| HS Code | 681260 |
| Density | 0.922 g/cm³ |
| Melt Flow Rate | 0.25 g/10 min |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 24.1 MPa |
| Elongation At Break | 600% |
| Flexural Modulus | 0.248 GPa |
| Vicat Softening Point | 94°C |
| Melting Point | 110°C |
| Haze | 7% |
| Gloss | 80% |
| Coefficient Of Friction | 0.20 |
| Dart Drop Impact | 180 g |
| Elmendorf Tear Strength | 200 g |
As an accredited Westlake Hifor SC74560-F Clear Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Westlake Hifor SC74560-F Clear Polyethylene comes in 55 lb multiwall bags, supplied 40 bags per pallet (2,200 lb total). |
| Container Loading (20′ FCL) | 20′ FCL container loaded with palletized, shrink-wrapped bags of Westlake Hifor SC74560-F Clear Polyethylene, evenly distributed and secured for transport. |
| Shipping | Westlake Hifor SC74560-F Clear Polyethylene is non-hazardous and not regulated for transport by DOT, IMDG, or IATA. Ship in original sealed bags or bulk containers on secure pallets. Protect from moisture, heat, sparks, and sunlight. Handle with care, avoid punctures, and provide SDS with shipment. Store in a cool, dry area. |
| Storage | Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original containers/packages sealed, clean, and dry; protect from moisture, dust, and physical damage. Stack pallets securely to prevent deformation. Maintain ambient temperature, avoid prolonged UV exposure, use first-in, first-out rotation, follow local regulations/SDS, and do not smoke or use open flames. |
| Shelf Life | Shelf life is typically 12 months when stored in original, unopened packaging in a cool, dry, well-ventilated area away from sunlight. |
Westlake Hifor SC74560-F Clear Polyethylene enters a blown film operation through a single-screw extruder with a 25:1 to 30:1 L/D ratio and a 200 mm annular die. The processing window is controlled less by barrel temperature than by bubble cooling uniformity and melt temperature history. A dual-lip air ring delivering 4 m/s to 8 m/s air velocity and a frost line height held at 2.5 to 4 die diameters stabilize the bubble when the blow-up ratio is maintained at 2.2:1 to 3.0:1. If melt temperature exceeds 205°C for more than 5 min to 8 min, oxidative gel formation produces visible optical defects, so residence time in the adapter and die is limited to 8 min at 190°C. The formulation for fresh produce and bread bag applications uses a non-migratory silica antiblock masterbatch at 3 wt% to 5 wt% let-down ratio and a primary amide slip masterbatch at 1 wt% to 2 wt%; these ratios are adjusted only after haze and coefficient-of-friction measurements fall outside ASTM D1003 haze below 8% and ASTM D1894 kinetic coefficient below 0.35. The finished film is converted on a servo-driven bag machine running at 60 m/min to 75 m/min, sealed at 120°C to 140°C with 0.5 MPa bar pressure and 0.5 s dwell, and tested for food-contact compliance to FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011 with its 10 mg/dm² overall migration limit. Open published data specific to this exact grade in blown film is limited, so the supplier technical data sheet remains the governing input for melt index and density.
Extrusion coating of paperboard for beverage cups and frozen food folding cartons imposes a different thermal profile: the resin is extruded through a T-slot die with a die gap of 0.5 mm to 1.0 mm and drawn down to a coating weight of 12 g/m² to 25 g/m². The melt temperature at the die is raised to 315°C to 330°C to oxidize the polyethylene surface for bond formation with the board. At that temperature, residence time beyond 4 min to 6 min produces gel formation and edge neck-in instability. Drawdown is limited by melt strength; for high-clarity polyethylene, the maximum draw ratio is usually 40:1 to 60:1 before web breaks occur on a laminator running at 120 m/min. A chill roll temperature of 10°C to 18°C is maintained with a polished chrome finish of 0.1 µm Ra to prevent matte surface defects. No slip or antiblock additive is incorporated; additive addition is rejected if peel adhesion measured to TAPPI T 540 falls below the converter’s validated minimum after 24 h conditioning at 23°C and 50% relative humidity. Adhesion is anchored to a corona-treated board surface with a minimum 42 dyn/cm surface tension measured by DIN ISO 8296 test inks. The final cupstock or carton blank is tested to FDA 21 CFR 176.170(c) for aqueous and fatty food contact and TAPPI T 540 for peel adhesion at 0°C.
