCL containers, kept dry and ventilated, and protected from moisture, sunlight, and contamination. No UN hazard class applies.
    Storage Store Yanchang China Coal Yulin (Shaanxi) HDPE 5502 in a cool, dry, well-ventilated warehouse. Keep original bags or containers sealed, palletized, off the floor, and away from direct sunlight, heat, flames, and strong oxidizers. Avoid moisture, contamination, physical damage, and excessive stacking. Maintain ambient temperature, good housekeeping, and first-in, first-out rotation. Follow the SDS and local regulations.
    Shelf Life Stable for at least 24 months under proper storage conditions; protect from heat, moisture, and UV light in sealed packaging.
    Application of Yanchang China Coal Yulin (Shaanxi) HDPE 5502

    In monolayer extrusion blow molding for pasteurized milk, aseptic juice, edible oil and condiment containers, Yanchang China Coal Yulin HDPE 5502 is specified when the closure finish must resist splitting, the pinch-off weld must survive drop loads, and the resin must generate minimal taste and odour transfer. Regulatory conformity is established under FDA 21 CFR 177.1520 for olefin polymers, EU Regulation (EU) No 10/2011 with its overall migration limit of 10 mg/dm², and GB 4806.6-2016 for food-contact polyolefin articles; additives are selected against GB 9685 authorisation lists. The grade is positioned in the blow molding viscosity window with a melt flow rate of 0.30–0.40 g/10 min under ASTM D1238-20 at 190°C and 2.16 kg, and density in the 0.954–0.958 g/cm³ band under ASTM D1505-18. The addition ratio for direct food contact is 97.0–99.5 wt% HDPE 5502, 0.5–2.0 wt% titanium dioxide white masterbatch, and 0.02–0.05 wt% processing aid. Slip agents are not added as a default because they can contribute to taste and odour transfer; if closure torque control requires surface lubricity, erucamide is limited to ≤0.10 wt% and the finished article is re-tested for organoleptic neutrality and migration. Post-consumer recyclate is not used in EU food-contact monolayer structures because source-consistent migration validation under EU No 10/2011 is not available for this configuration.

    The downstream process on continuous shuttle or rotary-wheel extrusion blow molding lines uses barrier screws with L/D 25:1–30:1, feed-throat cooling, and a melt temperature of 180–205°C; die-head temperature is held at 190–205°C to prevent melt fracture on small-bottle parisons. Blow air at 0.6–0.8 MPa expands the parison into moulds maintained at 10–20°C, with the die gap adjusted from 1.2–1.8 mm for a 1 L bottle and the flash pocket trimmed to leave no pinch-off stringing. HDPE 5502 does not require hygroscopic drying when the resin is stored in closed packaging; if exposed to ambient relative humidity above 80%, superficial pellet condensation is removed by forced-air drying at 80°C for 1–2 h before extrusion. The terminal products are 200 mL–5 L mono-layer bottles for fresh milk, juices, edible oils, vinegar, and liquid condiments; the grade is not recommended for hot-fill processing above 70°C or for oxygen-sensitive products requiring high gas barrier.

    When the Same Parison Enters a UN-Certified Industrial Chemical Jerrycan

    The controlling failure mechanism changes from migration and organoleptic stability to environmental stress crack resistance at the pinch-off weld and along the handle root when HDPE 5502 is converted into detergent, hypochlorite, water-treatment and industrial cleaner jerrycans. Compliance in this segment follows the UN Model Regulations Chapter 6.1 for dangerous goods packagings, ADR/RID and IMDG Code transport provisions, and, for general industrial chemicals, REACH Annex XVII restrictions on substances in packaging. The packaging certificate for a plastic jerrican is issued under code 3H1; qualification requires drop testing at -18°C after conditioning, leakproofness at 30 kPa internal air pressure, hydraulic proof pressure, and stack compression after filling. HDPE 5502 is retained at 95.0–98.0 wt%, with colourant or carbon black masterbatch at 1.0–3.0 wt% and antioxidant stabiliser at 0.05–0.15 wt%. Regrind from edge trim and rejected bottles is allowed up to 10–15 wt%; above this range ESCR results under ASTM D1693-21 Condition B become formulation-dependent, and drop-weight failures at the weld often increase because lower melt strength produces uneven weld thickness.

