| HS Code | 121427 |
| Density | 0.960 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.35 g/10 min |
| Melt Flow Rate 190 C 21 6 Kg | 22 g/10 min |
| Tensile Stress At Yield | 28 MPa |
| Tensile Strain At Break | >600% |
| Flexural Modulus | 1300 MPa |
| Charpy Notched Impact Strength 23 C | 12 kJ/m² |
| Shore D Hardness | 65 |
| Vicat Softening Temperature | 126°C |
| Heat Deflection Temperature 0 45 Mpa | 78°C |
| Environmental Stress Cracking Resistance | >1000 h |
| Brittleness Temperature | < -70°C |
| Water Absorption | <0.01% |
As an accredited Versalis HDPE SB 60 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis HDPE SB 60 comes in 25 kg polyethylene bags, palletized and stretch-wrapped for industrial shipping and storage. |
| Container Loading (20′ FCL) | Versalis HDPE SB 60 in 25 kg bags, palletized and shrink-wrapped, safely loaded and secured inside a 20-foot FCL container. |
| Shipping | Versalis HDPE SB 60 is shipped as non-hazardous, solid polyethylene pellets in 25 kg bags, jumbo bags, or octabins, palletized and shrink-wrapped for road, rail, or sea transport. Not regulated as dangerous goods. Store dry, ventilated, away from heat, sunlight, and moisture. |
| Storage | Store Versalis HDPE SB 60 in its original, closed packaging in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and oxidizing agents. Protect from moisture, dust, oils, and chemical contamination. Keep pallets stable and avoid excessive stacking. Use clean handling equipment and follow FIFO. Consult the SDS for detailed precautions. |
| Shelf Life | Store in original packaging in a cool, dry, ventilated area away from sunlight; typical shelf life is 12 months. |
On continuous shuttle extrusion blow-moulding lines equipped with 24:1 to 30:1 L/D barrier screws and grooved feed sections, Versalis HDPE SB 60 is processed at melt temperatures between 180 °C and 230 °C, with die-head temperatures maintained in the 190–210 °C band to control parison sag on tooling with 15–40 mm die diameters. The material’s nominal melt flow rate of 0.60 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022 positions it for opaque detergent, household cleaner and personal-care bottles in the 0.25–5 L range where high melt strength and excellent pinch-off weld integrity are required. A representative formulation for a trigger-spray bottle body is 97.0 wt% HDPE SB 60, 2.0 wt% titanium dioxide masterbatch based on an LDPE carrier, and 1.0 wt% slip-antiblock masterbatch; total calcium stearate in the formulation should be held below 0.1 wt% to reduce die-lip plate-out during runs exceeding 72 h. Bottle wall thickness is typically maintained between 0.3 mm and 0.8 mm, with parison programming applying 10–20% die-gap reduction near the pinch-off zone to compensate for localized thinning. Blow-air pressure is set at 0.6–1.0 MPa, and mould temperature is kept in the 5–15 °C range to stabilise bottle geometry without excessive condensation in high-humidity packaging halls. Top-load resistance of finished bottles is assessed under ASTM D2659-11, while environmental stress-cracking resistance is verified under ASTM D1693-15 Condition B using 100% Igepal CO-630. The terminal parts include opaque trigger-spray bodies, refill pouches with HDPE necks, cosmetic cream pump bottles and HDPE jars where translucency is acceptable rather than optical clarity. A production-scale failure mode observed on shuttle machines is bottom pinch-off flash tearing caused by parison temperature below 180 °C; this is remediated by raising extruder Zone 3 and die-head setpoints by 5–10 °C and closing the die gap during the final 10% of parison extrusion.