Because parison sag rather than melt strength controls extrusion blow molding of clear polyethylene into 50 mL to 500 mL dropper bottles and laboratory wash bottles, the tooling set points are optimized for low shear heating and short die residence. A shuttle press with 120 kN clamp force per cavity and a 0.8 mm to 1.2 mm die gap produces parison swell of 40% to 70% when melt temperature is 170°C to 190°C. Mold cooling at 8°C to 15°C and blow air pressure of 0.6 MPa to 0.9 MPa generate wall thickness in the pinch-off zone of 0.3 mm to 0.8 mm, with a machine cycle of 15 s to 20 s. The compound contains 0.1 wt% to 0.3 wt% antistatic additive to reduce dust attraction on laboratory bottles; no slip additive is included in articles intended for aqueous solutions because it raises haze above 8% measured by ASTM D1003. When the bottle is used for pharmaceutical or laboratory reagent storage, the finished article is tested to USP <661.1> and Ph. Eur. 3.1.3, and the plastic material is checked for leachable metals and antioxidants under the pharmacopeial extraction conditions. The finished articles are leak-tested at 20 kPa internal air pressure for 5 s and drop-tested at 1.2 m at −20°C in accordance with ASTM D5276.
| Application | Standard or Regulation | Critical Condition or Test |
|---|---|---|
| Blown film food packaging | FDA 21 CFR 177.1520 | Olefin polymer extractives under food simulants |
| Blown film food packaging | EU Regulation (EU) No 10/2011 | Overall migration limit 10 mg/dm² |
| Extrusion coating on paperboard | FDA 21 CFR 176.170(c) | Aqueous and fatty food contact tables |
| Extrusion coating on paperboard | TAPPI T 540 | Peel adhesion at 0°C |
| Extrusion blow molded bottles | USP <661.1> | Physicochemical packaging system evaluation |
| Extrusion blow molded bottles | Ph. Eur. 3.1.3 | Polyolefin containers heavy metals and leachables |
| Blow-fill-seal pharmaceutical containers | USP <788> | Subvisible particulate matter |
| Blow-fill-seal pharmaceutical containers | ISO 14644-1 Class 8 | Controlled environment for particle counts |
| Cleanroom medical device overwrap | ISO 11607-1 | Sterile barrier system validation |
| Cleanroom medical device overwrap | ASTM F88 | Minimum seal strength 15 N/25 mm |
Collation shrink film made from high-clarity polyethylene is produced on a two-stage air-cooled blown film line in which orientation is induced by a 2.2:1 to 3.5:1 blow-up ratio and a high frost line held at 4 to 6 die diameters. The unstretched film is converted into a collation wrap and then passed through a shrink tunnel at 110°C to 140°C. Unrestrained shrink, measured by ASTM D2732, typically falls in the range of 20% to 35% in machine direction and 8% to 18% in transverse direction at 120°C. Shrink force, measured by ASTM D2838, decays within 48 h if the film is stored above 30°C; this is an operational boundary for hot-climate warehouses. The formulation includes a silica antiblock at 2 wt% to 4 wt% masterbatch let-down and a secondary amide slip at 1 wt% to control blocking without creating seal-quality defects. The converted shrink overwrap is tested for seal strength per ASTM F88 using a 25 mm specimen and 300 mm/min jaw speed. Compliance for beverage multipacks rests on FDA 21 CFR 177.1520; no direct food contact is required for collated bottles, but the film must comply with heavy metal limits in EU Packaging Directive 94/62/EC, Article 11.
| Parameter | Blown Film | Extrusion Coating | Extrusion Blow Molding |
|---|---|---|---|
| Melt temperature | 160°C to 190°C | 315°C to 330°C | 170°C to 190°C |
| Die gap | 1.5 mm to 2.5 mm | 0.5 mm to 1.0 mm | 0.8 mm to 1.2 mm |
| Key process control | Frost line height 2.5 to 4 die diameters | Neck-in 40:1 to 60:1 draw ratio | Parison swell 40% to 70% |
| Finished article | Produce or bread bags | Coated paperboard cupstock | 50 mL to 500 mL bottles |
Blow-fill-seal processing of ophthalmic and unit-dose pharmaceutical containers from clear polyethylene places the polymer under ISO 14644-1 Class 8 or better environment because the formed container is filled immediately after mold closure. The extruder melt temperature is held between 170°C and 190°C, and the parison is inflated with 0.8 MPa to 1.0 MPa filtered compressed air. The machine’s clamp force of 80 kN to 150 kN per container station determines maximum container dimensions of 5 mL to 15 mL. Extractables from the polymer are controlled by the additive package: only a hindered phenolic antioxidant at 0.03 wt% to 0.08 wt% and a phosphite stabilizer at 0.02 wt% to 0.05 wt% are tolerated, because higher levels increase total organic carbon above the pharmacopeial limit measured by USP <643>. The sealed ampoules are tested to USP <790> for visible particulates and USP <788> for subvisible particulate matter, with pharmacopeial packaging system evaluation per USP <661.1>. Drug contact is regulated by EU Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm² and by FDA 21 CFR 177.1520. Terminal sterilization at 121°C for 15 min after filling is possible only if the container geometry avoids panel collapse because the polyethylene softens above 100°C.
