Versalis Hdpe Mr80u

Versalis HDPE MR80U

    • Product Name: Versalis HDPE MR80U
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 253765
    Polymer Type High Density Polyethylene (HDPE)
    Density 0.960 g/cm3
    Melt Flow Rate 190 C 2 16 Kg 8 g/10 min
    Tensile Stress At Yield 30 MPa
    Tensile Strain At Break >600%
    Flexural Modulus 1400 MPa
    Charpy Notched Impact Strength At 23 C 5 kJ/m2
    Vicat Softening Temperature 127°C
    Shore D Hardness 65
    Melting Temperature 135°C
    Thermal Conductivity 0.4 W/m·K
    Water Absorption <0.01%
    Uv Stabilization Yes
    Electrical Resistivity >10^15 ohm·cm
    Dielectric Constant 1 Mhz 2.3

    As an accredited Versalis HDPE MR80U factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis HDPE MR80U is supplied in 25 kg sealed bags, palletized and stretch-wrapped, protecting the polyethylene pellets during storage and transport.
    Container Loading (20′ FCL) Versalis HDPE MR80U in 20′ FCL: 25 kg bags stacked on pallets, shrink-wrapped, evenly distributed and secured for sea transport.
    Shipping Versalis HDPE MR80U is a high-density polyethylene grade supplied as pellets in 25 kg PE bags, octabins, or bulk trucks. It is non-hazardous and not regulated for transport under ADR, IMDG, or IATA. Keep dry, avoid direct sunlight, and use standard industrial handling to prevent contamination.
    Storage Store Versalis HDPE MR80U in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, acids, bases, solvents, and strong oxidizing agents. Keep in original, sealed bags or containers, palletized off the floor, to prevent moisture pickup and contamination. Avoid excessive stacking and prolonged outdoor exposure. Maintain good housekeeping and use first-in, first-out stock rotation. Handle with care.
    Shelf Life Shelf life: typically 24 months when stored in original packaging, dry, below 40°C, away from direct sunlight and contaminants.
    Application of Versalis HDPE MR80U

    Logistics crates and heavy-duty pallets injection-moulded from HDPE MR80U are typically compounded with 75–85 wt% virgin MR80U, 15–25 wt% closed-loop post-industrial regrind, and 2–4 wt% carbon-black masterbatch at 40 wt% carbon-black loading. The regrind fraction is deliberately capped because loadings above 30 wt% are associated with a measurable loss of notched Charpy impact at −20°C under ISO 179-1:2023, a failure point that appears in cold-chain distribution environments. For load-bearing pallets, compliance is assigned under ISO 8611-2:2021 for bending, racking, and diagonal stiffness paths; where export pallets require stiffness classification, ASTM D6108-19 is used as the incoming inspection reference. The injection process runs on a reciprocating-screw machine with a 20:1 to 24:1 L/D screw, melt temperature 220–250°C, mould temperature 15–40°C, and holding pressure 35–55 MPa; on a 12,000 kN clamp-force line, gate freeze for a 55 mm top-deck rib is reached after 8–16 s. Sink marks at the intersection of the top deck and fork pockets occur when holding pressure decays below 30 MPa before gate freeze, and the corrective action is to increase shot-weight cushion rather than raise barrel temperature. Batch tensile yield under ASTM D638-14 typically falls within 24–28 MPa, while flexural modulus measured to ISO 178:2019 is in the 1,000–1,200 MPa band depending on conditioning humidity. The finished articles produced under this processing window are ISO pallets, collapsible bulk containers, ventilated distribution crates, and nestable dairy crates in which high-cycle mechanical stacking is the primary load mode.

    What closes the loop between seal integrity testing and HDPE MR80U closure formulation?