Accumulator-head intermittent blow-moulding machines producing 20-L UN-certified jerry cans from HDPE SB 60 require accumulator shot capacity in the 1–3 kg range, clamp force from 600 kN to 1,200 kN, and extruder screw cooling to manage the adiabatic temperature rise from high-shear plastication. Wall-thickness distribution is programmed through an axial parison controller with top-section targets of 3.0–3.5 mm, mid-body targets of 2.0–2.5 mm, and pinch-off zone targets of 3.5–4.0 mm, because the handle area and side weld are the dominant stress concentrators in UN drop testing. The grade’s density class near 0.960 g/cm³ under ISO 1183-1:2019 provides moderate stiffness, while stacking performance at 40 °C is evaluated under ASTM D2659-11 for a duration of 28 days; in practice, stacking failure is often governed by seam thinning rather than bulk yield. Environmental stress-cracking resistance under ASTM D1693-15 Condition B is the controlling property for detergent and hydrocarbon-contaminated filling lines, and converters should verify batch-specific values above the 200 h threshold used as a common industrial screening criterion for this MFI and density class. UN certification under 6.1.5.3 includes drop tests at −18 °C, hydraulic pressure tests at 100 kPa for 30 min, and stacking tests; jerry cans must show no leakage after these sequences. A typical black industrial container formulation uses 2.0 wt% carbon black masterbatch with a PE carrier, 0.5 wt% antioxidant package, and 97.5 wt% HDPE SB 60, but UV-stabilised versions intended for outdoor storage add 0.3–0.5 wt% hindered amine light stabiliser masterbatch. Heavy-metal limits in packaging are referenced to EU 94/62/EC, with the sum of lead, cadmium, mercury and chromium VI not exceeding 100 mg/kg of packaging material. Terminal parts include jerry cans for lubricating oils, water-based emulsions, detergents and non-classified industrial liquids; dangerous goods rated UN 3H1/Z require additional permeation and compatibility testing specific to the filled chemical.
| Test | Standard | Condition | Operational boundary |
|---|---|---|---|
| Melt flow rate | ISO 1133-1:2022 | 190 °C/2.16 kg | 0.55–0.65 g/10 min for consistent parison hang-up |
| Density | ISO 1183-1:2019 | 23 °C | 0.958–0.962 g/cm³ |
| ESCR | ASTM D1693-15 | Condition B, 100% Igepal CO-630 | Above 200 h screening threshold |
| Top load | ASTM D2659-11 | 40 °C, 28 days | No seam splitting or yielding beyond test criterion |
| UN drop impact | UN 6.1.5.3 | −18 °C, 1.2 m for Packing Group II equivalent | No leakage from body, handle, or closure |
Food-contact jars and wide-mouth containers produced from HDPE SB 60 are subject to dual compliance burdens: the bulk polymer must meet the extractive and compositional limits of FDA 21 CFR 177.1520(c) for olefin polymers, and the finished article must comply with the overall migration limit of 10 mg/dm² under EU 10/2011 when tested with food simulants A, B, C and D2. Published migration data for this specific grade under fatty-food simulant D2 are limited; converters must commission specific migration testing on the final container because colour masterbatch carriers and external lubricants can alter extractive behaviour. Organoleptic performance is evaluated under DIN EN 1230-1 or equivalent sensory panel protocols, and the high molecular weight fraction in HMW-HDPE can contribute to low residual odour only if the melt temperature does not exceed 230 °C and the extruder is adequately vented. Hot-fill performance of HDPE SB 60 is constrained by the Vicat softening temperature class near 126 °C under ISO 306; sustained fill temperatures above 60 °C can cause neck ovalisation and closure back-off, making the grade unsuitable for pasteurised or hot-fill applications. A food-grade jar formulation typically uses 98.5 wt% HDPE SB 60 and 1.5 wt% food-contact white masterbatch; no regrind from non-food lines may be introduced unless the converter maintains a dedicated food-grade scrap stream. Mould cavity venting and surface polish control contact clarity, but HDPE SB 60 retains high haze in natural form, making it appropriate for dry-food jars, supplement bottles and opaque dairy-adjacent packaging rather than water-clear containers. Closure torque retention is tested according to ASTM D2063 or customer-specific protocols, with long-term cap removal torque sensitive to creep in the bottle neck at warehouse temperatures above 40 °C.
