Wanhua Chemical Yantai Hdpe Gc 7260

Wanhua Chemical (Yantai) HDPE GC 7260

    • Product Name: Wanhua Chemical (Yantai) HDPE GC 7260
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 276119
    Density 0.960 g/cm³
    Melt Flow Rate 7.0 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 30.0 MPa
    Tensile Elongation At Break 500%
    Flexural Modulus 1.20 GPa
    Notched Izod Impact Strength 5.0 kJ/m²
    Vicat Softening Temperature 126°C
    Melting Temperature 135°C
    Crystallization Temperature 115°C
    Heat Deflection Temperature 75°C at 0.46 MPa
    Shore D Hardness 65
    Mold Shrinkage 1.5–3.0%
    Water Absorption <0.01%
    Volume Resistivity >1×10^16 Ω·cm
    Dielectric Strength 20 kV/mm
    Dielectric Constant 2.3
    Thermal Conductivity 0.5 W/m·K
    Coefficient Of Linear Thermal Expansion 1.2×10^-4 /°C
    Flammability UL94 HB

    As an accredited Wanhua Chemical (Yantai) HDPE GC 7260 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Wanhua Chemical (Yantai) HDPE GC 7260 is packaged in 25 kg bags and 1,000 kg jumbo bags for convenient transport.
    Container Loading (20′ FCL) Wanhua Chemical (Yantai) HDPE GC 7260 in 25 kg bags, palletized, shrink-wrapped, loaded in 20′ FCL, about 17 MT net.
    Shipping Wanhua Chemical (Yantai) HDPE GC 7260 is shipped as non-hazardous polyethylene pellets in 25 kg PP woven bags or 1,000 kg jumbo bags, palletized and stretch-wrapped. Transport by truck, rail, or sea in clean, dry containers. Store cool, dry, ventilated, away from sunlight, moisture, and ignition sources.
    Storage Store Wanhua Chemical (Yantai) HDPE GC 7260 in a cool, dry, well-ventilated warehouse. Keep sealed in original packaging, palletized, and off the floor. Protect from direct sunlight, heat, moisture, and contamination. Avoid strong oxidizers, acids, bases, and ignition sources. Do not expose to open flames or excessive temperatures. Maintain safe stacking, inspect packaging regularly, and follow manufacturer’s shelf-life and local storage regulations.
    Shelf Life Wanhua Chemical (Yantai) HDPE GC 7260: two-year shelf life if stored cool, dry, ventilated, and away from direct sunlight.
    Application of Wanhua Chemical (Yantai) HDPE GC 7260
    Wanhua Chemical (Yantai) HDPE GC 7260 is an injection-moulding high-density polyethylene with a nominal melt mass-flow rate of 7.2 g/10 min determined under 190°C and 2.16 kg load in ISO 1133-1:2022, and a density of 0.960 g/cm³ by ISO 1183-1:2019. The melt-flow profile positions the resin in high-cavitation, short-cycle rigid packaging where shear rates at the gate exceed 1,000 s⁻¹ and where the melt-flow length to wall-thickness ratio commonly reaches 150:1 to 220:1. Application coverage is limited to injection-moulded HDPE end-uses observable in established downstream value chains; blow-moulding, film, sheet extrusion, and pipe-grade substitutions are excluded because the molecular architecture and melt-flow profile do not support those conversion routes.
    Compliance checklist for HDPE GC 7260 downstream application segments
    SegmentStandard / regulationRelevant test method or clauseThreshold or condition
    Thin-wall food containersEU 10/2011, 21 CFR 177.1520(c) 2.1, GB 4806.7-2016Overall migration per EN 1186-3:2002; density per ISO 1183-1:201910 mg/dm² overall migration; aqueous or dairy simulant
    Beverage closuresEU 10/2011, 21 CFR 177.1520(c), GB 4806.7-2016Torque retention ASTM D2063; seal integrity ASTM D3078Strip torque 0.8–1.7 N·m for 28 mm PCO; no leak at -20 kPa
    Returnable cratesREACH Annex XVII, EU 10/2011 where direct food contact occursCharpy notched ISO 179-1/1eA; multiaxial ISO 6603-2Charpy impact ≥ 4 kJ/m² at 23°C
    Cosmetic packagingEU 1223/2009, REACH, USP <661.1>Plastic class identification by infrared; heavy metals per USP <231>No SVHC > 0.1 wt%; PE class confirmed
    Domestic storageREACH, EN 71-3 where toy-accessible claim existsElement migration by EN 71-3:2019Category-dependent migration limits
    Industrial pail lidsUN Model Regulations, ISO 16103:2005Drop test UN 6.1.5.3; stack test ISO 2234Packing Group II drop height 1.2 m; no rupture
    At wall thicknesses between 0.45 mm and 0.80 mm, the flow path in a multi-cavity thin-wall dairy tub tool exceeds 180 mm from the hot-tip gate to the rim, producing a flow-length-to-wall-thickness ratio above 200:1. In this regime, the high melt-flow of GC 7260 shifts the limiting defect from short-shot to rim flash and gate blush, so injection velocity is set by cavity pressure rather than melt temperature alone. Field operation on accumulator-driven thin-wall machines with clamp force between 250 t and 450 t typically uses melt temperature 220–240°C, mould cooling water at 10–18°C, and injection pressure at the screw tip of 90–130 MPa; cavity sensors are maintained at 35–50 MPa during filling and 20–30 MPa during holding. The screw cushion is held at 3.0–5.0 mm because a cushion below 2.0 mm produces shot-weight variation and inconsistent part mass after decompression. The formulation is 97.0–98.0 wt% virgin GC 7260 with 2.0–3.0 wt% titanium dioxide-loaded white masterbatch, and closed-loop regrind is allowed up to 20 wt% only where the food-contact layer is separated or where the converter can document compliance with EU 10/2011 overall migration below 10 mg/dm² under the intended dairy or spread simulant. The downstream production process is high-speed injection moulding followed by automated stacking in chilled air tunnels for 90–120 s; terminal finished articles include 125–500 mL thin-wall dairy tubs, portion cups, rectangular deli containers, and friction-fit lids.

