| HS Code | 206651 |
| Density | 0.934 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 5.0 g/10 min |
| Melting Point | 124 °C |
| Vicat Softening Temperature | 104 °C |
| Tensile Strength At Break | 20 MPa |
| Elongation At Break | 600% |
| Flexural Modulus | 400 MPa |
| Shore D Hardness | 50 |
| Haze | 20% |
| Gloss 45 | 50% |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
As an accredited Versalis Pharmalene® MR 50 PH Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis Pharmalene® MR 50 PH Linear Low Density Polyethylene is packaged in 25 kg polyethylene bags, palletized for industrial handling. |
| Container Loading (20′ FCL) | 20′ FCL container loading: Versalis Pharmalene® MR 50 PH Linear Low Density Polyethylene in 25 kg bags, palletized and shrink-wrapped. |
| Shipping | Versalis Pharmalene® MR 50 PH Linear Low Density Polyethylene is non-hazardous and not regulated for transport. It is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped. Ship in clean, dry, covered trucks or containers. Protect from moisture, direct sunlight, heat, odors, punctures, contamination, and excessive stacking. |
| Storage | Store Versalis Pharmalene® MR 50 PH in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep in original, tightly closed packaging, palletized and off the floor. Protect from moisture, dust, and contamination. Avoid prolonged elevated temperatures, static buildup, and strong oxidizers. Do not store outdoors; follow local regulations and good housekeeping practices. |
| Shelf Life | Typically 24 months when stored unopened in original packaging, cool and dry, protected from direct sunlight and moisture. |
Pharmalene MR 50 PH is processed in high-output blown-film lines for oral powder sachets where seal initiation temperature, hot-tack strength, and coefficient of friction control final packaging performance. In a three-layer coextrusion configuration with 30:1 L/D barrier screws and 1.8–2.2 mm die gap, the resin is run at melt temperature 195–215°C, blow-up ratio 2.4–2.8, and frost-line height 400–550 mm. The formulation addition rate is 65–80 wt% Pharmalene MR 50 PH, 15–25 wt% high-pressure LDPE for bubble stability, and 5–10 wt% silica/erucamide antiblock-slip masterbatch letdown; free-flow additives are not dry-blended into the main feed unless pre-dispersed, because localized slip accumulation causes seal-strength scatter under ASTM F88/F88M-21. Compliance verification for the finished film references EU Regulation (EU) No 10/2011 Annex I overall migration limit of <10 mg/dm², FDA 21 CFR 177.1520 olefin polymer specifications, Ph. Eur. 3.1.3 for polyolefins, and Ph. Eur. 3.1.5 where the material is used in packaging for aqueous oral preparations. Destructive seal strength is tested at 2.0 N/15 mm minimum for non-peelable sachets and 0.5 N/mm minimum for peelable configurations after 0.3–0.6 MPa crimp-jaw pressure. Terminal product types include unit-dose oral powder sachets, granule sachets for reconstitution, and desiccant sachets inserted into secondary packaging; each converter lot requires migration verification for total non-volatile residue and specific migration of slip additives under the applicable food-contact monograph.
Pharmalene MR 50 PH is processed in biaxial rotational moulding cells for single-use bioprocess containers where wall-thickness uniformity, low extractables, and smooth internal surfaces are critical. The powder charge is typically 100 wt% resin with 0.10–0.20 wt% hindered phenolic antioxidant and 0.05–0.15 wt% zinc stearate or phosphite processing stabilizer; addition of recycled regrind is limited to 10–15 wt% because thermal history shifts peak internal air temperature and increases the risk of incomplete particle coalescence. Moulds are rotated at a primary/secondary ratio of 4:1, oven temperature 260–290°C, and peak internal air temperature is held at 190–200°C for LLDPE; exceeding 205°C accelerates surface oxidation and generates extractable degradation species, while stopping below 175°C leaves pinholes and sintered particle boundaries. Forced-air cooling is used to 90–95°C before water spray or mist cooling; cooling rates above 4 K/min in the 100–90°C window increase flat-panel warpage and create parting-line dimensional drift on large flat surfaces. Compliance verification includes USP <661.1> plastic materials of construction, USP <661.2> packaging systems for pharmaceutical use, ISO 10993-5:2009 in vitro cytotoxicity, and USP <87> biological reactivity. Terminal products include 5 L to 1,000 L single-use mixing vessels, buffer transport carboys, and sterile intermediate containers; published data for this specific grade at the upper 1,000 L scale is limited, so mould-specific qualification is required before routine production.