Agricultural chemical containers blown from HDPE SB 60 require separate verification of stress-cracking resistance under alkoxylate and ester formulations because high-density polyethylene with a density near 0.960 g/cm³ can exhibit reduced ESCR when processing conditions introduce excessive orientation or weld-line irregularities. Containers for pesticides, herbicides and adjuvants are commonly produced in the 5–20 L range on accumulator-head machines with a six-layer coextrusion structure: outer virgin HDPE SB 60, regrind layer, tie layer, EVOH barrier layer, tie layer, and inner virgin HDPE SB 60, with layer distribution near 22/35/2.5/3/2.5/35 expressed as percentages of total wall thickness. The EVOH layer delivers oxygen barrier performance measured under ASTM D3985-17 at 23 °C and 50% relative humidity, but its barrier function degrades abruptly above 80% RH unless the correct EVOH grade and desiccant additive are used. Environmental stress-cracking resistance is assessed under ASTM D1693-15 Condition C, which uses a more aggressive wetting agent than Condition B, and the finished container must pass drop tests from 1.2 m after conditioning at −18 °C for Packing Group II equivalents. Closure systems for agricultural containers are tested for torque retention and gasket compatibility under ASTM D3890 or fixed-torque leak tests; gaskets containing plasticisers can migrate into HDPE and accelerate stress cracking at the neck. A carbon black container formulation uses 2.0 wt% carbon black masterbatch, 0.5 wt% process stabiliser masterbatch and 97.5 wt% HDPE SB 60, while coloured coextruded containers for product coding use 3.0–4.0 wt% pigment masterbatch in the outer skin only. Terminal products include jerry cans for glyphosate formulations, selective herbicide concentrates, water-based fungicides and sprayer-ready adjuvants; compatibility testing is conducted according to the filler’s UN packing instruction and may include 28-day storage at 40 °C with 90% relative humidity to simulate tropical warehouse exposure.
Industrial solvent bottles produced from HDPE SB 60 as the structural layer are constructed with polyamide or EVOH barrier layers to reduce permeation of aromatic hydrocarbons, ketones and chlorinated solvents. The outer and inner layers of virgin HDPE SB 60 provide drop-impact resistance and environmental stress-cracking resistance, while a central barrier layer of EVOH with 32–38 mol% ethylene content or a PA6/PA66 blend restricts solvent transmission; published hydrocarbon permeation data for this specific multilayer configuration are limited, and converters must validate each solvent package gravimetrically or by gas chromatography according to SAE J1737 or equivalent internal protocols. Layer distribution in a five-layer construction is commonly set at 35/10/10/10/35 percent HDPE/tie/barrier/tie/HDPE, with the regrind layer replacing a portion of the HDPE outer layer only after barrier layer trim is kept below 5 wt% of the total structure to avoid degrading permeation performance. Incompatibility with strongly polar solvents such as methanol and certain brake fluids should be confirmed, because HDPE can soften or extract into these media; the grade is generally suited to aliphatic white spirits, aromatics in diluted formulations, and solvent-based cleaners in short-term packaging, not for indefinite storage of aggressive aromatic concentrates. Bottles for solvent-based products require closure systems with fluorinated gaskets and torque-loss testing at 40 °C for 7 days, because liner swelling is the primary cause of leakage in transit. Blow-moulding of these containers on intermittent accumulator machines uses the same melt-temperature window as standard HDPE SB 60, but die-head residence time must be kept below 4 min when EVOH is coextruded to prevent yellowing and interfacial instability. Terminal parts include 1–5 L bottles for white spirit, paint thinner, adhesive solvents, degreasing solvents and aromatic hydrocarbon formulations sold through industrial distribution channels.
Post-industrial regrind of HDPE SB 60 from bottle trim, start-up scrap and rejected preforms is reincorporated into cosmetic bottle production on continuous extrusion blow-moulding machines only when the regrind is kept below 30 wt% of the total formulation, because higher letdown rates reduce drop-impact consistency and narrow the parison programming window. A three-layer cosmetic bottle construction may place regrind in the core at 40–50 wt% of total wall thickness while maintaining virgin HDPE SB 60 skins at 25–30% each; this structure preserves surface gloss and stress-cracking resistance while allowing internal reuse of trimmed flash. Post-consumer recyclate is not incorporated into food-contact bottles, but cosmetic and personal-care packaging can use PCR at 15–25 wt% in the core if the PCR stream is washed, melt-filtered to 120–150 µm mesh and tested for lot-to-lot melt flow variation under ISO 1133-1:2022. Pre-drying of HDPE SB 60 is generally unnecessary at relative humidity below 60%, but regrind containing surface moisture should be dried at 70–80 °C for 1.0–1.5 h to eliminate splay marks on bottle shoulders. Drop-impact resistance of finished bottles is measured according to ISO 179-1/1eA at 23 °C and −20 °C, with the lower-temperature condition exposing brittleness introduced by degraded regrind. Odour in PCR-containing cosmetic bottles is evaluated by sensory panels under DIN EN 1230-1, and any residual odour above the panel threshold is controlled by limiting PCR to 20 wt% or adding 0.5–1.0 wt% odour-scavenging masterbatch. Terminal products include opaque lotion bottles, shampoo bottles with pump necks, cream jars and cosmetic refill containers where post-industrial recyclate is used in the core layer and virgin HDPE SB 60 forms the product-contact surface.
