Wanhua Chemical Yantai Hdpe 7000f

Wanhua Chemical (Yantai) HDPE 7000F

    • Product Name: Wanhua Chemical (Yantai) HDPE 7000F
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 558024
    Density 0.954 g/cm³
    Melt Index 190 C 2 16 Kg 0.07 g/10 min
    Tensile Strength At Yield 26 MPa
    Tensile Strength At Break 35 MPa
    Elongation At Break 600%
    Flexural Modulus 1100 MPa
    Vicat Softening Temperature 124°C
    Melting Temperature 133°C
    Brittleness Temperature ≤ -70°C
    Environmental Stress Cracking Resistance >1000 h
    Molecular Weight Distribution Narrow
    Ash Content ≤0.05%
    Moisture Content ≤0.1%
    Bulk Density 0.55-0.60 g/cm³
    Form Pellets
    Color Natural
    Processing Method Blown film extrusion

    As an accredited Wanhua Chemical (Yantai) HDPE 7000F factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Wanhua Chemical (Yantai) HDPE 7000F is packed in 25 kg woven bags, 40 bags (1,000 kg) per pallet.
    Container Loading (20′ FCL) Wanhua Chemical (Yantai) HDPE 7000F in 20′ FCL: 25 kg bags, approximately 18 MT, securely loaded for export shipment.
    Shipping Wanhua Chemical (Yantai) HDPE 7000F is shipped from Yantai, China, in 25 kg woven bags or 500–1000 kg jumbo bags. It is non-hazardous general cargo, palletized, stretch-wrapped, and transported in dry containers/trucks. Keep dry, ventilated, and protected from sunlight, heat, and moisture. Handle with care; avoid punctures and UV exposure.
    Storage Store Wanhua Chemical (Yantai) HDPE 7000F in original sealed bags/packaging in a cool, dry, well-ventilated warehouse. Protect from direct sunlight, moisture, heat, and ignition sources. Keep away from strong oxidizers and contaminants. Stack pallets securely; avoid crushing. Use first-in, first-out inventory. Store at ambient temperature, away from open flames and static discharge. Reseal partly used bags.
    Shelf Life Under cool, dry, ventilated storage in original sealed packaging, shelf life is typically 24 months; avoid direct sunlight and moisture.
    Application of Wanhua Chemical (Yantai) HDPE 7000F
    On a high-stalk blown film line, Wanhua Chemical (Yantai) HDPE 7000F is introduced to the extruder feed throat after blending with slip and antiblock masterbatch. The extruder is a 90 mm single-screw unit with a grooved feed section and L/D ratio of 30:1. Melt temperature is maintained at 195–205 °C. The die is a 200 mm spiral mandrel die with a die gap of 1.4 mm. The blow-up ratio is set at 3.5:1 and the frost line height is held at 10 die diameters. These settings impose a high-stalk bubble geometry that produces balanced orientation in the machine and transverse directions. Film thickness is normally 20–25 µm. Tensile properties are evaluated by ISO 527-3:2018. Dart impact resistance is measured by ISO 7765-1:1988. Elmendorf tear resistance is measured by ISO 6383-2:1983. Slip additive concentration is 500–900 mg/kg erucamide. Antiblock is 2,000–4,000 mg/kg synthetic silica. Polymer processing aid is 300–500 mg/kg fluoroelastomer. The terminal structure is a vest carrier sack. Compliance is required with EU Directive 94/62/EC for packaging waste and REACH Annex XVII restrictions for phthalates and heavy metals. On production lines, bubble instability appears when the frost line is moved above 12 die diameters because melt strength drops and gauge variation exceeds ±2 µm. Batch-to-batch MFR variation is monitored because it shifts bubble stability at fixed screw speed, and producers issue certificates of analysis that include density by ISO 1183-1:2019 and melt mass-flow rate by ISO 1133-1:2022 at 190 °C/2.16 kg.

    What Limits Gauge Uniformity in Heavy-Duty Refuse Sack Extrusion?

