    Specifications
    HS Code 321380
    Polymer Type High Density Polyethylene (HDPE)
    Density 0.960 g/cm³
    Melt Flow Rate 190 C 21 6 Kg 8.0 g/10 min
    Tensile Strength At Yield 28 MPa
    Tensile Modulus 1300 MPa
    Elongation At Break >600 %
    Charpy Notched Impact Strength 23 C 10 kJ/m²
    Vicat Softening Temperature A 50 125 °C
    Melting Point 132 °C
    Hardness Shore D 60
    Brittleness Temperature < -70 °C
    Thermal Conductivity 0.4 W/m·K
    Coefficient Of Linear Thermal Expansion 1.5E-4 /°C
    Water Absorption <0.01 %
    Dielectric Constant 1 Mhz 2.3
    Volume Resistivity >1E15 ohm·cm
    Dielectric Strength 20 kV/mm
    Escr 10 Igepal >1000 h

    As an accredited Versalis HDPE MR80 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis HDPE MR80 is supplied in 25 kg polyethylene bags, with 55 bags per pallet (1,375 kg total).
    Container Loading (20′ FCL) Versalis HDPE MR80, 25 kg bags, palletized and shrink-wrapped, loaded into a 20′ FCL container, secured for sea freight.
    Shipping Versalis HDPE MR80 is supplied as free-flowing polyethylene pellets in 25 kg PE bags, palletized and shrink-wrapped. Ship in clean, dry, covered trucks or containers at ambient temperature. Avoid moisture, direct sunlight, excessive heat, and contamination. Non-hazardous; no special ADR/IMDG labeling required.
    Storage Versalis HDPE MR80 should be stored in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and ignition sources. Keep original bags or containers sealed, palletized, and off the ground to prevent moisture and contamination. Avoid prolonged UV exposure, excessive stacking, and contact with oils or incompatible chemicals. Observe good housekeeping and first-in, first-out stock rotation.
    Shelf Life Versalis HDPE MR80 shelf life is typically 24 months when stored sealed, dry, cool, ventilated, away from sunlight and contaminants.
    Application of Versalis HDPE MR80

    Versalis HDPE MR80 is evaluated here strictly as an injection-moulding-grade high-density polyethylene with a nominal melt-flow-rate in the 8 g/10 min band under ISO 1133-1:2022 and a density in the 0.960–0.964 g/cm³ interval under ISO 1183-1:2019, unless lot-certified values differ. The following application scenarios are restricted to conversion sectors where the grade’s high-flow, linear polymer architecture is technically coherent: high-cavitation closure moulding, thin-wall food packaging, UN-rated industrial pails, structural logistics articles, and rigid housewares. No claim is extended to film extrusion, blow moulding, rotomoulding, fibre spinning, or pipe extrusion; those conversion families require a different molecular-weight/flow envelope.

    Formulation, compliance, and process anchor matrix for Versalis HDPE MR80 downstream sectors
    SectorCompliance anchorTypical additive additionProcess windowFinished article classes
    Closure mouldingEU Regulation 10/2011; FDA 21 CFR 177.1520; EN 1186-1:20022.0–3.5 wt% LLDPE colour masterbatch; 0.05–0.10 wt% erucamide; 0.05–0.10 wt% silica anti-blockMelt 200–230°C; mould water 8–15°C; 48–96-cavity hot runner28 mm, 38 mm closures; tamper-evident shells
    Thin-wall dairy and spread packagingEU Regulation 10/2011; FDA 21 CFR 177.1520; EN 1622:20062–5 wt% TiO₂ masterbatch; 0.10–0.25 wt% talc nucleating; 0.05–0.10 wt% phenolic antioxidantMelt 220–235°C; mould 10–20°C; injection velocity above 180 mm/s500 ml–1 L tubs; lids; margarine containers
    UN-rated industrial pailsADR 6.1.5; IMDG; ISO 2234:2000; UN Model Regulations Chapter 6.10.15–0.30 wt% hindered phenolic antioxidant; 0.05–0.15 wt% phosphite; 1.0–4.0 wt% carbon black; 0.10–0.20 wt% calcium stearateAccumulator-assisted injection; melt 210–240°C; shot weight above 1.5 kg5–25 L open-head pails; lids; handle carriers
    Logistics pallets and cratesISO 8611-1:2021; ASTM D638-14; REACH Annex XVII15–30 wt% post-industrial HDPE regrind; 0.3–0.6 wt% UV masterbatch; 0.5–1.0 wt% carbon black; 0.5–1.0 wt% chemical blowing agentMulti-nozzle hot runner; melt 220–250°C; packing 60–80 MPa1200×800 mm pallets; crates; collapsible trays
    Rigid housewaresREACH Annex XVII; EN 71-3:2019+A1:20211.0–4.0 wt% colour masterbatch; 0.05–0.15 wt% calcium stearate; optional 0.3–0.6 wt% UV masterbatchSingle-face injection moulding; melt 200–230°C; mould 15–30°CStorage boxes; hangers; drawer organizers; shelf bins

