| HS Code | 286994 |
| Productname | Yanchang China Coal Yulin (Shaanxi) HDPE 43049 |
| Manufacturer | Yanchang China Coal Yulin (Shaanxi) Energy and Chemical Co., Ltd. |
| Polymertype | High Density Polyethylene (HDPE) |
| Grade | 43049 |
| Form | Pellets |
| Density | 0.949 g/cm³ |
| Meltflowrate | 4.0 g/10 min at 190°C/2.16 kg |
| Meltingpoint | 130-135 °C |
| Vicatsofteningtemperature | 120-125 °C |
| Tensileyieldstrength | 26 MPa |
| Elongationatbreak | ≥600% |
| Flexuralmodulus | 1100 MPa |
| Notchedizodimpactstrength | 20 kJ/m² |
| Hardnessshored | 60-65 |
| Waterabsorption | <0.01% |
| Volumeresistivity | >10^16 Ω·cm |
| Dielectricconstant | 2.3 |
| Thermalconductivity | 0.4 W/(m·K) |
| Crystallinity | 70-80% |
| Thermalexpansion | 1.2E-4 /°C |
As an accredited Yanchang China Coal Yulin (Shaanxi) HDPE 43049 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Yanchang China Coal Yulin (Shaanxi) HDPE 43049 is supplied in 25 kg woven bags, with 1,000 kg per palletized load. |
| Container Loading (20′ FCL) | Full 20-foot FCL container loading of Yanchang China Coal Yulin (Shaanxi) HDPE 43049 grade, securely packed for ocean shipment. |
| Shipping | Yanchang China Coal Yulin (Shaanxi) HDPE 43049 ships from Yulin, Shaanxi, China, in 25 kg bags or 1,000 kg jumbo bags, palletized and stretch-wrapped. As a non-hazardous polymer, it moves by truck to port, then sea freight in 20'/40' FCL or LCL containers. Store dry and ventilated. |
| Storage | Store Yanchang China Coal Yulin (Shaanxi) HDPE 43049 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags sealed, clean, palletized, and off the floor. Prevent moisture, dust, and UV exposure. Observe safe stacking limits and first-in, first-out stock rotation. Do not store near food, feed, or incompatible materials. |
| Shelf Life | Recommended use within 24 months when stored in original, unopened packaging under dry, cool, ventilated conditions away from direct sunlight. |
High-speed thin-wall injection lines processing Yanchang China Coal Yulin HDPE 43049 into dairy cups, portion packs, and food-service containers operate most stably when nozzle melt temperature is held within 210 °C to 235 °C, mould surface temperature is controlled at 15 °C to 35 °C, and injection velocity is set to deliver a screw forward time below 0.35 s for wall stocks of 0.6 mm to 0.9 mm. The nominal melt mass-flow rate of 4.0 g/10 min under ISO 1133-1:2022 and the nominal density of 0.949 g/cm³ under ISO 1183-1:2019 place the grade in a viscosity window that is high enough to retain melt cushion stability but low enough to fill multi-cavity thin sections when gate geometry is correct. Tools above 32 cavities require balanced hot-runner manifolds with melt-channel temperature not exceeding 240 °C, because higher temperatures promote oxidative gel formation at the gate land and produce surface streaks. Gate diameter at the part should be no less than 0.8 mm for side-wall entry into a dairy cup, with a land length of 0.5 mm to 1.0 mm, and edge gates should feed into the rim rather than the base to prevent jetting across the bottom. Cycle times for a 200 ml cup generally remain between 6 s and 10 s when cooling water enters the mould at 8 °C to 12 °C and the part is ejected with a mould-open stroke set to clear the stack height. Dimensional acceptance data are meaningful only after 24 h conditioning at 23 °C and 50% RH, because post-mould secondary crystallization shrinks the part by a geometry-dependent amount and stabilizes the rim ovality. Food-contact compliance for EU destinations is governed by EU No 10/2011; migration testing under the EN 1186-series must demonstrate an overall migration not exceeding 10 mg/dm² or 60 mg/kg in the assigned food simulant. For U.S. distribution, 21 CFR 177.1520 covers olefin polymer repeat-use and single-use articles, provided the final lot certificate confirms the density is within the specified olefin polymer range and the finished article passes extraction tests under the relevant simulant. For China domestic food-contact articles, GB 4806.7 applies to plastic materials and articles, and migration testing must follow the prescribed simulant and time-temperature conditions for the intended use. Warpage control in thin-wall food packaging is quantified by rim ovality: a 75 mm diameter cup should maintain ovality no greater than 0.5 mm after conditioning, otherwise the filling line sealing head may lose contact pressure and cause leakers. Because HDPE 43049 may be supplied without intentional slip agents unless confirmed in the lot documentation, processors often add a low loading of a food-grade erucamide slip masterbatch; any additive carrier or active substance must be listed in EU No 10/2011 Annex I or cleared under the applicable U.S. or China food-contact regulation.
