| HS Code | 324689 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Density | 0.920 g/cm3 |
| Melt Flow Rate 190 C 2 16 Kg | 2.0 g/10 min |
| Melting Point | 120 °C |
| Vicat Softening Temperature | 90 °C |
| Brittleness Temperature | < -70 °C |
| Tensile Strength At Break | 25 MPa |
| Elongation At Break | 600% |
| Tensile Modulus | 250 MPa |
| Flexural Modulus | 250 MPa |
| Shore D Hardness | 50 |
| Haze | 20% |
| Gloss | 60% |
| Water Absorption | <0.01% |
As an accredited Versalis Pharmalene® MS 20 PH Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis Pharmalene® MS 20 PH: typically supplied in 25 kg polyethylene bags, palletized and stretch-wrapped; 1,000 kg octabins may be available. |
| Container Loading (20′ FCL) | 20′ FCL loaded with palletized 25 kg bags of Versalis Pharmalene® MS 20 PH linear low density polyethylene, stretch-wrapped, securely stowed. |
| Shipping | Shipping description: Polyethylene, linear low density, solid; not regulated as dangerous goods. Versalis Pharmalene MS 20 PH is supplied as pellets in sealed bags or octabins. No UN number, hazard class, or packing group assigned. Keep dry, away from heat/UV; use clean, dry, covered freight. |
| Storage | Store Versalis Pharmalene® MS 20 PH LLDPE in a cool, dry, well-ventilated area, away from direct sunlight, heat, and ignition sources. Keep original containers closed and protect from moisture, dust, and contaminants. Avoid contact with oxidizing agents. Maintain clean, segregated storage. Recommended ambient storage; avoid prolonged temperatures above 50°C. Follow local regulations and SDS. Use first-in, first-out stock rotation. |
| Shelf Life | Versalis Pharmalene MS 20 PH: typically 2 years from manufacture when stored unopened in original packaging, dry, below 40°C, away from direct sunlight. |
On rotary blow-fill-seal equipment with 12–24 filling stations, Pharmalene MS 20 PH is incorporated at 20–40 wt% within an LDPE-rich wall formulation to raise environmental stress crack resistance while preserving parison hang strength. The governing pharmacopoeial framework is Ph. Eur. 3.1.5 for polyethylene with additives for parenteral and ophthalmic preparations, supplemented by USP <661.1> for container plastics and extractables profiling under ICH Q3D. In this process, barrel zones are run from 165°C to 200°C and the die head at 185–200°C; wall thickness distribution is held within ±0.05 mm, and filling and sealing are completed in a single mould station with mould-clamping force between 30 kN and 100 kN per cavity depending on container mass. Addition above 40 wt% of the LLDPE fraction produces a measurable drop in parison tensile elongation, leading to swing and fold-over defects on high-cavitation lines, while addition below 20 wt% does not provide sufficient resistance to autoclave flex-cracking. Gravimetric dosing at the feed throat is controlled to ±0.5 wt% because poor dispersion at lower melt temperatures yields unmelted LLDPE domains visible as fish-eyes in the container wall. Terminal formats include single-dose ophthalmic droppers, 0.4–5 mL nebulising solution ampoules, and preservative-free saline units requiring low additive migration and low particulate load.
For primary large-volume parenteral and enteral nutrition bags, Pharmalene MS 20 PH is used as the sealant web at 70–100 wt%, with the balance being LDPE or an EVA-free tie resin to avoid vinyl acetate migration into the liquid contact layer. The film is produced on three-layer blown-film lines with a die gap of 1.8–2.4 mm and a blow-up ratio of 2.0–2.5; extruder diameters are typically 50–70 mm with L/D 30:1 barrier screws to limit shear-induced gel formation. Heat-seal strength is tested under ASTM F88/F88M-21, and the seal initiation temperature for the LLDPE-rich layer is 105–115°C; production sealing windows are set at 135–160°C with dwell times of 0.5–1.2 s. If the LDPE diluent rises above 30 wt%, seal strength after autoclave post-treatment at 121°C becomes unstable due to reduced hot-tack and stress-cracking resistance at the seal interface. Compliance is demonstrated under USP <661.1>, Ph. Eur. 3.1.5, ISO 10993-5, and ISO 10993-10 for leachables following terminal steam sterilisation. On high-output lines, the limiting defect is seal-web scatter: when screw speed exceeds 90 rpm on 60 mm grooved-feed extruders without fluoropolymer PPA, die lip build-up produces visible gel specks in the sealant web, forcing a line interruption every 8–12 h. Terminal products include 100–5000 mL non-PVC IV bags, irrigation fluid bags, and enteral feeding containers.