Cleanroom overwrap converting uses the same base resin in a 45 µm to 65 µm monolayer film that is heat-sealed into pouches inside an ISO Class 7 cleanroom. The sealant layer must achieve a seal strength of at least 15 N/25 mm after a 0.5 s dwell at 140°C when tested to ASTM F88 with a 200 mm/min jaw speed. The film is produced on a 50 mm single-screw extruder with a 24:1 L/D ratio and a die gap of 1.5 mm; melt temperature is kept at 160°C to 180°C. No solvent-based inks or laminating adhesives are introduced, because they contribute volatile residue above the detection threshold of 0.1 mg/m². The formulation includes a non-migratory antistatic additive at 0.5 wt% to 1.0 wt% to keep surface resistivity below 1×10¹² Ω/square when measured by IEC 61340-5-1. The finished pouches are validated to ISO 11607-1 and ISO 11607-2 for sterile barrier performance, and sealing parameters are requalified after any change in film thickness greater than ±5 µm. A 25 mm peel test in a 90° fixture per ASTM F88 is used to reject packages with seal failure below 12 N/25 mm after accelerated ageing at 40°C and 75% relative humidity for 30 days.
Competitive Westlake Hifor SC74560-F Clear Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Westlake Hifor SC74560-F Clear Polyethylene is supplied as a high-clarity low-density polyethylene homopolymer for thin-gauge flexible packaging. Supplier literature typically aligns this grade with a melt flow rate near 0.75 g/10 min at 190°C/2.16 kg under ASTM D1238 and a density near 0.923 g/cm³ under ASTM D1505; lot-specific values are reported in the certificate of analysis. SC74560-F is differentiated from general-purpose LDPE film resins by a formulated slip/antiblock package, lower optical gel count, and a clarity profile intended for overwrap and produce-packaging applications. The grade should be evaluated for exact melt flow rate, density, and additive concentration before die sizing.
On 50–90 mm single-screw extruders with L/D 24:1–30:1 barrier screws, SC74560-F is processed at melt temperatures of 160–190°C. Barrel-zone set points are typically distributed as 140–160°C in zone 1, 150–170°C in zone 2, 160–180°C in zone 3, and 170–190°C at the adapter. Die temperatures are held 5–10°C above adapter temperature to reduce die-lip deposit. The recommended die gap for high-clarity LDPE is 0.8–2.0 mm; narrower gaps increase shear rate and may produce melt fracture at output rates above 1.5 kg/h per mm of die circumference. Bubble stability is maintained at blow-up ratios from 2.0:1–3.0:1, with frost line height from 5 to 8 die diameters. Internal bubble cooling lowers frost line and reduces haze, but excessive cooling below 12°C can create surface condensation and blocking. Optical quality degrades when melt temperature exceeds 205°C, because residence time above 12 min raises gel-particle formation and yellowness index. On production lines, pressure variation before the melt pump greater than 0.5 MPa is associated with gauge bands; screw speed should be adjusted to keep melt-pressure ripple below that threshold.
The shape of the melt-extrusion curve in the die land is influenced by shear rate. For high-clarity LDPE, die-land shear rates above 800 s⁻¹ can initiate sharkskin; this is lower than for butene LLDPE, which tolerates 1,200 s⁻¹ under identical die temperatures. The die land length should be 10–20 times the die gap to allow relaxation; short lands amplify extrudate surface roughness and increase haze measured under ASTM D1003. On 300 mm annular dies, gauge uniformity of ±5% requires die-lip alignment and a dual-lip air ring with adjustable lower and upper lips.
Cooling rate controls crystalline texture and optical haze. Rapid cooling on a chilled roll or low frost line produces smaller spherulites and lower haze, but excessive cooling creates surface quench marks. High-clarity LDPE film should have a frost line height between 5 and 8 die diameters; lower than 4 die diameters risks blocking, higher than 10 die diameters increases haze and reduces mechanical strength. For cast film, chill-roll temperature below 15°C can generate condensation and surface mottle; above 25°C increases haze and reduces gloss measured under ASTM D2457 at 60°.
Substituting SC74560-F into a cast film line previously set for butene-copolymer LLDPE requires a reduction in chill-roll temperature to 15–25°C and an increase in die gap to 0.5–0.8 mm. Because LDPE has a lower melt fracture threshold than butene LLDPE, line speed must be balanced against die-lip shear stress. On 25 µm film, haze is governed by quench uniformity and air-knife position; surface mottle indicates insufficient quench or excessive draw resonance. Edge trim regrind at 10–20 wt% may be reintroduced if the grind is uniform and melt temperature is not raised to compensate for viscosity variation. Film blocking is evaluated under ASTM D3354; blocking force above 50 g/10 cm typically indicates slip-agent bloom failure or excessive wound-roll tension.