    Which Closure Performance Constraints Govern High-Speed Injection of HDPE GC 7260?

    In high-cavity closure tools, the limiting defect is not short-shot but inconsistent bridge tear-away torque after the tamper-evident band is moulded. GC 7260 is processed on high-speed injection moulding machines with 48- to 96-cavity hot-runner stack moulds; the valve-gate manifold is balanced to hold inter-cavity temperature spread below ±5°C, because a 5°C rise at the gate shortens melt-cooling time and produces ovality in the thread start. Melt temperature is set at 210–230°C, mould temperature at 12–20°C, holding pressure between 40 MPa and 60 MPa, and cycle times of 6–9 s. Screw decompression after plasticising is limited to 3–5 mm; larger suck-back pulls air through the hot runner and causes splay at the gate vestige. The addition ratio for beverage closures is 100 wt% GC 7260 with erucamide at 400–800 ppm for PCO 28 mm screw caps; for non-fatty dry product closures the slip level is raised to 1,000–1,200 ppm, while colour masterbatch remains 1.0–2.0 wt%. The compliance framework includes EU 10/2011, FDA 21 CFR 177.1520(c), and China GB 4806.7-2016; torque retention is tested by ASTM D2063, and seal integrity by vacuum leak at -20 kPa for carbonated beverage applications. Terminal finished product types include PCO 28 mm and 38 mm tamper-evident bottle caps, flip-top dispensing closures, and child-resistant closures where the outermost body is polyethylene.

    When Returnable Logistics Crates Require Impact Strength Above 4 kJ/m²

    The operational conflict in returnable crate production arises from the opposing requirements of high-cavitation productivity and thick-section impact strength. GC 7260 is injection-moulded in open-side crates with wall thicknesses of 2.5–4.0 mm and rib intersections reaching 6.0 mm; the high melt-flow resin fills at lower pressure, but high flow alone reduces packing control at rib roots, where sink marks form if the holding-pressure decay is faster than 2 MPa/s. On production lines with hydraulic toggle clamps from 500 t to 1,000 t, melt temperature is controlled at 220–250°C, mould temperature at 15–35°C, and holding pressure at 60–80 MPa for 12–20 s before cooling. A stepped holding profile is frequently used, with 80 MPa applied for the first 3 s and 50 MPa for the remaining packing phase, to suppress rib-root sink without increasing cycle time. The formulation for indoor logistics crates is 70–100 wt% GC 7260 with up to 30 wt% closed-loop regrind; for outdoor exposure, a hindered-amine light stabilizer masterbatch is added at 2.0–3.0 wt% and carbon black at 2.0–2.5 wt%, consistent with REACH Annex XVII restrictions on polycyclic aromatic hydrocarbons. Impact performance is specified by ISO 179-1/1eA Charpy notched values above 4 kJ/m² at 23°C and ISO 6603-2 multiaxial impact at -10°C; compliance for returnable food crates additionally references EU 10/2011 where the crate contacts unpackaged vegetables. Downstream production processes include sequential cavity-pressure-controlled injection, post-mould thermal jigs for flatness correction, and inbound RFID tag insertion for logistics trackability. Terminal articles are returnable bottle crates, bakery trays, vegetable harvest crates, distribution totes, and pallet-hanging side rails.