| Film structure | Sealant layer addition ratio | Blown film process window | Seal strength requirement | Terminal format |
|---|---|---|---|---|
| 3-layer LDPE / tie / LLDPE | 70–100 wt% Pharmalene MS 20 PH | die gap 1.8–2.4 mm, BUR 2.0–2.5, melt temperature 185–210°C | ASTM F88/F88M-21 ≥ 2.5 N/15 mm | 100–5000 mL IV and irrigation bags |
| 5-layer PP / tie / LLDPE / tie / PP | sealant layer 80 wt% Pharmalene MS 20 PH / 20 wt% LDPE | die gap 2.0–2.4 mm, BUR 2.2–2.6, melt temperature 200–220°C | ASTM F88/F88M-21 ≥ 3.0 N/15 mm | 1000–3000 mL enteral nutrition bags |
Sterile barrier pouches for Class II and Class III devices are converted from multi-layer laminates in which a 40–80 µm LLDPE sealant web carries the sealing function and is corona treated to 38–42 mN/m before lamination. The recommended formulation is 80 wt% Pharmalene MS 20 PH with 20 wt% LDPE and 1–2 wt% silica-free slip/antiblock masterbatch; exceeding 2 wt% additive creates visible haze and reduces peroxide sterilisation compatibility of the seal. Compliance is governed by ISO 11607-1:2019 for packaging design and ISO 11607-2:2019 for process validation, with material biocompatibility assessed under ISO 10993-5 and ISO 10993-10. On pouch-making lines, seal bars are run at 125–150°C with pressure 0.4–0.8 MPa and dwell 0.5–1.0 s; burst strength is checked under ASTM F2054/F2054M-21 and seal integrity by dye penetration to ASTM F1929-15. The sealant layer must remain below 60 µm where Tyvek lid peel initiation is required, because thicker LLDPE webs increase peel-force variability and can transfer heat through the lamination during rotary sealing. Terminal types include pre-sterilised catheter pouches, syringe blister lids, wound-care kit pouches, and surgical procedure kit overwrap.
Cleanroom layflat tubing for aseptic transfer and bulk pharmaceutical powder handling is extruded from 100 wt% Pharmalene MS 20 PH; no regrind is permitted when the film is intended for product-contact sampling. The process is run on single-layer blown-film lines equipped with 45–65 mm barrier screws, L/D 30:1, melt filtration at 100–150 µm, and HEPA-filtered cooling air. Bubble stability is maintained at a blow-up ratio of 1.8–2.2 and die gap 1.2–2.0 mm; the melt temperature is limited to 190–210°C because higher temperatures accelerate low-molecular-weight species migration into the tube surface. Die drool is the principal production fault: once the die lip accumulates oxidised polymer, film gel defects exceed the reject threshold of 0.3 mm and the line must be purged. In-process melt flow rate is verified under ISO 1133-1:2022 and density by ASTM D792-20 to detect batch-to-batch shifts that would alter bubble geometry. Compliance references FDA 21 CFR 177.1520 for olefin polymers in drug contact, USP <661.1> for plasticised container components, and USP <88> Class VI for systemic injection testing. Published data for the exact gel-count distribution on this grade in Class 100 laminar-flow tubing is limited, so incoming resin lot acceptance must include an internal film extrusion test rather than relying solely on pellet inspection. Terminal products include sterile API sampling bags, disposable liner bags for 50–200 L drums, and component transfer bags used in isolator-based filling lines.
