| HS Code | 858392 |
| Density | 0.950 g/cm³ |
| Melt Flow Rate | 23 g/10 min |
| Tensile Strength At Yield | ≥ 24 MPa |
| Elongation At Break | ≥ 500% |
| Flexural Modulus | ≥ 900 MPa |
| Vicat Softening Temperature | ≥ 120 °C |
| Melting Point | 130-135 °C |
| Shore D Hardness | 60-65 |
| Water Absorption | < 0.01% |
| Mold Shrinkage | 1.5-3.0% |
| Brittleness Temperature | ≤ -70 °C |
| Ash Content | ≤ 0.03% |
As an accredited Yan'an Energy & Chemical HDPE 23050 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Yan'an Energy & Chemical HDPE 23050 is packaged in 25 kg polyethylene bags, 40 bags per pallet (1,000 kg total). |
| Container Loading (20′ FCL) | 20′ FCL container loading: Yan'an Energy & Chemical HDPE 23050, 25 kg bags, palletized, securely stowed, container sealed for export. |
| Shipping | Yan'an Energy & Chemical HDPE 23050 is packed in 25 kg PP woven bags or 1000 kg jumbo bags, palletized and shrink-wrapped. It ships as a non-hazardous polymer via sea, rail, or truck in dry containers, protected from moisture, heat, and direct sunlight, with clear labeling and documentation. |
| Storage | Store Yan'an Energy & Chemical HDPE 23050 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags sealed and palletized to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Do not store outdoors; protect from rain, snow, and mechanical damage. Follow good industrial hygiene practices. |
| Shelf Life | Shelf Life: 24 months under cool, dry, well-ventilated storage in original packaging, away from direct sunlight and ignition sources. |
Yan’an Energy & Chemical HDPE 23050 is typically supplied as a high-molecular-weight natural HDPE extrusion resin with a nominal density of 0.950 g/cm³ and a melt index of 0.23 g/10 min at 190°C/5.0 kg under ISO 1133-1:2022. The viscosity profile places the grade in the high-melt-strength region for thick-wall pipe, geomembrane, and large-part blow moulding. All downstream processing decisions are controlled by the batch certificate for density, melt index, stabilizer content, and moisture; pre-drying is required only when the resin has been stored at relative humidity above 60% and surface condensation is visible.
Potable water mains manufactured from HDPE 23050 are typically compounded to PE100 classification under ISO 12162 by blending the natural resin with a carbon black masterbatch at 5.0–6.0 wt%, yielding a final carbon black content of 2.0–2.5 wt% as required by ISO 4427-1. The compound is processed on a single-screw extruder with an L/D ratio of 30:1 to 33:1 and a barrier screw compression ratio of 3.0:1 to 3.5:1. Barrel temperatures are set from 180°C to 210°C across the feed, compression, and metering zones; the die head is held at 200°C to 220°C. Melt temperature at the die exit must not exceed 230°C because thermal degradation accelerates oxidative chain scission and reduces hydrostatic life. The melt is formed in a spiral or basket die and calibrated under vacuum in a closed water tank at 20°C to 35°C, followed by spray cooling chambers. Wall thickness is measured by ultrasonic or gravimetric haul-off after ambient conditioning. Terminal pipes are produced in SDR11, SDR13.6, and SDR17 pressure classes with outside diameters up to 630 mm for municipal mains. Hydrostatic strength is verified under ISO 1167 at 20°C/100 h/12.4 MPa, and slow crack growth resistance is checked under ISO 13479 at 80°C/4.0 MPa for a minimum of 500 h.