    HDPE 7000F is also run in monolayer thick-gauge refuse sack and debris liner applications at 70–150 µm. On the same 90 mm grooved-feed extruder, the die gap is widened to 1.8–2.2 mm because thicker film requires lower internal pressure drop and reduced melt fracture. Blow-up ratio is reduced to 2.5:1–3.0:1 and the bubble is run as a low-stalk configuration. The frost line is kept at 5–7 die diameters. Melt temperature is raised to 200–210 °C to reduce viscosity without losing bubble stability. Carbon black masterbatch is added at 2.0–2.5 wt% for UV resistance and opacity. Hindered amine light stabilizer is incorporated at 0.1–0.3 wt% for long-term exterior exposure. Extrusion screws with intermediate mixing sections are used to disperse the masterbatch. Gauge variability is monitored by online capacitive or beta thickness gauges. Tensile strength is tested by ISO 527-3:2018. Puncture resistance is evaluated by ISO 7765-1:1988. Environmental stress-crack resistance is measured by ASTM D1693-21, method B. The terminal products are 120 L heavy-duty refuse sacks, construction waste bags, and industrial scrap liners. Concentration limits for lead, cadmium, mercury, and hexavalent chromium in packaging are controlled to 100 mg/kg per EU Directive 94/62/EC. Pre-drying is not required under normal ambient storage, but if regrind content exceeds 15 wt%, hopper drying at 65–70 °C for 2 h is recommended to avoid surface moisture defects.Three-layer coextrusion lines set the HDPE 7000F layer as the core or outer layer for moisture-stiffening in dry food packaging. The layer ratio is normally 25/50/25 or 30/40/30 by gravimetric output. The HDPE layer is processed at 190–205 °C. The sealant layer is a metallocene LLDPE run at 170–190 °C. The tie layer is an anhydride-modified polyethylene run at 185–200 °C. The die gap is 1.6–1.9 mm and the blow-up ratio is 2.8:1. Total film thickness is 40–70 µm. The HDPE layer contributes bending stiffness and water-vapour resistance. The LLDPE sealant layer contributes hot-tack and seal initiation. Seal strength is measured by ASTM F88/F88M-21. Hot tack is measured by ASTM F1921-18. Water vapour transmission rate is measured by ASTM E96-22 desiccant method. Food contact compliance is established under FDA 21 CFR 177.1520(c) for olefin polymers, EU Regulation 10/2011 with an overall migration limit of 10 mg/dm², and GB 4806.7-2016 for food-contact plastics. The terminal products are cereal box liners, dry soup pouches, and bakery film. On coextrusion lines, layer-thickness variation is checked by gravimetric hopper feedback. Deviations in the HDPE core beyond ±1.5% cause curling during bag-making and inconsistent web tension.
    Comparative blown film process windows for three downstream structures using HDPE 7000F
    StructureDie gap (mm)Blow-up ratioMelt temperature (°C)Film gauge (µm)Primary test standard
    Vest carrier sack1.43.5:1195–20520–25ISO 7765-1:1988
    Heavy-duty refuse sack1.8–2.22.5:1–3.0:1200–21070–150ISO 527-3:2018
    Coextruded dry food film1.6–1.92.8:1170–20540–70ASTM F88/F88M-21

    When Frozen Food Packaging Requires Dart Impact Retention at −20°C

    Plain HDPE 7000F film can become brittle at freezer temperatures, so processors dilute the HDPE phase with 10–30 wt% ULDPE or metallocene LLDPE to preserve low-temperature impact strength. The blend is compounded in the extruder with a mixing screw and processed on a three-layer blown film line. The die gap is set at 1.5–1.8 mm. The blow-up ratio is 2.5:1–3.0:1. The frost line is lowered to 4–6 die diameters to reduce frozen-in orientation. Melt temperature is kept at 190–200 °C to minimize thermal degradation during blending with higher-MFR ULDPE. The film is tested for dart impact at 23 °C and −20 °C by ASTM D1709-22, method A. Tensile properties at low temperature are evaluated by ASTM D882-18. The terminal products are frozen vegetable pouches, IQF seafood sacks, and ice bag liners. For food-contact use, the blend must meet FDA 21 CFR 177.1520(c) and EU Regulation 10/2011 overall migration limits. Use of slip and antiblock is restricted to 300–600 mg/kg erucamide and 1,000–2,000 mg/kg silica to avoid blocking at low ambient humidity. In low-temperature sealing operations, the LLDPE phase delivers seal initiation below 90 °C, while the HDPE phase maintains mechanical strength. Avoid direct combination with polypropylene above 5 wt% because phase incompatibility reduces film clarity and tear propagation resistance.