Induction-seal liner webs are formulated with 60–80 wt% Pharmalene MS 20 PH, 20–40 wt% LDPE, and, where barrier function is required, a 0.05–0.10 mm aluminium foil layer is introduced by adhesive lamination rather than coextrusion. The film is produced by cast extrusion at melt temperatures of 200–230°C and then die-cut into liner discs; downstream induction sealing is conducted at 0.8–1.5 s with a frequency of 350–500 kHz depending on cap diameter. The olefin layer must satisfy FDA 21 CFR 177.1520 and USP <661.1>; extractables testing is performed under ICH Q3D and USP <1663>. Terminal types include induction-sealed HDPE and PET pharmaceutical bottles for liquid oral products and effervescent tablets. A documented boundary is that the liner should not be specified for autoclaved closures at 121°C because the sealant layer softens and torque retention drops; published data for this specific configuration is limited.
Freezer-grade overwrap for vaccine cold-chain distribution and frozen clinical trial kits uses Pharmalene MS 20 PH as the main polyolefin layer at 100 wt% or in a 90/10 blend with LDPE for improved seal initiation. Film is blown on 50–70 mm extruders at melt temperatures of 180–210°C with a die gap of 1.5–2.0 mm, then converted into pre-formed sleeves and gusseted bags; dart impact at -40°C is evaluated under ASTM D1709-22. The cold-chain packaging specification is supported by ISTA 7E for insulated shipping containers and WHO temperature-controlled distribution guidance; material compliance is covered by FDA 21 CFR 177.1520 and EU 10/2011 where the film is not classified as primary pharmaceutical packaging. Terminal formats include secondary overwrap for frozen investigational medicinal products, gel-pack pouches, and insulated shipper liners with dimensional stability down to -40°C. The film should not be used for primary cell therapy contact without additional extractables and endotoxin validation under USP <85> and USP <161>.
Competitive Versalis Pharmalene® MS 20 PH Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis Pharmalene® MS 20 PH Linear Low Density Polyethylene is manufactured as a controlled polyolefin for primary pharmaceutical packaging and medical device components. The grade designation places it within the Pharmalene family, which is differentiated from general-purpose LLDPE by restricted additive selection, lot-level documentation, and alignment with pharmacopoeial and food-contact compliance pathways. The numerical suffix 20 is conventionally associated with a nominal melt flow rate of 20 g/10 min when determined under ISO 1133-1:2022 at 190 °C and 2.16 kg, but the current Versalis technical datasheet is the controlling source for lot-specific values. Published third-party data for this exact configuration are limited; therefore values below that are not grade-specific are explicitly identified as typical linear low density polyethylene class ranges.
Injection moulding of thin-wall pharmaceutical vessels and closures with this class of LLDPE is typically performed on hydraulic or electric toggle presses with clamp force between 600 kN and 2500 kN, depending on projected area and cavity count. A general-purpose polyolefin screw with an L/D ratio of 18:1 to 22:1 and compression ratio of 2.5:1 to 3.0:1 is specified. Barrel zone settings from feed to nozzle are commonly 180 °C, 200 °C, 215 °C, and 220 °C; the nozzle is usually held at 215 °C to 230 °C. Mould temperature is maintained at 15 °C to 40 °C for rapid solidification and low haze. Because LLDPE has a relatively narrow oxidative stability window, residence time at melt temperature above 240 °C should be minimised; prolonged hold-up in hot-runner manifolds above 6 min can shift molecular weight distribution and increase yellowing. No predrying is normally required when bulk moisture is below 0.05 wt%. If resin has been stored in uncontrolled humidity above 60% RH, a desiccant hopper at 65 °C for 2 h is applied to prevent splay in thin-wall sections.
When hot-runner tools with multiple valve gates are used, melt pressure at the nozzle is usually held between 60 MPa and 120 MPa, with holding pressure from 40 MPa to 70 MPa and back pressure from 0.5 MPa to 1.5 MPa. The fast-crystallising nature of linear low density polyethylene supports short cooling times in sections of 0.8 mm to 1.5 mm, but gate freeze time should be confirmed by short-shot studies because premature gate freeze can produce sink marks in thicker bosses. Screw rotation speed during plastication is typically limited to 80 min⁻¹ to 120 min⁻¹ for melt flow rates near 20 g/10 min to limit shear heating. Check-ring condition and reverse-flow leakage should be monitored batch-to-batch, because excessive clearance increases melt residence time and degrades the additive package.
