Vinmar International Hdpe Hd5502h

Vinmar International HDPE HD5502H

    • Product Name: Vinmar International HDPE HD5502H
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 189312
    Density 0.955 g/cm³
    Meltflowrate 0.35 g/10 min (190 °C/2.16 kg)
    Tensilestrengthatyield 24 MPa
    Elongationatbreak 600%
    Flexuralmodulus 1000 MPa
    Vicatsofteningtemperature 127 °C
    Meltingtemperature 130-135 °C
    Environmentalstresscrackresistance >1000 h
    Hardnessshored 60
    Waterabsorption <0.01%
    Thermalexpansioncoefficient 1.3E-4 /°C
    Thermalconductivity 0.4 W/m·K
    Volumeresistivity >10^16 ohm·cm
    Dielectricconstant 2.3
    Crystallinity 70-80%
    Molecularweightdistribution Broad

    As an accredited Vinmar International HDPE HD5502H factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Vinmar International HDPE HD5502H is supplied in 25 kg bags, 40 bags per pallet, totaling 1,000 kg.
    Container Loading (20′ FCL) 20′ FCL container loading of Vinmar International HDPE HD5502H resin in 25 kg bags, palletized and stretch-wrapped for export.
    Shipping Vinmar International HDPE HD5502H is shipped as non-hazardous high-density polyethylene resin pellets. Standard packaging includes 25 kg bags or 1,000 kg jumbo bags, palletized and shrink-wrapped. It is transported in clean, dry containers or trucks, protected from moisture, heat, contamination, and ignition sources; no special transport regulations apply.
    Storage Store Vinmar International HDPE HD5502H in a cool, dry, well-ventilated warehouse. Keep original bags sealed, palletized, and off the floor. Protect from direct sunlight, moisture, heat, flames, and oxidizing agents. Avoid contamination and prolonged UV exposure. Maintain normal ambient temperatures; prevent extreme heat that may soften or degrade the resin. Practice good housekeeping to control spilled pellets.
    Shelf Life Vinmar International HDPE HD5502H: stable under normal storage; store sealed, cool, dry, away from heat and sunlight; no specific shelf life.
    Application of Vinmar International HDPE HD5502H

    Extrusion blow molding lines configured with 65 mm–90 mm reciprocating-screw extruders and 24:1–30:1 L/D barrier screws convert Vinmar International HDPE HD5502H into UN 3H1 jerrycans in the 5 L–30 L range. The converging parison head is fitted with a 45 mm–70 mm divergent die and a 20 mm–35 mm core pin; parison wall-thickness programming between 0.8 mm and 2.4 mm is applied to compensate for sag at the lower chime and to thicken the handle pinch-off and top shoulder radius. Melt temperature is controlled at 200°C–215°C, die-zone temperature at 210°C–215°C, and mold temperature at 10°C–25°C. Pre-blow delay of 0.2 s–0.6 s and blow pressure of 0.5 MPa–0.7 MPa are used after mold close; single-station cycle time for a 20 L container is typically 15 s–25 s. On production-scale machines, die-head pressure fluctuations above ±0.3 MPa produce visible wall-thickness deviation at the bottom corner radius, increasing sidewall splitting under drop test.

    Formulation addition ratio for this downstream track keeps HD5502H between 70 wt% and 85 wt% of the melt, with closed-loop flash and trim regrind dosed at 15 wt%–30 wt% after grinding to bulk density above 0.28 g/cm³ and drying to <0.08% moisture. Color masterbatch is dosed at 1.0 wt%–2.5 wt% at the feed throat; UV stabilizer package is kept between 0.15 wt% and 0.40 wt% when outdoor storage is specified. Filler is not used because calcium carbonate or talc concentrate reduces low-temperature drop impact and ESCR at the pinch-off weld. The terminal article is a UN 3H1 jerrycan in 5 L, 10 L, 20 L, 25 L, and 30 L configurations for solvents, agrochemical concentrates, inks, and lubricants. Compliance is demonstrated under UN Model Regulations Chapter 6.1, drop testing at 1.2 m after conditioning at -18°C for 24 h, leakproofness, hydrostatic pressure, and stack testing; US shipments additionally reference 49 CFR §178.509 and §178.605.

