| HS Code | 836894 |
| Density | 0.954 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.8 g/10 min |
| Tensile Strength At Yield | 27 MPa |
| Tensile Strength At Break | 32 MPa |
| Elongation At Break | 600% |
| Tensile Modulus | 1100 MPa |
| Flexural Modulus | 1200 MPa |
| Izod Notched Impact Strength 23 C | 20 kJ/m² |
| Shore D Hardness | 60 |
| Vicat Softening Temperature | 125 °C |
| Melting Temperature | 130 °C |
| Thermal Conductivity | 0.4 W/m·K |
| Specific Heat | 1.9 J/g·°C |
| Coefficient Of Thermal Expansion | 1.5 × 10⁻⁴ /°C |
| Water Absorption 24 H | 0.01% |
| Volume Resistivity | 1 × 10¹⁶ Ω·cm |
| Dielectric Constant 1 Mhz | 2.3 |
| Dielectric Strength | 20 kV/mm |
As an accredited Versalis HDPE MS80 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis HDPE MS80 is typically supplied in 25 kg polyethylene bags, palletized, or 1,000 kg octabin bulk containers for shipping. |
| Container Loading (20′ FCL) | 20′ FCL container loading of Versalis HDPE MS80 in 25 kg polyethylene bags, palletized and shrink-wrapped for sea transport. |
| Shipping | Versalis HDPE MS80 is a non-hazardous high-density polyethylene resin. It is typically shipped in 25 kg polyethylene bags or octabins on pallets, stretch-wrapped, and labeled. Transport as general cargo in clean, dry vehicles; avoid moisture, heat, and direct sunlight. No special dangerous goods documentation required; follow standard warehousing and handling practices. |
| Storage | Store Versalis HDPE MS80 in original, sealed packaging in a dry, cool, well-ventilated warehouse. Protect from direct sunlight, moisture, heat, and ignition sources. Keep pallets off the floor and away from strong oxidizers, acids, and bases. Maintain clean, dust-free conditions, avoid static buildup, and follow first-in, first-out rotation. Recommended ambient storage below 50°C. Do not expose to open flames or excessive heat. |
| Shelf Life | Versalis HDPE MS80 has a 24-month shelf life if stored sealed in its original packaging, cool, dry, and protected from sunlight. |
High-flow high-density polyethylene injection-moulding grades with an ISO 1133-1:2022 melt-flow index of 8.0 g/10 min at 190 °C/2.16 kg and a nominal density of 0.960 g/cm³ under ISO 1183-1:2022 occupy a narrow processing window in high-cavitation closure production. The balance between spiral-flow length and short-term mechanical strength governs the design of tamper-evident band hinges and threaded bridge sections. In food-contact closure qualification under FDA 21 CFR 177.1520, the olefin polymer specification and its extractables limits apply directly, while EU converters must demonstrate compliance with Commission Regulation (EU) No 10/2011 Annex I and Annex II, with overall migration not exceeding 10 mg/dm² in food simulants A, B, and D2 according to EN 1186-1. Formulation addition ratios are typically 100 wt% virgin Versalis HDPE MS80 compounded with 1.0–2.0 wt% olefinic colour masterbatch; slip and static-control additives added at 0.05–0.20 wt% alter surface coefficient-of-friction without exceeding the positive-list restrictions of the food-contact regulation. Processing on a 96-cavity hot-runner tool with valve-gated drops calls for melt temperatures between 220 °C and 240 °C at the nozzle, mould surface temperatures of 10 °C–18 °C, and hold-pressure decay profiles tuned to prevent gate-stringing on separation of the tamper-evident band. Cycle times of 6–9 s at part weights of 1.5–2.5 g are attainable only when injection velocity is staged: fast initial fill to 95% volume, short packing transition at screw position corresponding to 2–3 mm before full stroke, and reduced pressure during band folding. Melt residence time beyond 15 min at temperatures above 280 °C is avoided because thermo-oxidative chain scission raises the gel count and reduces impact strength. Finished product types in this segment include 29/25 mm and 38 mm closures for milk, edible oil, and water; PCO 1881 carbonated soft-drink closures; and tamper-evident snap-on lids for dry nutritional powder cans.