Buried gas distribution pipe produced from HDPE 23050 must achieve rapid crack propagation arrest under ISO 13477 S4 testing at 0°C with a critical pressure of at least 10 bar for PE100 materials. The density of 0.950 g/cm³ and the low melt index of 0.23 g/10 min contribute to high RCP resistance only when the compound contains no carbon black agglomerates above the dispersion limits in ISO 18553. Compounding uses the same 5.0–6.0 wt% carbon black masterbatch ratio; reclaimed or post-consumer polyethylene is excluded by ISO 4437-1, with only clean in-house trimmings from the same production line permitted. Extrusion is run on a grooved-feed single-screw extruder at a melt temperature of 210°C to 225°C. A melt pump between screw tip and die is used when wall thickness tolerance must be held below ±0.15 mm on outside diameters above 200 mm. The pipe is cooled in two vacuum sprays, then marked with yellow identification stripes and scanned online. Oxidative induction time at 210°C should be at least 20 min under ISO 11357-6; this threshold identifies premature stabilizer consumption before outdoor storage. Terminal products include SDR11 and SDR17.6 black PE100 gas mains up to 400 mm, tested to ISO 4437-2 and EN 1555-2. The pipe operates at a maximum operating pressure of 10 bar with a design factor of 2.0; fusion jointing is controlled by ISO 21307:2017.
| Property | Test condition | PE100 requirement | Standard |
|---|---|---|---|
| Hydrostatic strength | 20°C, 100 h, 12.4 MPa | No failure | ISO 1167 |
| Slow crack growth | 80°C, 4.0 MPa, notched pipe | ≥500 h | ISO 13479 |
| Rapid crack propagation S4 | 0°C, full-scale | Pc ≥10 bar | ISO 13477 |
| Carbon black content | pyrolysis | 2.0–2.5 wt% | ISO 6964 |
| Carbon black dispersion | microtome section | ≤ grade 3 | ISO 18553 |
In geomembrane flat-die extrusion, HDPE 23050 is blended with a carbon black masterbatch at a letdown that gives a final carbon black concentration of 2.0–3.0 wt% and a post-compounding density of at least 0.940 g/cm³. The compound is processed on a single-screw extruder with a slot die of 2,400–3,600 mm width, a melt temperature of 215°C to 230°C, and a die gap of 1.6–2.4 mm. A screen changer with 80/100/120 mesh stacked screens removes unmelted gels and carbon black agglomerates; dispersion is rated no poorer than grade 3 under ISO 18553. The extrudate is polished by a three-roll stack with roll temperatures from 70°C to 95°C and cooled gradually to reduce residual stress. Terminal sheets of 1.5 mm, 2.0 mm, and 3.0 mm are joined by hot wedge welding at a wedge temperature of 380°C to 450°C and a travel speed of 1.0 m/min to 2.0 m/min; seam peel strength is evaluated under ASTM D6392 with a minimum value of 80% of parent sheet yield. Main containment applications include landfill base liners, mining heap leach pads, and wastewater lagoon liners. Stress cracking resistance is tested under ASTM D5397; published data for HDPE 23050 in this specific configuration is limited, and batch certificates should be consulted before final specification.
Large industrial containers such as 200 L tight-head drums and 1,000 L intermediate bulk containers are produced from HDPE 23050 by extrusion blow moulding on accumulator-head machines with an extruder L/D ratio of 24:1 to 30:1 and a cooled feed zone. The melt index at 190°C/5.0 kg indicates high melt strength, but successful wall thickness control depends on parison sag and die swell. A die gap of 2.0–4.0 mm and a melt temperature of 210°C to 220°C are used; axial and radial parison programming with a 100-point controller adjusts the wall profile during continuous extrusion. Blowing air pressure is set at 0.6–0.8 MPa, and clamp force for a 200 L drum is typically 600–1,200 kN. Process windows narrow below 200°C, where flow marks and weak knit lines form at the pinch-off, and above 230°C, where sag produces a thin sidewall below the regulatory minimum for dangerous goods packagings. Terminal drums are tested under UN 1H1 and the IMDG Code; food-contact status is governed by FDA 21 CFR 177.1520(c). Drop performance at -18°C follows 49 CFR 178.603. The resin should not be combined with amine-based antistatic concentrates because amine additives can interfere with the stabilizer system during multiple regrind passes.
