Yanchang China Coal Yulin Shaanxi Hdpe 23050

Yanchang China Coal Yulin (Shaanxi) HDPE 23050

    • Product Name: Yanchang China Coal Yulin (Shaanxi) HDPE 23050
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 728398
    Melt Flow Rate 190 C 2 16 Kg 23 g/10 min
    Density 0.950 g/cm³
    Tensile Strength At Yield ≥22 MPa
    Elongation At Break ≥500%
    Flexural Modulus ≥900 MPa
    Notched Izod Impact Strength ≥40 J/m
    Vicat Softening Temperature ≥120 °C
    Melting Point 130 °C
    Shore D Hardness 60
    Water Absorption <0.01%
    Volume Resistivity >10^16 Ω·cm
    Dielectric Constant 2.3
    Physical Form Pellets
    Color Natural

    As an accredited Yanchang China Coal Yulin (Shaanxi) HDPE 23050 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Yanchang China Coal Yulin (Shaanxi) HDPE 23050 is supplied in 25 kg polyethylene bags, palletized, or 1,000 kg jumbo bags.
    Container Loading (20′ FCL) 20' FCL container loading of Yanchang China Coal Yulin (Shaanxi) HDPE 23050, packed in 25kg bags, securely stowed for shipment.
    Shipping Yanchang China Coal Yulin (Shaanxi) HDPE 23050 is typically shipped as non-hazardous polyethylene pellets in 25 kg woven bags or 1,000 kg jumbo bags, palletized and shrink-wrapped. Transport in clean, dry containers or trucks; protect from moisture, sunlight, and contamination. Standard export documentation and MSDS accompany shipments.
    Storage Store Yanchang China Coal Yulin (Shaanxi) HDPE 23050 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original bags sealed, palletized, and off the floor to prevent moisture, dust, and contamination. Avoid prolonged UV exposure, high temperatures, and incompatible materials. Do not stack excessively. Follow local regulations and manufacturer’s handling and storage recommendations.
    Shelf Life Shelf life: typically 24 months when stored unopened, dry, cool, and protected from direct sunlight and heat.
    Application of Yanchang China Coal Yulin (Shaanxi) HDPE 23050

    Potable water pressure pipe produced from Yanchang China Coal Yulin HDPE 23050, a bimodal high-density polyethylene with nominal melt flow rate 0.23 g/10 min under 2.16 kg at 190 °C and nominal density 0.950 g/cm³, is governed by ISO 4427 and EN 12201. The grade belongs to the PE100 class in pressure pipe according to ISO 9080, with an extrapolated 50-year hydrostatic strength at 20 °C of 10.0 MPa and a water service design stress of 8.0 MPa under ISO 4427-1 and EN 12201-1. The processing window is defined by single-screw extruders with L/D 30:1–36:1 and barrier screws; barrel zones are set from 180 °C to 220 °C, while die head temperature is maintained between 210 °C and 220 °C to prevent melt fracture in thick-wall SDR 11 pipe. For outdoor UV resistance, natural HDPE 23050 is dry-blended with a 40 wt% carbon black masterbatch at an addition rate of 2.0–2.5 wt% of final compound, which yields a carbon black content of 2.0–2.5 wt% and is verified by pyrolysis; dispersion is assessed according to ISO 18553. A compound intended for pressure pipe must pass the intrapipe hydrostatic tests of ISO 1167-1 at 20 °C and 80 °C, the notched pipe slow crack growth test of ISO 13479, and oxidation induction time testing under ISO 11357-6 at 200 °C with a minimum of 20 min. SDR 11 pipe in this material is rated PN 16 at 20 °C, SDR 17 is rated PN 10, and SDR 9 is rated PN 20. A processing limit is that melt temperature should not exceed 250 °C; above this, thermal-oxidative chain scission increases the melt flow rate unpredictably and degrades hydrostatic strength. The grade is not injection-moulded into thin-wall closures because the low melt flow rate increases filling pressure and cycle time. Potable water service with high chlorine residuals must be validated case by case; published data for this specific HDPE 23050 configuration at chlorine residuals above 2 mg/L combined with temperatures above 60 °C is limited.

    What governs gas distribution pipe certification for HDPE 23050?

