Versalis Hdpe Ms80u

Versalis HDPE MS80U

    • Product Name: Versalis HDPE MS80U
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 746692
    Density 0.958 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.25 g/10 min
    Melt Flow Rate 190 C 21 6 Kg 20 g/10 min
    Tensile Stress At Yield 28 MPa
    Tensile Strain At Yield 9%
    Tensile Strain At Break >600%
    Flexural Modulus 1300 MPa
    Charpy Notched Impact Strength At 23 C 25 kJ/m²
    Charpy Notched Impact Strength At 30 C 8 kJ/m²
    Vicat Softening Temperature 125°C
    Melting Temperature 133°C
    Thermal Conductivity 0.40 W/m·K
    Water Absorption <0.01%
    Shore D Hardness 65
    Environmental Stress Cracking Resistance >1000 h
    Deflection Temperature At 0 46 Mpa 75°C

    As an accredited Versalis HDPE MS80U factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis HDPE MS80U is typically supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for safe storage and transport.
    Container Loading (20′ FCL) Versalis HDPE MS80U is loaded into a 20′ FCL container as palletized 25 kg bags, shrink-wrapped and secured for export.
    Shipping Versalis HDPE MS80U is shipped as non-hazardous polyethylene pellets, typically in 25 kg bags, big bags, or bulk containers. Transport in clean, dry vehicles; avoid moisture, heat, and UV exposure. No dangerous goods classification; comply with local transport and storage regulations.
    Storage Versalis HDPE MS80U should be stored in a cool, dry, well-ventilated area, away from direct sunlight, heat, and ignition sources. Keep bags or containers sealed, clean, and off the ground to prevent moisture and contamination. Avoid prolonged exposure to high temperatures. Use proper stacking to prevent package damage. Observe all local regulations and supplier recommendations.
    Shelf Life Typically 24 months when stored unopened in original packaging, dry, at ambient temperature, away from direct sunlight and heat.
    Application of Versalis HDPE MS80U

    Returnable beverage crates produced from HDPE MS80U on a 1,300 t hydraulic clamp injection line require melt-temperature control between 220 °C and 250 °C and a nozzle temperature not exceeding 255 °C, because prolonged residence above 260 °C initiates chain scission and raises residual volatile content. The barrel profile on a 90 mm three-zone screw is set at 190 °C/210 °C/230 °C/240 °C/245 °C, back pressure is held between 0.5 MPa and 1.2 MPa, and screw speed is limited to 40–70 rpm to prevent shear-induced melt-temperature overshoot. Mould temperature is controlled at 10–30 °C with chilled water; cooling time for a 2.0 mm nominal wall crate is 14–22 s. Injection pressure at transfer is set between 70 MPa and 110 MPa, while hold pressure is maintained at 35–55 MPa for 6–10 s to control sink marks opposite rib intersections. The base polymer is normally processed without predrying; however, silo storage at relative humidity above 60% can introduce surface moisture that produces splay on the crate base, so a 70 °C desiccant drying step for 2 h is applied before moulding. Regrind from sprues and rejected crates is reincorporated at 15–25 wt%; addition above 30 wt% measurably reduces notched impact strength under ISO 179-1/1eA and lowers environmental stress-crack resistance under ASTM D1693. For crates intended for incidental food-contact surfaces, the olefin polymer falls within FDA 21 CFR 177.1520, and EU compliance is evaluated under Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm². The terminal article is a returnable bottle crate with slotted side walls, stack ledges and drainage openings; production-scale failure modes include short-shots at the handle bosses, warping from asymmetric ejection, and corner cracking after repeated 1.8 m drop cycles.

    How do gate geometry and hold pressure affect cap sealability under carbonated beverage conditions?

