    Specifications
    HS Code 753102
    Density 0.950 g/cm³
    Melt Mass Flow Rate 190 C 2 16 Kg 0.35 g/10 min
    Tensile Strength At Yield 26 MPa
    Tensile Strength At Break 30 MPa
    Elongation At Break 600%
    Flexural Modulus 1170 MPa
    Vicat Softening Temperature 125 °C
    Heat Deflection Temperature 0 45 Mpa 70 °C
    Shore D Hardness 60
    Environmental Stress Crack Resistance 10 Igepal 1000 h
    Melting Temperature 130 °C
    Bulk Density 0.58 g/cm³
    Water Absorption <0.01%
    Thermal Conductivity 0.35 W/m·K
    Coefficient Of Linear Thermal Expansion 1.2E-4 cm/cm/°C

    As an accredited Vinmar International HDPE HHM50100 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Vinmar International HDPE HHM50100 is typically packaged in 25 kg multiwall paper bags, 40 bags per pallet, stretch-wrapped.
    Container Loading (20′ FCL) 20′ FCL loading Vinmar International HDPE HHM50100 resin: 25 kg bags, palletized, shrink-wrapped, and securely stowed for ocean export.
    Shipping Vinmar International HDPE HHM50100 is typically shipped as non-hazardous solid resin pellets in bags, bulk bags, or bulk truck/rail containers. It is not regulated for transport. Keep containers closed, dry, and away from heat. Handle with standard industrial practices; avoid dust and static buildup. Suitable for truck, rail, or ocean freight.
    Storage Store Vinmar International HDPE HHM50100 in a cool, dry, well-ventilated area in closed original packaging. Keep away from heat, sparks, open flames, strong oxidizers, and direct sunlight. Prevent moisture, dust, and contamination. Use first-in, first-out stock rotation. Follow SDS and local regulations.
    Shelf Life Stable under normal storage conditions; no fixed shelf life if kept cool, dry, sealed, and away from sunlight and contaminants.
    Application of Vinmar International HDPE HHM50100

    Vinmar International HDPE HHM50100 is processed in high-stalk blown film lines where the melt exits an annular die at a die gap of 1.2–2.0 mm and is inflated at a blow-up ratio between 3:1 and 5:1. The resin’s high molecular weight provides melt tension sufficient to preserve bubble geometry at frost line heights 8–12 die diameters above the die. Barrel zones are normally profiled from 160 °C at the feed throat to 210 °C at the adapter, with die zones held at 200–215 °C. If the die gap is reduced below 1.0 mm, melt fracture and bubble instability appear at output rates above 180 kg/h on an 80 mm, 30:1 L/D extruder. The finished film in the 12–25 μm gauge range is converted into T-shirt bags, grocery sacks, and produce bags. Compliance under food-contact conditions is assessed using FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011, subject to migration testing for the specific food simulant and temperature condition. The lot-certified melt flow index and density must be verified against the batch certificate before barrel profiles and die gaps are fixed; typical HMW-HDPE extrusion grades in this sector fall between 0.05 and 0.15 g/10 min at 190 °C/2.16 kg and between 0.947 and 0.952 g/cm³.

    Blending HHM50100 with 10–20 wt% C4-LLDPE at the hopper reduces transverse-direction tear propagation in heavy-duty refuse sacks; the melt flow mismatch between the two resins must be kept below 0.5 g/10 min to avoid gauge banding. A concentrate containing 20 wt% silica antiblock and 10 wt% erucamide slip is added at 1.0–3.0 wt% to maintain openability and unwind behavior. Addition above 4.0 wt% is not recommended because the inorganic particles create stress-concentration sites and depress dart impact; processors must validate each formulation with ASTM D1709-22. Barrel temperatures from 150 °C to 200 °C, die temperatures of 190–210 °C, and blow-up ratios from 2.5:1 to 4.0:1 are used for this segment. Film thickness is 25–80 μm for industrial refuse sacks and 80–150 μm for construction debris bags. Tests include ASTM D1709-22 for dart impact, ASTM D624 for tear strength, and ASTM D1894-14 for coefficient of friction. End products include bin liners, contractor bags, and heavy-duty industrial liners.