Although melt-flow is the most quoted hand-book parameter, the practical limiting factor in thin-wall polyolefin container moulding is often pressure drop across the cavity as wall thickness falls below 0.8 mm. At a flow-length-to-wall-thickness ratio above 250:1, Versalis HDPE MS80 with an ISO 1133-1:2022 MFR of 8.0 g/10 min requires injection velocities in the 300–600 mm/s range and peak hydraulic pressures at the material inlet approaching 90–140 MPa, depending on hot-runner balance and gate diameter. For dairy tubs, deli trays, and takeaway bases, the compliance route is Regulation (EU) No 10/2011 for EU markets; US converters validate under FDA 21 CFR 177.1520 and may apply EC 1935/2004 Articles 3, 4, and 5 for general traceability and good manufacturing practice. Formulation addition ratios commonly include 1.0–2.5 wt% white masterbatch based on an olefin carrier; anti-block and slip additives are introduced at 0.05–0.20 wt% to address nesting and denesting friction, and clean in-house regrind from edge trim and rejected cups may be incorporated up to 30 wt% if the converter demonstrates that it does not raise overall migration beyond the 10 mg/dm² limit. Drying is not required at storage relative humidity below 60%; surface moisture at relative humidity above 80% can be removed in a hopper dryer at 80 °C for 1–2 h. Downstream processing is a high-speed injection moulding process with 0.4–0.8 mm nominal wall, cold-runner or hot-runner layouts, and cooling times of 1.5–4.0 s; process control focuses on switch-over position, holding pressure, and mould temperature uniformity because differential shrinkage across the lid rim causes leakage after capping. At wall sections below 0.35 mm, the melt-flow requirements for long-flow deep tubs exceed the practical limits of this grade unless melt temperatures are raised into the degradation band, so flow simulation is required before tool construction. Terminal finished product types include 500–1000 ml dairy tubs, 250–750 ml deli containers, snap-on overcap lids, and disposable takeaway bases with anti-leak rims.
| Application segment | Primary regulation or standard | Qualification method or condition |
|---|---|---|
| Caps and closures for food contact | FDA 21 CFR 177.1520, EU 10/2011 | Overall migration per EN 1186-1; extractables per 21 CFR 177.1520(c) |
| Thin-wall food containers | EU 10/2011, EC 1935/2004, FDA 21 CFR 177.1520 | Migration in simulants A, B, D2; organoleptic per ISO 13302 |
| Industrial crates and pallet components | REACH, ISO 8611-1:2021, ISO 11469:2016 | SVHC 0.1% w/w; stacking and creep load |
| Housewares and small appliance parts | REACH, EN 71-3 where toy-like, FDA 21 CFR 177.1520 where food contact | Migration of elements; extractables |
| Cosmetic primary packaging | EU 1223/2009, ISO 22716:2007, REACH | GMP documentation; component compatibility testing |
| Household chemical dispensing closures | CLP 1272/2008, REACH, ADR/RID where dangerous goods | ESCR per ASTM D1693; chemical immersion per ASTM D543 |
For stack/nest crates and pallet feet, the processing window narrows because nominal wall sections of 2.5–4.0 mm impose cooling-time-dominated cycles and the long flow distances demand sufficient hold pressure to control sink marks at ribs and bosses. The grade is processed at melt temperatures of 220 °C–250 °C, with injection rates moderated to 80–200 mm/s screw advance depending on part weight; clamp force requirements are estimated from 4–6 kN/cm² projected cavity area, and multi-stage holding profiles are used to reduce internal void formation at the junction of sidewalls and runners. Industrial crate compliance falls under REACH (EC) No 1907/2006 Annex XVII and the 0.1% w/w SVHC article threshold, with marking per ISO 11469:2016 for polymer identification; where the crate is intended for direct food-contact distribution, EU 10/2011 or FDA 21 CFR 177.1520 applies to the finished article and to any masterbatch. Formulation addition ratios involve 100 wt% Versalis HDPE MS80 plus 2.0–5.0 wt% colour masterbatch; outdoor service versions are modified with 0.10–0.50 wt% hindered-amine light stabiliser and 0.05–0.20 wt% antioxidant, while clean post-industrial regrind is added up to 40 wt% only when the particle homogeneity and melt-viscosity shift are controlled by in-line rheometry. Production is usually performed on large-platen injection moulding machines of 1500–3500 t clamp force for single or multiple cavity tools, with sequential valve-gated hot runners to minimise weld lines along load-bearing corners; ejection requires part temperature below 70 °C to avoid deformation. The high density of 0.960 g/cm³ reduces creep under long-term stacking but lowers low-temperature impact; thin-wall crate use below -10 °C should be avoided unless the design includes adequate radiusing and the converter validates Charpy behaviour per ISO 179-1/1eA. Terminal finished products include stackable logistics crates, ventilated fruit and vegetable crates, industrial totes, automotive part dunnage trays, and pallet components such as top decks, feet, and corner blocks under ISO 8611-1:2021 load classes.