Cast-film sealant layers for pre-sterilized medical device pouch lidding are subject to seal-strength stability after ethylene oxide or gamma sterilization. In a cast coextrusion line with chill-roll surface temperature 18–22°C and automatic gauge control maintaining ±2% thickness deviation, MR 50 PH is formulated at 80–90 wt% of the sealant skin, with 10–20 wt% metallocene-catalyzed LLDPE to lower seal initiation temperature to 80–85°C. The sealant layer thickness is normally 20–40 µm within a 70–120 µm total structure. Compliance for the finished pouch is verified against ISO 11607-1:2019, ASTM F88/F88M-21 seal strength, ASTM F1929-15 dye penetration after seal, and ISO 10993-5 where the pouch contacts a medical device. Downstream processing includes slitting of cast rollstock, multi-lane pouch converting with heated crimp jaws at 0.3–0.6 MPa seal pressure, and ethylene oxide sterilization at 50–55°C without seal delamination or fiber tear. Terminal product types include chevron peel pouches, header pouches for syringes, and lidding webs for in-vitro diagnostic reagent kits; each of these requires seal verification after both unstressed and sterilized conditions to account for slip-additive migration to the seal surface.
| Application scenario | Primary standard | Test method / monograph section | Finished-article target |
|---|---|---|---|
| Blown sachet film | Ph. Eur. 3.1.3 / 3.1.5 | Non-volatile residue, heavy metals, acidity/alkalinity | Monograph conformance |
| Rotational-moulded bioprocess vessel | USP <661.1> / <661.2> | Physicochemical tests | No adverse biological reactivity |
| Cast-film medical pouch lidding | ISO 11607-1:2019 | ASTM F88/F88M-21, ASTM F1929-15 | Seal strength ≥0.5 N/mm; no dye channel |
| Blow-moulded bottle | FDA 21 CFR 177.1520 | End test / extraction per conditions of use | Conforms to olefin polymer specifications |
| Injection-moulded fitment | USP <661.1> | USP <381> where applicable | Elastomeric closure conformance if used in delivery |
| Extrusion coating on foil | EU 10/2011 | EN 1186 series, overall migration | <10 mg/dm² or 60 mg/kg |
Blow-moulded squeeze bottles require higher melt strength than LLDPE provides alone, so the formulation uses 80–90 wt% MR 50 PH with 10–20 wt% HDPE of melt flow rate 0.3–0.8 g/10 min; this blend preserves flex-crack resistance while reducing parison sag on long-stroke shuttle machines. The resin is processed on blow moulders with 24:1 L/D screws, melt temperature 180–205°C, accumulator head or continuous parison programming, and mould temperature 10–15°C. Parison length is controlled by a conical die gap from 2.0 mm to 3.5 mm; a 0.5 mm change in die gap at the upper setting alters top-load and sidewall distribution by more than 5%, requiring revalidation of drop test and volumetric fill tolerance. Compliance is evaluated under FDA 21 CFR 177.1520 for olefin polymers, EU Regulation (EU) No 10/2011, Ph. Eur. 3.1.5, and USP <661.1> where the bottle is part of a dosage delivery system. Terminal products include 20 mL to 250 mL collapsible oral liquid bottles, dropper bottles with LDPE tips, and irrigation squeeze containers; batch-to-batch variance in parison sag is monitored by recording parison length at 90 s after extrusion stop and correlating that value with sidewall thickness at the label panel.