    Which accumulator-head parameters govern sidewall uniformity in tight-head drums?

    On accumulator-head machines producing 30 L–220 L tight-head drums and open-head drums, HD5502H is processed on extruders with 100 mm–150 mm screw diameter, 30:1 L/D, and shot capacity of 20 kg–60 kg. First-in/first-out accumulator design prevents melt stagnation and molecular weight degradation at the die head. Melt temperature is held at 195°C–215°C, and accumulator push-out speed is programmed between 0.5 s and 1.2 s per shot to maintain parison wall at 2.5 mm–4.0 mm for a 200 L drum sidewall and 4.0 mm–7.0 mm at the top and bottom chimes. Die-head pressure fluctuations above ±0.3 MPa can generate shark-skin or melt fracture at the die lip and cause wall-thickness variation that reduces drop performance. Parison sag becomes a failure mode when shot size exceeds 60 kg and melt temperature rises above 220°C; this produces thin upper-chime sidewalls and thick pinch-off flash, raising regrind load and cycle time.

    In 1H1 tight-head drums for hazardous liquids, regrind is limited to 25 wt% because environmental stress crack resistance at the bottom pinch-off weld declines when total closed-loop regrind exceeds 30 wt%. The base HD5502H fraction is 60 wt%–85 wt%, carbon black masterbatch is used at 1.5 wt%–2.5 wt% for outdoor stock, and non-black color masterbatch is 0.5 wt%–2.0 wt%. Regrind moisture below 0.08% is required; higher moisture produces melt foaming and pinholes at the pinch-off. The terminal articles are UN 1H1 tight-head drums and UN 1H2 open-head drums used for industrial solvents, detergents, adhesives, and solid chemical powders. Compliance references UN Model Regulations Chapter 6.1, IMDG Code P001/P002, and ASTM D1693 condition B for environmental stress crack resistance. Hydrostatic pressure testing follows 49 CFR §178.605, stack testing follows 49 CFR §178.606, and drop testing follows 49 CFR §178.603.

    When ethylene vinyl alcohol coextrusion replaces monolayer fuel tank design

    When a monolayer tank design is replaced by six-layer coextrusion, HD5502H is allocated to the outer skin and inner liner layers because high ESCR and parison stability are required for pinch-off weld integrity and crash-impact ductility. The coextrusion head is fed by a 90 mm–150 mm main extruder for HD5502H outer and inner layers, a secondary extruder for maleated LLDPE tie resin, and an EVOH barrier extruder. Processing is maintained at 200°C–220°C for HDPE layers and 190°C–210°C for EVOH; die temperature spread across the head must not exceed ±3°C or layer distortion occurs. Wall-thickness programming across a 40 L–70 L tank uses 1.8 mm–3.8 mm parison profiles with thicker sections at the filler neck and shear wall. Mold cooling water is set at 8°C–15°C to reduce EVOH crystalline growth and improve barrier after drop impact. Edge delamination and EVOH interlayer instability are production failure modes when layer ratio control drifts beyond ±0.5 wt%.

    Layer distribution for a barrier tank is outer HD5502H 18 wt%–25 wt%, outer tie 1.5 wt%–2.5 wt%, EVOH 2.0 wt%–3.5 wt%, inner tie 1.5 wt%–2.5 wt%, regrind 35 wt%–45 wt%, and inner HD5502H 25 wt%–35 wt%. Regrind must remain below 0.08% moisture and below 0.15 wt% polypropylene contamination because PP domains nucleate EVOH crystallization and reduce barrier performance. Monolayer tank designs based on HD5502H without EVOH require surface fluorination to a depth of 0.2 µm–0.5 µm for hydrocarbon permeation resistance, but published data for this specific configuration is limited. The terminal product is a 35 L–100 L automotive fuel tank for gasoline and ethanol-blended fuels up to E10/E20, validated under UN ECE Regulation No. 34, FMVSS 301 (49 CFR §571.301), and OEM evaporative emission test procedures.

