    Specifications
    HS Code 792237
    Density 1.30 g/cm3
    Melt Flow Rate 20 g/10 min
    Melting Point 220-225 °C
    Tensile Strength 50 MPa
    Elongation At Break 50%
    Flexural Strength 80 MPa
    Flexural Modulus 2400 MPa
    Notched Charpy Impact Strength 5 kJ/m2
    Heat Deflection Temperature 60 °C at 1.82 MPa
    Vicat Softening Temperature 175 °C
    Mold Shrinkage 1.5-2.0%
    Water Absorption 0.1-0.3%

    As an accredited Xinjiang Blue Ridge Tunhe General-grade PBT TH6100 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Xinjiang Blue Ridge Tunhe General-grade PBT TH6100 is supplied in 25 kg moisture-proof bags, 40 bags per pallet (1,000 kg).
    Container Loading (20′ FCL) 20′ FCL container loaded with Xinjiang Blue Ridge Tunhe general-grade PBT TH6100 in 25 kg bags, palletized and secured for ocean shipment.
    Shipping Typically shipped as non-hazardous PBT resin pellets in 25 kg moisture-barrier bags on pallets, by standard sea or land freight. Keep dry, away from direct sunlight and contamination; no special dangerous-goods handling required.
    Storage Store Xinjiang Blue Ridge Tunhe general-grade PBT TH6100 in a cool, dry, well-ventilated warehouse, away from direct sunlight, rain, moisture, heat sources, and open flames. Keep original bags or containers tightly sealed and off the floor. Avoid contact with strong oxidizers, acids, and alkalis. Maintain good housekeeping and follow local regulations; dry before processing if moisture uptake is suspected.
    Shelf Life Store in a cool, dry, well-ventilated area in original sealed packaging; shelf life is approximately 24 months.
    Free Quote

    Competitive Xinjiang Blue Ridge Tunhe General-grade PBT TH6100 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Xinjiang Blue Ridge Tunhe General-grade PBT TH6100 is an unfilled polybutylene terephthalate resin positioned for injection moulding where medium melt viscosity, rapid crystallisation, and dimensional control are required. The grade is specified by solution viscosity rather than melt-flow alone: intrinsic viscosity is 1.00 ± 0.02 dL/g when measured in 60/40 phenol/tetrachloroethane at 25 °C under ISO 1628-5, with density of 1.31 g/cm³ under ISO 1183-1. Differential scanning calorimetry according to ISO 11357-3 gives a melting temperature normally reported at 225 ± 2 °C. As a general-grade resin, TH6100 is supplied without flame retardants, glass-fibre reinforcement, or impact modifiers; the molecular structure is a linear saturated polyester of 1,4-butanediol and terephthalic acid, which provides low equilibrium moisture uptake relative to aliphatic polyamides but retains the hydrolysis sensitivity of ester linkages. Lot-specific certificate-of-analysis limits commonly include carboxyl end groups at ≤ 30 mmol/kg and colour b-value at ≤ 1.0 using ISO 11664-4. Melt volume-flow rate for the unfilled medium-viscosity class is commonly measured at 250 °C under 2.16 kg load using ISO 1133-1:2022; the class typically falls within 15–25 cm³/10 min, but the TH6100 certificate of analysis should be used for process setup because lot-specific molecular weight can shift within the stated intrinsic-viscosity window.

    What Limits Moisture Uptake and Hydrolytic Stability in Hopper Handling?