    For pail lids and overcaps intended for non-carbonated industrial liquids, HDPE MR80U is compounded at 94–97 wt% resin, 2–5 wt% slip/antiblock masterbatch, and 0.5–1.5 wt% nucleating additive to stabilise the seal channel against differential shrinkage. The applicable compliance chain for UN 1H2 pails includes ISO 16106:2020 transport packaging provisions, closure torque retention under ASTM D3475-17 where child-resistant closure ratings are required, and melt-flow conformity under ISO 1133-1:2022 at 8.0 g/10 min. The manufacturing route is valve-gated hot-runner injection moulding with four to six drops, melt temperature 215–245°C, mould temperature 12–30°C, and a clamp-force allocation of 500–800 kN per cavity for a 285 mm lid diameter. Gate vestige is held below 0.3 mm because a larger protrusion prevents the sealing bead from sitting flush in the pail rim; drop-test leakage is frequently traced to overpacking at the gate, where vertical flash compromises the interference fit at the seal ledge. Cavity-pressure transducers are set to switch from pack to hold at 35 MPa within 0.4 s, and machine cushion is maintained at 3–5 mm to avoid the “long-stroke venting” condition that creates warpage in the tamper-evident band. The product category supplied to downstream converters includes injection-moulded pail lids, tamper-evident overcaps, and spouted closure bases for non-carbonated industrial liquids.

    When UV ageing crosses 12 months, which carbon-black dispersion limit protects impact retention in stackable crates?

    In outdoor stack-and-nest crates and agroindustrial handling bins, the formulation shifts toward 3.0–4.5 wt% carbon-black masterbatch at 40–50 wt% carbon-black concentration, with 90–94 wt% HDPE MR80U, 2–4 wt% antioxidant preblend, and 0.5–1.0 wt% acid-neutralising masterbatch. Carbon-black primary particle size in the 20–30 nm range provides the UV-screening function, but dispersion above ISO 18553:2002 degree B initiates surface microcrazing that reduces Charpy impact after 2,000 h xenon exposure under ISO 4892-2:2013. The producer datasheet does not disclose the proprietary hindered-amine versus benzotriazole partitioning in the UV package; published data for this specific configuration is limited, so outdoor approval must be based on finished-article weathering rather than resin-level claims. Processing is injection moulding with a matched-metal cooling fixture that clamps the sidewalls during solidification; melt temperature is held at 220–240°C, and a cushion of 4–6 mm is maintained to compensate for the viscosity increase caused by carbon-black loading. Warpage in the base grid becomes the dominant production bottleneck when mould temperature exceeds 45°C, because differential shrinkage reduces stack interference below 2 mm and creates unstable palletised loads. Finished products under this route are ventilated agricultural crates, non-food fish distribution boxes where food-contact status must be separately verified under EU 10/2011 and FDA 21 CFR 177.1520, and outdoor industrial storage bins exposed to multi-year solar load.

    Masterbatch carrier resin thresholds under L/D 48:1 twin-screw compounding

    As a carrier resin for high-load carbon-black masterbatch, MR80U is formulated at 55–75 wt% with furnace black at 20–35 wt%, a PE-wax dispersant at 2–5 wt%, and a hindered-phenolic/phosphite antioxidant system at 0.3–0.8 wt%. The density of 0.964 g/cm³ under ISO 1183-1:2019 and melt flow rate of 8.0 g/10 min under ISO 1133-1:2022 permit side-feeding at screw speeds of 500–800 rpm without excessive melt-temperature rise on a co-rotating twin-screw extruder with L/D 48:1. The barrel segment from the side feeder to the die is maintained at 180–210°C to avoid thermal degradation of the PE wax; if the die-head melt temperature exceeds 210°C, volatilisation of low-molecular-weight wax causes surface bubbles on the pellet. Dispersion quality is assessed by ISO 18553:2002 on a pressed film, while filter-pressure rise across a 25 μm mesh screen pack serves as a production-line proxy for undispersed agglomerates. The compound is strand-pelletised through a 3–4 mm die plate and cooled in a water bath at 35–50°C; strand temperature above 60°C at the pelletiser intake can produce pellet tails that alter downstream metering in let-down equipment. Compliance for masterbatch export includes REACH EC 1907/2006 and, where food-contact let-down is intended, EU 10/2011 verification on the final compound; RoHS 2011/65/EU applies only if the masterbatch is used in electronics-adjacent polymers, not in packaging. The terminal product type is a high-load black masterbatch granule, not a finished article.