Installation of HDPE 23050 pipe in pressure networks uses electrofusion fittings with embedded resistance wire and a barcode-defined constant-power input. The standard fusion supply is usually 35–42 V, with fusion time adjusted according to ambient temperature; at 5°C, the jointing time is extended by 6–10% and the assembly is restrained until the interfacial melt reaches 130°C. Pipe surfaces must be scraped to remove 0.1–0.2 mm of oxidized skin before insertion into the fitting; failure to do so prevents molecular diffusion and causes peel or tensile decohesion during pressure testing. The density of 0.950 g/cm³ and low melt index of 0.23 g/10 min produce a melt that expands against the fitting and develops interfacial pressure; energy input more than 8% above the barcode recommendation can distort the fitting and reduce long-term hydrostatic strength. Joint performance is checked under ISO 13956 for internal pressure resistance and ISO 13955 for peel resistance. The completed joints are used in water and gas networks; solvent cement is never used with this material. The processing window is narrow because under-fusion and over-fusion both reduce the 50-year performance defined by ISO 12162.
Mining slurry pipeline systems use HDPE 23050 in black or UV-stabilized solid-wall pipe with wall thickness 10–30% greater than equivalent water mains because abrasion resistance depends on pipe stiffness and stress crack resistance. The pipe is extruded on a grooved-feed single-screw extruder with L/D 30:1 and a melt temperature of 210°C to 230°C, then butt-fused in the field under ISO 21307:2017. Terminal products include tailings lines, dredge floaters, and heap leach solution pipes. The limiting operational boundary is slurry velocity: for quartz sand with particles above 0.5 mm, abrasion becomes significant above 5 m/s, and the pipe should be derated or rotated every 90° of circumference. The material is not recommended for prolonged exposure to concentrated oxidizing acids above 40°C because oxidative degradation reduces hydrostatic strength. Published data for this specific configuration is limited; design should use pressure derating factors from the pipe manufacturer’s hydrostatic regression data or established site-specific wear data.
Competitive Yan'an Energy & Chemical HDPE 23050 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Yan'an Energy & Chemical HDPE 23050 is a high-density polyethylene resin produced by Yan'an Energy & Chemical Co., Ltd. on coal-to-olefins polyethylene lines in Shaanxi, China. The grade is supplied as white pellets and is intended for high-stiffness blown film, general-purpose HDPE extrusion, and selected sheet or profile applications where a low melt index of 0.23 g/10 min at 190°C/2.16 kg and a nominal density of 0.950 g/cm³ are required. Published technical data sheets list the grade as a low-flow HDPE film resin with elevated melt strength and high modulus; detailed molecular weight distribution curves are not always included in standard certificates of analysis. The resin’s low melt flow rate relative to general-purpose film grades imparts higher melt strength and deeper bubble stability in blown film, while also reducing suitability for thin-wall injection molding and rotational molding.
The table below consolidates representative values published for Yan'an Energy & Chemical HDPE 23050. The values are typical lot-averaged data and should not be interpreted as minimum or maximum specification limits unless stated in a formal certificate of analysis. Where standard designations are cited, the testing follows the corresponding ISO or ASTM procedure.
| Property | Test Method | Typical Value |
|---|---|---|
| Melt flow rate, 190°C/2.16 kg | ISO 1133-1:2022 / ASTM D1238 | 0.23 g/10 min |
| Density | ISO 1183-1:2019 / ASTM D1505 | 0.950 g/cm³ |
| Tensile stress at yield | ISO 527-2/1A/50 | 26 MPa |
| Tensile elongation at break | ISO 527-2/1A/50 | >600% |
| Flexural modulus | ISO 178 | 1050 MPa |
| Environmental stress crack resistance, 10% Igepal, F50 | ASTM D1693-21 | >100 h |
| Vicat softening temperature, A50 | ISO 306 | 124 °C |
| Brittleness temperature | ASTM D746 | < -70 °C |
| Water absorption, 24 h | ISO 62 | <0.01% |
It should be noted that melt flow rate measured according to ISO 1133-1:2022 is a single-point low-shear viscosity index. It does not fully define the shear-thinning behavior of the resin. For converters running high-shear dies, capillary rheometry according to ISO 11443 at 190°C and shear rates from 100 s-1 to 1000 s-1 may be necessary to predict die pressure accurately. Published data for this specific rheological configuration is limited in standard grade datasheets.