SC74560-F occupies the high-clarity LDPE position in the film resin range. Unlike butene-copolymer LLDPE and metallocene LLDPE, the long-chain branch topology of LDPE provides higher melt strength and greater bubble stability in tubular extrusion, but lower tensile strength and puncture resistance. The selection decision should be based on calibrated tests rather than nominal resin class.
| Property | Standard | High-clarity LDPE SC74560-F class | General-purpose LDPE | Butene LLDPE | Metallocene LLDPE |
| Haze on 25 µm film | ASTM D1003 | 4–8% | 6–12% | 8–15% | 2–6% |
| Dart impact | ASTM D1709 | 80–150 g | 60–120 g | 150–300 g | 300–600 g |
| Tensile strength at break, MD | ASTM D882 | 20–28 MPa | 18–26 MPa | 30–45 MPa | 40–55 MPa |
| Elmendorf tear strength, MD | ASTM D1922 | 150–250 g | 100–200 g | 300–500 g | 350–600 g |
In downgauged overwrap film, replacing a butene LLDPE with SC74560-F requires an increase in film gauge of 5–10% to compensate for lower dart impact. Conversely, replacing a general-purpose LDPE with SC74560-F can reduce haze by 2–4 percentage points under the same die and cooling configuration, provided gel content is controlled. The resin is therefore suited to applications in which optical uniformity and melt strength outweigh puncture resistance.
For food-contact packaging, Westlake Hifor SC74560-F can be evaluated under FDA 21 CFR §177.1520(c) when the olefin polymer composition and end-use extraction conditions fall within the specified limitations. European direct-contact uses are evaluated under EU Regulation No 10/2011, Annex I, Table 1 with overall migration testing per EN 1186-1. Processing aids and additives must be covered by a positive list. REACH registration under Regulation (EC) No 1907/2006 and absence of Substances of Very High Concern above 0.1% w/w should be documented at lot level. The grade is not supplied for medical implant use; validation for pharmaceutical device packaging requires USP Class VI or ISO 10993 extraction data, which is not automatically provided.
Warehouse conditioning at 23±2°C and 50±5% RH is recommended for film gauge consistency. The resin should be kept in sealed containers when relative humidity exceeds 60%; condensation can generate surface defects and raise haze on thin-gauge film. Regrind use beyond 20 wt% is not recommended for high-clarity applications because gel contamination from degraded trim accumulates faster than the optical specification allows.
Optical quality in SC74560-F is governed by gel count, melt homogeneity, additive bloom, and surface roughness. Optical gel content is evaluated by visual inspection of 25 µm film against a black background; optical gel counts above 10 particles/m² larger than 200 µm are considered unacceptable for high-clarity overwrap. Melt homogeneity is verified by melt pressure stability and by the absence of visible die lines on the collapsed bubble. Die-lip deposit generated by slip-agent decomposition under high shear can transfer to the film surface and must be controlled by maintaining temperature limits and cleaning intervals.
Rheological characterization by parallel-plate oscillatory shear in 0.1–100 rad/s reveals the characteristic LDPE shear thinning and shear elasticity. Tan delta at 0.1 rad/s is lower for SC74560-F than for butene LLDPE, indicating higher melt elasticity and greater bubble stability. Coefficient of friction is measured per ASTM D1894; after 72 h aging, film-to-film COF outside 0.20–0.35 indicates slip-agent imbalance. Antiblock performance is evaluated by ASTM D3354 blocking load; blocking force above 50 g/10 cm may indicate excessive antiblock or insufficient slip bloom under high humidity. Additive bloom can also alter heat-seal initiation temperature; seal strength testing is performed under ASTM F88/F88M on 25 µm film, with seal pressure 0.3 MPa and dwell times 0.5–1.0 s.
In multi-layer films, SC74560-F is used as a sealant or clarity layer adjacent to a high-strength LLDPE or HDPE core. Coextrusion of a 10–20 µm high-clarity LDPE sealant layer onto a 30–40 µm LLDPE core maintains optical properties while increasing total dart impact. The grade may also be blended with up to 20 wt% metallocene LLDPE to improve dart impact without eliminating the LDPE-rich clarity profile; however, blending alters melt strength and bubble stability, so the film tower must be rebalanced. Published data for this specific configuration is limited; pilot-line trials on the target extruder are required to establish the haze, dart impact, and seal-initiation relationship before commercial scale-up.