    Because the ester linkage in PBT is susceptible to hydrolytic chain scission, residual moisture at the hopper is a first-order control on melt stability and moulded-part toughness. Pellets exposed to ambient air at relative humidity above 60 % can develop surface moisture and initiate hydrolysis during plastification; therefore, pre-drying is required before injection moulding. Industrial desiccant dryers with dry-air dew point at or below -40 °C and hopper inlet air flow of 1.5–2.0 m/s are commonly used to bring the resin to a moisture level below 0.02 % before processing. Drying at 120 °C for 4 h is typical, whereas prolonged drying at temperatures above 140 °C may cause pellet discolouration and thermal-oxidative chain scission. Moisture analysis by Karl Fischer titration should be used to confirm residual moisture rather than relying on fixed drying time alone. Hydrolysis kinetics in unmodified PBT are autocatalytic because chain scission generates carboxylic acid end groups that further catalyse ester cleavage; a single wet lot entering the screw can therefore reduce molecular weight, melt viscosity, and mechanical properties. On production-scale injection machines, batch-to-batch moisture differences have appeared as inconsistent fill pressure and surface gloss in thin-walled connector housings when hopper residence time exceeds 2 h under humid ambient conditions. For such conditions, closed hopper feeding and dry-air purge of the hopper throat are recommended. Published data for TH6100-specific hydrolysis rate constants are limited; however, the generic PBT response is well documented in polymer-stability literature.

    At the press, TH6100 is processed in the melt-temperature band of 250–260 °C, with the upper limit set by thermal degradation rather than crystallisation rate. Barrel zones are typically profiled from 230 °C in the rear feed section to 255 °C at the nozzle, with nozzle temperature maintained at 250 °C to prevent drool without freezing the melt. A mould surface temperature of 40–80 °C is used to balance crystallinity, dimensional stability, and cycle time; higher mould temperatures within this range reduce post-mould shrinkage and increase crystallinity but prolong cycle time. Injection speed is commonly set to fill the cavity within 0.8–2.5 s for wall sections of 1.0–2.0 mm; holding pressure is generally 50–70 MPa hydraulic or 40–60 % of the peak injection pressure for multi-cavity moulds. Screw rotation with low back pressure of 0.2–0.7 MPa limits frictional heating and prevents melt-temperature overshoot. These parameters are production-scale guidance derived from standard PBT injection moulding practice and should be adjusted to specific machine clamp force, nozzle geometry, and gate placement.

    Hot-Runner Residence-Time Boundaries and Thermal Degradation Signatures

    Processing faults in hot-runner and valve-gate tooling are often traced to prolonged residence time or dead spots in the manifold, because unmodified PBT enters a thermal degradation cascade when exposed to melt temperature above 260 °C for more than 8–10 min. The degradation signature includes a gradual accumulation of carboxyl end groups, loss of intrinsic viscosity, yellowing, and the evolution of volatile organic compounds that can plate on mould surfaces. In production-scale hot-runner systems with 4–16 drops, melt residence time is governed by manifold volume, shot weight, and screw recovery time. For a machine producing small connectors with a shot weight below 20 g, the ratio of manifold volume to shot volume can create residence times above the acceptable limit unless the barrel is purged between interruptions and the hot-runner temperature is reduced during standby. Thermal stability is typically checked by successive injection cycles at constant temperature while monitoring melt mass-flow rate or melt pressure variation; a shift of more than 5 % in melt pressure at fixed screw position during a 30 min hold indicates incipient degradation. Nitrogen blanketing on the hopper and hot-runner drool control assist in excluding oxygen, but PBT degradation under these conditions is primarily thermal rather than oxidative. For TH6100, published data for specific hot-runner geometries are limited; therefore, moulders should establish residence-time limits experimentally by measuring melt viscosity retention after repeated cycles under ISO 1133-1:2022.

    When TH6100 Replaces Higher-Viscosity Extrusion PBT in Thin-Wall Moulding

    TH6100 is frequently selected as a replacement for higher-viscosity extrusion PBT when filling thin-wall connectors or bobbins because the lower melt viscosity reduces injection pressure and permits longer flow lengths at reduced wall thickness. The trade-off is lower melt strength and lower notched impact resistance in thick sections; substitution should be validated by mechanical testing rather than inferred from nominal melt-flow data alone. For a wall thickness of 0.8 mm, a general-grade unfilled PBT with MVR in the 15–25 cm³/10 min band can fill a flow-length-to-wall-thickness ratio of approximately 150:1 under 120 MPa injection pressure, but this is highly dependent on gate geometry and mould temperature. In contrast, an extrusion-grade PBT with intrinsic viscosity above 1.2 dL/g may require higher melt temperature or injection pressure and may show freeze-related short shots in thin ribs. Direct substitution of TH6100 for glass-fibre-reinforced PBT is not appropriate: unfilled TH6100 exhibits lower tensile strength and lower heat distortion temperature, typically in the range of 55–60 MPa tensile strength and 60–70 °C HDT at 1.8 MPa for the unfilled class, compared with approximately 130 MPa and 205 °C for glass-fibre-reinforced PBT. The unfilled grade offers lower anisotropy, lower mould wear, and better surface appearance in parts where the loading and thermal requirements are moderate.