Multi-cavity housewares tooling filled through hot-runner manifolds demands dimensional stability in long-flow parts because post-ejection shrinkage anisotropy can cause lid-base mismatch. The downstream production process is medium-wall injection moulding with wall thicknesses between 1.2 mm and 3.5 mm, melt temperatures of 210 °C–240 °C, and cooling times of 10–30 s depending on section thickness; the screw back pressure is held at 3–8 bar to homogenise masterbatch without excessive shear heating. Regulatory status for general housewares sold in the EU is customarily addressed through REACH and the General Product Safety Regulation, whereas articles intended for dry or aqueous food-contact service must comply with EU 10/2011 or FDA 21 CFR 177.1520; if the item is marketed as a toy or child-care article, EN 71-3 migration of elements and phthalate restrictions under REACH Annex XVII entries 51 and 52 become relevant. Formulation addition ratios are usually 100 wt% Versalis HDPE MS80 with 1.0–3.0 wt% colour masterbatch; UV-stabilised outdoor articles require an additional 0.10–0.40 wt% hindered-amine light stabiliser, while dry colour or liquid pigment systems must be verified not to increase the melt-flow index above 10 g/10 min or reduce impact below the design limit. For thick-walled buckets above 12 L capacity, cooling time dominates the cycle, and turbulent cooling-channel flow with mould temperatures of 10–20 °C is applied to prevent surface sink and prolonged hold-pressure demand. Terminal product types include storage boxes, buckets, planters, laundry baskets, indoor refuse containers, and appliance housings with snap-fit assembly features. Transparent houseware applications are outside the suitability envelope because the grade has limited clarity and is intended for opaque or coloured service.
Because co-injection and recyclate-backed structures alter the thermal balance of the cavity, the core layer, which may contain 20–30 wt% clean in-house scrap, is encapsulated by virgin Versalis HDPE MS80 skin layers. The downstream production process is injection moulding of thick-walled jars and caps with wall sections from 1.8 mm to 4.0 mm, using melt temperatures of 220 °C–250 °C for the skin and a core melt that is maintained at least 10 °C below the skin to preserve layer integrity; injection-compression moulding is often used for flat rims and moulded sealing surfaces. Regulatory compliance under EU Regulation (EC) No 1223/2009 requires that packaging does not adversely affect the cosmetic product, and documentation under ISO 22716:2007 GMP is used to trace masterbatch and process changes; where the package is dual-purpose and may contact food, EU 10/2011 or FDA 21 CFR 177.1520 is applied. Formulation addition ratios include 1.0–2.0 wt% colour masterbatch in the skin, 0.05–0.20 wt% slip/antiblock if required for closure torque, and 0.10–0.40 wt% UV stabiliser for coloured packs exposed to retail lighting; the recyclate core should not exceed 30 wt% when surface-finish or odour barriers are critical. Published formal migration data for co-injected HDPE MS80 with recyclate core are often converter-specific and not available in public datasheets, so validation must be performed on finished-layer structures rather than extrapolated from virgin-only plaques. Terminal finished product types include cream jars, loose-powder bases, overcap lids, lotion and shampoo closure covers, and outer shells for lipstick or mascara overpacks where high surface gloss and dimensional stability prevent visible warpage.
