Wanhua Chemical Pbt Unfilled Wanthane Pbt P100

Wanhua Chemical PBT Unfilled WANTHANE PBT-P100

    • Product Name: Wanhua Chemical PBT Unfilled WANTHANE PBT-P100
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 467404
    Density 1.30 g/cm³
    Melt Flow Rate 260 C 2 16 Kg 18 g/10 min
    Tensile Strength 55 MPa
    Tensile Elongation At Break 50%
    Flexural Modulus 2400 MPa
    Notched Izod Impact Strength 23 C 4 kJ/m²
    Heat Deflection Temperature 0 45 Mpa 150°C
    Heat Deflection Temperature 1 82 Mpa 60°C
    Melting Point 225°C
    Vicat Softening Temperature 180°C
    Water Absorption 24 H 0.08%
    Molding Shrinkage 1.5–2.0%
    Dielectric Strength 20 kV/mm

    As an accredited Wanhua Chemical PBT Unfilled WANTHANE PBT-P100 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Wanhua Chemical PBT Unfilled WANTHANE PBT-P100 is packaged in 25 kg moisture-barrier bags, palletized for secure industrial transport and storage.
    Container Loading (20′ FCL) 20′ FCL loading: Wanhua Chemical PBT Unfilled WANTHANE PBT-P100 in bagged/palletized form, stowed and secured for ocean shipment.
    Shipping Wanhua Chemical PBT Unfilled WANTHANE PBT-P100 ships as non-hazardous solid resin pellets, typically in 25 kg moisture-proof bags on palletized loads. It is not regulated for transport; keep dry, avoid heat and direct sunlight, and handle according to the SDS and local regulations.
    Storage Store Wanhua Chemical PBT Unfilled WANTHANE PBT-P100 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and moisture. Keep containers closed to prevent contamination and moisture pickup. Maintain stable stacking, avoid prolonged exposure to humid air, and follow the supplier’s SDS and local regulations.
    Shelf Life Shelf life: 24 months from date of manufacture when kept in original unopened packaging under dry, cool, recommended storage conditions.
    Free Quote

    Competitive Wanhua Chemical PBT Unfilled WANTHANE PBT-P100 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Wanhua Chemical WANTHANE PBT-P100 is an unfilled polybutylene terephthalate resin supplied as cylindrical pellets for injection moulding and selected extrusion operations. The product is formulated without glass fibre, mineral filler, or halogenated flame-retardant synergists; the neat-polymer composition is therefore characterised by low particulate loading, predictable melt rheology, and reduced mould-surface abrasion relative to reinforced PBT grades. A nominal melt volume-flow rate of 19 ± 3 cm³/10 min is determined at 250 °C under 2.16 kg according to ISO 1133-1:2022, placing PBT-P100 in the medium-flow unfilled injection-moulding class. Density is 1.31 g/cm³ per ISO 1183-1, ash content is typically below 0.05 % by ISO 3451-1, and mould shrinkage is 1.5–2.0 % in the flow direction and 1.7–2.2 % transverse to flow when measured under ISO 294-4. These values are the basis for tool dimensional allowances in relay bases, terminal blocks, coil formers, and connector housings.

    Prior to any melt-processing operation, residual moisture is reduced below 0.02 % by weight using Karl Fischer titration per ISO 15512 or an equivalent calibrated loss-on-drying method. A closed-loop desiccant dryer with air dew point below -40 °C and hopper temperature of 120 °C for 4 h is the minimum recommended condition for virgin pellets at 50 % ambient relative humidity. Warehousing above 60 % RH or regrind addition beyond 20 % requires extension of drying time to 6 h or reduction of hopper fill depth. Inadequately dried PBT undergoes hydrolytic chain scission during plastication; the production-floor evidence is unstable melt pressure, silver streaking at sprue and gate regions, and a 10–15 % reduction in tensile elongation at break compared with dry pellets. Because the hydrolysis reaction is autocatalytic once free carboxylic acid end groups accumulate, continuous return-air dew-point monitoring is a mandatory process control rather than a periodic laboratory check.

    What distinguishes unfilled PBT-P100 from glass-fibre-reinforced PBT grades?