    Mould-Filling Behaviour in Cosmetic Jar and Airless Pump Platforms

    Surface replication and gate blush are the primary defects in cosmetic side-wall moulding, where the visible surface cannot be hidden by a label. GC 7260 is run in single-face, multi-cavity cosmetic tools with polished A-side steel; mould temperature is raised to 30–40°C to prevent flow-mark freeze-off, while melt temperature is kept at 210–230°C to minimise thermal degradation of pearlescent masterbatch at 1.0–2.0 wt%. Filling is performed at moderate injection speeds with screw positions profiled to prevent jetting; cavity pressure at switchover is 25–35 MPa, and holding pressure is 30–50 MPa for 6–10 s. The addition ratio is 98.0–99.0 wt% GC 7260, with the remainder being colour masterbatch or a slip-additive masterbatch limited to 0.5–1.0 wt% where cap-to-jar opening torque must remain below 2.0 N·m. The compliance framework includes EU 1223/2009 for cosmetic product packaging, REACH SVHC screening below 0.1 wt%, and USP <661.1> for plastics used in personal-care product contact; published data for this specific grade in airless pump housing applications is limited, so validation relies on torque retention by ASTM D2063 and dimensional stability after 48 h at 40°C. Terminal finished product types include cosmetic jars, airless pump outer housings, compact cases, and loose-powder containers.

    Differential Cooling, Not Pack Pressure, Determines Flatness in Domestic Storage Lids

    For non-food domestic storage baskets, bin lids, and garment hangers, GC 7260 is processed in standard cold-runner injection moulds at melt temperatures of 200–230°C with a 1.0–2.0 wt% colour masterbatch and up to 30 wt% internally generated regrind, screened under REACH SVHC and, where the article is claimed as toy-accessible, EN 71-3 migration limits; the production constraint is warpage from differential cooling in long flat sections, which is controlled by maintaining core/cavity temperature spread below 10°C rather than by increasing pack pressure, and terminal articles are storage bins, under-bed boxes, hangers, and stackable utility boxes.

    What Limits Dimensional Stability in Injection-Moulded Industrial Pail Lids?

    Pail lid moulding shifts the difficulty from filling to cooling-induced elliptical distortion over diameters greater than 250 mm. GC 7260 is moulded in 2.5–3.0 mm thick lids with outer diameters from 250 mm to 350 mm for open-head steel and plastic pails; the process uses sequential hot-runner valve gates and cavity pressure sensors to balance filling across the central sprue field, with melt temperature at 230–250°C, mould temperature at 20–35°C, holding pressure of 50–70 MPa, and cooling time of 25–35 s. The formulation is 100 wt% GC 7260 for unpigmented lids, or 98.0–99.0 wt% with carbon black masterbatch at 1.0–2.0 wt% for UV-marked industrial pails; regrind is limited to 20 wt% where dimensional stability after stack testing must be documented. Compliance for dangerous goods pails follows UN Model Regulations Chapter 6.1 with drop test at 1.2 m for Packing Group II solids, ISO 16103:2005 for rigid plastics packaging, and stack load per ISO 2234. The operational boundary is that post-mould shrinkage of 1.5–2.0% requires lids to be flat-tested after 24 h conditioning at 23°C and 50% RH; terminal finished product types include gasketed pail lids, tamper-evident covers, and screw-top lids for UN-certified open-head pails.
    Free Quote

    Competitive Wanhua Chemical (Yantai) HDPE GC 7260 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Wanhua Chemical (Yantai) HDPE GC 7260 is a high-density polyethylene resin positioned within the manufacturer’s polyolefin range for extrusion blow molding of industrial packaging and rigid containers. The product is supplied as pellets and is typically identified on the certificate of analysis by its melt flow rate, density, and lot-specific mechanical property results. Representative values for the grade include a melt flow rate of 0.72 g/10 min when determined at 190 °C under 2.16 kg load in accordance with ISO 1133-1, and a density of 0.956 g/cm³ when tested under ISO 1183-1. These values place HDPE GC 7260 in the high-molecular-weight, high-density segment for blow molding, where melt strength and environmental stress crack resistance are more critical than maximum throughput or short injection cycle time. The grade is not designed for injection molding or thin-gauge film, and substitution into those processes can produce melt fracture, excessive parison drawdown, or insufficient flow to fill thin-wall tools.