    Heavy-gauge sheet extrusion of HD5502H into 2 mm–8 mm sheet for thermoformed dunnage and interlayer separators uses 120 mm–150 mm single-screw extruders with 30:1–34:1 L/D, a barrier screw, and a polished three-roll stack with vertical roll gap. The melt is discharged through a 1,200 mm–1,800 mm coat-hanger die; roll temperatures are set at 40°C–60°C top roll, 70°C–90°C middle roll, and 40°C–60°C bottom roll to control sheet gloss and internal stress. Thickness tolerance at 6 mm gauge is held to ±0.05 mm by automatic die bolt adjustment. Thermoforming uses double-sided quartz heating to 160°C–180°C surface temperature, followed by vacuum forming at -0.08 MPa and plug assist at 65°C–80°C. If melt curtain instability appears as edge draw-in or thickness striping, draw ratio is reduced or roll gap opening is increased; density and MFR checks follow ISO 1183-1:2019 and ISO 1133-1:2022.

    Formulation addition ratio for dunnage sheet is 70 wt%–85 wt% HD5502H, 15 wt%–30 wt% closed-loop regrind, and 1.5 wt%–2.5 wt% carbon black masterbatch for UV-stabilized outdoor service; antistatic masterbatch at 1 wt%–3 wt% is used only in electrostatically sensitive logistics lines. Filler is omitted because mineral concentrates reduce flexural fatigue resistance under repeated forklift loading. Terminal articles are thermoformed pallet top decks, dunnage sheets, interlayer separators for glass and stamped metal, and heavy-gauge material handling trays. Load-bearing pallet components are tested under ISO 8611-1:2021, and indirect food-contact dunnage used in dry food logistics is assessed under FDA 21 CFR §177.1520 and EU No 10/2011 migration limits only when direct contact is demonstrated.

    Large-part blow molded water storage tanks and agricultural reservoirs

    Production of 200 L–5,000 L vertical and horizontal tanks from HD5502H is carried out on accumulator-head machines with 100 mm–150 mm extruders, 30:1 L/D, 30 kg–100 kg shot capacity, and 100 mm–250 mm die tooling. Melt temperature is kept at 190°C–210°C to limit parison sag in heavy shot weights. Parison programming places 2.5 mm–7.0 mm walls with additional thickness at the dome, bottom knuckle radius, and drain insert. Mold cooling water at 10°C–25°C is circulated through conformal channels around the chime and neck; cycle time for a 1,000 L tank ranges from 300 s to 1,200 s depending on wall thickness and ambient shop conditions. Inadequate clamp face contact at the pinch line or die-head temperature variation above ±3°C produces internal weld-line folds that lower hydraulic burst pressure.

    HD5502H is used at 70 wt%–80 wt%, with post-industrial regrind at 20 wt%–30 wt%; UV-stabilized black masterbatch or HALS package is dosed at 2.0 wt%–2.5 wt% for continuous agricultural exposure. No calcium carbonate is added because microvoids at weld lines reduce hydrostatic burst strength and ESCR. Potable water tanks require all additives and processing aids to comply with FDA 21 CFR §177.1520 and the full tank to meet NSF/ANSI/CAN 61 extraction limits. Terminal products are 200 L–5,000 L water storage tanks, sprayer tanks, fertigation reservoirs, and industrial chemical dosing tanks. Continuous service is limited to 60°C fluid temperature; aromatic solvents and oxidizing chemicals above 5 wt% are outside the established operating envelope.

    Free Quote

    Competitive Vinmar International HDPE HD5502H prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Vinmar International markets HDPE HD5502H as a pelletized high-density polyethylene copolymer blow moulding resin intended for thick-walled rigid packaging. The grade carries a nominal density of 0.955 g/cm³ determined by ASTM D1505 and a melt flow rate of 0.2 g/10 min at 190 °C and 2.16 kg load according to ISO 1133-1:2022. A high-load melt index of 18 g/10 min at 190 °C and 21.6 kg load under ASTM D1238 is typically listed. These values place HD5502H in the high-molecular-weight HDPE class used for industrial containers, chemical service drums, open-top pails, and large-part logistics packaging where melt strength and environmental stress-crack resistance are specified.