Closure moulding with HDPE 43049 on 48- to 64-cavity tools imposes a narrower thermal window than thin-wall packaging because thread definition and tamper-evident band formation are both sensitive to low-viscosity deviations. Nozzle melt temperature should be set between 215 °C and 230 °C; below 215 °C, the thread crests may not fully pack out, while above 230 °C the melt tends to enter vent channels and form flash at the bridge tears. Hot-runner systems with valve-gated tips reduce stringing and allow the use of a mould surface temperature of 10 °C to 25 °C, which is necessary for high-speed unscrewing cycles. The tamper-evident band bridges should have a nominal thickness of 0.30 mm to 0.45 mm and a tear-slit land length no more than 0.4 mm, because longer slit lands produce high demoulding force and partial band fusion. Unscrewing tooling requires core rotation time to be integrated with the cooling timer; when wall stock at the closure side is 1.0 mm to 1.5 mm, cooling time typically ranges from 4 s to 7 s. Application and removal torque should be measured according to ASTM D3198 or ASTM D2063, with acceptance limits tied to the bottle finish specification and capping machine head configuration. For pharmaceutical closures, the final article must also comply with USP 661.1 plastic packaging tests for physicochemical properties, and for food closures the relevant EU No 10/2011, 21 CFR 177.1520, or GB 4806.7 conditions apply. A critical failure mode on high-cavitation lines is nozzle drool at hot-runner shut-off, which is suppressed by a positive shut-off nozzle and a decompression distance not exceeding 3 mm to 5 mm; excessive decompression draws air into the melt stream and produces splay. The grade should not be blended with polypropylene regrind or barrier regrind without segregation, because PP contamination reduces creep resistance and causes inconsistent torque retention.
Unlike thin-wall food packaging, industrial crates, logistics trays, and pallets require a cold-wall processing strategy in which mould surface temperature is intentionally held below 30 °C to accelerate skin solidification and reduce cycle time. For nominal wall sections of 3 mm to 6 mm, melt temperature at the nozzle is set from 220 °C to 250 °C, and injection speed is profiled so that the melt front advances at a moderate velocity through thick ribs without jetting; the velocity profile is often run as 50% rapid fill to 65% volume, followed by a slow fill to 95% and a short high-pressure pack. Packing pressure should be maintained at 60% to 80% of peak injection pressure for 4 s to 8 s, or until the gate freeze-off time is confirmed by cycle-based weighing stability within 0.2% part weight variation. Sink marks at rib roots opposite gas channels or handle webs should be controlled to a depth no greater than 0.05 mm, measured with a profilometer or optical comparator, because deeper sinks reduce flatness and concentrate stack load. Stackability of open-top crates is governed by rib orientation and draft angle rather than resin density alone; draft angles below 0.5° on deep ribs increase ejection force and cause scuffing, while draft angles above 1.5° reduce usable internal volume. Flexural modulus should be measured under ISO 178 or ASTM D790, tensile yield strength and elongation under ISO 527-2 or ASTM D638, and notched Charpy impact under ISO 179-1/1eA; these mechanical values are used as incoming resin lot checks, not as direct load ratings for finished crates. Load-rating assignments for stacking under cyclic warehousing conditions must be derived from whole-part compression tests conducted at the intended service temperature, because plastic buckling and side-wall rib stability depend on part geometry, moulded-in stress, and creep under load.