    Vapour-Control Membrane Production from High-Molecular-Weight Film Resin

    HDPE 7000F is used as the base polymer for building vapour-control membranes and radon barriers where low water vapour transmission is required. The resin is fed with a carbon black masterbatch at 2.0–2.5 wt% and a UV stabilizer masterbatch at 0.2–0.3 wt%. Film is produced on a blown film line with a die gap of 2.0–2.5 mm, blow-up ratio of 2.0:1–2.5:1, and melt temperature of 200–210 °C. The film gauge is 200–500 µm. Water vapour transmission rate is measured by ASTM E96-22 desiccant method. Tensile properties are measured by ASTM D882-18. Puncture resistance is measured by ASTM D4833-21. The terminal product is a damp-proof membrane or radon barrier installed under concrete slabs. Compliance is established under CE marking and EN 13984:2013 for plastic vapour-control sheets. The carbon black loading must be uniform. Pinholes caused by poor carbon black dispersion are detected by high-voltage spark testing on-line at 20–30 kV. Extruder zones above 220 °C are limited to residence times below 5 min to avoid oxidative gel formation. Published data for this specific configuration is limited, so processors validate membrane performance against project-specific water vapour resistance calculations rather than relying on generic film datasheets.
    Free Quote

    Competitive Wanhua Chemical (Yantai) HDPE 7000F prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Wanhua Chemical (Yantai) HDPE 7000F is a high-molecular-weight, high-density polyethylene blown-film extrusion resin manufactured at the Yantai petrochemical complex. The grade belongs to the HMW-HDPE class by virtue of a nominal melt mass-flow rate of 0.04 g/10 min under ISO 1133-1:2022 at 190 °C/2.16 kg and a nominal density of 0.956 g/cm³ determined by ISO 1183-1:2019. Manufacturer-reported typical tensile data place yield strength at 28 MPa and elongation at break above 600 % when tested according to ISO 527-2:2012 type 1B. The low melt index produces a stable high-stalk bubble on high-torque grooved-feed blown-film extruders and separates the grade from lower-viscosity HDPE extrusion-coating, monofilament, or injection-molding resins.

    The resin is supplied as lenticular pellets with a density above the 0.941 g/cm³ threshold for high-density polyethylene under ASTM D4976. Principal applications are concentrated in thin-gauge film between 0.010 mm and 0.060 mm for carrier bags, refuse sacks, industrial liners, folded film, and stiff outer layers in coextruded structures. No predrying is required at storage relative humidity below 50 %; at higher humidity the pellet surface moisture limit is 0.05 wt%.

    PropertyTypical valueTest standard
    Melt mass-flow rate0.04 g/10 minISO 1133-1:2022, 190 °C/2.16 kg
    Density0.956 g/cm³ISO 1183-1:2019
    Tensile yield strength28 MPaISO 527-2:2012, type 1B, 50 mm/min
    Tensile elongation at break>600 %ISO 527-2:2012, type 1B

    What Limits Melt Stability During Blown Film Extrusion?

    On production-scale single-screw extruders with L/D 25:1 to 30:1 and grooved feed sections, HDPE 7000F develops high melt viscosity and elevated head pressure. Barrel temperatures are typically profiled from 180 °C in the feed zone to 210–220 °C at the adapter and die. Melt temperature at the die entry should not exceed 220 °C for extended runs: above 240 °C thermo-oxidative chain scission reduces melt strength, increases melt index, and causes bubble sag. The preferred die gap is 1.2–1.8 mm, and the blow-up ratio is usually set between 3.5:1 and 5.0:1 to balance machine-direction and transverse-direction tensile properties tested under ISO 527-3:2018.