    PropertyNominal valueTest method
    Density0.955 g/cm³ASTM D1505
    Melt flow rate at 190 °C and 2.16 kg0.2 g/10 minISO 1133-1:2022
    High-load melt index at 190 °C and 21.6 kg18 g/10 minASTM D1238
    Tensile strength at yield30 MPaASTM D638
    Elongation at break>800%ASTM D638
    Flexural modulus1400 MPaISO 178
    Environmental stress-crack resistance, F50, 10% Igepal>1000 hASTM D1693
    Notched Izod impact at 23 °C30 kJ/m²ISO 180

    What Distinguishes HD5502H from General-Purpose Butene-Copolymer Blow Moulding Resins?

    The primary differences from general-purpose butene-copolymer blow moulding resins are density, melt flow rate, and molecular architecture. HD5502H is formulated around a high-molecular-weight copolymer chain. The high-load melt index of 18 g/10 min combined with the low melt flow rate of 0.2 g/10 min signals a broad molecular weight distribution. That distribution yields higher shear viscosity at low-stress melt extension, which increases parison hang strength and reduces sag during accumulator blow moulding. In comparison, a 0.952 g/cm³ general-purpose HDPE with a melt flow rate of 0.35 g/10 min sags faster at the same parison weight and requires either a lower melt temperature or a narrower die gap to maintain thickness distribution.

    HD5502H also differs in environmental stress-crack resistance. The ASTM D1693 F50 value in 10% Igepal is typically quoted above 1000 h, whereas general-purpose butene-copolymer grades may fall below 200 h under identical conditions. This difference becomes significant in containers holding surfactant-based detergents, emulsions, or hydrocarbon-containing service fluids, where microcracks at pinch-off seams propagate from residual stress near welds and die lines.

    At a 60 mm single-screw extruder with 25:1 L/D and a smooth-bore feed zone, the recommended start-up barrel temperatures are 175 °C, 185 °C, 195 °C, 200 °C, and 205 °C, with the head and die maintained at 195 °C to 205 °C. Screw speed on this size line is normally kept between 30 rpm and 60 rpm, and melt temperature is held below 220 °C. At temperatures above 230 °C, the polymer begins to oxidize, producing gel particles that disturb parison surface quality and weaken pinch-off welds. Head pressure is monitored because pressure above 30 MPa may indicate a blocked screen pack or a high-viscosity melt condition that generates additional shear heating. The resin does not require predrying for normal indoor storage; outdoor storage at elevated relative humidity may introduce surface condensation, which is removed by a hopper dryer at 80 °C for 1 h before extrusion.

    When HD5502H Replaces a 0.952 g/cm³ Grade in Existing Tooling

    When HD5502H is substituted into tooling optimized for a lower-viscosity HDPE, three process adjustments are commonly observed. First, the denser melt increases parison weight per unit wall thickness; moulds designed for a 0.952 g/cm³ resin can produce heavier parts unless the parison length or die gap is reduced. Second, die swell is typically higher, so the parison diameter may increase by 8% to 15% relative to the die diameter, depending on shear history and head tooling. Third, the lower melt flow rate demands higher extrusion head pressure or a 5 °C to 10 °C increase in die temperature to avoid shark-skin melt fracture on the outer parison surface. These changes affect container weight control, flash thickness, and weld-line integrity and should be evaluated with production-scale trials rather than small-lot laboratory extrusion.