    Thirty-eight-millimetre beverage closures moulded from HDPE MS80U in 48–96 cavity hot-runner tools use a material with a density of 0.960 g/cm³ under ISO 1183-1 and a melt flow rate of 8.0 g/10 min under ISO 1133-1:2022. Gate diameters are set between 0.6 mm and 1.2 mm, with gate freeze times of 0.4–0.8 s, because premature gate freeze blocks hold-pressure transfer and permits shrinkage-void formation in the thread root. Melt temperature is maintained at 215–245 °C, hot-runner tip temperatures are held at 230–250 °C, and mould coolant is controlled at 12–25 °C to stabilise post-mould shrinkage. Hold pressure is set between 45 MPa and 65 MPa for 0.5–1.0 s; cycle time for a 2.2 g closure on high-speed electric machines is typically 4.5–7.5 s. Addition of a slip/antiblock masterbatch at 0.5–1.0 wt% reduces thread friction but can lower coefficient of friction from approximately 0.4 to 0.2, requiring thread root diameter compensation of 0.2–0.4 mm after 48 h post-mould shrinkage of 0.9–1.3%. For carbonated soft drink closures, the retained seal must withstand internal carbon dioxide pressure of 0.25–0.45 MPa at 25 °C, and the tamper-evident band hinge must resist fracture under repeated flexural deformation rather than a single tensile event. Compliance is assessed under FDA 21 CFR 177.1520 and Regulation (EU) No 10/2011 with overall migration below 10 mg/dm², while mechanical data are generated under ASTM D638-14 for tensile yield and ISO 179-1/1eA for notched Charpy impact. Production-scale failure modes include inconsistent band breakage from hot-runner manifold temperature drift of more than ±3 °C and thread-roundness deviation exceeding 0.15 mm caused by uneven ejection.

    Industrial pail wall section uniformity and side-core weld line strength

    On a five-litre to twenty-litre pail tool with side-core handle lugs, HDPE MS80U is processed at melt temperatures of 225–250 °C and injection velocities of 60–120 mm/s, using a fast-to-slow velocity profile across the filling stage to avoid jetting past the side-core pins. Nominal wall thickness is 1.8–2.4 mm, mould coolant is held at 10–25 °C, and cooling time for a 12 L pail is 18–28 s. The gate is positioned off-centre in the base to keep the flow front away from the handle lugs; a gate placed directly opposite a side-core pin can create a weld line that reduces notched impact strength under ISO 179-1/1eA by up to 25% relative to the bulk polymer. Hold pressure is set at 40–60 MPa for 8–12 s to consolidate the rim and minimise sink marks around the seal lip. For pails intended for dangerous goods, UN certification as packaging type 3H1 requires drop testing in accordance with 49 CFR 178.603 and ADR 6.1.5.3 at -18 °C, with drop heights of 1.2 m for packaging group II and 1.8 m for selected higher-hazard materials. The formulation incorporates 2.0–5.0 wt% carbon black or UV stabiliser masterbatch for outdoor storage and chemical handling; addition above 5.0 wt% reduces melt flow and can generate weld-line delamination at the handle lug. Terminal products are open-head pails, closed-head containers with bung threads, and stacking industrial containers. Production failure modes include radial cracking at the seal lip after top-load stacking at 60 °C for 28 days, and handle-lug fracture in field drops below 0 °C when the weld line is not consolidated with sufficient hold pressure.

    Under tropical UV exposure, HDPE MS80U must be compounded with a UV stabiliser masterbatch at 2.5–3.5 wt% before injection moulding of outdoor storage boxes, garden benches and compost-bin bodies. The unmodified base resin alone typically retains less than 60% of tensile elongation at break after 2000 h xenon arc exposure under ISO 4892-2:2013, whereas the stabilised compound retains above 70% and exhibits a colour change ΔE below 4. Carbon black masterbatch at 2.0–3.0 wt% is preferred for uncoloured industrial outdoor parts because it acts as a physical UV absorber, but it raises compound viscosity and forces melt temperatures toward the upper end of the processing window. Moulding is performed at melt temperatures of 225–255 °C, mould temperatures of 12–25 °C, injection pressures of 75–115 MPa and cooling times of 15–25 s for wall sections up to 3.0 mm. Large flat panel sections in storage boxes are susceptible to warpage; the cooling circuit is designed to hold a cavity-to-core temperature differential of no more than ±2 °C, and ribs are limited to 50–60% of nominal wall thickness to reduce sink marks. Outdoor articles are not normally direct food-contact items, so REACH SVHC screening and RoHS Directive 2011/65/EU compliance are the main chemical requirements. Mechanical verification uses ISO 527-2 for tensile properties, ISO 178 for flexural modulus and ISO 179-1/1eA for notched Charpy impact. Production failure modes include surface chalking on unstabilised ribs, stress cracking around screw bosses after thermal cycles from -20 °C to 60 °C, and ejection damage from insufficient draft angles below 1.5°.