| Processing variable | Thin-wall food containers | Closures | Crates / pallets | Open-head pails | Light-gauge sheet |
|---|---|---|---|---|---|
| Melt temperature | 210 °C to 235 °C | 215 °C to 230 °C | 220 °C to 250 °C | 215 °C to 240 °C | 205 °C to 220 °C |
| Mould / roll temperature | 15 °C to 35 °C | 10 °C to 25 °C | 20 °C to 30 °C | 15 °C to 25 °C | 70 °C to 90 °C |
| Fill-speed control | Screw forward time below 0.35 s | Valve-gated high-speed fill | Profiled medium fill, then pack | Medium fill, hold to gate freeze | Roll gap pressure, low sag |
| Packing / hold | Short hold, 2 s to 4 s | Cooling 4 s to 7 s | 60% to 80% peak pressure | 8 s to 15 s hold | Chill-roll gap control |
| Gate / land geometry | Gate 0.8 mm, land 0.5 mm to 1.0 mm | Bridge thickness 0.30 mm to 0.45 mm | Rib draft 0.5° to 1.5° | Gate 2.0 mm to 3.0 mm | Die gap 0.5 mm to 0.8 mm |
When open-head pails of 5 L to 25 L are injection moulded from HDPE 43049, the handle lug geometry, not the resin, becomes the primary failure site under drop-load conditions. Wall thickness at the lug transition should be increased gradually over a length of at least 15 mm to avoid sharp thickness gradients that create sink voids or stress-centre points. The melt temperature for pail bodies is typically held at 215 °C to 240 °C, with a mould surface temperature of 15 °C to 25 °C and a longer holding pressure than used for thin-wall parts; hold time is commonly extended until the gate diameter of 2.0 mm to 3.0 mm at the base centre freezes, which may require 8 s to 15 s depending on part weight. Injection pressure is generated by a shot size that is 60% to 75% of barrel capacity to maintain residence-time uniformity, and the screw cushion is held between 3 mm and 6 mm. Drop impact performance of loaded pails should be tested according to ASTM D5276 or ASTM D2463 after conditioning at the specified lowest service temperature, typically -18 °C for frozen or refrigerated logistics; pails for dangerous goods must also meet the applicable UN packaging requirements for open-head plastics packaging, including stacking and leakproofness assessments. Environmental stress crack resistance should be evaluated under ASTM D1693 or ISO 22088 in a relevant stress-cracking medium if the container is intended for detergent, surfactant, or oxygenated chemical distribution, because HDPE can lose ductility at lug and base radii when simultaneously loaded and exposed to polar liquids. For food-grade pails, the same EU No 10/2011, 21 CFR 177.1520, or GB 4806.7 migration requirements apply, and the colour masterbatch must be supplied with documented food-contact status for the intended region.
| Application area | Relevant standard / regulation | Measurement / acceptance |
|---|---|---|
| Thin-wall food packaging | EU No 10/2011, EN 1186-series, 21 CFR 177.1520, GB 4806.7 | Overall migration 10 mg/dm² or 60 mg/kg; organoleptic evaluation |
| Injection-moulded closures | ASTM D3198, ASTM D2063, USP 661.1 | Application/removal torque; physicochemical integrity |
| Industrial crates / pallets | ISO 178, ISO 527-2, ISO 179-1/1eA | Flexural modulus, tensile yield, notched Charpy impact |
| Open-head pails | ASTM D5276, ASTM D1693, UN 1H2 where applicable | Loaded drop impact; ESCR in stress-cracking medium |
| Light-gauge sheet / thermoformed trays | EU No 10/2011, 21 CFR 177.1520 | Total migration; regrind loop validation |
Sheet extrusion from a resin with a melt mass-flow rate near 4.0 g/10 min is temperature-limited because the melt curtain loses tension before the chill-roll gap at process temperatures above 225 °C. A single-screw extruder with an L/D ratio of 25:1 to 30:1 and a barrier-type screw is preferred; melt temperature at the adapter should be controlled between 205 °C and 220 °C, while the flat-die melt temperature is kept at or below 220 °C. The die gap is typically set at 0.5 mm to 0.8 mm for light-gauge sheet of 0.3 mm to 1.0 mm final thickness, and the vertical drop from die lip to top roll must be minimized to reduce curtain sag. Chill-roll temperatures from 70 °C to 90 °C produce a sheet surface with adequate gloss and limited haze, but the upper roll temperature should be reduced if the sheet wraps too tightly due to rapid crystallisation at the surface. Thermoforming from HDPE 43049 sheet is restricted to shallow trays, lids, and flat-seal containers because the resin’s moderate melt strength limits deep-draw depth-of-draw ratios to roughly 1:1; published data for this specific configuration in high-draw thermoforming is limited, and processors should generate draw-ratio maps on in-house tooling before production release. The same food-contact migration limits under EU No 10/2011, 21 CFR 177.1520, and GB 4806.7 apply to the finished sheet, and any regrind loop must be validated for total migration and organoleptic change.