    Extrusion blow molding for this class uses an accumulator-head machine with screw diameter 60–90 mm and L/D 25:1–30:1. The accumulator delivers a heavy parison at 180–210°C melt temperature; parison programming is essential because the handle cut-out creates a path for non-uniform wall thinning, and the die gap is stepped from 1.5–2.5 mm at the body to 1.0–1.6 mm at the base weld. Mould clamping force is matched to the projected area of the jerrican, typically requiring 15–35 t for a 10 L container, and blow air pressure is held at 0.7–1.0 MPa. The main operational boundary is chemical compatibility: aggressive aromatic solvents, ketones, and chlorinated hydrocarbons should not be packed without barrier treatment because HDPE 5502 lacks the permeation resistance for these classes; published data for this specific configuration under solvent load is limited, and pack compatibility must be confirmed by weight-loss and panel deformation testing over 30 days at 40°C. Terminal products are 5–20 L UN-certified jerrycans for detergents, industrial cleaners, photographic chemicals, and water treatment formulations, where the closure system is matched to the UN gasket and torque-retention requirements of the hazardous goods certificate.

    Application segmentPrimary regulatory frameworkSupporting standard / methodArticle-specific limit or endpoint
    Food-contact bottlesFDA 21 CFR 177.1520; EU No 10/2011; GB 4806.6-2016ASTM D1238-20; ASTM D1505-18Overall migration ≤10 mg/dm²; organoleptic neutrality
    Pharma bottlesUSP <661.1>; Ph. Eur. 3.1.3; ICH Q3DUSP <671>; pharmacopoeial extractables profilingHeavy metals, non-volatile residue, pH shift within monograph limits
    Industrial jerrycansUN Model Regs Chapter 6.1; ADR/RID/IMDG; REACHASTM D1693-21 Condition B; drop test -18°CPackage code 3H1; no weld failure under drop/stack
    Cosmetic bottlesEC 1223/2009; REACH Annex XVII; California Prop 65Migration/interaction testing with fragrance, ethanol, surfactantsNo substance transfer altering cosmetic formulation quality
    Agrochemical/lubricant containersUN Model Regs Chapter 6.1; 49 CFR; REACH; FAO/WHO pesticide packaging guidelinesDrop test -18°C; permeation weight-loss 30 days/40°CWeight loss and paneling within product-specific tolerance

    Where the specification shifts from food migration limits to pharmacopoeial extractables, HDPE 5502 is converted on single-station shuttle machines into high-density polyethylene bottles for tablet and capsule packaging. Material compliance is assessed through USP <661.1> plastic packaging system tests and Ph. Eur. 3.1.3 polyolefin monographs, with elemental impurity data generated under ICH Q3D risk assessment if the finished container is supplied to pharmaceutical licence holders. The bottle must pass extractables profiling for UV absorbance, pH shift, turbidity, residue on ignition, non-volatile residue, and specific heavy metal limits; the resin itself is supplied on the understanding that the drug-contact layer is monolayer and the final article is validated per drug product stability protocol. The formulation ratio is 97.0–99.0 wt% HDPE 5502, 1.0–2.0 wt% titanium dioxide white masterbatch for opacity, and an antioxidant package at 0.05–0.10 wt%. Antistatic additives are normally excluded unless a specific dust-control requirement is demonstrated; any additive is restricted to pharmaceutical masterbatch grades with full extractables data. Regrind in this segment is limited to 0–10 wt%, and only first-generation internal scrap from the same production campaign is used to avoid contamination of the extractables profile.