The density of 0.950 g/cm³ corresponds to a semi-crystalline polymer with a crystalline mass fraction typical of HDPE. This level balances stiffness and environmental stress crack resistance. Increasing density beyond 0.955 g/cm³ raises modulus and surface hardness but reduces ESCR and low-temperature impact resistance, whereas decreasing below 0.945 g/cm³ improves flexibility and dart impact but sacrifices modulus. This is why HDPE 23050 is specified for high-stiffness sacks and rigid packaging films rather than flexible films requiring high elongation.
In blown film converting, HDPE 23050 is used where thin-gauge film must retain high modulus and tolerable tear resistance. The resin can be processed as a neat HDPE film or blended with LLDPE or LDPE to adjust dart impact and tear balance. The low melt index supports stable bubble formation at blow-up ratios between 3:1 and 5:1 when the die gap is maintained between 1.4 mm and 2.0 mm. Output stability on production lines with grooved-feed single-screw extruders of 30:1 L/D and die diameters from 150 mm to 250 mm depends on controlling the frost line height at 6–10 die diameters. Excessively high frost lines can produce wrinkles and film gauge variation; excessive die gaps combined with high blow-up ratios can reduce transverse direction tear strength.
Melt temperature measured at the die is typically maintained between 190°C and 220°C. At temperatures below 180°C, the high molecular weight fraction may not fully relax, and melt fracture can appear as surface roughness at high output rates. At temperatures above 230°C, oxidative degradation may begin to shift color and reduce film properties. The extruder profile is usually set from 160°C to 220°C from throat to die, with the die lip temperature controlled at the same level as the melt. Pre-drying is not normally required for HDPE because water absorption is below 0.01% according to ISO 62; however, condensation on pellets stored at low temperature and moved into a warm production hall can introduce surface moisture that causes bubble instability. In those cases, drying at 70–80°C for 2–4 h may be applied.
Compared with LLDPE blown film, HDPE 23050 provides higher modulus and lower elongation but generally lower dart impact and machine direction tear resistance. Film converters often blend the grade with 10–30% LLDPE or LDPE to balance stiffness, dart impact, and tear strength. Published data for this specific blending configuration is limited; the exact balance must be developed on the target production line. Water vapor transmission rate is lower than for LDPE and LLDPE of the same thickness because of the higher crystalline fraction associated with a density of 0.950 g/cm³. Exact WVTR should be measured according to ASTM E96/E96M-21 or ISO 15106-1 because film gauge, temperature, and relative humidity dominate the result.
End-use segments for HDPE 23050 include high-stiffness T-shirt bags, industrial liners, heavy-duty sacks, and packaging films where low elongation and high modulus are preferred. The grade is also considered for sheet extrusion and simple profiles where melt strength assists draw-down control. Rotational molding and high-flow injection molding are not appropriate due to the low melt index.
Processing trials on high-stiffness bag lines indicate that the low melt index produces higher melt pressure and higher motor load than a 0.7 g/10 min HDPE film grade under identical screw speed and die configuration. Extruders without grooved feed sections may show feed slippage and output surging, so a grooved-feed barrel is preferred. Screen pack configurations are typically 60/80/100 mesh or equivalent, but the exact filtration level depends on film gauge and downstream converting requirements. Because the grade has elevated melt strength, bubble stability is generally better than LLDPE at equivalent film gauge, but frost line temperature and cooling air flow must be adjusted to prevent excessive orientation in the transverse direction.
Color and additive masterbatches should use HDPE-compatible carriers. Typical let-down ratios between 2% and 4% by weight are established on production-scale gravimetric dosing units, but the exact ratio depends on pigment loading and film specification. In co-extruded structures, HDPE 23050 can serve as a stiff core or surface layer with LLDPE or LDPE as sealant layers. The difference in melt viscosity between a 0.23 g/10 min HDPE and a 1.0 g/10 min LLDPE may cause layer instability if the die is not designed for viscosity mismatch. Production lines with separate extruder temperature control and die gap adjustment are preferred.