    Gas distribution pipe certification is governed by ISO 4437 and EN 1555, which impose a PE100 minimum required strength of 10.0 MPa and a gas design coefficient of 2.0. The same low melt flow rate of 0.23 g/10 min and density of 0.950 g/cm³ are retained, but the compound and pipe must pass additional rapid crack propagation testing under ISO 13478 at 0 °C to demonstrate that a crack cannot propagate beyond a critical pressure above the maximum operating pressure. For SDR 11 pipe in PE100, the maximum operating pressure for natural gas is 10 bar at 20 °C; lower temperatures and lower operating pressures allow SDR 17 or SDR 21 dimensions. The extruded pipe is commonly black with yellow coextruded stripes or yellow jacketing, with carbon black added at 2.0–2.5 wt% and distributed per ISO 18553. Butt fusion welding is performed under ISO 21307 using matching heater plates at 210–230 °C, while electrofusion sockets are connected under ISO 12176; both processes require scrupulous removal of the oxidised skin by scraping before joining. Operators should not exceed the specified interfacial pressure during butt fusion, because excessive pressure ejects too much melt and creates a cold joint. HDPE 23050 is not recommended for gas service in condensing hydrocarbon environments with free aromatic liquid above 5 wt% unless the specific pipe system has passed chemical resistance evaluation under ISO 175 at the service temperature.

    SectorPrimary specificationTest anchor
    Potable water pressure pipeISO 4427-1/-2/-3/-5, EN 12201-1/-2/-3ISO 1167-1 hydrostatic, ISO 13479 notched pipe, ISO 11357-6 OIT
    Gas distribution pipeISO 4437-1/-2/-3/-5, EN 1555-1/-2/-3ISO 13478 rapid crack propagation, ISO 13479 slow crack growth, ISO 21307 butt fusion
    Non-pressure sewer pipeISO 21138-1, EN 13476-3ISO 9969 ring stiffness, ISO 21307 jointing
    Trenchless rehabilitation liningISO 11298-3, ASTM F714ISO 13479 slow crack growth, ISO 21307 field welding
    Blow-moulded industrial packagingUN Model Regulations Chapter 6.1Drop at -18 °C, stack at 40 °C, ASTM D1693 ESCR
    Geomembrane sheetGRI GM13ASTM D5397 stress crack, ASTM D6392 seam weld, ISO 175 chemical resistance

    Gravity sewer and land drainage systems convert HDPE 23050 into solid-wall and structured-wall pipes by direct extrusion. The ring stiffness of the finished pipe is measured per ISO 9969; SN4 and SN8 classes are achieved by selecting the wall thickness and pipe diameter. In corrugated structured-wall pipe conforming to EN 13476-3, the bimodal molecular structure retains melt strength when the parison is drawn into the corrugator blocks at a melt temperature of 210–230 °C. The outer and inner layers are produced from virgin material; some manufacturers coextrude a middle layer with post-industrial recyclate, but the recycled layer must not contact sewage and must comply with the formulation limits in EN 13476-1. Jointing is by bell-and-spigot with elastomeric seals or by butt fusion; butt fusion is tested under ISO 21307. Long-term creep deflection is controlled by the pipe ring stiffness, not by the resin alone; the design must use the measured creep ratio and backfill compaction specified in the installation standard for the specific sewer network.

    Abrasion Resistance Limits in Mining Slurry Laterals

    Slurry pipelines handling tailings, fly ash, and dredged solids place HDPE 23050 in direct contact with abrasive quartz and magnetite particles. The wear rate of HDPE is not an intrinsic property; it depends on particle size, solids concentration, and flow velocity. Designers should maintain operation within the pipe manufacturer’s velocity limits, commonly 3–5 m/s for coarse-particle slurries, and should periodically rotate the pipe when one side wears. Above 20 wt% solids and above 5 m/s, a sacrificial layer or wear-resistant steel insert should be considered. For above-ground exposed sections, UV stabilisation with 2.0–2.5 wt% carbon black is mandatory; buried sections are shielded from ultraviolet radiation but must be bedded in compacted fines to avoid point loading. The PE100 class provides high slow crack growth resistance, which is significant where the pipe is scored by rock abrasion; however, published data for this specific HDPE 23050 grade in high-solids mining slurry at temperatures above 40 °C is limited. Field operators should validate the abrasion rate against the specific ore using a portable pipe loop before full-scale installation.