    When Geomembrane Sheet Extrusion Requires Single-Point Notched Constant Tensile Load Verification

    Thick HMW-HDPE sheet from HHM50100 is processed on flat-die or blown-film lines configured for 0.5–2.0 mm final thickness. Long-term stress-crack resistance is quantified by ASTM D5397-19 using 30% Igepal CO-630 at 50 °C; a single-point notched constant tensile load value below 200 h is unacceptable for hazardous waste pond liners because the stress-cracking threshold governs long-term failure after installation, not short-term tensile yield. Extrusion temperature profiles from 220 °C to 245 °C are necessary to maintain melt homogeneity through a 120 mm, 36:1 L/D flat-die line with a melt pump; die temperatures above 250 °C cause oxidative gel accumulation on the die lip within 8–10 h and force line shutdown. The melt curtain is calendered and cooled on a stack maintained at 70–90 °C. Carbon black masterbatch is compounded in at 2.0–3.0 wt%, because carbon black dispersion below 2.0 wt% yields insufficient UV stabilization for long service life, while above 3.0 wt% lowers weld peel strength. Seam integrity of fabricated panels is evaluated by ASTM D4437 and GRI-GM19. Compliance for the finished geomembrane is referenced to GRI-GM13 for HDPE geomembranes and ASTM D4976 for the base resin. The minimum test matrix for sheet and seam qualification is shown below.

    PropertyTest standardMeasurement condition
    Sheet thicknessASTM D5199Average of 10 points per roll, 0.5–2.0 mm
    Single-point notched constant tensile loadASTM D5397-1950 °C, 30% Igepal CO-630
    Stress crack resistanceASTM D1693-1550 °C, 100% Igepal CO-630
    Carbon black dispersionISO 18553Microtome sections across thickness
    Seam peel strengthASTM D4437Field welded coupons, 23 °C ± 2 °C

    Extrusion blow molding of HHM50100 into containers up to 120 L uses accumulator-head machines with 25:1 to 30:1 L/D extruders. The melt temperature at the die is maintained at 210–230 °C; above 235 °C parison sag becomes difficult to control unless the head tooling is adjusted for a 1.5–2.0 mm annular gap. Mold temperature is held at 15–40 °C and blow pressure at 0.6–1.0 MPa. Continuous parison programming requires a divergent die gap profile to compensate for draw rates of 1.0–1.5 m/s. The high molecular weight gives sufficient swell for uniform wall distribution in 20–120 L jerry cans and drums. UN certification for dangerous goods packaging under 49 CFR 178.509 and IMO IMDG 6.1.5 requires drop tests, hydraulic pressure tests, and stack tests on each lot. Food and pharmaceutical containers must meet FDA 21 CFR 177.1520 and USP <661.1> where applicable. Color concentrate addition is maintained at 0.5–2.0 wt%; higher loadings alter parison draw and reduce top-load performance in finished containers.

    What Layer-Ratio Constraints Apply When HHM50100 Serves as the Structural Core in Coextruded Film?

    Coextrusion of HHM50100 as the structural layer in three-layer blown film places the resin between skins of LLDPE or metallocene LLDPE. The core layer typically constitutes 60–80 wt% of total thickness; below 60 wt% the HDPE stiffness contribution is lost, and above 80 wt% the seal initiation temperature rises above 135 °C. Differential viscosity between HHM50100 and the skin resins must be matched by selecting skin grades with melt flow indices within 0.5 g/10 min of the core. The die block is run at 195–210 °C, and the air ring is adjusted to a dual-lip configuration with 15–20 °C chilled air, which preserves bubble stability at a 3:1 blow-up ratio. Final film thickness from 30 μm to 100 μm is used in collation shrink, stand-up pouches, and form-fill-seal packaging. Heat seal strength is measured by ASTM F88/F88M at a sealing temperature of 145–165 °C and dwell time of 0.5–1.0 s; seal strength values below 15 N/25 mm are rejected for heavy payloads. This structure is specified where puncture resistance and moisture barrier dominate mechanical requirements, while the skins provide low seal initiation and hot-tack performance.