Flexible injection-moulded fitments for pharmaceutical packaging are produced by dosing MR 50 PH neat at 100% or with 2–4 wt% color and additive masterbatch where ultraviolet shielding or laser marking is specified. The processing window is narrower than for general-purpose injection moulding; barrel temperatures are set from 200°C at the feed to 230°C at the nozzle, screw back pressure 40–80 bar, and injection speed 80–150 mm/s depending on part thickness. Clamp force is selected at 6–8 kN/cm² of projected area because low melt viscosity produces flash at the parting line when clamp force is insufficient, altering dimensional tolerances for press-fit closures. Compliance for finished fitments references USP <661.1>, FDA 21 CFR 177.1520, and EU Regulation (EU) No 10/2011; if used in parenteral delivery, additional evaluation under Ph. Eur. 3.1.5 or USP <381> may be required depending on the final device classification. Terminal products include flexible over-caps, tamper-evident snap-fit rings, dispensing nozzle adapters, and integrated scoop dosage cups for powder packaging; published data for this specific grade in small multi-cavity tools is limited, so short-shot and ejection studies should be repeated after mould modifications because flow hesitation at thin hinges can produce dimensional instability.
Pharmalene MR 50 PH is applied as an extrusion coating on aluminium foil or metallised substrates when the lamination must combine moisture barrier with low seal initiation. The coating add-on is 25–40 g/m², with 85–90 wt% MR 50 PH and 10–15 wt% LDPE or metallocene-catalyzed LLDPE to reduce neck-in; ozone treatment at 0.5–1.0 kW/m die width and primer application are used to raise adhesion above 2.5 N/15 mm. Extruder temperatures are set at 280–310°C to oxidize the melt surface sufficiently for foil bonding; above 320°C gel formation and odour increase, while below 270°C peel adhesion becomes inconsistent across the web. Compliance is verified under EU Regulation (EU) No 10/2011 Annex I and FDA 21 CFR 177.1520 for the coated substrate, and seal strength is tested under ASTM F88/F88M-21 after 3-s dwell at 140–150°C jaw temperature. Terminal products include cold-form lidding foil, peel-push blister lidding for orally disintegrating tablets, and barrier overwrap laminates for effervescent formulations; the neck-in at die edges must be compensated by deckle adjustment of 10–15 mm per side to prevent edge-bead thickness deviation during subsequent slitting.
Competitive Versalis Pharmalene® MR 50 PH Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis Pharmalene® MR 50 PH Linear Low Density Polyethylene is a high-flow, pharmaceutical-grade linear low density polyethylene supplied for injection moulding of thin-wall closures and small precision components. The numeric portion of the grade, 50, denotes a nominal melt mass-flow rate of 50 g/10 min measured at 190 °C and 2.16 kg load in accordance with ISO 1133-1:2022. The PH suffix identifies the product within the Versalis pharmaceutical packaging portfolio, where additive composition and documentation are managed for pharmacopoeial contact applications.
The base polymer is an alpha-olefin copolymer characterised by short-chain branching distributed along a linear backbone. Published data from Versalis list a density of 0.928 g/cm³ when determined by ISO 1183-1:2019. That density position is higher than common film-grade LLDPE values in the 0.918–0.922 g/cm³ band, shifting the mechanical response toward greater modulus and higher top-load capacity in cylindrical closure designs. Because LLDPE architecture combines short-chain branches with low long-chain-branch content, environmental stress crack resistance is superior to low density polyethylene of comparable density and melt viscosity.