Competitive Versalis HDPE SB 60 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis HDPE SB 60 is a high-density polyethylene extrusion blow moulding grade supplied within the SB series of the Versalis polyethylene portfolio. Older commercial databases may list the material as Eraclene SB 60; current Versalis nomenclature identifies the same high-density polyethylene family under HDPE SB 60. The grade is intended for rigid containers and technical hollow bodies manufactured by continuous or accumulator-head blow moulding. Commercial documentation for the grade typically lists a melt flow rate of 0.60 g/10 min at 190 °C under 2.16 kg load, measured according to ISO 1133-1:2022, and a density of 0.960 g/cm³ measured according to ISO 1183-1:2019. These values place SB 60 in the medium-high molecular weight segment of unimodal high-density polyethylene, with sufficient melt strength for parison formation and a density associated with high crystallinity and stiffness. Lot release certificates from the manufacturer should be used for actual specification verification because commercial database entries may not reflect current stabilizer packages or production campaigns.
The melt flow rate of 0.60 g/10 min under ISO 1133-1:2022 limits the grade to processes in which the extruder can generate dispersion without excessive shear heating and in which the parison has adequate hang time. The melt is not as viscous as high-molecular-weight HDPE grades with melt flow rates below 0.30 g/10 min, nor as fluid as injection moulding HDPE grades with melt flow rates of 4–30 g/10 min. The density of 0.960 g/cm³ corresponds to a crystalline fraction that contributes to top-load strength, chemical resistance, and low moisture vapour transmission, while simultaneously reducing impact resistance at cryogenic temperatures. The balance between processability and environmental stress cracking resistance is governed by molecular weight distribution and comonomer type. Published data for the exact comonomer and molecular weight distribution of SB 60 is limited; the processor should therefore obtain the current technical data sheet and, for critical applications, request lot-specific rheological curves.
Shear viscosity at 190 °C and 100 s⁻¹ is estimated from the melt flow value to lie in the range typical for blow moulding HDPE, but this estimate cannot replace capillary rheometry. When a capillary rheometer is used, measurements should follow ISO 11443:2021 at melt temperatures of 190 °C and 210 °C. Lot-to-lot variation in melt flow rate should be monitored; a shift of 0.05 g/10 min can alter parison sag in deep tools and change wall-thickness distribution.
Lot acceptance checks in incoming quality control should include melt flow rate and density on every delivery. Specimens for mechanical testing are prepared by compression moulding in accordance with ISO 293:2023 and conditioned under ISO 291:2008 for 40 h at 23 °C and 50% relative humidity. Tensile yield stress, tensile elongation at break, and flexural modulus are measured on conditioned specimens; however, published values for this grade can vary between production campaigns and geometries. The processor should not design container thickness strictly from resin data sheet values without testing the finished bottle. For critical loads, finite element analysis of top-load and drop impact should be validated with at least 10 production samples per cavity.
On a single-screw continuous blow moulding line with screw diameter of 60–90 mm and L/D ratio of 24:1 to 30:1, the feed zone is set between 170 °C and 185 °C, the compression zone between 185 °C and 200 °C, and the metering zone between 195 °C and 210 °C. The die head and accumulator are held at 190–205 °C. Melt temperature measured by a hand-held probe should remain below 220 °C; prolonged excursions above 240 °C initiate chain scission, generate aldehydes, and produce gel-like defects in the parison. Screw speed is set to maintain a consistent shot weight; with a 24:1 L/D barrier screw, a screw speed range of 30–60 min⁻¹ is common for medium-sized containers. The exact speed depends on extruder diameter, motor load, and head pressure.