    When thin-wall food packaging pushes flow-length-to-thickness ratios above 180:1

    When thin-wall food containers with wall thickness from 0.6 mm to 1.0 mm require flow lengths above 180 mm, HDPE MS80U is processed at melt temperatures of 235–260 °C and injection speeds of 150–250 mm/s to avoid short shots; fill time is held below 0.5 s, and injection pressure reaches 120–160 MPa on high-speed accumulators. The grade's melt flow rate of 8.0 g/10 min under ISO 1133-1:2022 supports rapid filling, but tool wear beyond 0.02 mm at the parting line produces flash because the low melt viscosity cannot seal tool gaps at these pressures. Mould temperature is set at 10–25 °C, and cooling time is 4–8 s depending on wall thickness; asymmetric cooling of more than ±2 °C across the cavity causes bending distortion and lid-seal mismatch. Formulation for food containers is limited to the base polymer and a colour masterbatch at 1.0–2.0 wt%; slip agents are omitted where the container is filled with oil-in-water emulsions because additive migration can exceed the applicable specific migration limit. Terminal products are thin-wall takeaway containers, dairy spread tubs and freezer boxes. Food-contact compliance is assessed under Regulation (EU) No 10/2011 with overall migration below 10 mg/dm², and under FDA 21 CFR 177.1520 for olefin polymers. Mechanical data are generated under ASTM D638-14 for tensile properties and ISO 179-1/1eA for impact; freezing tests at -25 °C are used to assess breakage after stacking. Production failure modes include cracking at gate vestiges during demoulding, lid rim warpage when cooling time is shortened below 4 s, and melt-flow hesitation lines when the flow-length-to-thickness ratio exceeds 200:1 without a second gate.

    Free Quote

    Competitive Versalis HDPE MS80U prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis HDPE MS80U is a chromium-catalysed high-density polyethylene homopolymer supplied in natural pellet form. The grade is specified for injection moulding where low warpage, high creep resistance, and moderate surface hardness are required. Representative values published in supplier documentation indicate a density of 0.956–0.960 g/cm³ at 23 °C measured by ISO 1183-1:2019 and a melt flow rate of 0.75–0.85 g/10 min at 190 °C under 2.16 kg load using ISO 1133-1:2022. The designation MS80U identifies a narrow-molecular-weight-distribution grade optimised for rigid packaging, caps, closures, and industrial containers rather than for film or pipe extrusion. Compared with high-flow HDPE grades in the same density band, the lower melt flow rate increases melt viscosity and injection pressure requirement but reduces post-mould warpage and improves environmental stress crack resistance in the solid state.

    What Material Properties Govern Selection of MS80U for Rigid Packaging?

    The selection of MS80U for rigid packaging is controlled primarily by stiffness, impact resistance, and environmental stress crack resistance. Tensile stress at yield on ISO 527-2:2012 Type 1A specimens at 23 °C is typically 25–28 MPa. Flexural modulus according to ISO 178:2019 is reported in the range 1,000–1,200 MPa. Notched Charpy impact strength measured by ISO 179-1/1eA at 23 °C generally falls between 8 and 12 kJ/m²; however, test results are strongly influenced by mould cooling rate and the presence of weld lines. Vicat softening temperature under ISO 306:2022 Method A50 is close to 124–128 °C, while Shore D hardness under ISO 868:2003 lies between 62 and 65. These values give the material a higher heat-distortion resistance than typical low-density or linear-low-density alternatives, but the homopolymer nature limits low-temperature impact compared with copolymerised HDPE grades.