Pharmaceutical packaging resins are not self-certifying; they are supported by manufacturer documentation and end-use verification. The Pharmalene family is positioned for uses that require reference to Regulation (EU) No 10/2011 and its amendments for plastic food-contact materials, and to pharmacopoeial chapters for plastic containers. For olefin polymers used in contact with solid and liquid oral dosage forms, FDA 21 CFR 177.1520 establishes the permitted polymer structure and extractables limits, while USP <661> and Ph. Eur. 3.1.3 apply more directly to container materials. ICH Q3D is relevant only at the finished drug product level, with elemental impurity risk assessment supported by polymer composition data. Cytotoxicity testing under ISO 10993-5 is generally required only where the polymer is used for medical devices or implants; for simple packaging, the extraction tests of the pharmacopoeias are the primary concern.
| Standard / regulation | Scope | Applicability to MS 20 PH | Verification requirement |
|---|---|---|---|
| FDA 21 CFR 177.1520 | Olefin polymers for food contact | Requires density, extractives, and maximum soluble fraction limits | Lot-specific certification from Versalis |
| Regulation (EU) No 10/2011 | Plastic food-contact articles | Overall migration limit of 10 mg/dm² under specified simulants | End-use article testing |
| USP <661> | Plastic packaging systems | Physicochemical testing including extraction and UV absorbance | Material supplier data plus final container testing |
| Ph. Eur. 3.1.3 | Polyolefins for containers | Appearance, acidity/alkalinity, UV absorbance, reducing substances | Final product compliance |
| ICH Q3D | Elemental impurities | Risk assessment not direct resin test | Composition profile from supplier |
| ISO 10993-5 | Cytotoxicity | Only if medical device classification applies | Not normally required for primary packaging |
A direct substitution of Pharmalene MS 20 PH for a high-pressure LDPE in an existing tool will not yield identical process outcomes. LLDPE of the 20 g/10 min class has lower melt strength and less pronounced shear thinning than LDPE at similar density, which reduces pressure drop through narrow gates but can increase jetting if gate speed is not adjusted. Tensile yield stress in LLDPE class materials is roughly 8 MPa to 20 MPa compared with 6 MPa to 12 MPa for many LDPE film grades, while puncture resistance and environmental stress crack resistance are higher. The trade-off is reduced clarity in thick sections and a narrower heat-seal plateau, so sealing parameters determined for LDPE cannot be transferred without resealing trials. Compared with HDPE, MS 20 PH is expected to provide lower modulus and lower Vicat softening point, which can be beneficial for squeezable closures but limits steam sterilisation above 121 °C. Compared with pharmaceutical-grade polypropylene, LLDPE has lower continuous-use temperature, lower modulus, and higher flexibility, but it may exhibit higher permeability to oxygen and water vapour; barrier requirements therefore determine whether an additional coating or aluminium foil lamination is needed.
Selection of Pharmalene MS 20 PH is most defensible when the closure or container must combine stress crack resistance, sealability, and high flow for thin-wall moulding. Environmental stress cracking resistance under ASTM D1693 is typically higher for LLDPE than for HDPE in the same melt flow range, although test duration and failure criterion must be matched to the actual stress state. For child-resistant closures with snap features, LLDPE provides a lower flexural modulus than HDPE, reducing insertion force; however, the lower modulus also reduces torque retention in threaded caps unless thread height is increased. In blow-fill-seal applications, LLDPE melt strength is lower than that of high-pressure LDPE, so parison control requires downward adjustment of melt temperature and higher extrusion head pressure. Where autoclaving at 121 °C is required, polypropylene or HDPE may be preferred because typical LLDPE Vicat softening points fall between 85 °C and 110 °C. Final selection is governed by drug formulation, closure torque specification, and extraction profile rather than by a single mechanical property.