In household chemical dispensing closures, aggressive detergent and bleach-based formulations impose sustained hoop stresses on threaded plugs, making environmental stress-cracking resistance the dominant design criterion. Versalis HDPE MS80 in the 8.0 g/10 min MFI band provides a cycle-time advantage, but its higher melt-flow relative to blow-moulding HDPE grades can reduce stress-cracking resistance under continuous loading; therefore tooling must avoid sharp notches, weld lines at sealing surfaces, and excessive hoop strain from undercut designs. The compliance framework for household chemical packaging is primarily CLP Regulation (EC) No 1272/2008 for labelling, REACH for substances, and Directive 2019/904/EC for certain sustainability-related design considerations; where the container is part of a dangerous-goods pack, the outer packaging must meet applicable drop and stack requirements under ADR/RID and UN Model Regulations. Formulation addition ratios typically comprise 100 wt% Versalis HDPE MS80 with 2.0–4.0 wt% colour masterbatch, 0.05–0.20 wt% acid-neutralising lubricant where closure torque is controlled, and 0.10–0.20 wt% antioxidant; chlorinated or highly oxidising bleach packs require validation that stress-cracking lifetime under 60 °C accelerated exposure meets the specified shelf-life, and if not, a lower-MFR or copolymer grade is substituted. Injection moulding of such closures uses melt temperatures of 220 °C–250 °C, cold- or hot-runner tooling, and part walls of 1.5–3.0 mm; significant process control is applied to packing pressure and cooling to minimise residual stress. Terminal finished product types include child-resistant dosing caps, detergent bottle closures with integrated spouts, bleach overcap plugs, and trigger-spray connector adapters.
Competitive Versalis HDPE MS80 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis HDPE MS80 is a high-density polyethylene homopolymer injection-moulding grade distributed under the Eraclene trade name. The designation suffix 80 corresponds to a nominal melt flow rate of 8.0 g/10 min when determined at 190 °C under a 2.16 kg load according to ISO 1133-1:2022. The density of 0.960 g/cm³ at 23 °C places the material in the high-density class and provides the stiffness required for stackable transport packaging, closures, housewares, and dunnage trays. The primary processing route is reciprocating-screw injection moulding; the low melt viscosity enables thin-wall filling, whereas the low melt strength makes the grade unsuitable for extrusion blow moulding or blown film. The following sections present producer-published physical property data, processing boundaries, and comparative performance differences against lower-melt-index HDPE grades. Where a specific value is not published for a configuration, the text states that limitation.
The values in Table 1 are representative figures from Versalis technical documentation. Mechanical test specimens are injection-moulded and conditioned according to ISO 1873-2:2007 at 23 °C and 50 % relative humidity unless the referenced standard requires otherwise.
| Property | Test method | Representative value |
|---|---|---|
| Melt flow rate at 190 °C/2.16 kg | ISO 1133-1:2022 | 8.0 g/10 min |
| Density at 23 °C | ISO 1183-1:2019 | 0.960 g/cm³ |
| Tensile stress at yield | ISO 527-2:2012 | 28 MPa |
| Flexural modulus | ISO 178:2019 | 1350 MPa |
| Notched Izod impact at 23 °C | ISO 180/A | 4.5 kJ/m² |
| Vicat softening temperature, A50 | ISO 306:2013 | 127 °C |
| Shore D hardness | ISO 868 | 64 |
| Mould shrinkage | ISO 294-4 | 1.5–2.0 % |
The tabulated values are representative, not absolute minima or maxima. For tool design, the upper end of the shrinkage range should be used for cross-flow dimensions and the lower melt-flow limit for fill-pressure calculations. Batch-to-batch variation in melt flow rate is typically controlled within ±0.7 g/10 min; density variation is typically within ±0.002 g/cm³.