    Electrical connector bodies, relay housings, terminal blocks, and coil bobbins are typical conversion outlets for TH6100 because unfilled PBT combines high volume resistivity, high dielectric strength, and good dimensional stability in moulded parts. Volume resistivity for the unfilled PBT class is commonly reported at 1 × 1016 Ω·cm under IEC 62631-3-1, and dielectric strength at 18–20 kV/mm under IEC 60243-1. The material is also used in automotive sensor housings, lighting sockets, appliance switches, and fibre-optic connector components where warpage must be lower than that of glass-filled PBT. Dimensional stability after moulding is controlled by post-mould shrinkage; unfilled PBT parts can exhibit post-mould shrinkage of 0.15–0.35 % across the flow direction when annealed at 80 °C for 4 h, while glass-filled grades shrink less but show greater directional difference. For applications needing UL V-0, TH6100 must be modified with a flame-retardant system because the general-purpose unfilled grade is rated UL 94 HB in natural colour. Published data for specific connector life tests should be obtained from the end-user or compounder.

    Where TH6100 is used as a base resin for glass-fibre or mineral-filled compounds, it is processed on a co-rotating twin-screw extruder with L/D 40:1 rather than on single-screw equipment normally used for high-viscosity PBT. The base resin is fed into the main hopper and reinforcement added through a downstream side feeder to limit fibre breakage, with barrel temperatures held at 250–260 °C and screw speed adjusted to keep melt temperature below 270 °C. Strand pelletising is preferred when die-face accumulation is observed. Published data for TH6100-specific compounding on high-speed lines is limited; compounders should verify fibre wet-out and tensile strength retention after moisture conditioning under ISO 527-2.

    Property values are listed with their corresponding test-method designations below.

    Property or conditionTest method / equipment referenceTypical value or threshold
    Intrinsic viscosityISO 1628-51.00 ± 0.02 dL/g
    DensityISO 1183-11.31 g/cm³
    Melting temperatureISO 11357-3225 ± 2 °C
    Tensile strengthISO 527-255–60 MPa (unfilled PBT class)
    Flexural modulusISO 1782.3–2.6 GPa (unfilled PBT class)
    Notched Izod impactISO 180/A3–5 kJ/m² (unfilled PBT class)
    HDT at 1.8 MPaISO 75-2/A60–70 °C (unfilled PBT class)
    Volume resistivityIEC 62631-3-11 × 1016 Ω·cm (unfilled PBT class)
    Dielectric strengthIEC 60243-118–20 kV/mm (unfilled PBT class)
    Residual moisture before mouldingKarl Fischer titration<0.02 %
    Melt temperature bandMachine thermocouple / ISO 11357-3250–260 °C
    Mould surface temperatureThermocouple in tool40–80 °C

    Strongly alkaline additives, high-pH detergents, and hot-water immersion above 60 °C should be evaluated for hydrolytic attack because the ester linkages in PBT are not chemically resistant to prolonged alkali exposure. For parts operating in contact with automotive brake fluid, chlorinated solvents, or aqueous coolant at elevated temperature, material screening must include tensile property retention after fluid immersion under ISO 22088-2 or similar stress-cracking protocols. Published data for TH6100-specific chemical resistance across all fluid classes are limited; end-users should request lot-specific data or run qualification coupons on the intended tooling. Lot-to-lot variation in colour b-value and carboxyl end groups can affect melt stability and should be tracked through the certificate of analysis. The grade is intended for injection moulding and is not optimised for film extrusion, blow moulding, or foaming processes.