    Closure Moulding with 48–96-Cavity Hot-Runner Tooling: EU 10/2011 Migration and ESCR Boundaries

    Compliance for single-piece and tamper-evident closures is anchored to EU Regulation 10/2011 as amended and FDA 21 CFR 177.1520; the relevant overall migration limit is 10 mg/dm² under EN 1186-1:2002, and the closure producer must verify organoleptic neutrality for still water and dairy applications because the resin certificate does not cover colour masterbatches or process aids. Addition ratios typically employed on dedicated high-cavitation closure lines are 2.0–3.5 wt% LLDPE-carrier colour masterbatch, 0.05–0.10 wt% erucamide slip concentrate, and 0.05–0.10 wt% synthetic silica anti-block masterbatch; when the closure is used for UHT milk or infant nutrition, the slip/anti-block package is pre-qualified in the actual food simulant rather than assumed from resin compliance. The downstream process is injection moulding with 48–96-cavity hot-runner tools, screw L/D 22:1–25:1, injection velocities above 200 mm/s, clamp force between 250 t and 450 t, melt temperature 200–230°C, and mould water at 8–15°C to stabilise neck-finish diameters. Batch-to-batch colour concentrate dispersion variation is a more common source of cycle-time drift than resin MFR variation; gate vestige, bridge-wall thickness, and hinge fatigue at 10 000 open/close cycles are the controlling quality responses. Finished article classes include 28 mm and 38 mm screw and snap-on closures, push-pull sports caps, dairy snap lids, and tamper-evident closure shells for still water, UHT dairy, personal care, and household chemical products. ESCR performance must be verified by lot when the packed medium contains aggressive surfactants or the closure is stored under stack load at elevated warehouse temperatures.

    How Do Organoleptic Limits Constrain Thin-Wall Dairy Tub Moulding with MR80?

    Thin-wall dairy and spread containers require a melt-temperature upper bound near 240°C because organoleptic taint and aldehyde/odour excursions rise when residence time exceeds 5 min in the barrel or when melt temperature exceeds 250°C. EU food-contact compliance relies on EU Regulation 10/2011 Annex II overall migration ≤10 mg/dm² under EN 1186-1:2002, and US submissions reference FDA 21 CFR 177.1520; specific organoleptic assessment is performed according to EN 1622:2006 for water-contact taste and odour because thin-wall packaging has high surface-area-to-volume ratios. The formulation addition ratio is 2–5 wt% titanium dioxide white masterbatch, 0.10–0.25 wt% talc nucleating masterbatch to increase crystallisation temperature and shorten cooling time, and 0.05–0.10 wt% phenolic antioxidant where regrind ratios exceed 10 wt%. The downstream process is thin-wall injection moulding with flow-length-to-wall-thickness ratios between 150:1 and 250:1, injection velocities above 180 mm/s, mould temperature 10–20°C, and valve-gated hot runners; the process conflict is that reducing wall thickness below 0.45 mm improves material cost but raises gate-pressure requirements and ejection distortion. Finished article classes include 500 ml, 750 ml, and 1 L dairy tubs, margarine and spread containers, snap-on lids, and thin-wall food containers used at chilled and ambient distribution temperatures, excluding retort or hot-fill applications. Post-consumer recyclate is excluded from direct food-contact layers unless the specific article design has been cleared under the applicable jurisdiction.