    The conversion process uses extrusion blow molding with closed-loop parison thickness control, melt temperature 180–200°C, and mould temperature 10–15°C to stabilise wall thickness at 0.3–0.8 mm. After de-flashing, bottles are passed through leak detection and dimension inspection; the pinch-off area is trimmed to avoid particulate release into the drug product. HDPE 5502 provides moderate moisture vapour transmission resistance and is acceptable for oral solid dose products only when the stability protocol confirms no moisture-sensitive degradation; USP <671> container performance testing is used to determine whether the bottle meets the required moisture vapour transmission level for the specific drug formulation. Terminal products are 30–500 mL HDPE tablet and capsule bottles with continuous thread or child-resistant closure finishes for prescription and over-the-counter oral solid dose packaging.

    How Does Surface Replication in Cosmetic Bottle Tooling Alter the Processing Window?

    The processing challenge in personal care packaging is not mechanical strength alone but the need to force a semi-molten parison into fine engraved tooling and replicate textured or matte surfaces before freeze-off. Cosmetic containers made from HDPE 5502 are placed on the EU market under Regulation (EC) No 1223/2009 packaging safety principles, with REACH Annex XVII restrictions for phthalates, colourants and heavy metals; brand owners additionally require low odour and no interaction with fragrance, ethanol, or surfactant systems. The formulation ratio for custom-colour bottles is 94.0–98.0 wt% HDPE 5502, 2.0–6.0 wt% pigment masterbatch, 0.05–0.10 wt% slip additive, and 0.10–0.20 wt% UV stabiliser for light-sensitive shades. High pigment loading above 4.0 wt% increases melt viscosity variation and can reduce parison elongation, so the die gap is widened by 0.2–0.5 mm to compensate for lower draw-down and to maintain weld thickness at the base.

    Tooling in this segment uses polished or laser-textured cavities; mould temperature is set at 5–15°C to accelerate surface setting on shallow relief textures, but excessive cooling below 5°C can produce flow lines and frost zones that are unacceptable in premium packaging. Melt temperature is maintained at 190–210°C, blow air at 0.6–0.8 MPa, and extrusion screw speed is limited to prevent parison sharkskin. Parison swell in this grade is assigned a practical operating range of 20–40% depending on tooling diameter and output; the head tooling is sized so the blown diameter-to-die diameter ratio does not exceed 3:1, above which wall thinning around the pinch-off becomes difficult to correct. Terminal products are 50–750 mL monolayer HDPE bottles for shampoo, conditioner, body wash, lotion and cosmetic toners, with closure finishes that require consistent top-load sealing geometry rather than barrier performance.

    SegmentHDPE 5502 addition (wt%)Colorant/opacifier (wt%)Functional additives (wt%)Regrind/PCR ceiling (wt%)
    Food-contact bottles97.0–99.50.5–2.0 TiO₂Processing aid 0.02–0.05; slip ≤0.10No PCR in EU monolayer
    Industrial jerrycans95.0–98.01.0–3.0Antioxidant 0.05–0.1510–15
    Pharma bottles97.0–99.01.0–2.0 TiO₂Antioxidant 0.05–0.100–10 internal regrind
    Cosmetic bottles94.0–98.02.0–6.0Slip 0.05–0.10; UV 0.10–0.200–20 depending surface spec
    Agrochemical/lubricant containers96.0–99.01.0–2.0 carbon blackAntioxidant 0.10–0.20≤10

    Because agrochemical concentrates and automotive lubricants frequently contain ester-based carriers, surfactant co-formulants, or mild aromatic fractions, the pack is evaluated primarily for environmental stress crack resistance, cap-seal compatibility, and permeation weight loss. HDPE 5502 is used in this segment at 96.0–99.0 wt%, with carbon black or pigment masterbatch at 1.0–2.0 wt% and antioxidant stabiliser at 0.10–0.20 wt%. The addition ratio excludes plasticizers and ESCR-enhancing additives because no additive reliably compensates for molecular weight loss and weld thinning under sustained stress; regrind is held at ≤10 wt% and its particle size is controlled to 0.5–3.0 mm to minimise gels and unmelted domains. Compliance follows UN Model Regulations Chapter 6.1 packaging certification for dangerous goods, ADR/RID and 49 CFR transport provisions, and REACH Annex XVII where applicable to the packaged formulation. For agrochemical packaging, additional national registration requirements often require FAO/WHO pesticide container guidelines, cap torque retention, and permeation data under tropical storage conditions.