The following physical and mechanical values are representative release data for natural grade; they are not intended as specification limits. Certificates of analysis from the supplier control individual production lots against the purchaser’s agreed specification. Values are obtained on injection-moulded specimens conditioned at 23 °C and 50 % relative humidity for 48 h unless otherwise stated.
| Property | Test method | Typical value | Unit |
|---|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 | 50 | g/10 min |
| Density | ISO 1183-1:2019 | 0.928 | g/cm³ |
| Tensile stress at yield | ISO 527-2:2012 | 12 | MPa |
| Tensile strain at break | ISO 527-2:2012 | >300 | % |
| Vicat softening temperature | ISO 306:2013 A50 | 88 | °C |
| Shore D hardness | ISO 868:2003 | 56 | — |
High melt-flow rate reduces gate pressure loss and permits filling of wall sections between 0.6 mm and 1.0 mm without excessive shear heating. On a production-scale injection moulding machine with 1,200 kN clamp force, a 36 mm barrier screw, and a valve-gated hot runner, closure tools with 16 to 32 cavities are processed with melt temperatures between 210 °C and 240 °C. Sustained barrel temperature above 250 °C or residence time beyond 5 min can promote oxidative degradation and formation of low-molecular-weight odorous species. The shot volume is maintained between 25 % and 75 % of available barrel capacity to limit residence-time distribution in the screw.
The mould temperature is usually kept at 20–40 °C with turbulent water channels to achieve rapid skin solidification and short cycle times. Hold pressure is typically set between 40 MPa and 70 MPa at the hydraulic cylinder, but the set point must be confirmed against cavity-pressure transducer data. A gate-freeze study using cavity-pressure decay is required for each tool because high-flow grades can freeze thin gates rapidly after transfer to hold pressure.
At low shear rates the grade has lower melt viscosity than a 20–25 g/10 min LLDPE closure resin, which reduces pressure loss in hot-runner channels. The consequence is that high-cavitation filling can be achieved with lower injection pressure; however, the melt may also sag in large runner systems if decompression is insufficient. Apparent shear rates above 10,000 s⁻¹ in small direct gates can raise local temperature by 10–20 °C through viscous dissipation, narrowing the practical upper melt setpoint when the nominal barrel profile is already near 240 °C.
MR 50 PH is specified for primary pharmaceutical packaging applications where resin documentation must support regulatory submissions. The resin is evaluated under Ph. Eur. 3.1.3 for polyolefines and USP <661.1> for plastic packaging materials; compliance is demonstrated on the finished component because extraction conditions depend on surface-to-volume ratio, closure geometry, and processing history. In the United States, the base polymer may fall under 21 CFR 177.1520 for olefin polymers in contact with food or drugs, while pharmaceutical acceptability commonly requires a separate extractables assessment following USP <1663> and a leachables evaluation under USP <1664> in the actual drug product.
| Framework | Designation | Application boundary |
|---|---|---|
| US Pharmacopeia | USP <661.1> | Material of construction for plastic packaging systems |
| European Pharmacopoeia | Ph. Eur. 3.1.3 | Polyolefines for containers and closures |
| US FDA | 21 CFR 177.1520 | Olefin polymers for food and pharmaceutical contact |
| EU | Regulation (EU) No 10/2011 | Plastic food-contact materials and articles; overall migration limit 10 mg/dm² |
| ISO | ISO 10993-1:2018 | Biological evaluation of medical device components, only if the finished closure is part of a device claim |
Extractables behaviour is strongly influenced by the additive package. The grade is supplied with an additive system limited to an antioxidant and acid scavenger; the exact formulation is controlled under the pharmaceutical documentation package. Users requiring surface lubricity must qualify a masterbatch that will alter the extractables profile, because the unmodified granulate does not provide internal slip equivalent to conventional film and extrusion-coating grades. Published data for this specific configuration is limited for custom drug formulations, so verification of the finished closure under simulated-use conditions is mandatory before registration.
Under 21 CFR 177.1520(c)(1), the base olefin polymer may be subject to an n-hexane extractable fraction limit; exact values are lot-specific and should be obtained from supplier certificates of analysis. For EU food-contact applications, the plastic article falls under Regulation (EU) No 10/2011, and the overall migration limit of 10 mg/dm² applies as a screening value. Pharmaceutical closures frequently require more restrictive extractables acceptance criteria derived from toxicological assessment of the specific drug product.