    Buttress-thread drum closures, including 2-inch and 3/4-inch plugs, are injection-moulded from HDPE MR80U at 95–98 wt%, with 2–5 wt% UV masterbatch and an EVA gasket overmould or separate elastomeric seal. The governing compliance is the UN 1A2/1H2 closure retention test for hazardous-material drums, with a drop-side impact of 1.8 m for Packing Group II liquids and closure torque verification at 18–22 N·m after conditioning to −18°C. The production line uses multi-cavity cold-runner moulds with 8–24 cavities, tunnel gates, barrel temperature 215–245°C, and a cycle time of 18–28 s for wall thicknesses between 2.5 mm and 4.0 mm. Thread flash and ovality are controlled by maintaining a hold-to-cool time ratio of 1.5–2.0; if the part is ejected before core temperature falls below 85°C, the thread pitch diameter drifts by 0.2–0.4 mm, causing rejection in automatic torque testers after gasket assembly. The finished product is an injection-moulded drum plug or vent cap that carries the UN marking on the packaging certificate, not on the closure itself.

    Dunnage tray flatness after demoulding is governed by holding pressure decay, not by melt temperature alone

    Where warpage-controlled dunnage trays and interlayer boards are produced for automated pallet racking, HDPE MR80U is blended with 80–90 wt% virgin resin, 10–20 wt% closed-loop regrind, and 1–3 wt% antistatic masterbatch when static dissipation is required for electronics-adjacent logistics. Flatness after demoulding must remain within 2.0 mm/m for robotic pick-and-place compatibility; the critical process variable is holding pressure decay at the pack-to-hold transition, because wide-area flat parts exhibit warpage when the pressure integral during the first 3 s of cooling falls below 60% of peak pack pressure. The process runs on a moving-platen injection machine with a clamp force of 6,000–10,000 kN, a four-zone barrel at 210–240°C, and mould temperature of 20–35°C. When residual-stress audits exceed the flatness limit, parts are annealed at 80–90°C for 30 min; batch-to-batch drift in post-industrial regrind melt flow rate above 8.5 g/10 min correlates with gate-area flash, which is controlled by reducing barrel temperature rather than increasing clamp force. Compliance for logistics use is assessed by ISO 8611-1:2021 static load deflection and ASTM D638-14 tensile yield as an incoming batch check; where antistatic function is required, surface resistivity is verified to IEC 61340-5-1 in the 1×109–1×1011 Ω/sq range, but the additive can reduce tensile yield by up to 5% compared with an unfilled outer layer. Terminal product types are flat dunnage trays, racking interlayers, and injection-moulded pallet runners in which dimensional stability is the primary quality gate.

    Free Quote

    Competitive Versalis HDPE MR80U prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis HDPE MR80U is a high molecular weight high-density polyethylene blow-moulding grade produced by Versalis S.p.A. within its HDPE product range. The resin is specified by a nominal density of 0.958 g/cm³ when tested according to ISO 1183-1 and by a high-load melt mass-flow index of 8 g/10 min at 190 °C under a 21.6 kg piston load according to ISO 1133-1:2022. Those two data points classify the material in the high-molecular-weight blow-moulding segment rather than in injection-moulding or film-extrusion HDPE because the low-load 2.16 kg melt index is not the primary lot-release specification; the high-load value is used to control extrusion behaviour while preserving the melt elasticity needed for parison retention. The suffix U identifies a UV-stabilised additive package, which separates MR80U from the unstabilised MR80 base of the same nominal viscosity range. The product is intended for wide-thickness extrusion blow-moulded articles between 5 L and 30 L, such as jerry cans, detergent and agrochemical containers, and industrial fluid reservoirs. In comparison with general-purpose HDPE grades of equivalent density, MR80U shifts the performance envelope toward stress-crack resistance and elevated elongation at break while reducing low-shear fluidity and making thin-wall injection moulding unattractive. Published data for aggressive chemical service at continuous wall temperatures above 60 °C is limited, and end-use qualification remains necessary rather than relying solely on datasheet values.

    Why Is High-Load Melt Mass-Flow Index the Specification Rather Than a Low-Load Melt Index?