On a 60 mm three-zone screw with L/D ratio 20:1 and compression ratio 2.0:1–2.5:1, MS80 generally draws lower motor current than an HDPE blow-moulding grade with melt flow rate 0.3 g/10 min under identical barrel settings. The reduction occurs because the higher melt index lowers melt viscosity in the metering and pumping sections. If the screw is equipped with a mixing section, shear heating can add 5–10 °C above the front-zone setpoint when screw speed exceeds 120 rpm; nozzle melt-temperature measurement is therefore required before reducing cycle time. Lower melt viscosity also makes non-return valve wear operationally critical: clearance greater than 0.15 mm can produce short-shot variation on thin-walled parts because melt leaks back along the screw flights. Closed-loop injection-speed control should switch from velocity to pressure at 95–99 % of part fill to prevent overpacking and vent flash.
Barrel temperature settings for a standard screw are rear 180–210 °C, mid 200–230 °C, front 210–250 °C, and nozzle 210–250 °C. Mould surface temperatures of 20–50 °C are adequate; sections thinner than 1.2 mm may require the upper end to avoid premature freeze-off. Injection pressure normally lies between 60 MPa and 120 MPa. To estimate clamp force, projected area times cavity pressure can be used; for a 1.0 mm wall thickness, cavity pressure is typically 30–40 MPa, so a projected area of 500 cm² would require approximately 1,500–2,000 kN clamp force. Back pressure of 0.5–1.5 MPa and screw speed of 50–120 rpm are typical starting values. No predrying is required for dry resin; if condensation is present from outdoor storage, drying at 80 °C for 1–2 h prevents splay in transparent or light-coloured articles.
| Processing parameter | Starting range | Control limit |
|---|---|---|
| Barrel temperature | 200–250 °C | Do not exceed 260 °C |
| Mould temperature | 20–50 °C | Thin walls below 1.2 mm may require 50 °C |
| Injection pressure | 60–120 MPa | Higher pressures require clamp-force verification |
| Back pressure | 0.5–1.5 MPa | Avoid shear overheating above 260 °C |
| Screw speed | 50–120 rpm | Scale to screw diameter to avoid excessive shear |
| Residence time at 230 °C | 15–30 min | Purge after 30 min |
| Drying | Not required | If condensation: 80 °C/1–2 h |
The tensile yield stress near 28 MPa under ISO 527-2:2012 and flexural modulus near 1350 MPa under ISO 178:2019 reflect the density of 0.960 g/cm³. Lower-density HDPE copolymers at 0.945 g/cm³ typically show flexural modulus below 1000 MPa; MS80 therefore provides higher top-load stiffness in stackable crates at equal wall thickness. However, the room-temperature notched Izod impact energy near 4.5 kJ/m² under ISO 180/A is moderate compared with blow-moulding HDPE grades of melt flow rate below 1.0 g/10 min, which can exceed 8 kJ/m². Impact data from thick-walled blow-moulded parts should not be applied to thin-walled injection-moulded parts. The Vicat softening temperature of 127 °C under ISO 306/A50 limits continuous load-bearing service to well below that value; stackable crates under load should be tested for creep at the expected warehouse temperature.
For thin-walled caps and closures, submarine or pin gates with land length below 0.8 mm reduce gate-vestige tearing; a hot gate tip that remains too hot can produce stringing because MS80 has low melt viscosity. Vent depths should not exceed 0.02 mm in tools originally sized for polypropylene: HDPE flash can occur because melt pressure in thin sections can exceed 100 MPa. Ejector pins should engage before the part shrinks onto the core; mould shrinkage of 1.5–2.0 % under ISO 294-4 is high enough to create ejection drag on textured sidewalls. Draft angles of 1.0–2.0° are recommended for textured surfaces. Weld lines after multi-gate filling reduce notched impact more than in higher-molecular-weight HDPE because the lower entanglement density provides less resistance to crack growth.