Compared with a conventional LLDPE closure resin of 25 g/10 min melt mass-flow rate and similar 0.926–0.930 g/cm³ density, MR 50 PH reduces melt pressure loss in hot-runner channels and permits lower injection pressure for the same wall thickness. In high-cavitation tools, the grade may allow a reduction in melt temperature of 10–20 °C without short shots. These are rheological differences; they do not automatically translate into improved closure performance because top-load strength, strip torque, and seal integrity are geometry-dominated.
Higher melt flow also increases the tendency for flash on worn parting lines and can reduce melt strength around large gates when cushion control is imprecise. Mould maintenance intervals for parting line flatness should be shortened if flash appears at packing pressures previously accepted for a lower-MFR grade. The change from conventional general-purpose to pharmaceutical-designated LLDPE does not remove the need for purging previous polymers. A low-viscosity polyolefin purge or the same material at elevated melt temperature should be used after processing PVC or acetal, because residual contamination can produce surface specks in a closure wall.
Compared with low density polyethylene, the linear backbone provides higher tensile strength at equivalent density and greater environmental stress crack resistance in dilute detergent media under ASTM D1693-21. Compared with high density polyethylene, the 0.928 g/cm³ density reduces stiffness, which may lower thread strip torque but increases ductile failure resistance in drop impact under ASTM D2463-15. These differences position the grade for closures that must survive cold-condition handling without brittle fracture.
Application scope centres on oral pharmaceutical packaging components. Tamper-evident bands, child-resistant outer caps, dropper collars, and dispensing spouts exploit the resin’s high fluidity because wall thicknesses are often below 1.0 mm. Dimensional acceptance is governed by the closure specification, not by the resin datasheet; statistical process control on thread diameter and bridge thickness is conducted at the moulding machine. Child-resistant closure functionality is assessed under ISO 8317:2015; the resin is only an engineering input to the design and does not confer child-resistance by itself.
Post-mould conditioning for dimensional stability follows ISO 291:2008 class 23/50 conditions: 23 °C and 50 % relative humidity. Linear shrinkage for LLDPE injection mouldings commonly falls between 1.5 % and 2.0 %, but the value for MR 50 PH must be measured on the specific tool because packing pressure, gate freeze, and cooling time shift post-mould dimensions. Accelerated dimensional checking at 40 °C can be used during process validation to separate immediate shrinkage from progressive crystallisation.
MR 50 PH is not supplied sterile. Gamma irradiation and ethylene oxide terminal sterilisation are possible for polyethylene components, but published data for this specific grade under a defined radiation dose is limited. Polyolefins undergo free-radical reactions during irradiation; above a cumulative dose of approximately 25 kGy, colour shift, oxidation, and a measurable change in melt-flow or tensile elongation may appear in some LLDPE formulations. The closure manufacturer must validate the entire component, because polymer response depends on wall thickness, pigment package, and residual antioxidant concentration.
Ethylene oxide processes require subsequent aeration and residual gas testing under ISO 10993-7:2008. Autoclave treatment at 121 °C may approach or exceed the Vicat softening temperature of 88 °C, creating risk of dimensional distortion; autoclaving is not a default sterilisation route for this LLDPE closure material unless supported by part-specific dimensional data. The material is not indicated for implantable medical devices or long-term tissue contact and does not carry an automatic ISO 10993 biological assessment for that purpose.
The resin is insoluble in water and resistant to dilute aqueous acids and bases at ambient temperature, but aromatic solvents, chlorinated solvents, and some essential oils can cause stress cracking in loaded polyethylene mouldings. Environmental stress crack resistance should be screened under ASTM D1693-21 when the closure is in contact with aggressive drug-product formulations or cleaning agents. Strong oxidising agents are incompatible at processing temperatures; halogen-containing or peroxide concentrates may generate acid species and must not be introduced into the screw without prior purging with a chemically inert carrier.
No desiccant drying is required for the unmodified polyolefin granulate. If cold granules are transferred into a warm production room from an unheated warehouse, surface condensation is allowed to evaporate before hopper loading; residual surface moisture can produce splay in small gates.