    High-load melt index testing at 21.6 kg is used for blow-moulding grades because low-load 2.16 kg values are too small to discriminate among medium-high molecular weight resins and provide only weak correlation with extrusion output. MR80U is controlled at 8 g/10 min at 190 °C and 21.6 kg under ISO 1133-1:2022; the equivalent low-load value is deliberately not a lot-release target. The high-load value must be interpreted with die swell and zero-shear viscosity because two lots with identical 21.6 kg melt index can still show different parison hang time if the molecular weight distribution shifts. The molecular architecture responsible for the product’s ESCR performance increases extrusion die swell to a typical range of 25% to 40%. This viscoelastic memory effect is evaluated on production tooling rather than on a rheometer alone because laboratory capillary data do not completely capture the annular swell and sag interaction that occurs on an accumulator-head machine. Processing trials on 60–90 mm extruders with 24:1 to 30:1 L/D and low-compression barrier screws show that melt temperatures below 190 °C generate high backpressure and melt fracture at output rates above roughly 100 kg/h on a 60 mm line, while temperatures above 230 °C produce visible parison sag in lay-flats above 300 mm. This narrow corridor is a direct consequence of the high molecular weight fraction and is narrower than that of more fluid HDPE blow-moulding grades. Die land length-to-gap ratio should not fall below 15:1 to avoid surface roughness from melt fracture and to stabilise wall-thickness control in heavier articles.

    A preliminary comparison of MR80U with other HDPE grades should be made on the basis of the following published typical values. The tensile yield stress of 26 MPa under ISO 527-2 is slightly lower than that of high-stiffness injection-moulding HDPE compounds that use mineral fillers or higher crystallinity, but the trade-off is a tensile elongation at break above 600% and a Charpy notched impact value of 18 kJ/m² at 23 °C under ISO 179-1/1eA. Flexural modulus of 1200 MPa under ISO 178 places the material in the typical unfilled HDPE stiffness band. The Vicat softening point of 125 °C under ISO 306 A/50 does not imply hot-fill capability; continuous exposure to polar stress-cracking fluids above 60 °C requires separate testing because ESCR performance drops as temperature approaches the Vicat region. Under ASTM D1693 condition B in 100% Igepal at 50 °C, the environmental stress crack resistance exceeds 600 h, which is the primary specification for detergent and surfactant containers. The following table consolidates these values as a screening checklist.

    PropertyPublished typical valueTest designation
    Nominal density0.958 g/cm³ISO 1183-1
    Melt mass-flow index8 g/10 min at 190 °C, 21.6 kgISO 1133-1:2022
    Tensile yield stress26 MPaISO 527-2
    Tensile elongation at break>600%ISO 527-2
    Flexural modulus1200 MPaISO 178
    Charpy notched impact at 23 °C18 kJ/m²ISO 179-1/1eA
    Vicat softening point A/50125 °CISO 306
    Environmental stress crack resistance>600 h at 50 °C in 100% IgepalASTM D1693 condition B

    Parison Geometry, Die Swell, and Accumulator-Head Process Limits

    Parison control is more sensitive to die swell and melt strength than to barrel temperature alone. On shuttle and accumulator-head machines with clamp force in the 150–400 kN range, MR80U is used for containers with wall thickness from approximately 1.5 mm to 5 mm. At a die gap of 1.5 mm, extrudate swell can force the operator to increase the gap toward 2.5 mm or 3.0 mm to maintain the target parison wall, particularly when regrind is present. The grade tolerates up to 30% clean in-plant regrind from the same lot without major loss of drop-impact performance, provided that the scrap is dry and free of foreign polymer contamination. Moisture is not a bulk phase issue for HDPE, but surface condensation on cold pellets transferred from low-temperature storage into a production hall above 60% relative humidity can create surface defects; in such cases hopper-drying for 2 h at 80 °C removes condensed surface water. The melt-temperature corridor of 190–230 °C should be maintained at the screw tip, not merely at the barrel set points, because screw shear can add 5–15 °C of adiabatic temperature rise at high rotor speeds. The resin should not be blended with amine-based processing aids or reactive crosslinking masterbatches; these systems may initiate gel formation in overheated zones above 240 °C. Colour concentrate loading should be limited to the minimum required for opacity because excessive pigment can reduce pinch-off weld strength and lower the effective ESCR of the finished container.