    When PE100 Liners Are Pulled Through Deteriorated Culverts

    In slip-lining and close-fit lining operations, HDPE 23050 is extruded into solid-wall liner pipe, butt-fused into a continuous string, and pulled or winched into a deteriorated host culvert. The governing installation documents include ASTM F714 for polyethylene pipe and ISO 11298-3 for renovation of pressure pipelines; structural design checks combine the remaining host pipe strength with the liner’s ring stiffness and hydrostatic resistance. The pull force must be kept below the manufacturer’s allowable longitudinal stress, and the pulling head must distribute load evenly; point loads at spigot or bell transitions are a common failure mode. Fold-and-form liners rely on the same resin architecture to withstand repeated flexure during cold folding and re-rounding after insertion. The slow crack growth resistance verified by ISO 13479 is critical in this sector because the liner may be exposed to external soil pressure, groundwater, and local hard-face deposits. Site welds are made by butt fusion under ISO 21307; each joint must be documented. Operators should pre-dry the resin or the pipe surface if the storage humidity has exceeded 60% RH for more than 24 h, because surface moisture can cause weld porosity in butt fusion.

    Blow Moulded Drum Production and UN Drop-Test Compliance

    HDPE 23050 is used in extrusion blow moulding of open-head and tight-head drums and intermediate bulk containers with capacities from 30 L to 220 L. The low melt flow rate of 0.23 g/10 min provides high zero-shear viscosity and sag resistance for large parisons; accumulator-head blow moulding machines with 100–150 mm screw diameter and 24:1 L/D are typical. Melt temperature is held at 190–210 °C, die head temperature at 190–205 °C, and mould temperature at 10–20 °C to control warpage and wall-thickness uniformity. Parison programming is essential for heavy-walled chimes and corners; without programmed parison thickness, the wall-thickness variation can exceed 30% at the pinch-off line. The drum must pass the drop and stacking tests prescribed in the UN Model Regulations for dangerous goods packaging, including drop testing at -18 °C after conditioning and stack loading at 40 °C for 28 d. Environmental stress crack resistance is evaluated under ASTM D1693, Condition B, in 10% Igepal; PE100-type HDPE 23050 formulations are expected to deliver long failure times, but actual values depend on comonomer distribution and cooling rate. The grade is not suitable for continuous hot-fill service above 60 °C or for aggressive oxidising acids without service testing.

    Flat-die sheet and geomembrane lines process HDPE 23050 into rolls for landfill lining, canal lining, and pond lining. The grade is usually compounded with 2.0–2.5 wt% carbon black and an antioxidant package; the melt is discharged through a flexible-lip flat die and calendered to 1.5 mm or 2.0 mm nominal thickness. GRI GM13 requires minimum density 0.940 g/cm³, OIT retention after oven ageing, and stress crack resistance per ASTM D5397; HDPE 23050's PE100 molecular architecture supports these requirements when properly stabilised. For textured sheets, nitrogen gas is injected into the melt before the die to create a designed asperity pattern, but the gas flow must be tuned to prevent surface pinholes. Hot-wedge and extrusion fillet seams are welded according to ASTM D6392; seam peel and shear strength are tested in the field. Prolonged exposure to strong oxidising leachates or temperatures above 60 °C requires specific chemical resistance testing under ISO 175.

    Free Quote

    Competitive Yanchang China Coal Yulin (Shaanxi) HDPE 23050 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Yanchang China Coal Yulin (Shaanxi) HDPE 23050 is a bimodal high-density polyethylene resin produced at the Yulin, Shaanxi integrated coal-to-olefins complex. The grade designation encodes a nominal melt mass-flow rate of 0.23 g/10 min under a 5 kg load at 190 °C and a nominal density of 0.950 g/cm³ at 23 °C, as determined by ISO 1133-1 and ISO 1183-1. The material is classified as a PE100 pipe-grade resin under ISO 12162, with a minimum required strength of 10 MPa at 20 °C for a 50-year service life. The PE100 designation is an extrapolated long-term hydrostatic strength property and is not a lot-specific burst-pressure guarantee. Typical certificate-of-analysis data reported in producer documentation include a tensile yield stress of 23 MPa under ISO 527-2, tensile strain at break above 600 %, flexural modulus of 900 MPa under ISO 178, Charpy notched impact strength of 25 kJ/m² at 23 °C under ISO 179-1, and oxidation induction time above 30 min at 210 °C under ISO 11357-6. These are representative values and vary with lot, catalyst batch, and downstream processing history.