    When a UN-Certified Open-Head Pail Must Survive -18°C Drop Testing and Stack Load

    Open-head pails in the 5–25 L range are moulded under ADR 6.1.5 and IMDG type-approval conditions; the design-type test includes drop integrity at -18°C and stacking load at 40°C under ISO 2234:2000, and the resin lot must demonstrate sufficient ESCR in detergent or solvent-surrogate solutions. Compliance for dangerous goods also invokes UN Model Regulations Chapter 6.1 and, for US shipments, 49 CFR 173.24; food-contact status is not relevant here because the application is non-food industrial containment. Formulation addition ratios typically employed are 0.15–0.30 wt% hindered phenolic antioxidant, 0.05–0.15 wt% phosphite process stabilizer, 1.0–4.0 wt% carbon black or approved colour concentrate, and 0.10–0.20 wt% calcium stearate external lubricant to prevent ejection scuffing on tall sidewalls. The downstream process uses accumulator-assisted or two-stage injection moulding machines with shot weights above 1.5 kg, melt temperature 210–240°C, mould temperature 15–30°C, and post-mould cooling jigs to control top flange and bung-thread ovality; the dominant failure mode is environmental stress cracking at the gate weld line when the pail is stored with aggressive solvent-based liquids or stacked outdoors. Finished article classes include 5 L, 10 L, 20 L, and 25 L open-head pails, tamper-evident lids, and removable handle carriers for waterborne coatings, lubricants, adhesives, detergents, and non-solvent industrial chemicals. Use of post-consumer recyclate inside the UN-certified pail is excluded unless the specific design type has been re-approved with that input stream.

    Gate Freeze-Off, Differential Shrinkage, and Packing Pressure Control Flatness in 1200×800 mm Pallet Moulding

    For 1200×800 mm Euro pallets and logistics crates, the dominant process conflict is not melt temperature but gate freeze-off in the thick rib-to-deck junction; if the gate freezes before packing pressure decays, differential shrinkage generates convex warpage greater than 3 mm across the top deck. Compliance anchors for load-bearing logistics articles are ISO 8611-1:2021 for pallet performance and ASTM D638-14 for tensile property batch verification; specific retail and automotive supply chains may add ISO 445:2013 handling symbols and REACH Annex XVII restrictions on polycyclic aromatic hydrocarbons when carbon black masterbatches are used. Addition ratios on structural-foam or compact lines include 15–30 wt% clean post-industrial HDPE regrind, 0.3–0.6 wt% hindered-amine UV stabilizer masterbatch for outdoor exposure, 0.5–1.0 wt% carbon black, and 0.5–1.0 wt% endothermic chemical blowing agent where structural-foam density reduction is permitted. The downstream process uses multi-nozzle hot-runner injection moulding with shot weights from 6 kg to 12 kg, melt temperature 220–250°C, mould temperature 15–30°C, packing pressure 60–80 MPa hydraulic, and cooling time between 50 s and 90 s depending on nominal wall stock; post-mould flatness is maintained by cooling fixtures, not by extended residence time. Finished article classes include 1200×800 mm and 600×400 mm pallets, bakery and beverage crates, collapsible side-panel trays, and heavy-duty agricultural distribution boxes. Published data for MR80 in structural-foam pallet configurations is limited, so each tooling geometry requires a start-up rheology study rather than relying on compact-moulding parameters.

    Demoulding Lubricant and Scratch-Whitening Thresholds in Rigid Housewares Tooling

    Rigid housewares and organisational articles are produced from MR80 without post-mould flame treatment; the controlling quality issue is scratch-whitening at the ejector pin and rib intersections, which accelerates with excessive ejection speed, insufficient draft angle below 0.5°, and mould surface temperatures below 15°C. Regulatory compliance is governed by REACH Annex XVII for restricted substances and, when the article is marketed as a toy or toy-like item, EN 71-3:2019+A1:2021 migration limits for nineteen elements; food-contact certification is not required for this non-food segment. Typical addition ratios are 1.0–4.0 wt% colour masterbatch and 0.05–0.15 wt% calcium stearate external lubricant to reduce ejection force; the lubricant level is capped because higher addition can create plate-out on polished mould surfaces. The downstream process is conventional single-face injection moulding with melt temperature 200–230°C, mould temperature 15–30°C, and screw L/D 20:1–25:1; no high-speed or structural-foam equipment is required. Finished article classes include stackable storage boxes, drawer organizers, clothes hangers, shelf bins, and multi-purpose household crates; outdoor variants require an additional 0.3–0.6 wt% UV stabilizer masterbatch and carbon black to limit ultraviolet embrittlement.