    The most direct differentiation is mechanical load capacity. Unfilled PBT-P100 typically exhibits tensile stress at break of 55 MPa and tensile modulus of 2600 MPa under ISO 527-2/1A, while a 30 wt% glass-fibre-reinforced PBT reference may reach 120 MPa tensile stress and 10000 MPa tensile modulus. Flexural modulus for PBT-P100 is near 2500 MPa per ISO 178, and notched Izod impact strength at 23 °C is 4.5 kJ/m² per ISO 180/1A. The unreinforced grade is therefore unsuitable for structural snap-fit components or brackets requiring sharp corner loading. Conversely, the absence of glass fibre reduces screw and barrel wear, decreases weld-line visibility in multi-gate connector housings, and produces less divergence between longitudinal and transverse mould shrinkage. The unfilled melt also has lower thermal conductivity than glass-filled systems, so cycle-time optimisation for PBT-P100 relies more on hold-pressure profile than on elevated mould temperature alone.

    Table 1. Comparative representative property data for unfilled WANTHANE PBT-P100 and a 30 wt% glass-fibre-reinforced PBT reference.
    PropertyTest standardPBT-P10030 wt% GF PBT
    DensityISO 1183-11.31 g/cm³1.53 g/cm³
    Tensile stress at breakISO 527-2/1A55 MPa120 MPa
    Tensile modulusISO 527-2/1A2600 MPa10000 MPa
    Flexural modulusISO 1782500 MPa8500 MPa
    Notched Izod impact at 23 °CISO 180/1A4.5 kJ/m²9.0 kJ/m²
    Heat deflection temperature at 0.45 MPaISO 75-2/B155 °C220 °C
    Heat deflection temperature at 1.8 MPaISO 75-2/A60 °C205 °C
    Mould shrinkage flow / transverseISO 294-41.5–2.0 % / 1.7–2.2 %0.3–0.6 % / 0.7–1.1 %
    Dielectric strengthIEC 60243-117 kV/mm15 kV/mm

    In thin-wall connector housings with section thickness below 0.8 mm, tool design must account for freeze-off of the unreinforced melt at gate dimensions below 0.6 mm. A rectangular edge gate with land length of 0.8–1.0 mm and depth equal to 60–70 % of the part wall is used. Mould venting at flow-path ends is set to 0.02–0.03 mm to prevent diesel-effect burning. In multi-cavity coil-former tools, cavity-to-cavity mass variation should be held below 0.5 % for balanced filling; this requires nozzle temperature stability within ±5 °C of the optimised setpoint. Above this deviation, unfilled PBT can transition from stable laminar filling to gate jetting, producing surface splay and short-shot variability that is frequently misdiagnosed as inadequate venting.

    Injection Moulding Parameter Envelope and Thermal Stability Limits

    Barrel-temperature profiling for PBT-P100 follows a rear-to-front sequence of 230 °C, 240 °C, 250 °C, and 250–260 °C at the nozzle. Melt temperature measured by an immersion probe should not exceed 270 °C, and residence time above 260 °C should not exceed 5 min. At 280 °C or under extended residence, unfilled PBT undergoes depolymerisation to tetrahydrofuran and butadiene derivatives; the moulded part shows yellowish-brown discolouration, surface splay, and a viscosity reduction that can mislead shot-size control. A general-purpose screw with L/D 20:1 to 22:1 and compression ratio 2.5:1 is acceptable, with a sliding check ring having 2.5–3.0 mm axial travel to limit shear heating. Straight-through hardened-steel nozzle tips are preferred over reverse-taper designs because unfilled PBT can string under high decompression.

    Mould temperature directly controls crystallinity and post-moulding dimensional stability. For PBT-P100, a mould temperature of 60 °C may be sufficient for simple thick-wall parts, but 80–100 °C is used for connector bodies and relay bases to achieve crystallinity adequate for service stability. Below 50 °C mould temperature, as-moulded parts can retain amorphous regions that re-crystallise over time, leading to warpage and centre-to-hole pitch drift of 0.1–0.3 % after 24 h at 23 °C. This is a critical processing conflict: lower mould temperature reduces cycle time but transfers shrinkage into the field, whereas higher mould temperature increases cycle time and energy consumption but stabilises dimensions. At mould temperatures above 110 °C, ejection becomes difficult because unfilled PBT has low heat-deflection stiffness; mould release requires textured surfaces and draft angles of 1.0–1.5 ° per side.