Head pressure in front of the screen pack is recorded and controlled within a specified band rather than a universal value. For a 60 mm extruder running this grade, pressure fluctuations greater than ±5% across the batch may indicate filter blockage, inconsistent feed, or degraded material in dead zones. Parison swell is moderate; die gap and bushing positioning often require diameter adjustments of 10–20% to achieve target wall thickness. Pre-blow air pressure between 0.1 MPa and 0.3 MPa and final blow air pressure between 0.6 MPa and 1.0 MPa are typical for bottles with wall thickness of 0.6–2.5 mm. Mould cooling water at 10–25 °C is supplied to the cavity and pinch-off zones; lower temperatures shorten cycle time but increase flow lines and dimensional variation.
Moisture control is required at relative humidity above 60%. Pellets stored in unsealed silos or open gaylords can pick up surface moisture that hydrolyzes stabilizers and produces splay on the container surface. Drying at 80 °C for 2–4 h in a hot-air or desiccant dryer is specified before extrusion when exposed conditions exceed that threshold. Regrind use is permissible in non-food containers at levels up to 30% by weight, provided the regrind is dense, dust-free, and free of incompatible polymer contamination. At higher regrind percentages, molecular weight loss from repeated extrusion can reduce parison hang time and raise the scrap rate due to uneven wall thickness.
Mould dimensions for SB 60 are affected by shrinkage after demoulding. For an HDPE density of 0.960 g/cm³, linear mould shrinkage is typically 1.5–3.0%, but actual values depend on wall thickness, mould temperature, and cooling rate. Containers measured 24 h after demoulding show dimensional changes driven by secondary crystallization; final quality checks should therefore be performed after conditioning at 23 ± 2 °C for at least 24 h. Pinch-off weld strength depends on mould temperature, clamp force, and parison thickness. For containers with a pinch-off length greater than 150 mm, a mould temperature of 15–20 °C and adequate clamp force are required to fuse the molten parison without excessive flash. Inadequate pinch-off pressure produces weak seams and leak paths in the base; excessive pressure creates internal stress and notch sensitivity.
Failure modes encountered on production lines include parison fold-over during transfer, uneven top load distribution from non-uniform wall thickness, and die lines from degraded material accumulating on the die lip. These effects are controlled by purge procedures using a polyolefin purge compound after shutdowns, by inspection of the accumulator head for carbonized deposits, and by maintaining constant melt temperature. Pigment addition is performed using a compatible LDPE or LLDPE carrier masterbatch at a let-down ratio of 1–4% by weight. For opaque containers, titanium dioxide and calcium carbonate masterbatches may increase melt viscosity and reduce parison sag; for thin-wall bottles, the masterbatch should have a melt flow rate within ±0.3 g/10 min of the base resin to prevent layer nonuniformity.
In coextrusion blow moulding, SB 60 can be used as the structural layer in 3-layer HDPE/tie/EVOH/tie/HDPE structures. The melt streams are combined in a feedback block or multi-manifold die at 200–210 °C. Viscosity matching between SB 60 and the barrier layer influences layer distribution; for a standard EVOH barrier with a melt flow rate of 1.5–3.0 g/10 min at 210 °C, adjustments in the melt temperature of SB 60 and the tie resin are required to avoid interfacial melt fracture. Scrap from coextruded multilayer containers should not be dry-blended back into monolayer SB 60 without adequate separation because EVOH domains cause gloss defects and reduced mechanical integrity.
Typical end uses for SB 60 include extrusion blow moulded bottles and containers for liquid detergents, household cleaners, personal-care products, and industrial chemicals. Container sizes from 250 mL to 10 L are within the grade’s usual processing window, while larger containers up to 25 L may require adjustments in die gap, parison programmer profile, and cooling time. Top-load testing according to ASTM D2659-16 or an equivalent in-house procedure is used to verify container strength under stack loading. Drop impact testing at −20 °C according to ASTM D2463-15 assesses low-temperature toughness. Environmental stress cracking resistance is measured on compression-moulded or bottle specimens under ASTM D1693-21 condition B in 100% Igepal CO-630 or under ISO 22088-3:2006 using a bent-strip method. The result is strongly affected by internal stress and aggressive liquid; a container that passes with one surfactant formulation may fail with a solvent-based cleaner. Published data for this specific configuration is limited for aggressive chemical classes, so pre-production storage testing in the filled, capped condition is required.