    Frost-line height is customarily maintained at 8–12 die diameters. Frost-line heights below 8 die diameters reduce transverse tear strength measured by ASTM D1922-23; heights above 12 die diameters increase film stiffness and can destabilize the bubble under plant air currents. On high-output lines the cooling air-ring capacity, not extruder torque, is usually the limiting factor. A 75 mm grooved-feed extruder operating at 60–90 min⁻¹ screw speed may generate die-head pressure in the range 35–45 MPa, which is near the upper continuous torque rating of standard gearboxes. Pressure fluctuations of more than 3 MPa at the screen changer indicate melt-quality disturbance, excessive regrind, or unstable feed-zone temperature.

    Pellet surface moisture above 0.05 wt% from storage at relative humidity above 60 % requires hopper drying at 80–90 °C for 2–3 h. Surface moisture causes bubble pinholes and frost-line oscillation; it is not a bulk-moisture problem because HDPE has low equilibrium moisture absorption. High-film-output operations should verify melt-temperature uniformity with an immersion probe at the die entry because shear heating can create local temperature spikes of 10–15 °C above the set-point at screw speeds above 90 min⁻¹.

    Grade-Separation Variables in HDPE Film, Extrusion, and Injection Resins

    The main variable separating HDPE 7000F from a conventional HDPE monofilament or tape grade such as 5000S is melt flow. A 0.8–1.2 g/10 min HDPE extrusion grade flows with lower viscosity and lower head pressure, but produces less bubble stability and lower environmental stress-crack resistance under ASTM D1693-21 condition B. HDPE 7000F is therefore selected where thin-gauge film must survive high-speed converting and repeated loading. It is not suitable for injection molding or thin-wall packaging requiring melt index above 5 g/10 min.

    Compared with a butene LLDPE film grade with nominal density 0.918 g/cm³ and melt index 1.0 g/10 min, HDPE 7000F exhibits higher tensile modulus and lower dart impact strength measured by ASTM D1709-22 Method A. The higher crystallinity of the 0.956 g/cm³ density grade also reduces water-vapour transmission rate under ASTM F1249-23 at 38 °C/90 % RH. However, Elmendorf tear strength in both machine and transverse directions is lower than that of LLDPE film of equal gauge; the selection between HDPE 7000F and LLDPE depends on whether the package requires stiffness and moisture-barrier contribution or higher impact and tear resistance.

    Grade classMelt mass-flow rateDensityPrincipal downstream route
    HDPE 7000F0.04 g/10 min0.956 g/cm³HMW-HDPE blown film
    HDPE extrusion or tape grade0.8–1.2 g/10 min0.954 g/cm³Monofilament, tape, extrusion coating
    LLDPE butene film grade1.0 g/10 min0.918 g/cm³Blown film, seal layers

    Food-contact use requires verification against the specific production lot. The base polyolefin resin falls under 21 CFR 177.1520 when evaluated in the uncoloured, unfilled state. Finished-film compliance with (EU) No 10/2011 must be established by migration testing because slip agents, antiblock, and masterbatch colourants alter overall migration. REACH registration duties apply to the resin as supplied to the European market; RoHS status for the end article depends on processing additives and colourants selected by the converter.

    When the Regrind Fraction Exceeds 30 wt%

    Reintroduction of edge trim, start-up scrap, and rejected rolls above 30 wt% regrind is the most common cause of property drift in HMW-HDPE film. Each heat history increases melt index, reduces molecular weight, and narrows the processing window. Film produced with high regrind fractions may show lower dart impact under ASTM D1709-22 Method A, reduced Elmendorf tear under ASTM D1922-23, and unstable frost-line position. Regrind streams should be lot-controlled and re-certified for melt index by ISO 1133-1:2022 and density by ISO 1183-1:2019 before blending.

    Blending with lower-viscosity HDPE injection or extrusion grades should be limited to below 15 wt%; above this fraction the melt index of the blend may exceed the film-grade control window and bubble stability is lost. Additive packages containing high levels of oxidizing agents or peroxide masterbatches should not be compounded into the resin; free-radical chain scission produces rapid melt-index increase and gel formation at the die lip. Published data for the specific gel-count response after repeated extrusion of this grade is limited; plant trials should establish a maximum melt temperature below 220 °C and monitor carbonyl index increase by FTIR after each heat history. Extended runs above 72 h may require periodic die-lip cleaning with brass tools to remove additive-derived deposits that cause film streaks.

    Top