    The process is extrusion blow molding with parison accumulator, melt temperature 180–205°C, and die-head pressure control to maintain uniform wall thickness around the handle of a 5 L or 20 L container. Post-moulding, the containers are subjected to drop tests at -18°C and leak tests at 30 kPa internal air pressure, with a subset subjected to weight-loss testing after filling with the actual formulation for 30 days at 40°C to detect paneling and permeation. For high-volatility or oxygen-sensitive agrochemicals, in-line fluorination of the inner surface is applied after moulding; the fluorinated layer is thin, alters surface energy, and must be re-qualified for cap seal and label adhesion. HDPE 5502 should not be used with aromatic solvent-based formulations above the level established by compatibility testing, nor with chlorinated solvents, because these penetrate and soften the monolayer wall. Terminal products are 1 L–20 L containers for automotive lubricants, agrochemical diluents, fertigation chemicals, and maintenance fluids, where the cap-gasket system and the container both belong to the same transport certification application.

    Free Quote

    Competitive Yanchang China Coal Yulin (Shaanxi) HDPE 5502 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Shaanxi Yanchang China Coal Yulin Energy & Chemical Co., Ltd. supplies the high-density polyethylene grade designated Yanchang China Coal Yulin (Shaanxi) HDPE 5502 as a high-molecular-weight, low-melt-mass-flow extrusion resin intended for blow moulded industrial containers, thick sheet, and large-surface-area profiles. The product is classed in the 0.30–0.40 g/10 min melt mass-flow rate band at 190°C under 2.16 kg, with a density of 0.954–0.956 g/cm³. The relevant test methods are ISO 1133-1:2022 and ISO 1183-1:2019. The resin originates from a coal-to-olefins production route at the Yulin complex; published comonomer identity is limited, but the density suppression relative to an ethylene homopolymer indicates short-chain branching from an α-olefin comonomer. Exact polyethylene molecular weight distribution is not stated in available trade literature.

    Capillary rheometry on a laboratory twin-bore rheometer at 190°C typically shows shear viscosity from 2,000 Pa·s at 100 s⁻¹ to 300 Pa·s at 1,000 s⁻¹ for this general class; exact values for the subject grade are not published. Melt strength measured by a Rosand or Rheotens unit is not specified, but the low melt mass-flow rate corresponds to high sag resistance. Lot-to-lot variation in melt mass-flow rate should be controlled within ±0.04 g/10 min to avoid process drift on accumulator blow moulders; wider variation can shift parison length and wall thickness distribution.

    Why Does the 0.35 g/10 min Melt Flow Rate Constrain Extruder Barrel Temperature Selection and Accumulator Head Fill?

    A melt mass-flow rate of 0.35 g/10 min at 190°C and 2.16 kg indicates high melt viscosity. On a 90 mm single-screw extruder with 30:1 L/D, screw speed required to fill an 8 kg accumulator head may raise melt temperature to 205–215°C from viscous dissipation alone. Barrel set points are therefore programmed with a reverse or flat profile, for example 180°C feed, 200°C compression, 195°C metering, and 200°C head, to limit oxidative chain scission. The screw should use a barrier flight design with a compression ratio of 2.5:1 to 3.2:1; lower compression reduces shear heating but may leave unmelted cores in thick sections.