    If regrind incorporation exceeds 20–25 %, melt-pressure variance may rise by 5–7 % because reclaimed flakes have lower bulk density and residual moisture. Wet regrind should be recrystallised at 120 °C for 2 h before blending to prevent hopper bridging. Central drying systems that maintain -50 °C air dew point and switch desiccant beds on a differential pressure of 5 °C give the most stable shot-to-shot melt cushion for PBT-P100 in production-scale machines with clamp force from 35 kN/cm² of projected area.

    When post-moulding annealing is required for dimensional stability

    Post-moulding annealing is applied when service temperature is expected to exceed 100 °C in under-hood automotive housings, lamp sockets, or power-tool brush holders. The moulded article is placed in a forced-air convection oven at 120 °C for 1–2 h immediately after ejection, followed by slow cooling to 40 °C before packaging. Annealing increases crystalline fraction and reduces residual moulded-in stress; without annealing, rear-moulded connector bodies can exhibit stress-cracking when exposed to hot hydrocarbon vapours or to cyclic temperatures between -40 °C and 120 °C. The dimensional change during annealing is anisotropic and depends on gate location; edge-gated flat parts show an average length decrease of 0.2–0.5 % along the flow axis, while the transverse direction may show 0.1–0.3 % increase. These changes must be compensated in tool design rather than by altering hold pressure after the tool is cut.

    Thermal oxidative degradation of unfilled PBT during long-term service above 140 °C is accelerated in the presence of metal oxides and halogenated residues. Unfilled PBT-P100 is therefore not recommended for continuous use above 120 °C under mechanical load, and it should not be exposed to hot water above 60 °C for prolonged periods because the ester linkage undergoes hydrolytic attack. In fuel-contaminated environments, external seals are required because PBT swells in aromatic and oxygenated fuels; published data for this specific configuration is limited.

    Applications in appliance terminal blocks, relay sockets, and power-tool brush holders require documented electrical and regulatory performance. Unfilled PBT grades in the PBT-P100 viscosity class typically exhibit comparative tracking index of 400–600 V under IEC 60112 and volume resistivity above 1×1015 Ω·cm under IEC 60093, although lot-specific certificates of analysis should be used for design values. Flammability classification is determined by IEC 60695-11-10; an unfilled natural PBT-P100 moulding at 0.8 mm may be classified HB, while black or custom-coloured versions must be retested because colorants can alter ignition resistance. The material is intended for evaluation within the scope of EU Directive 2011/65/EU RoHS and for SVHC tracking under Regulation (EC) No 1907/2006 REACH; the supplier’s lot-specific SDS and product stewardship declaration should be consulted for Article 33 communication.

    Table 2. Regulatory and safety assessment framework for WANTHANE PBT-P100 moulding compounds.
    AssessmentReferenceInformation required from supplier
    RoHS homogeneous material restrictionsDirective 2011/65/EU Annex IILead, mercury, cadmium, hexavalent chromium, PBB, PBDE, and phthalate declarations
    REACH SVHC trackingRegulation (EC) No 1907/2006Candidate-list SVHC content above 0.1 % and Article 33 duty
    Flammability classificationIEC 60695-11-10Supply-chain test report or UL yellow card for specified colour and thickness
    Food-contact statusEU 10/2011Not intended for direct food-contact use unless separately confirmed
    WEEE disposalDirective 2012/19/EUPlastic energy-recovery route

    Processing of PBT-P100 on production-scale injection machines requires a screw-back position that maintains a 3–5 mm melt cushion, hydraulic hold pressure of 60–80 MPa, and hydraulic back pressure of 0.3–0.7 MPa. Gate shear rate should not exceed 50,000 s-1 for unfilled PBT; above this threshold, melt fracture appears as rough gate-area surface and is frequently mistaken for insufficient venting. In coil-former and relay-base tools, submarine or tunnel gates of 0.8–1.2 mm diameter are common because they provide automatic degating, but they increase shear heating; nozzle temperature is reduced by 5 °C when tunnel gating is used. WANTHANE PBT-P100 is therefore applied in high-volume electrical parts where low particulate loading, repeatable unfilled-polyester processing, and predictable shrink are controlling requirements; it is not the material of choice for high-impact structural brackets, continuous under-hood temperatures above 120 °C, or hot-water pump housings.

    Top