    Form-Fill-Seal Heavy-Duty Sack Conversion and the Heat Seal Envelope

    On form-fill-seal filling lines, HHM50100-based tubular film is converted into gusseted sacks with 25–80 μm wall thickness. Because the resin’s high melting point delays seal initiation, the seal bar temperature is set between 150 °C and 170 °C, with dwell times of 0.3–1.2 s and pressure of 0.3–0.6 MPa. Seal strength must exceed film tear propagation resistance, otherwise the sack fails at the seal corner during drop tests. The FFS film is corona-treated to 38–42 mN/m for ink adhesion and printed with water-based flexographic inks; surface tension below 36 mN/m results in ink rub-off on palletized bags. Slip and antiblock additives are kept below 3.0 wt% to preserve seal integrity. End products include fertilizer, resin, petrochemical, and agricultural product sacks. Drop testing follows ISO 7965-2 and tear testing follows ISO 6383-2. The FFS conversion window is narrower than standard blown film because sealing pressure and dwell must be coordinated with fill speed; line rates above 1,800 sacks/h require seal bar temperature compensation to avoid cold seals at the gusset fold.

    Pipe coating and protective wrap applications use HHM50100 in 200–400 μm sheet or extruded profile as a mechanical damage barrier over anti-corrosion coatings on steel pipe. The material is extruded at 220–240 °C and laminated to hot pipe at 180–200 °C with a silicone roll nip pressure of 0.4–0.8 MPa. The HDPE layer must have elongation at break greater than 300% in both machine and transverse directions to survive field bending; ASTM D638-14 specimens are cut in both orientations and conditioned per ASTM D618. The outer wrap is supplied with a 0.5–1.5 wt% carbon black concentrate for UV resistance unless the specification permits unpigmented natural material. Performance under simulated soil stress is evaluated by ASTM D1693 ESCR and ASTM D638 tensile. Published independent data for HHM50100 in this specific buried wrap configuration is limited; qualification must use lot-specific ESCR and oxidation induction time data. No long-term buried service warranty should be issued without site-specific electrochemical and microbial data covering the backfill environment.

    Free Quote

    Competitive Vinmar International HDPE HHM50100 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Vinmar International supplies HDPE HHM50100 as a high-density polyethylene resin intended for blown film conversion, thin-gauge sack production, and industrial liner applications. The grade designation belongs to the high-molecular-weight HDPE film class. Distributor technical summaries identify a nominal density of 0.950 g/cm³ under ASTM D1505 and a high-load melt index of 10 g/10 min under ASTM D1238 at 190 °C with a 21.6 kg piston load. Lot-specific certificates of analysis should govern acceptance because commercial polyethylene tolerances allow variation around nominal values. The standard 2.16 kg melt flow condition yields values below 0.1 g/10 min, which approaches the resolution limit of ASTM D1238 Procedure A; therefore the high-load condition is used for routine melt flow quality control. The resin is not intended for injection molding or extrusion blow molding. Its melt viscosity and high-stalk bubble stability are suited to oriented thin-gauge films in which machine-direction and transverse-direction tear balance is controlled through stalk height, blow-up ratio, and frost line position.

    Class-Level Differentiation Among Polyethylene Film and Blow Molding Resins
    ParameterHDPE HHM50100 reported classHDPE blow molding gradeLLDPE film grade
    Nominal density (ASTM D1505)0.950 g/cm³0.955–0.960 g/cm³0.918–0.925 g/cm³
    Melt flow condition10 g/10 min at 21.6 kg, 190 °C0.25–0.40 g/10 min at 21.6 kg0.8–1.2 g/10 min at 2.16 kg
    Primary conversion processblown film, thin-gauge sacksextrusion blow moldingcast or blown film
    Melt strength / bubble stabilitymoderate-high; high-stalk possiblehigh; parison sag resistancelow-moderate; low-stalk preferred
    Machine-direction / transverse-direction tear balancebalanced via high-stalk orientationnot applicabletransverse-direction dominant in blown film
    Moisture barrier at equivalent gaugehigher than LLDPEsimilar to HHM50100, slightly higherlower than HDPE

    What Distinguishes HHM50100 from Conventional Bimodal HDPE Film Resins?

    Distributor literature for HHM50100 does not always disclose the full comonomer type, molecular weight distribution shape, or catalyst residue profile. Published data for this specific configuration is limited; however, the combination of 0.950 g/cm³ density and 10 g/10 min high-load melt index indicates a resin optimized for moderate melt strength with lower extrusion head pressure than HDPE grades having HLMI values below 7 g/10 min. Compared with conventional bimodal HDPE film resins, HHM50100 can permit higher specific throughput at equivalent extruder torque, but the lower melt viscosity can reduce high-stalk bubble stability. A converter moving from a grade with HLMI 5 g/10 min to HHM50100 should anticipate a reduction in die pressure and may need to reduce die gap or adjust air ring settings to maintain bubble geometry.