    Lot-to-lot variation in the 21.6 kg melt index of approximately ±0.5 g/10 min can shift die swell sufficiently to require a die-gap adjustment of 0.2–0.4 mm in heavy-wall articles. This is not an out-of-specification condition but a normal production correction. Processors that mould with fixed die gaps should monitor parison length and lay-flat width rather than relying on melt temperature alone, because parison length changes of 2–5% are detectable before the finished article exceeds its wall-thickness tolerance. The grade is not intended for injection moulding; attempts to use MR80U in high-shear injection applications produce excessive pressure drop and weld-line weaknesses. In blow moulding, purging after downtime should use a lower-viscosity HDPE or polypropylene purge compound to shorten transition, but the purge material must be cleared completely to avoid delamination. The product’s molecular weight distribution is designed to support high extrusion output under high-load conditions while retaining the tie-chain population required for stress-crack resistance. This is the central difference from standard injection-moulding HDPE grades, where molecular weight is reduced for flow and ESCR performance drops accordingly.

    When the Container Must Survive Drop Impact at Sub-Zero Temperatures

    For containers used in cold-chain or outdoor winter service, room-temperature Charpy data overstate finished-part toughness. The notched impact value of 18 kJ/m² at 23 °C falls to approximately 8 kJ/m² at -30 °C under ISO 179-1/1eA. Designers should therefore increase pinch-off radius, avoid sharp tail flash on handles, and specify drop-impact testing on filled containers at the lowest expected storage temperature. A drop height of 1.2 m onto concrete is commonly used for 20 L jerry cans at -20 °C, but the pass criterion is specific to the filling ratio, cap design, and moulded-in handle geometry. The high molecular weight fraction in MR80U helps retain ductile failure in thick-wall sections, but weld lines and pinch-off areas are the most likely fracture initiation sites. Processors should ensure that the pinch-off zone remains above 200 °C during mould closure; if the mould is too cold or the cycle is too slow, the apparent bulk material impact value no longer represents the finished article. This is a critical process boundary: a cold pinch-off line can reduce drop-impact energy by more than half. Published data for this specific configuration is limited, so production validation must include sectioned parts and instrumented drop testing rather than resin database screening alone.

    Where outdoor service and regulatory compliance overlap, MR80U is supplied as a UV-stabilised blow-moulding grade suitable for intermediate-term exterior storage in temperate climates. The base polymer may be evaluated under Commission Regulation (EU) No 10/2011 as amended and FDA 21 CFR §177.1520 for polyolefin articles, but these clearances do not automatically cover colour concentrates, barrier layers, adhesives, or post-moulding treatments. The stabiliser package in the U suffix separates MR80U from the unstabilised MR80 base; the mechanical property envelope remains substantially the same, but outdoor surface embrittlement occurs later in the U version. The exact improvement in weathering retention depends on wall thickness, ultraviolet irradiance, and local temperature cycling, and published data for this specific configuration is limited. In chemical service, high ESCR does not equal full chemical resistance: strong oxidisers, aromatic solvents, and halogenated agents can still reduce service life at stressed pinch-off lines or moulded-in handles. The following compliance matrix summarises the most commonly requested designations during material qualification.

    Regulatory areaDesignationQualification context
    EU food-contact plasticsCommission Regulation (EU) No 10/2011 as amendedSpecific migration limits depend on the food simulant, contact time, and surface-to-volume ratio
    US FDA food-contact21 CFR §177.1520Olefin polymer acceptance subject to end-use limitations
    REACHRegulation (EC) No 1907/2006Substance registration and SVHC screening apply at the raw material level
    RoHSDirective 2011/65/EU as amendedRestricted heavy metals are not intentionally added

    For fuel containers and aggressive solvent packaging, the unmodified MR80U wall is generally insufficient as a permeation barrier. High-density polyethylene has a finite permeation coefficient for aromatic and aliphatic hydrocarbons, and although the high ESCR of MR80U improves stress-cracking hold-out, it does not create the low-permeation structure required for evaporative emission limits. Fluorination, sulphonation, or a polyamide barrier layer is used, with MR80U functioning as the structural skin at wall thicknesses from 1.5 mm to 5 mm. This application boundary distinguishes MR80U from lower-viscosity HDPE blow-moulding grades: the higher melt strength supports heavy-wall parisons and pinch-off integrity, but it also narrows the melt-temperature window and requires closer die-gap management when article weight changes. The grade is not recommended for packaging that depends on HDPE alone for petrol or solvent retention.