    Accumulator head fill pressure is a more sensitive control than extruder discharge pressure. With a 0.35 g/10 min melt, head fill pressure can exceed 20 MPa at narrow tooling gaps; die gaps below 1.5 mm may produce melt fracture and sharkskin unless die land temperatures are raised 10–15°C above the head set point. Existing tooling sized for 0.85–1.2 g/10 min blow moulding grades may require widening of the die pin gap by 0.3–0.8 mm to avoid excessive backpressure and delayed shot fill.

    On production-scale accumulator blow moulders with 30:1 L/D single-flighted barrier screws, the resin is processed with clamp force settings from 400 to 1,200 kN for containers up to 30 L, depending on mould projected area and pinch weld geometry. Blow pressure is typically 0.6–0.8 MPa; insufficient blow pressure causes incomplete part definition at the pinch-off, while excessive pressure increases flash generation and mould parting line wear. Parison programming should use diverging die gaps, for example 0.8 mm at the die land to 1.6 mm at the exit, on accumulator heads with shot capacities between 20 and 60 kg to compensate for sag-induced wall thinning. Die swell for this high-molecular-weight class is typically 30–50%; tooling cut is therefore 10–20% smaller than the mould cavity diameter, with exact dimensions derived from spiral mandrel shear history.

    For sheet extrusion, gear-pump-assisted lines set the pump inlet pressure at 5–10 MPa to avoid cavitation, with screen packs of 40/60/80 mesh. Melt temperature at the flat die is typically 210–230°C, and chill roll temperatures of 70–85°C are used to balance frozen-in stress and surface gloss. Thicker sheet above 4 mm requires lower chill roll temperatures or longer cooling tunnels to prevent centreline voids, particularly when regrind content exceeds 20 wt%.

    Density, Tensile Yield, and Environmental Stress Crack Resistance in Heavy-Walled Container Stock

    At 0.955 g/cm³, the resin balances stiffness and environmental stress crack resistance. Typical property class values are tensile stress at yield of 27–30 MPa tested at 50 mm/min under ISO 527-2:2012 or ASTM D638, flexural modulus of 1,150–1,350 MPa under ISO 178:2019 at 2 mm/min, and elongation at break exceeding 500%. Vicat softening temperature by the A50 method is generally 124–128°C under ISO 306:2022.

    Environmental stress crack resistance is the controlling property for surfactant and detergent packaging. Thick-walled 5502 containers are tested under ASTM D1693 Condition B (100% Igepal CO-630) or ASTM D2561 for moulded bottle stress cracking. Published data for this specific grade are limited; the resin class typically exhibits F50 values above 40 h for moulded articles, but converters should request lot-specific ESCR certificates for aggressive surfactant systems. The property is influenced by comonomer distribution and moulded-in stress, not by density alone. Weld lines created by multi-cavity tooling reduce ESCR by a factor that cannot be predicted from pellet data.

    When 5502 Is Positioned Against Injection and Pipe-Grade HDPE Resins

    Compared with a high-flow injection moulding HDPE with a melt mass-flow rate of 8 g/10 min and density 0.964 g/cm³, HDPE 5502 requires longer shot fill and higher moulded-in orientation but provides better ESCR and lower notch sensitivity in thick sections. It is not a substitute for a PE 100 pressure pipe grade: the hydrostatic stress classification and slow crack growth resistance required by ISO 12162 are not claimed for this grade, and it is not intended for pressurised water or gas distribution networks. Compared with a thin-wall film HDPE of 1.0 g/10 min, the 5502 melt mass-flow rate permits longer parison hang time and lower draw-down before mould closing.

    Injection moulding of HDPE 5502 is generally limited to thick-walled structural parts with sprue and runner diameters of at least 3 mm; thin-wall caps and closures require flow lengths that exceed the resin’s apparent viscosity at practical injection pressures. Moulders should not select this grade for parts with section thickness below 1.2 mm unless flow simulation is supported by high-injection-pressure equipment above 150 MPa. Rotational moulding is also not an appropriate process because pellet stabilisation and particle size distribution are not optimised for long oven residence times.