Housewares and small storage products made from HDPE 43049 tend to be evaluated for surface aesthetics, dimensional consistency, and colour uniformity rather than structural load; however, two processing defects dominate when tools are not vented correctly. Trapped gas at the end-of-fill regions creates burn marks at the perimeter of bins, while insufficient clamp force on deep-draw storage containers produces flash along the parting line and the latch undercuts. A mould vent depth of 0.02 mm to 0.03 mm is recommended for semi-crystalline HDPE with the grade’s viscosity; vent lands should be cut 5 mm to 10 mm wide and spaced along the final fill path. Melt temperature for housewares is typically set from 210 °C to 240 °C, with mould surface temperature between 20 °C and 35 °C. Textured cavity surfaces require draft angles at least 1° per side to avoid ejection drag, and any colour masterbatch should be pre-dried to 0.03% maximum moisture when hygroscopic carriers are used. If the finished storage bins are intended for children’s articles or food-contact kitchenware, the relevant regional restrictions under EU No 10/2011, 21 CFR 177.1520, or toy safety standards apply; however, colour pigments and processing aids must be verified individually because their migration behaviour is not determined by the base resin food-contact status.
Competitive Yanchang China Coal Yulin (Shaanxi) HDPE 43049 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Yanchang China Coal Yulin (Shaanxi) HDPE 43049 is supplied as a high-density polyethylene granulate from the Yulin coal-to-olefins complex. The grade code 43049 identifies the resin within the producer’s polyethylene range and appears on certificates of analysis alongside lot number, density, melt flow rate, additive package, and production date. In commercial practice the material is categorized as an HDPE with a density above 0.940 g/cm³ and a melt flow rate measured at 190°C under a 2.16 kg load. The resin is applicable to rigid packaging, industrial pails, closures, small-diameter pressure and non-pressure pipe, and profile extrusion, provided the selected application is validated against the producer’s grade-specific data.
The product should not be inferred from the designation 43049 alone. Some HDPE coding systems use suffixes to denote nominal melt flow rate or density, but the producer’s technical datasheet must be consulted to decode the grade. In a receiving laboratory, a standard qualification panel is applied to confirm that the delivered resin matches the supplier’s declared values and to detect transit damage, moisture uptake, or cross-contamination from other polymers in bulk unloading. Because open-access grade-specific datasheets for this configuration are limited, procurement and incoming inspection should treat the producer’s certificate of analysis as normative.
Incoming lots of HDPE 43049 are typically qualified by density according to ISO 1183-1:2019 or ASTM D1505-18, melt mass-flow rate according to ISO 1133-1:2022 or ASTM D1238-20, and residual moisture by ISO 15512:2019. For pressure-pipe and detergent packaging candidates, environmental stress crack resistance is evaluated under ASTM D1693-21 at 50°C in 100% Igepal CO-630 or under ISO 22088-1; oxidative stability is screened by oxidative induction time at 200°C using ISO 11357-6:2018 or ASTM D3895-19. The table below summarises the standard battery and class-typical HDPE observations for preliminary equipment setup. These values are not lot certification.