    Against HDPE blow molding grades with densities of 0.955 g/cm³ to 0.960 g/cm³ and lower HLMI, HHM50100 provides easier drawdown at thin gauge but lower parison sag resistance. It is therefore unsuitable for extrusion blow molding of large containers. Against LLDPE film resins with densities of 0.918 g/cm³ to 0.925 g/cm³, HHM50100 yields higher modulus, lower elongation, and higher moisture barrier, but lower dart impact at equivalent thickness unless film gauge is increased or orientation is optimized. The material also differs from standard injection molding HDPE grades, whose melt flow rates under 2.16 kg are typically above 8 g/10 min; HHM50100 cannot be processed in conventional injection molding equipment without excessive pressure and melt heating.

    Film tensile properties are assessed under ASTM D882 or ISO 527-3 using 500 mm/min crosshead speed. For HDPE film of this density class, machine-direction tensile strength at break is generally reported in the 25 MPa to 40 MPa range, transverse-direction tensile strength at break in the 20 MPa to 35 MPa range, and elongation at break above 300%; these are class-level values, not HHM50100 lot guarantees. Dart impact resistance is measured under ASTM D1709 Method A; class-level values at 25 µm thickness typically fall between 150 g and 250 g. Elmendorf tear resistance under ASTM D1922 is strongly influenced by high-stalk orientation and can shift from machine-direction tear values below 20 g to values above 40 g as blow-up ratio and stalk height increase. Published data for this specific configuration is limited, and converter trials are required to establish lot-specific values.

    Rheological Boundaries During High-Shear Extrusion

    Melt processing of HHM50100 requires control of shear heating and residence time. On production-scale grooved-feed extruders with length-to-diameter ratios of 24:1 to 30:1, barrel settings are typically staged from 160 °C in the feed zone to 200 °C to 230 °C at the die. The melt temperature should be maintained below 235 °C to avoid thermo-oxidative chain scission, gel formation, and loss of dart impact. Conversely, melt temperatures below 195 °C may produce melt fracture, elevated die pressure, and poor bubble stability. The usable processing window is therefore approximately 195 °C to 230 °C, with tighter control required when regrind levels exceed 20 wt%.

    Melt pressure at the die depends on die gap, output rate, and melt temperature. For film dies with gap settings of 1.2 mm to 1.8 mm, die pressures between 25 MPa and 40 MPa are common for HDPE grades in this HLMI class. If die pressure exceeds 45 MPa, the die gap should be increased, screen pack mesh reduced, or melt temperature increased within the stated limit. Extruder screw designs with barrier flights and Maddock mixing sections are preferred for high-molecular-weight HDPE; smooth-bore extruders with L/D below 20:1 are not recommended for sustained thin-gauge production. Specific energy input on grooved-feed machines in this resin class typically falls between 0.25 kWh/kg and 0.35 kWh/kg at screw speeds of 80 min⁻¹ to 120 min⁻¹ on 65 mm extruder diameters, although actual values vary with gear pump usage, screen pack condition, and die restriction.

    Where a converter shifts from a lower-HLMI HDPE grade to HHM50100, the initial extrusion run should map melt pressure against screw speed at constant melt temperature. A pressure response that is lower than the previous grade confirms the expected viscosity reduction, but if the bubble becomes unstable before target output is reached, the die gap should be reduced or the air ring flow increased before raising melt temperature. Purging after processing HHM50100 should use a non-abrasive HDPE or LLDPE purge resin. Avoid purging with rigid PVC, polycarbonate, or polyamide compounds without complete transition; residual polar materials form gels and degrade film appearance. When changing from a resin with higher melt viscosity, a viscoelastic purge sequence of increasing melt index may be necessary to remove stagnant melt from the die lips. Long residence time above 230 °C increases the risk of crosslinked gel particles; shutdown procedures should include immediate screw rotation stop and die cooling.