    Table 1 summarises representative lot values and test designations.

    PropertyRepresentative valueTest method
    Melt mass-flow rate0.23 g/10 min (190 °C, 5 kg)ISO 1133-1
    Density0.950 g/cm³ (23 °C)ISO 1183-1
    Tensile stress at yield23 MPaISO 527-2
    Tensile strain at break>600 %ISO 527-2
    Flexural modulus900 MPaISO 178
    Charpy notched impact strength25 kJ/m² at 23 °CISO 179-1
    ESCR, F50>1,000 hASTM D1693-15
    Oxidation induction time>30 min at 210 °CISO 11357-6
    Vicat softening temperature, A50128 °CISO 306

    What Limits Continuous Pipe Extrusion Throughput?

    Throughput in continuous pressure-pipe extrusion of HDPE 23050 is constrained by three process variables: melt pressure at the screen pack, melt temperature at the die lip, and sag of the extrudate before calibration. On grooved-barrel single-screw extruders with 33:1 to 38:1 L/D and barrier screws, this resin typically falls into a melt temperature corridor of 210 °C to 230 °C. Exceeding 240 °C produces measurable reductions in oxidation induction time under ISO 11357-6, while operating below 200 °C raises power draw and increases melt fracture risk in small-diameter pipe. At an 800 mm diameter SDR 11 line, die-head pressures of 250 bar to 350 bar are reported in extruder OEM selection guides for PE100 resins of this melt flow index. The high zero-shear viscosity reduces sag, but requires vacuum calibration tank air pressure of 0.2 bar to 0.5 bar and water spray temperatures of 15 °C to 25 °C to stabilize the outer diameter. Published data for this specific configuration are limited, so line trials with torque monitoring and melt-pressure transducers are required for throughput validation.

    Slow crack growth resistance is monitored by notched-pipe tests under ISO 13479, with specimens conditioned at 80 °C and internal pressure of 4.6 MPa. In producer technical literature, failure times above 1,000 h are reported for stabilized lots, but this value depends on notch depth, residual stress, and test rig vibration. Full-scale gas distribution pipeline data for this specific grade are limited. Converters carrying out lot qualification should specify notched-pipe failure time and ductile-to-brittle transition criteria rather than relying on melt flow index and density alone.

    Bimodal Molecular Architecture and the Role of the Low-Molecular-Weight Fraction

    The bimodal chain-length distribution separates the high-molecular-weight chains that provide tie-molecule density and slow crack growth resistance from a lower-molecular-weight fraction that reduces melt viscosity during extrusion and increases crystalline order. In practice this means the resin exhibits lower shear sensitivity than unimodal HDPE of similar density, with a broader processing window but higher zero-shear viscosity. Differential scanning calorimetry at 10 K/min reveals a main melting peak near 132 °C, consistent with a density of 0.950 g/cm³ and crystallinity near 60 %. The high-molecular-weight tail raises extrudate swell and elastic memory, which affects pipe wall-thickness control. Die gap settings must account for swell ratios of 1.2 to 1.5, depending on die land length and shear rate. Producer bulletins indicate that chromic acid etching of compression-moulded plaques shows a fine spherulitic structure, but spherulite size is not a reliable quality indicator for pipe performance.

    If the Converter Replaces a Unimodal PE100 with HDPE 23050

    Substitution of a unimodal PE100 pipe grade with HDPE 23050 requires adjustment of screw speed, barrel temperature profile, and calibration vacuum. The most immediate difference is increased melt strength and sag resistance in thick-wall pipe, but this is accompanied by higher head pressure and a narrower window for internal surface finish. A conventional unimodal PE100 may extrude with melt temperatures of 190 °C to 210 °C; HDPE 23050 typically requires 210 °C to 230 °C to maintain surface gloss and fusion pressure. Feedstock color concentrates based on milled calcium carbonate or carbon black should be predispersed at 6 wt% to 8 wt% carrier addition for carbon black pipe masterbatch, and mixing homogeneity verified by dispersion tests such as ISO 18553. The resin is not intended for injection moulding or thin-gauge film because its low melt index and high elastic memory produce excessive orientation and gate freeze-off. Published data for this specific configuration are limited, but comparative line trials generally show a throughput reduction of 5 % to 15 % relative to lower-viscosity PE100 grades when the same screw geometry is retained.