| Property | Reference method | Typical HDPE class observation | Basis for HDPE 43049 |
|---|---|---|---|
| Density | ISO 1183-1:2019 / ASTM D1505-18 | 0.943–0.960 g/cm³ in rigid packaging and pipe grades | Producer CoA normative |
| Melt mass-flow rate | ISO 1133-1:2022 / ASTM D1238-20 | 0.2–1.2 g/10 min for pipe and blow grades; injection grades higher | Producer CoA normative |
| Tensile yield stress | ISO 527-2:2012 / ASTM D638-14 | 22–32 MPa for HDPE | Producer CoA normative |
| Flexural modulus | ISO 178:2019 / ASTM D790-17 | 900–1500 MPa | Producer CoA normative |
| Charpy notched impact | ISO 179-1:2010 | 3–15 kJ/m² at 23°C depending on molecular weight | Producer CoA normative |
| Environmental stress crack resistance | ASTM D1693-21 | 3–1000 h depending on comonomer and MWD | Producer CoA normative |
| Oxidative induction time | ISO 11357-6:2018 | >20 min at 200°C for stabilised grades | Producer CoA normative |
| Moisture | ISO 15512:2019 | <0.03 wt% as supplied | Producer CoA normative |
| Bulk density | ASTM D1895-17 / ISO 60:1977 | 0.54–0.58 g/cm³ for HDPE pellets | Producer CoA normative |
Class-typical values in the third column are for preliminary equipment setup only and must not be used for lot acceptance. A lot failing the producer’s certified range for melt flow rate or density should be placed on hold and investigated for cross-contamination, regrind errors, or handling damage.
For HDPE grades with moderate-to-high molecular weight, the melt temperature in pipe extrusion is generally maintained between 180°C and 220°C. If 43049 is a bimodal or broad-MWD product, the usable window may be narrower; comparable high-molecular-weight pipe grades have shown surface oxidation and gel formation when melt temperature excursions exceed 5°C above the target for extended residence times. The extruder should be equipped with thermocouples in each barrel zone and a melt probe before the screen pack. Temperature profile settings should be validated by capillary rheometry at 190°C under ISO 11443:2021 and by actual melt-pressure stability.
On grooved-barrel single-screw extruders with L/D 30:1 to 36:1, a barrier screw with compression ratio 3:1 to 4:1 is common for HDPE pipe and sheet. The grooved feed section improves conveying but can raise melt temperature if the screw speed is set too high; production lines often observe a rapid increase in die-head pressure and surface melt fracture when the screw speed exceeds the optimized range. For injection molding, melt temperatures between 200°C and 260°C and mold temperatures from 10°C to 40°C are typical for HDPE closures and pails, but the actual values depend on wall thickness, flow length, and gate size. Inadequate mold temperature control can produce warpage because HDPE crystallization continues after demolding.
Moisture in HDPE pellets is usually below 0.03 wt% as supplied and does not require drying for standard extrusion. However, if bags are stored at relative humidity above 80% or opened in an unheated warehouse, surface moisture can increase and cause porosity or splay in molded parts. A desiccant dryer operating at 75–85°C for 1–2 h is generally sufficient; drying above 90°C for prolonged periods may consume antioxidant and should be avoided unless the resin supplier has approved the cycle.
In production-scale HDPE pipe extrusion, matte bands or sharkskin at the pipe surface are often caused by melt temperature below the critical value or die lip contamination. When the grade is run on a coextruded pipe line with a stripe layer, the main layer melt temperature must be kept within the producer’s validated range; deviation can lead to layer thickness variation and reduced burst strength. These field observations emphasise the need for closed-loop melt temperature control rather than reliance on barrel setpoints alone.
When HDPE 43049 is compounded with carbon black or additive masterbatch, the dilution ratio should be controlled by the masterbatch supplier and verified by ash content under ISO 3451-1:2019 or ASTM D5630-22. In a corotating twin-screw extruder with L/D 44:1, dispersion is usually achieved in the melting zone, and a screen pack of 20–40 mesh is placed upstream of the die. A pressure rise across the screen beyond 8–10 MPa indicates agglomeration or screen blocking, requiring pack change. High screw speeds and unforgiving shear profiles reduce molecular weight; the resulting melt flow rate shift can be confirmed by ISO 1133-1:2022 after compounding.