    Applications are concentrated in extrusion blow molding of containers and technical parts with wall thickness from 1.5 mm to 5 mm and part volumes from 5 L to 25 L, including jerry cans, automotive fluid reservoirs, agrochemical containers, and industrial packaging that requires resistance to aggressive liquid media. The material selection is supported by its environmental stress crack resistance of more than 600 h under ASTM D1693-B, 100% Igepal, F50 conditions, which is a requirement for containers holding surfactants, oils, or mild solvents. The notched Charpy impact strength at 23 °C of 14 kJ/m² according to ISO 179-1/1eA contributes to drop-impact performance for filled containers, although final drop-test requirements should be validated on the actual container geometry and filling weight.

    What standardized property set defines HDPE GC 7260 for extrusion blow-molding design?

    Design validation for rigid packaging and industrial containers requires a defined mechanical and thermal property set. The following representative values are published for HDPE GC 7260; they are not release limits and should be confirmed against the lot-specific certificate of analysis.

    PropertyTest methodTypical valueUnit
    Melt flow rate (190 °C, 2.16 kg)ISO 1133-10.72g/10 min
    DensityISO 1183-10.956g/cm³
    Tensile stress at yieldISO 527-227MPa
    Tensile elongation at breakISO 527-2>600%
    Flexural modulusISO 1781200MPa
    Charpy notched impact strength, 23 °CISO 179-1/1eA14kJ/m²
    Environmental stress crack resistance, 100% Igepal, F50ASTM D1693-B>600h
    Vicat softening temperature, A50ISO 306127°C
    Hardness Shore DISO 86864—

    The combination of 0.956 g/cm³ density and 0.72 g/10 min melt flow rate is central to the material’s behavior. The density provides high flexural modulus and top-load strength, while the relatively low melt flow rate limits parison sag on large accumulator-head tools. In thick-wall industrial containers, this balance is preferred over higher-flow HDPE grades because it allows repeated parison programming without losing dimension stability. The tensile stress at yield of 27 MPa gives a defined short-term load-bearing limit under ISO 527-2, but creep and chemical exposure must be evaluated separately when long-term deformation is a risk.

    On extrusion blow-molding equipment, the processing window for HDPE GC 7260 should be established with respect to the actual screw design, accumulator volume, and die gap programming. Published resin-specific machine settings for this configuration are limited; industrial practice for HDPE with a melt flow rate near 0.72 g/10 min commonly begins with barrel temperatures from 180 °C to 220 °C, head and die temperatures from 200 °C to 220 °C, and mold cooling temperatures from 10 °C to 30 °C. Barrel zones should be profiled to avoid local overheating above 230 °C, which can reduce melt viscosity and create parison hang-time variability. Excessive melt temperature in the accumulator head can also lower the environmental stress crack resistance of the molded part because degradation increases carbonyl concentration and embrittles the inner parison surface. Accumulator-head machines with screw diameters from 60 mm to 90 mm and L/D ratios near 24:1–30:1 are typical for this grade’s viscosity range, although continuous shuttle machines may also process it when parison weight is below 5 kg.

    Unlike hygroscopic engineering resins, HDPE GC 7260 does not require predrying for normal closed-warehouse storage. If surface condensation occurs after transfer from cold storage, a hopper dryer at 80 °C for 1–2 h may be used to prevent surface splay and melt flow instability. The mold surface should be cooled uniformly; a temperature differential across the pinch-off region can generate residual stress at the weld line and reduce burst resistance. During start-up, purging with a lower-viscosity polyolefin and then transitioning to HDPE GC 7260 reduces the risk of gel particles and black specks in the first production containers. On production lines, batch-to-batch variance in melt flow rate is commonly observed within ±0.05 g/10 min when release testing is performed at 190 °C and 2.16 kg. A shift toward the upper end of the melt flow range can require a reduction in head temperature by 5–10 °C to avoid parison sag, while a shift toward the lower end may require an increase in die gap of 0.1–0.3 mm to maintain target parison thickness.

    When the grade is specified for blow-molded industrial packaging, how does it differ from other HDPE classes?

    HDPE GC 7260 occupies a different flow and stiffness position than film, injection molding, and pipe grades. Compared with high-density polyethylene film grades that typically exhibit melt flow rates below 0.15 g/10 min, HDPE GC 7260 has a higher melt flow rate that permits higher extrusion throughput in blow molding while retaining sufficient melt strength for moderate parison lengths. Compared with injection-molding HDPE grades with melt flow rates above 10 g/10 min, the 0.72 g/10 min flow of HDPE GC 7260 is more resistant to drawdown and sag but slower to fill thin-wall, long-flow-length injection tools. The viscosity difference is directly measurable through ISO 1133-1 melt flow rate and through shear-viscosity testing on capillary rheometers; higher-flow injection grades require lower injection pressure for thin-wall geometries, while HDPE GC 7260 is intended for thicker-wall blow-molded cross sections.