In closure and crate applications, MS80 is sometimes compared with impact-copolymer polypropylene. The Vicat softening temperature of 127 °C under ISO 306/A50 is lower than Vicat values of 150–155 °C typical of heterophasic PP copolymers. MS80 should not be specified for hot-fill containers above 100 °C or for continuous service near boiling-water limits. HDPE retains sub-zero impact better than many PP homopolymers; closures that must survive -20 °C drop tests can be designed with MS80 if the part is not sharply notched and wall sections are not heavily frozen-in. The higher flow of MS80 relative to medium-flow PP can reduce injection pressure in thin-wall packaging, but the tensile modulus of PP is generally higher; MS80 therefore requires thicker sections or additional ribbing to match PP top-load stiffness. Processing comparisons should be made on the same tool with equivalent flow length and wall thickness, not on property data alone.
Incoming quality control should include melt flow rate per ISO 1133-1:2022, density per ISO 1183-1:2019, and notched Izod impact per ISO 180/A at 23 °C. A production line that receives a batch at the upper MFR limit may experience flash at vents that were sized for a lower-flow batch; a batch at the lower MFR limit may produce short shots in thin-walled tools. When changing silos from a different HDPE, the transition period should be tracked by melt-pressure sensors at the machine nozzle. A stable nozzle melt temperature of 210–250 °C and screw recovery time within ±0.5 s across shots indicate uniform melt quality. Incoming bags should be protected from UV; outdoor storage of unpigmented resin can degrade the stabilizer package and reduce long-term oxidative stability as measured by ISO 11357-6:2018.
This substitution applies only to injection-moulding tools, not to blow-moulding equipment. Barrel temperatures can usually be reduced by 10–20 °C from settings used for a low-melt-index blow-moulding HDPE because the melt viscosity of MS80 is lower. Shot-size repeatability is improved if the screw tip and check ring are in good condition; a worn non-return valve with clearance greater than 0.15 mm can produce short shots in thin-wall cavities. In hot-runner tools, manifold temperatures should remain below 260 °C, and the material should be purged after 30 min residence at 230 °C to avoid oxidation and black specks. Prototype parts should be measured after conditioning at 23 °C and 50 % relative humidity for 24 h before applying the 1.5–2.0 % shrinkage correction to tool dimensions.
HDPE MS80 is resistant to dilute aqueous acids, bases, and saline solutions; it is not resistant to aromatic hydrocarbons, chlorinated solvents, or strong oxidizers. Immersion testing under ISO 175:2010 should be performed on moulded parts when a new contact fluid is introduced. A mass increase above 1.0 % after 72 h immersion is a significant compatibility signal. Stress-cracking agents such as nonylphenol ethoxylate-based surfactants and terpene-containing cleaners can reduce environmental stress-crack resistance; ASTM D1693 testing on production parts is more relevant than plaque data because weld lines and moulded-in stress dominate failure.
Food-contact suitability is controlled by the formulated product, not by HDPE density or melt flow rate alone. MS80 may be covered by a producer compliance certificate under FDA 21 CFR 177.1520 for olefin polymers in food-contact use and under Commission Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm² for non-fatty food simulants under specified time/temperature conditions. Additives, masterbatches, and post-consumer recycled content can invalidate the certificate. Processors should obtain the current certificate and test final packaging under the intended food type and sterilization or hot-fill temperature.
Dimensional control requires attention to shrinkage anisotropy. Along-flow shrinkage on a standard plaque is typically 1.5 %, while cross-flow shrinkage can reach 2.0 % under ISO 294-4. Turbulent water flow in cooling channels with Reynolds number above 10,000 is preferred; laminar flow below 2,300 increases cycle time and creates non-uniform cooling. Ejection should occur below 80 °C to avoid fold-over and denting during stacking. If parts are stacked above 80 °C, creep under load can create permanent contact marks. Conditioning at 23 °C and 50 % relative humidity for 24 h before dimensional audit allows post-demoulding thermal relaxation to settle.
For outdoor applications, HDPE MS80 is not inherently UV-stable. A carbon black masterbatch at 2.0–2.5 wt% or a UV stabilizer package is required for long-term exposure. Weathering evaluations should follow ISO 4892-2:2013 with defined irradiance and moisture cycle; published data for this specific configuration is limited, so end-use validation on production mouldings is required before specifying outdoor warranty periods.