Regrind addition is application-dependent. For pressure pipe, long-term hydrostatic tests under ISO 1167 and ISO 9080 must be repeated if regrind ratios exceed the producer’s validated limit; for non-pressure injection-molded articles, melt flow rate, tensile yield stress, and notched impact should be monitored on first-generation regrind. Uncontrolled regrind from mixed lots can introduce density and viscosity inhomogeneity, causing weld-line weakness and dimensional variability. Avoid melt blending HDPE 43049 with polypropylene, PET, or PVC; melt-phase separation and interfacial delamination are probable.
Molecular architecture controls ESCR: high-molecular-weight tail fractions and tie molecules bridge lamellae; their absence in low-Mw grades leads to slow crack growth. For HDPE 43049 in detergent packaging, ESCR data should be generated under ASTM D1693-21 condition B with 100% Igepal CO-630 at 50°C. If the resin is intended for pipe, notched pipe hydrostatic tests under ISO 13479 and full-scale stress rupture under ISO 9080 are better indicators than bottle ESCR. Published data for this specific configuration is limited.
Compared with a general-purpose unimodal HDPE injection grade of similar density, a 43xxx-series resin designed for high ESCR typically has a broader molecular weight distribution and higher melt elasticity. This difference can be detected by dynamic frequency sweep measurements under ISO 6721-10:2015 and by elongation at break under ISO 527-2:2012. The practical consequence is lower injection speed, higher clamp force per projected area, and improved slow-crack-growth resistance under ASTM D1693-21 or ISO 16770.
Compared with C6-LLDPE grades, HDPE 43049 is expected to exhibit higher flexural modulus measured by ISO 178:2019, lower dart drop impact by ISO 7765-1:2017, and a narrower heat-seal window because of its higher crystalline melting point. These differences must be accounted for in multilayer film, cap, or duct designs. HDPE also differs from polypropylene in low-temperature impact and oxidative degradation behavior.
Compared with a blow-molding HDPE of similar density, 43049 may show lower melt strength or higher melt flow rate if designed for injection. If it is a pipe-grade HDPE, blow molding may be possible only with accumulator-type heads and low melt temperature, because continuous extrusion blow molding may produce parison sag. Melt strength should be measured with a capillary rheometer with a haul-off attachment rather than inferred from melt flow rate alone.
For food-contact applications, the supplier’s compliance statement is required. Olefin polymers may be evaluated under FDA 21 CFR 177.1520; EU food-contact materials require documentation under Regulation (EU) No 10/2011, including overall migration testing in prescribed simulants. For China, GB 4806.7-2016 is applicable. RoHS compliance against Directive 2011/65/EU Annex II typically involves limits of 1000 mg/kg for lead, mercury, hexavalent chromium, PBB and PBDE, and 100 mg/kg for cadmium. REACH SVHC screening is performed under EC 1907/2006, with a threshold of 0.1% w/w for article-based declarations.
Storage and conveying installations should be configured for HDPE pellets. Dense-phase pneumatic transport with a conveying air dew point below -30°C and air temperature below 70°C reduces moisture pickup and angel hair formation. High-speed dilute-phase conveying, especially with long pipe runs and many elbows, may generate fines and streamers that cause bridging in hopper outlets and feed fluctuation at the extruder throat. In bulk railcar or truck unloading, the receiving lot should be sampled after stabilization to room temperature to avoid condensation on cold pellets.
When the resin is used in pressure-pipe applications, the long-term failure mode is slow crack growth rather than simple yield. The designer must not use short-term tensile yield as a substitute for hydrostatic design basis. Hydrostatic stress-rupture data under ISO 9080, notched pipe tests under ISO 13479, and creep crack growth resistance under ASTM F1473-18 are required for pressure rating. Published data for this specific configuration may be limited; therefore qualification must be based on product-specific values from the producer or an accredited pipe testing laboratory.