    Against general-purpose blow-molding HDPE grades with density near 0.952 g/cm³, HDPE GC 7260 has a higher density of 0.956 g/cm³ and correspondingly higher flexural modulus of 1200 MPa, which translates into improved top-load capacity in standardized compression testing. The trade-off is a reduction in low-temperature impact absorption; grades with lower density and higher comonomer content can exhibit Charpy notched impact values above 20 kJ/m² at −30 °C, while HDPE GC 7260 is normally specified for service at ambient or mildly subzero temperatures. The environmental stress crack resistance above 600 h under ASTM D1693-B is nevertheless elevated for a grade of this density and is the primary differentiator when compared with high-stiffness injection HDPE grades, which may fail below 50 h in the same ESCR test because of narrower molecular architecture and higher density.

    Compared with pipe-grade HDPE designed for long-term hydrostatic strength under ISO 9080, HDPE GC 7260 is not suitable for pressure piping because its melt flow rate and comonomer distribution are not aligned with PE100 requirements. Certification to ISO 4427 requires long-term hydrostatic strength evaluation at 20 °C and 80 °C for 10,000 h, which is outside the intended use of this blow-molding grade. For containers above 25 L, a lower-melt-flow HDPE with higher parison hang strength may be required, especially in single-head accumulator machines where parison length exceeds 800 mm and gravitational drawdown becomes the controlling variable.

    Compliance evaluation matrix and lot-release property checks

    For materials management and incoming inspection, the following matrix summarizes the evaluation pathways used for unfilled HDPE GC 7260. The matrix is not a substitute for the certificate of analysis or regulatory clearance for the final article.

    AssessmentReferenced method or regulationTypical acceptance criterion
    Melt flow rateISO 1133-10.72 ± 0.05 g/10 min or producer lot tolerance
    DensityISO 1183-10.956 ± 0.002 g/cm³
    Environmental stress crack resistanceASTM D1693-B, 100% Igepal, F50>600 h
    Food-contact statusFDA 21 CFR 177.1520Conforms to olefin polymer specifications subject to end-use extraction limits
    EU chemical safetyREACH 1907/2006SVHC communication below 0.1% w/w
    RoHS restricted heavy metalsIEC 62321, RoHS 2011/65/EUCd 100 mg/kg, Pb 1000 mg/kg, Hg 1000 mg/kg, Cr(VI) 1000 mg/kg

    For compliance evaluation, HDPE GC 7260 is subject to the polyolefin regulatory framework. The resin can be assessed under European Union REACH Regulation 1907/2006 for substance registration and authorization obligations; the supplier is required to communicate the presence of substances of very high concern above 0.1% w/w through the safety data sheet. Under United States food-contact use, high-density polyethylene complying with 21 CFR 177.1520 may be permitted for contact with food, subject to end-use limitations based on density, extraction tests, and conditions of use; final food-contact approval must be confirmed for the specific packaging structure and food type. Under RoHS Directive 2011/65/EU, unfilled polyethylene grades are not expected to contain the restricted heavy metals above threshold levels, but compliance should be verified through production lot testing for cadmium, lead, mercury, and hexavalent chromium. The grade is typically supplied without intentionally added perfluorinated or polyfluorinated processing aids; if such additives are used in downstream masterbatch or purge compounds, regulatory status must be re-evaluated.

    Operational boundaries for HDPE GC 7260 are determined by the polymer’s thermal and chemical stability. The resin should not be processed above 230 °C for extended residence times, and it should not be purged with acidic or oxidizing purge compounds that can generate carbonyl species and reduce ESCR. It is incompatible with strong oxidizing acids such as concentrated nitric acid and should not be used for long-term storage of chlorinated solvents above 50 °C without specific permeability and stress-crack testing, because solvent vapor penetration can initiate environmental stress cracking at molded-in stress points. The product is not recommended for direct sustained exposure to ultraviolet radiation in outdoor service unless formulated with 2–3% carbon black or an equivalent UV stabilizer package, since unstabilized HDPE undergoes chain scission and embrittlement under extended UV exposure. For containers requiring food-contact approval, migration testing under EU Regulation 10/2011 or FDA 21 CFR 177.1520 must be performed on the final article because processing aids, pigments, and multilayer structures can alter overall migration and specific migration limits.

    Top