    ParameterHD5502H typicalGeneral-purpose 0.952 g/cm³ butene HDPE typicalTest method
    Density0.955 g/cm³0.952 g/cm³ASTM D1505
    Melt flow rate at 190 °C and 2.16 kg0.2 g/10 min0.35 g/10 minISO 1133-1:2022
    High-load melt index at 190 °C and 21.6 kg18 g/10 min24 g/10 minASTM D1238
    Flexural modulus1400 MPa1100 MPaISO 178
    Environmental stress-crack resistance, F50, 10% Igepal>1000 h>100 hASTM D1693
    Notched Izod impact at 23 °C30 kJ/m²15 kJ/m²ISO 180

    Extrusion Blow Moulding Set-Points and Screw Geometry Constraints

    Screw design matters with HD5502H because the resin is shear-sensitive and has a broad molecular weight distribution. A compression ratio of 2.5:1 to 3.5:1 and an L/D of 24:1 to 30:1 are typical. A barrier screw with a Maddock mixing section can disperse pigments but may generate excessive shear heating if the mixer clearance is below 0.5 mm, pushing melt temperature past 220 °C. Accumulator heads should maintain first-in-first-out flow with minimum dead spots; stagnant melt in an overheated manifold leads to degradation gels. On a 100-point accumulator head used for 60 L drums, the parison drop time is set so that the parison length reaches approximately 95% of the mould cavity length before inflation. This is a production-bottleneck parameter because a fast drop increases drawdown and a slow drop cools the outer skin, both of which produce nonuniform wall thickness.

    Batch-to-batch melt flow rate variation in high-molecular-weight HDPE grades is typically controlled within ±0.02 g/10 min. Incoming lots outside the supplier’s melt flow rate specification should be quarantined because even small shifts alter parison sag, die swell, and pinch-off weld penetration. On an operating line, the permissible melt temperature window is approximately 10 °C to 15 °C; temperatures below 180 °C produce high melt viscosity and poor weld fusion, while temperatures above 220 °C promote oxidative chain scission. Published data for this specific configuration is limited; production trials are required to lock the final set-point window.

    Stress-crack resistance and pinch-off weld strength improve when the high-molecular-weight fraction is retained during processing

    The high-molecular-weight fraction in HD5502H is the main contributor to environmental stress-crack resistance and weld strength. Aggressive screw mixing or repeated regrind can cause shear-chain scission and reduce that fraction. The resin can be reprocessed as trimmed flash or rejected containers; however, regrind addition should not exceed 20% to 30% by weight in critical environmental stress-crack-resistance applications unless process capability data demonstrate otherwise. The pinch-off weld of a blow moulded container is the most vulnerable zone for environmental stress cracking. Under ASTM D1693 testing, a failed F50 time of less than 100 h in a moulded part usually indicates a cold weld or excessive orientation at the pinch-off tail rather than a bulk resin issue. Maintaining the mould pinch-off insert temperature near 70 °C to 90 °C can improve weld strength by slowing cooling at the seam.

    Specifying HD5502H for UN-Certified Industrial Packaging

    For UN-certified packaging, short-term hydraulic and stack test results depend on wall thickness distribution and weld quality. HD5502H is used in 20 L to 220 L top-asymmetric and L-ring drums. When specifying the grade on a purchase order, the exact melt flow rate, density, and environmental stress-crack-resistance methods should be stated. The producer’s typical data sheet lists a density of 0.955 g/cm³ and high-load melt index of 18 g/10 min; incoming inspection should verify each lot against these values using ISO 1133-1:2022 and ASTM D1505. In addition, the finished commercial article must comply with FDA 21 CFR 177.1520 for food-contact applications and with the applicable sections of the UN Manual of Tests and Criteria for hazardous-materials containers. REACH registration and RoHS Directive 2011/65/EU are generally addressed by the supply chain; a completed long-form safety data sheet and a REACH statement should be obtained from the seller for the specific batch.

    HD5502H is not recommended for continuous service with strong oxidizing acids, aromatic hydrocarbons, or halogenated solvents; the polymer may swell, permeate, or lose mechanical strength under those conditions. It is also not suitable for rotational moulding or for injection moulding where the low melt flow rate would require excessive melt temperatures and may cause freezing before complete mould filling. Compounding with high levels of low-density polyethylene, ethylene-vinyl acetate, or amorphous polyalphaolefins is generally avoided if maximum environmental stress-crack resistance and top-load stiffness of the moulded article are required. When additives are used, the carrier resin should be matched to an HDPE base, and addition levels should be verified by moulding trial because some masterbatch carriers reduce environmental stress-crack resistance and weld strength.

    Top