Compliance status for food contact, European food packaging, heavy metals, and chemical inventory depends on the specific production campaign and the final migration test. The grade as a polyolefin may be evaluated under the following standards. A supplier declaration is necessary for each target market and application.
| Property/Requirement | Standard/Regulation | Test/Designation |
|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 | 190 °C, 2.16 kg |
| Density determination | ISO 1183-1:2019 | Method A, immersion |
| Tensile properties | ISO 527-2:2012 | Type 1A specimen |
| Flexural modulus | ISO 178:2019 | Three-point bending |
| Environmental stress cracking resistance | ASTM D1693-21 | Condition B, 100% Igepal CO-630, 50 °C |
| Vicat softening temperature | ISO 306:2022 | Method B50 |
| Food contact for polyolefins | US FDA 21 CFR 177.1520 | Extraction/migration testing per subpart B |
| EU plastic food contact | Regulation (EU) No 10/2011 | Overall migration limit ≤ 10 mg/dm² |
| REACH registration | Regulation (EC) No 1907/2006 | SVHC communication under Article 33 |
| RoHS heavy metals | Directive 2011/65/EU | ≤ 0.1 wt% for Pb, Hg, Cr(VI), PBB, PBDE; ≤ 0.01 wt% Cd |
Within extrusion blow moulding, a lower-flow grade with melt flow rate of 0.30–0.45 g/10 min has higher molecular weight, higher melt viscosity, and generally better environmental stress cracking resistance and parison hang time for large containers, but requires higher extruder torque and may reduce output. A higher-flow grade with melt flow rate of 0.80–1.20 g/10 min permits lower melt temperature, shorter cycle time, and thinner wall sections, but has lower melt strength and can produce parison length variations in deep tools. SB 60 occupies an intermediate position: it offers adequate melt strength for many bottles and jerrycans, lower melt pressure than high-molecular-weight polyethylene, and faster processing than low-flow grades. Compared with injection moulding HDPE grades with melt flow rates of 8–20 g/10 min, SB 60 is unsuitable for thin-wall injection moulds because the high viscosity prevents complete filling of long flow paths at standard injection pressures. Compared with bimodal pipe grades, SB 60 does not have the long-term hydrostatic strength classification or slow crack growth resistance required for pressure pipe under ISO 9080:2022. Compared with HDPE film grades, SB 60 has higher density and lower melt flow, which favour stiffness and melt strength but not blown film bubble stability.
If the base resin is a butene comonomer HDPE, its environmental stress cracking resistance is generally lower than a hexene-modified grade at the same density and melt flow; users requiring aggressive detergent resistance should benchmark SB 60 against hexene-modified blow moulding grades. Published comonomer data for SB 60 is limited, so such comparisons require analytical confirmation by ¹³C NMR or infrared spectroscopy. Differences in additive packages between grades can also affect colour, odour, and taste for personal-care packaging. SB 60 is not formulated for pharmaceutical blow-fill-seal applications unless a specific grade is qualified under relevant pharmacopoeia chapters.
Operational boundaries for SB 60 include a maximum continuous melt temperature of 220 °C, after which the stabilizer consumption rate increases. Contact with strong oxidizing acids, aromatic hydrocarbons, and chlorinated solvents at elevated temperature is not recommended because these media plasticize or swell the polymer and accelerate crack growth under stress. Ultraviolet stabilization is not inherent unless the grade is supplied with carbon black or UV stabilizers; outdoor exposure of natural containers leads to surface oxidation and embrittlement. Storage in unopened bags is normally limited to 12 months from the production date at 23 ± 2 °C and 50 ± 5% relative humidity. Bags that have been opened should be re-sealed and kept away from direct sunlight, steam, and rain. The product should not be mixed with PET, PVC, or acetal resins; even small amounts of these contaminants can cause delamination, gels, or black specks in blow moulded parts. When changing from PVC to SB 60, the line must be purged with a dedicated transition compound until the melt temperature is below the PVC degradation threshold, because residual PVC decomposes and corrodes tool steel.