    PropertyRepresentative rangeTest method
    Density at 23 °C0.956–0.960 g/cm³ISO 1183-1:2019
    Melt flow rate, 190 °C/2.16 kg0.75–0.85 g/10 minISO 1133-1:2022
    Tensile stress at yield, 23 °C25–28 MPaISO 527-2:2012
    Tensile elongation at break, 23 °C>600%ISO 527-2:2012
    Flexural modulus, 23 °C1,000–1,200 MPaISO 178:2019
    Charpy notched impact, 23 °C8–12 kJ/m²ISO 179-1/1eA
    Vicat softening temperature, A50124–128 °CISO 306:2022
    Shore D hardness62–65ISO 868:2003

    The tabulated values are representative specification envelopes rather than guaranteed lot-specific minima. Lot-to-lot variation for chromium-catalysed HDPE is generally narrow in density but may appear as subtle differences in pellet colour because no optical brighteners are added. In high-speed injection moulding, the mechanical response of parts deviates from datasheet values due to frozen-in orientation. Tensile stress at yield can increase by 5–10% in thin-wall mouldings with strong flow-induced orientation, while weld-line impact strength may fall below 4 kJ/m² depending on melt temperature and venting.

    Processing on production-scale reciprocating-screw injection moulding machines requires a barrel temperature profile between 200 °C and 240 °C. Mould temperature should be held at 10–40 °C; lower mould temperatures shorten cycle time but increase frozen-in stress and reduce dimensional stability after demoulding. A general-purpose screw with L/D ratio of 20:1 to 25:1 and compression ratio of 2.5:1–3.0:1 is adequate for homogenisation. Because the melt flow rate is low, screw recovery time can become the limiting step in thin-wall articles; increasing back pressure to 5–15 bar improves melt homogeneity but also extends recovery. Holding pressure is typically maintained at 600–1,000 bar for rigid container lids and closures, depending on wall thickness and gate design. Insufficient holding pressure produces sink marks at the gate region; excessive holding pressure increases moulded-in stress and ejector pin penetration. Published data for this specific configuration is limited, so process parameters should be confirmed by in-mould pressure transducers and short-shot studies.

    Melt Rheology and Injection Compounding Boundaries

    The melt rheology of MS80U follows pseudoplastic behaviour typical of narrow-molecular-weight-distribution high-density polyethylene. Capillary rheometry at 190 °C shows shear viscosity in the range 1,200–1,800 Pa·s at 100 s⁻¹ and 300–450 Pa·s at 1,000 s⁻¹, although grade-specific data should be obtained from the supplier. The power-law index is close to 0.35–0.45 over the shear-rate window relevant to injection moulding. At processing temperatures above 250 °C, the homopolymer begins to undergo thermo-oxidative chain scission that increases melt flow rate and reduces impact strength. Therefore the melt temperature should not exceed 240 °C in production, except for short residence times below 5 min. Heated hot-runner systems should use sequential valve-gate timing to reduce thermal exposure in the manifold.

    Material handling prior to processing is simple under normal indoor conditions. Polyethylene absorbs less than 0.01% moisture at 23 °C and 50% relative humidity; pre-drying is not required unless the pellets have been stored in an unheated warehouse or exposed to condensation. In such cases, drying at 70–80 °C for 1–2 h using a desiccant dryer with dew point below -20 °C is sufficient. The resin should not be processed with regrind levels above 20% without evaluating lot-specific melt flow retention, because repeated shear and thermal history can increase the melt index and alter shrinkage anisotropy. Contamination with polypropylene at levels greater than 2 wt% is not recommended; the immiscible polypropylene phase decreases notched impact strength and may cause delamination at the surface.

    Compared with general-purpose injection-moulding HDPE grades having melt flow rates of 12–22 g/10 min, MS80U requires longer filling times and higher injection pressure. In a multi-cavity closure tool, this can reduce cavitation by 10–20% relative to high-flow HDPE on the same injection unit. Conversely, the lower melt flow rate provides higher melt strength, which reduces flash and improves part weight consistency in hot-runner systems. Against unimodal high-stiffness HDPE grades of similar density, the grade offers improved resistance to slow crack growth under constant strain. Against bimodal blow-moulding grades, it shows lower sag resistance and is not intended for extrusion blow moulding of large containers. Metallocene HDPE grades can exceed MS80U in clarity and low-temperature impact, but often at lower modulus and lower heat-distortion temperature.