    Comparative property and application matrix for HDPE 5502 and adjacent high-density polyethylene grades
    ParameterHDPE 5502Injection HDPEPE 100 pipe HDPE
    Melt mass-flow rate (ISO 1133-1:2022)0.30–0.40 g/10 min7–9 g/10 min0.22–0.30 g/10 min
    Density (ISO 1183-1:2019)0.954–0.956 g/cm³0.963–0.965 g/cm³0.958–0.961 g/cm³
    Tensile stress at yield (ISO 527-2:2012)27–30 MPa28–32 MPa25–28 MPa
    ESCR (ASTM D1693)Moderate class typical (F50 >40 h)Low class typical (F50 <5 h)High class typical (F50 >500 h)
    Primary applicationBlow moulding, sheet, thick profilesCaps, crates, thin-wall containersPressurised water and gas pipe

    The designation 5502 is used by multiple producers; direct substitution between HDPE 5502 grades from different manufacturers is not automatic. Stabiliser package, catalyst residue, molecular weight distribution, and pellet handling affect melt fracture onset, colour, odour, and organoleptic performance. A changeover to Yanchang China Coal Yulin HDPE 5502 from an incumbent 5502 should include full lot-to-lot capillary rheometry comparison at shear rates from 10 s⁻¹ to 1,000 s⁻¹, plus bottle drop and ESCR trials. Chevron Phillips Marlex HHM 5502BN and Ineos Rigidex HD5502 occupy the same nominal melt flow/density class; however, processing stabilisers and molecular architecture differ by production technology. Users should not assume identical die swell, melt fracture onset, or additive acceptability.

    Regulatory conformity is determined by additive package and article end use

    Food-contact status is not automatic. Olefin polymers may be cleared under FDA 21 CFR 177.1520 for article-specific end uses, provided extractives remain within the regulation’s limits. EU food-contact compliance is evaluated under Regulation (EU) No 10/2011 and its amendments; no specific migration limit can be assumed without finished-article testing. The resin manufacturer’s certificate of composition should be requested for each lot, because pellet-level purity does not guarantee compliance after colour concentrates, regrind, or processing aids are introduced. REACH registration under EC No 1907/2006 and RoHS Directive 2011/65/EU heavy metal limits are normally addressed at chemical substance and article levels, respectively.

    Compliance verification matrix for HDPE 5502 converting operations
    Regulation or standardScopeTypical verification activity
    FDA 21 CFR 177.1520Olefin polymers for food contactFinished-article extractive testing; end-use limitation review
    Regulation (EU) No 10/2011Plastics intended for food contact in the EUSpecific migration testing on finished article
    REACH EC No 1907/2006Registration, evaluation, authorisation of chemical substancesConfirm registration dossier includes the grade and import volume
    RoHS Directive 2011/65/EURestricted substances in electrical and electronic equipmentHeavy metal screening if used in EEE components
    ISO 1133-1:2022Melt mass-flow rateLot release and incoming inspection
    ASTM D1693Environmental stress crack resistanceQualification for surfactant-containing service

    Storage should prevent condensation when pellets are transferred from unheated silos to warm packaging halls above 60% relative humidity. Although polyethylene is non-hydroscopic, surface moisture causes splay and weld-line porosity. The grade should not be blended with polypropylene, PET, or EVOH without a dedicated tie layer; incompatible regrind domains reduce weld-line strength and surface quality. Outdoor articles require an effective UV stabiliser package; the natural grade is not UV-stabilised unless specified. Processing with melt temperature above 240°C can generate odour, yellowing, and reduced ESCR through chain scission, especially when regrind residence time is extended.

    Lot release documentation should include melt mass-flow rate, density, tensile stress at yield, and ash content. If the application requires organoleptic performance, separate odour and taste tests on the finished article are required because pellet-level odour data do not capture the effect of melt history and additive degradation products.

    Top