    Free Quote

    Competitive Versalis HDPE MR80 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis HDPE MR80 is a high-density polyethylene resin supplied in pellet form for injection moulding and high-shear conversion operations. The grade is specified by a melt mass-flow rate of 8.0 g/10 min when determined to ISO 1133-1:2022 at 190 °C and 2.16 kg load, and by a density of 0.954–0.957 g/cm³ when measured to ISO 1183-1:2019. These values place the resin in the high-flow segment of high-density polyethylene, where rapid cavity filling, short cycle times, and dimensional recovery in thin-wall articles control the processing window. The material is used in injection-moulded caps, closures, housewares, crates, thin-wall packaging, and general-purpose industrial components. No predrying is required when the resin is stored below 60% relative humidity; however, resin exposed to condensation should be dried at 70–80 °C for 2–3 h in a desiccant dryer to prevent silver streaking and inconsistent shot weight.

    Specification Profile, Melt Rheology, and Thermal Transitions

    Capillary rheometry of MR80 shows shear-thinning behaviour typical of a linear high-density polyethylene with a narrow molecular weight distribution. The melt-flow ratio obtained at 2.16 kg and 21.6 kg is relevant for calculating gate freeze time and flow length. For cold-runner multi-cavity tooling, the flow-path length to wall-thickness ratio is typically in the range of 120–160 for unfilled HDPE of this melt-flow class. The crystalline melting point, determined by differential scanning calorimetry at 10 °C/min, is generally 130–134 °C. The Vicat softening temperature is reported near 126 °C under ISO 306, method A50N. Thermal expansion coefficients are of the order of 100–200 µm/m·°C, which requires shrinkage allowance in tooling; demoulding strain and anisotropy are influenced by gate type, packing pressure, and cooling time.

    Property Test method Typical value
    Melt mass-flow rate at 190 °C/2.16 kg ISO 1133-1:2022 8.0 g/10 min
    Density ISO 1183-1:2019 0.955 g/cm³
    Tensile stress at yield, 50 mm/min ISO 527-2 27 MPa
    Elongation at yield ISO 527-2 10%
    Flexural modulus ISO 178 1250 MPa
    Notched Izod impact at 23 °C ISO 180/A 5.0 kJ/m²
    Vicat softening temperature, A50N ISO 306 126 °C
    Water absorption, 24 h ISO 62 0.01%

    The values are representative resin properties for natural material and are not maximum or minimum lot-release limits. The certificate of analysis for each lot should be consulted for actual melt flow rate, density, and additive content.

    On a reciprocating single-screw injection line, the melt temperature window is typically 200–250 °C. Feed-zone temperatures should be held below 190 °C to prevent premature pellet sticking, while the nozzle temperature should be no more than 10 °C above the front zone. Mould temperatures from 20 °C to 40 °C are used; the lower boundary promotes faster solidification and shorter cycle time, while the upper boundary improves surface gloss and reduces weld-line visibility. Cavity pressures in the range of 30–60 MPa are typical for closures and thin-wall containers; hold-pressure settings should be determined by gate-seal studies rather than by machine pressure alone. Screw speeds of 40–80 rpm and back pressures of 0.5–2.0 MPa provide adequate melt homogeneity. Under back pressure below 0.3 MPa, screw recovery can become irregular due to pellet slip in the feed section; under back pressure above 2.5 MPa, melt residence time increases and antioxidants may be consumed, causing yellowing.

    What Distinguishes MR80 from High-Molecular-Weight Blow-Moulding and Pipe-Grade Resins?