Pharmaceutical-grade LLDPE typically contains a phenolic or phosphite antioxidant system at total loading below 0.1 wt%, plus a neutraliser such as calcium stearate or zinc stearate at 0.02 wt% to 0.05 wt%. Slip and antiblock additives may be present for demoulding, but their specific chemistry and loading are not disclosed in third-party literature. Extractable hydrocarbon oligomers are controlled by polymerisation process and pellet degassing; residual comonomer and low molecular weight waxes are reduced to avoid failing UV absorbance limits in Ph. Eur. 3.1.3 and USP <661>. Because olefins are inherently hydrophobic, aqueous extraction values are typically low; however, lipophilic drug formulations may require additional migration testing with the actual drug product or a suitable simulate such as 95% ethanol under Regulation (EU) No 10/2011.
The apparent viscosity of a 20 g/10 min LLDPE at 200 °C under injection moulding shear rates of 10³ s⁻¹ to 10⁴ s⁻¹ is typically 40 Pa·s to 80 Pa·s, but the precise curve is grade-specific and should be obtained from capillary rheometry under ISO 11443:2021. Compared with a 2 g/10 min LLDPE film grade, the 20 g/10 min class provides lower pressure drop in thin-wall sections but lower melt strength and greater potential for gate blush. For multicavity filling, melt pressure drop in a cold runner of 1.2 mm diameter and 20 mm length can exceed 20 MPa at high injection speeds; runner sizing must therefore balance pressure loss against premature gate freeze. Processors should avoid melt temperatures above 240 °C because thermal-oxidative degradation of the phenolic antioxidant package reduces stabilisation capacity and can increase peroxide content.
Comparative mechanical and thermal property ranges for LLDPE, LDPE, HDPE, and polypropylene are listed in Table 2. These values are class ranges from public standards and are not grade-specific for Pharmalene MS 20 PH.
| Property | Test method | LLDPE class | LDPE class | HDPE class | PP class |
|---|---|---|---|---|---|
| Density | ISO 1183-1:2019 | 0.915–0.940 g/cm³ | 0.910–0.935 g/cm³ | 0.940–0.970 g/cm³ | 0.890–0.910 g/cm³ |
| Tensile yield stress | ISO 527-2:2012 | 8–20 MPa | 6–12 MPa | 20–32 MPa | 25–40 MPa |
| Elongation at break | ISO 527-2:2012 | >500% | >300% | >300% | >50% |
| Vicat softening point | ISO 306 | 85–110 °C | 80–100 °C | 110–130 °C | 140–160 °C |
| Flexural modulus | ISO 178:2019 | 200–500 MPa | 150–350 MPa | 800–1600 MPa | 900–1700 MPa |
On a production-scale packaging line, lot-to-lot variation in melt flow rate should be monitored using ISO 1133-1:2022 and density under ISO 1183-1:2019. A shift of melt flow rate from 19 g/10 min to 22 g/10 min can alter fill time by 0.2 s to 0.5 s in a 16-cavity hot-runner tool, which may affect flash formation in thin-wall parts. Density drift of 0.002 g/cm³ can modify secant modulus and closure dimensions. Incoming resin should therefore be sampled according to AQL 0.65 or AQL 1.0 depending on criticality, and the cavity pressure curve should be archived for each batch. For extruder-based processes, gel count and black specks are evaluated by film optical inspection according to ISO 12625 or internal vendor methods; a rise in gel count above the agreed limit indicates additive agglomeration or contamination and requires line shutdown.
Within the Pharmalene family, grades are differentiated by melt flow rate, density, and additive package. A nominal 20 g/10 min product such as MS 20 PH is intended for high-speed injection moulding of thin-wall components, whereas lower melt flow rate grades in the same family are likely intended for blown film or blow moulding where higher melt strength is required. The PH suffix indicates pharmaceutical documentation, but does not by itself guarantee compliance with a particular pharmacopoeia; end-users must confirm that the specific grade appears on the supplier’s drug master file or food-contact declaration.