The following comparison places HDPE 23050 relative to representative HDPE film and blow molding resins. The comparison values are typical commercial ranges and do not constitute a formal specification for any named product.
| Attribute | HDPE 23050 | General-Purpose HDPE Film Grade | HDPE Blow Molding Grade |
|---|---|---|---|
| Melt flow rate, 190°C/2.16 kg | 0.23 g/10 min | 0.7 g/10 min | 0.35 g/10 min |
| Density | 0.950 g/cm³ | 0.949 g/cm³ | 0.955 g/cm³ |
| Primary conversion | blown film | blown film | extrusion blow molding |
| Melt strength | high | medium | high |
| Bubble stability at thin gauge | good | moderate | moderate |
| Thin-wall injection molding suitability | limited | moderate | moderate |
| Environmental stress crack resistance | >100 h | 50–100 h | >100 h |
The lower melt flow of HDPE 23050 differentiates it from general-purpose HDPE film grades by reducing shear thinning and increasing melt viscosity. This supports high stalk bubble configurations where the melt is drawn less aggressively and maintains a deeper air ring cooling length. In contrast, a 0.7 g/10 min general-purpose HDPE film grade would typically allow higher throughput on the same extruder but may show lower bubble stability and reduced stiffness. Against a blow molding grade of 0.35 g/10 min and 0.955 g/cm³, HDPE 23050 has a slightly lower density, which yields lower part weight for the same wall thickness but can reduce top-load strength in rigid containers.
For applications requiring contact with surfactants, oils, or weak acids, environmental stress crack resistance is often more decisive than tensile strength. The ASTM D1693-21 ESCR test under 10% Igepal with F50 failure criterion provides a comparative measure. HDPE 23050 published typical data exceed 100 h, which is suitable for many rigid packaging and industrial film applications but does not automatically qualify the grade for long-term pressure pipe service. For pressure pipe, long-term hydrostatic strength testing such as ISO 9080 and PE100 certification would be required; published data for this specific configuration is limited.
In tensile testing according to ISO 527-2/1A/50, the grade exhibits a yield stress of about 26 MPa and elongation at break above 600%. These values position it among standard high-stiffness HDPE film resins. Flexural modulus around 1050 MPa under ISO 178 supports high film rigidity, but converters should note that stiffness gains may coincide with reduced puncture and dart impact compared with LLDPE-rich formulations. The brittleness temperature below -70°C under ASTM D746 indicates low-temperature toughness in the unfilled state, but finished film performance depends on gauge, orientation, and additive package.
For barrier packaging, HDPE 23050 is not a substitute for EVOH, polyamide, or PVDC. Oxygen and carbon dioxide permeability are characteristic of semi-crystalline polyethylene and are controlled mainly by thickness and temperature. Any use requiring low oxygen transmission must be tested under ASTM D3985 or ISO 15105-2.
For food contact, HDPE 23050 may support compliance with FDA 21 CFR 177.1520 for olefin polymers and EU Regulation No 10/2011 when produced and handled under the manufacturer’s stated conditions. Compliance of the finished article depends on migration testing, additives, printing inks, and converting conditions. The resin is also subject to chemical inventory obligations under REACH and, where applicable, RoHS; converters must verify the current status with the supplier.
Storage in a dry area below 50°C is recommended; prolonged exposure to direct sunlight may cause surface oxidation and yellowing. The resin is incompatible with strong oxidizing agents, chlorinated solvents, and aromatic hydrocarbons. Continuous end-use temperatures above 60°C may reduce load-bearing capacity and should be evaluated case by case. The product should not be used in medical devices or implants without additional biocompatibility validation. No amine-based additives are involved in standard stabilization packages, but converters should confirm additive composition before use where odor and taste are critical.
When compared with HDPE grades produced via conventional naphtha-based routes, Yan'an Energy & Chemical HDPE 23050 from coal-to-olefins may contain trace hydrocarbon species characteristic of the feedstock. Published quality certificates typically report low catalyst residues and a clean pellet surface. Converters with high-speed film lines should request lot-specific ash, gel, and antioxidant data because coal-to-olefins HDPE can exhibit minor lot-to-lot variance in antioxidant concentration. The 0.23 g/10 min melt index and 0.950 g/cm³ density should be confirmed on each certificate of analysis before setting extrusion recipes.