    Table 2 compares HDPE 23050 with generic HDPE classes commonly used in adjacent conversion operations.

    Resin classMelt mass-flow rateDensityClassificationPrimary conversion process
    HDPE 23050 bimodal PE1000.23 g/10 min (5 kg)0.950 g/cm³PE100, 10 MPa MRSThick-wall pressure pipe, large-diameter water and gas mains
    Unimodal HDPE pipe grade0.4 g/10 min to 0.6 g/10 min (5 kg)0.945 g/cm³ to 0.952 g/cm³PE80 to PE100Small-diameter pipe, corrugated drainage, cable conduit
    High-load melt-index blow moulding HDPE0.25 g/10 min to 0.35 g/10 min (21.6 kg)0.950 g/cm³ to 0.955 g/cm³Not classified for pressure pipeLarge-part blow moulding, industrial containers
    HDPE film grade0.7 g/10 min to 1.2 g/10 min (2.16 kg)0.951 g/cm³ to 0.957 g/cm³Not classified for pressure pipeBlown film, sacks, liners

    Primary applications are pressure pipe systems for potable water distribution, industrial water transport, gas distribution, mining slurry lines, and sewage force mains. In potable water service, compliance with ISO 15494 or local drinking-water contact standards is required; the resin itself is not potable-water certified until formulated into a compound with approved stabilizer and pigment packages. For gas distribution, installation under ISO 12176 fusion procedures is typical, and butt-fusion weldability depends on melt viscosity matching between pipe ends. Operators report that the high melt strength of HDPE 23050 helps maintain bead shape during butt fusion at ambient temperatures below 10 °C, but published field data for this specific grade in cold-weather gas networks are limited. In mining slurry lines, the resin’s abrasion resistance is derived from high molecular weight and density; comparative wear data should be generated using slurry abrasion tests such as ISO 15527 before replacing rubber-lined steel.

    Regulatory Compliance and Hydrostatic Design Basis

    Hydrostatic design basis is established by long-term pressure testing according to ISO 1167-1 and ISO 9080. The material’s PE100 classification under ISO 12162 states a lower confidence limit of 10 MPa at 20 °C for 50 years. For distribution networks, the allowable operating pressure is calculated from the MRS, service coefficient, and standard dimension ratio. At SDR 17, the nominal pressure rating is 10 bar for water at 20 °C; at SDR 11, the rating is 16 bar, with derating factors applied above 20 °C according to ISO 13760. Compliance with FDA 21 CFR 177.1520 for olefin polymers is available only for specific formulated lots; converters must request food-contact certificates from the producer for each grade and lot. The resin is generally regarded as REACH-compliant for monomer contents below 0.1 % residual ethylene as supplied, but SVHC declarations should be confirmed through the producer’s safety data sheet. Oxidative resistance in chlorinated water service should be evaluated under ASTM F2263 or equivalent; potable water disinfectant exposure can reduce long-term hydrostatic strength, and published data for this specific resin under chlorine dioxide are limited.

    Large-Diameter Cooling and Residual Stress Management

    Residual stress in thick-wall HDPE 23050 pipe arises from differential cooling between the outer and inner surfaces during vacuum tank calibration. If the outer surface is quenched before the inner wall crystallizes, frozen-in stresses can reduce slow crack growth resistance and increase susceptibility to circumferential splitting during hydrostatic testing. For diameters above 800 mm, staged cooling is used: a first spray chamber at 25 °C to 35 °C, a second chamber at 15 °C to 20 °C, and a final air stabilization zone of 3 m to 5 m before cutting. Internal calibration pressure is maintained at 0.2 bar to 0.5 bar, with diameter feedback from laser gauges sampling at 10 Hz or faster. Operators should avoid rapid reductions in line speed during start-up because a drop in melt temperature at the die lip causes variable extrusion swell and wall-thickness oscillation. Drying is required when pellet surface condensation appears after storage at relative humidity above 60 %; 80 °C for 2 h to 4 h in a desiccant hopper dryer is sufficient. No post-extrusion annealing is normally required for pipe with wall thickness below 60 mm.