    When MS80U Replaces High-Flow Injection Moulding Grades in Thin-Wall Closures

    Direct substitution of a high-flow HDPE with MS80U in thin-wall closures requires adjustment of the melt temperature, injection speed, and holding pressure. With a wall thickness below 0.8 mm, a high-flow grade typically fills at melt temperatures of 200–220 °C and injection speeds above 150 mm/s. Under identical conditions, MS80U can exhibit short shots because its melt viscosity is higher. Increasing melt temperature to 230–240 °C and using dynamic filling with profiled injection speed of 100–180 mm/s have been required in production trials to achieve complete cavity filling without gate freeze-off. Clamp force requirements on a 2,500 kN toggle press do not usually limit the process; instead, the maximum available injection pressure at the screw tip, typically 1,200–1,600 bar, becomes the controlled variable. In comparable substitutions, reduced warpage of flat lids has been observed, but published data for this specific configuration is limited and results vary with gate location.

    ParameterVersalis HDPE MS80UGeneral-purpose injection moulding HDPEBimodal blow moulding HDPE
    Nominal MFR at 190 °C/2.16 kg0.75–0.85 g/10 min12–22 g/10 min0.2–0.5 g/10 min
    Density range at 23 °C0.956–0.960 g/cm³0.953–0.962 g/cm³0.949–0.955 g/cm³
    Typical melt temperature200–240 °C180–230 °C190–220 °C
    Typical mould temperature10–40 °C10–30 °C10–30 °C
    Reported structural signatureHigher stiffness and ESCR at low flowRapid filling of thin sectionsHigh ESCR and sag resistance

    In hot-runner tools with multiple drops, the pressure drop across the manifold and nozzle should be measured and kept below 200–300 bar to avoid shear-induced melt temperature rise above 5 °C. The use of positive shut-off nozzles is preferred; open nozzles can drool because the melt has enough elastic recovery at low shear rates. Cavity filling simulations using Cross-WLF viscosity coefficients from capillary data and pvT data obtained by ISO 17744:2004 are recommended before tool construction. Simulation alone cannot replace short-shot moulding because the crystallisation kinetics of chromium-catalysed HDPE are sensitive to cooling rate, and the datasheet density may not reflect the actual crystallinity of the moulded skin layer.

    Pigmentation of MS80U is typically performed with polyethylene-based masterbatches at 2–4% addition. High pigment loading above 5% can reduce the melt flow rate below 0.6 g/10 min and increase injection pressure. Inorganic pigments such as titanium dioxide act as nucleating agents and may increase crystallisation onset temperature by 2–3 °C, altering shrinkage. Therefore mould shrinkage allowances should be determined using production-similar masterbatch concentration; a typical mould shrinkage value for this density band is 0.015–0.025 mm/mm in the flow direction and 0.020–0.030 mm/mm transverse to flow. Published data for this specific configuration is limited.

    Typical applications for Versalis HDPE MS80U are injection-moulded caps and closures with diameters between 28 mm and 120 mm, thin-wall food containers with wall thickness above 0.8 mm, crates, pallets, technical parts for automotive fluid reservoirs, and housewares that require hot-water contact resistance. In closure applications, the material is selected when the part must pass a strip-torque test after 24 h of conditioning at 23 °C and 50% relative humidity. Because the resin has no slip additives in its base stabilisation package, coefficient of friction and opening torque must be controlled by masterbatch addition of erucamide or oleamide at 0.05–0.15 wt%, depending on cap diameter and neck finish. Overlubrication above 0.3 wt% can cause surface bloom and print adhesion failure.

    For food-contact use, the resin must be evaluated under EU 10/2011 and FDA 21 CFR 177.1520 olefin polymer provisions. Lot-specific migration testing for overall migration and specific migration of catalysts is the responsibility of the converter. The grade is not formulated with intentionally added perfluorinated processing aids; REACH and RoHS declarations should be confirmed per production site. Operational boundaries for MS80U are set by its homopolymer backbone. The material should not be used for continuous service above 80 °C under load without creep testing, because creep modulus falls rapidly as temperature approaches the Vicat softening point. It is not recommended for outdoor exposure exceeding 2 years without UV stabilisation; carbon black masterbatch at 1.5–2.5 wt% is required for weatherable parts. Avoid combination with amine-based additives in the melt, as they can interact with chromium catalyst residues and shift colour. The grade is not designed for rotational moulding or extrusion blow moulding because its melt strength at low shear rates is insufficient to maintain parison sag resistance.

    Top