    Starting Process Conditions for HDPE Film Extrusion with HLMI 10 g/10 min
    Process ZoneSetpoint or Range
    Barrel zone 1160–180 °C
    Barrel zone 2190–210 °C
    Barrel zone 3200–220 °C
    Adapter / die205–230 °C
    Melt temperature195–230 °C
    Die gap1.2–1.8 mm
    Blow-up ratio3:1–5:1
    Frost line height6–10 die diameters
    Air ring air temperature10–15 °C
    Regrind additionup to 20 wt%

    High-stalk bubble geometry is typically used for HDPE film grades in the HLMI 8 g/10 min to 12 g/10 min class. Start-up conditions for HHM50100 often begin with a blow-up ratio of 3:1 to 5:1, a die gap of 1.4 mm, and a frost line height of 6 to 10 die diameters. Single-lip and dual-lip air rings with chilled air at 10 °C to 15 °C provide external bubble cooling; internal bubble cooling is used where available to increase output. Thin-gauge production down to 12 µm is attainable when the bubble is stable, but gauge variation below 10 µm may increase due to die gap tolerance and melt temperature fluctuations. Bubble instability at high output is often corrected by raising the stalk height, reducing the blow-up ratio, or reducing melt temperature within the processing window.

    When High-Stalk Bubble Geometry Is Required for Thin-Gauge Film

    High-stalk processing is selected when balanced machine-direction and transverse-direction tear properties are required. In this configuration, the molten tube is allowed to travel upward before radial expansion; the resulting orientation improves transverse-direction tear while retaining machine-direction strength. On a line equipped with a 65 mm grooved-feed extruder and a 200 mm die, initial trial parameters for HHM50100 frequently set the stalk height at 8 die diameters and adjust the frost line into the upper third of the cooling cone. Bubble breathing or oscillation in the upper cooling zone is an early indication of insufficient melt strength relative to air pressure and output; operators should reduce air ring flow or lower melt temperature before adjusting the blow-up ratio. Published data for this specific configuration is limited, and start-up mapping should record bubble stability, frost line position, output, and film gauge against blow-up ratio and melt temperature.

    Moisture absorption is low; pre-drying is generally not required unless surface condensation has formed after storage below 10 °C or when regrind contains polar contaminants. Drying at 80 °C for 2 h may be used for wet pellets. Avoid mixing with polyamide or polyester contaminants. Even 0.1 wt% polyamide contamination can produce gels and visual defects in HDPE film. Lot-to-lot variance should be monitored through gel count on a 50 µm blown film sample. Gels larger than 200 µm may indicate contamination or thermal degradation. Film haze under ASTM D1003 and gloss at 60° under ASTM D2457 are common quality checks for HDPE film. For HHM50100, published data for haze and gloss are limited; converter trial data should define internal limits.

    Industrial liners produced from HDPE film of this class are typically converted at thicknesses of 50 µm to 100 µm. High-stalk processing provides tear resistance and stiffness; heat sealing is performed at 140 °C to 160 °C with dwell times of 0.5 s to 1.5 s. Seal strength is evaluated under ASTM F88; converter trials should establish minimum seal strength for filled sack drop tests. Chemical resistance of HDPE liners to dilute acids, alkalis, and brine is generally good; contact with aromatic hydrocarbons, chlorinated solvents, and strong oxidizing acids should be avoided above 40 °C due to solvent swelling and potential stress cracking. Environmental stress crack resistance of HDPE is measured under ASTM D1693; class-level HDPE film resins with density 0.950 g/cm³ often show ESCR values above 100 h in 100% Igepal CO-630 at 50 °C, but HHM50100-specific ESCR data are not routinely supplied in distributor summaries.

    Food-contact compliance must be verified through the supplier’s lot-specific statement. Unmodified high-density polyethylene intended for food contact is generally covered by FDA 21 CFR 177.1520(c) and, for the European Union, by Regulation (EU) No 10/2011 with overall migration limits of 10 mg/dm² for general food contact. The resin may be used in packaging if the converter confirms migration limits under the intended food simulant and temperature conditions. REACH registration under Regulation (EC) No 1907/2006 and restriction compliance under Annex XVII should be confirmed with the Vinmar International commercial documentation. Heavy-metal and hazardous substance restrictions under RoHS Directive 2011/65/EU are applicable where polyethylene components are incorporated into electrical and electronic equipment. No conflict with the REACH SVHC candidate list is assumed unless stated in the supplier declaration. Compliance with NSF/ANSI 61 is not presumed for potable water contact unless the grade is specifically certified.