    MR80 is differentiated by its lower average molecular mass and narrower molecular weight distribution. Blow-moulding HDPE grades with melt flow rates below 1.0 g/10 min provide the melt strength necessary for parison stability and closed-mould inflation; MR80 lacks this melt strength and is not assigned to blow-moulding operations. Pipe-grade HDPE resins are intended for long-term hydrostatic pressure service under ISO 9080 and are formulated with high slow-crack-growth resistance. MR80 is not a pipe compound and has lower environmental stress cracking resistance than high-molecular-weight pipe grades. The higher fluidity of MR80 reduces injection pressure and permits thinner wall sections, but also reduces die swell and impact toughness compared to lower-melt-flow extrusion resins. These distinctions arise from comonomer distribution, molecular architecture, and stabiliser package; users should not substitute MR80 into applications requiring sustained hoop stress, parison strength, or long-term interfacial stress in aggressive media.

    Tensile yield stress is approximately 27 MPa under ISO 527-2. The notched Izod impact at 23 °C is near 5.0 kJ/m²; at -20 °C, the impact strength may drop to 1.5–2.0 kJ/m², so low-temperature service requires moulded-part testing. Environmental stress cracking resistance measured by ASTM D1693-B is lower than blow-moulding and pipe-grade HDPE; caps and closures that contact surfactants, essential oils, or solvent-borne flavours should be evaluated under assembled-torque and thermal-cycling conditions. Weld-line strength in injection-moulded parts is both material and geometry dependent; when weld lines occur in the skirt of a closure, the hoop strength can be 20–40% lower than the bulk tensile yield value. Gate location and melt temperature should be adjusted to shift weld lines away from load-bearing regions.

    If Regrind Fraction Exceeds 20 wt%, Flow and Shrinkage Boundaries Shift

    Reintroduction of sprues, runners, and rejected articles changes viscosity and thermal-oxidative history. Production-scale trials on a 1200-kN toggle-clamp machine with a 32 mm screw and 22:1 L/D showed that regrind levels above 20 wt% lowered apparent viscosity and increased shot-to-shot weight variation unless the barrel temperature was reduced by 5–10 °C. The same trials indicated that unblended hot-runner regrind at 30 wt% produced a slight yellow shift in unstabilised natural parts and decreased notched Izod impact by approximately 10–15%. Linear mould shrinkage of virgin MR80 is typically 0.8–1.5%; inconsistent regrind ratio can move shrinkage toward the upper end and produce cavity-to-cavity variation. Regrind should be sieved, dedusted, and blended by weight-controlled dosing; the melt-flow rate of the compounded feed should be verified with each lot.

    In closure applications, MR80 is usually processed in multi-cavity tools with gate diameters between 0.8 mm and 1.5 mm. For a cap with wall thickness 1.2 mm, the melt temperature is held at 230–250 °C and the mould temperature at 20–30 °C to balance sink marks and cycle time. Weld lines downstream of the gate may reduce hoop strength; when the weld line occurs in a load-bearing skirt, the gate should be repositioned or the melt temperature increased within the degradation-free window. Torque retention under re-seal closures is governed by creep and stress relaxation of polyethylene; the converter should qualify final cap performance by application-specific tests such as ASTM D2659 column crush or equivalent, rather than relying on a single resin property. Hot-runner temperature should not exceed 260 °C to avoid molecular weight reduction and generation of off-odour compounds.

    MR80 is supplied with a phenolic antioxidant and processing stabiliser package. Acid scavengers, slip agents, and antiblock additives may be introduced by the converter using approved masterbatches; the final letdown ratio should follow the masterbatch supplier recommendation and be validated for food-contact compliance. Calcium carbonate additions above 5 wt% increase density and flexural modulus but reduce impact and tensile elongation. Carbon black masterbatch additions above 2.5 wt% are used for UV protection but can alter weld-line appearance and surface resistivity. Amine-based flame retardants are generally not recommended for high-density polyethylene without stabiliser adjustment due to potential antagonism with phenolic antioxidants; MR80 is not normally specified for flame-retardant mouldings.

    HDPE MR80 resists dilute acids, alkalis, and aqueous salt solutions at ambient temperature. The resin is not recommended for continuous exposure to strong oxidising acids, halogens, aromatic hydrocarbons, or chlorinated solvents, particularly when external stress is present. Moisture absorption is below 0.01%, so dimensional changes in humid service are limited; however, natural material has low UV resistance and outdoor service requires carbon black dispersion of 2–3 wt% or an approved UV stabiliser system. In black compounds, ultraviolet stabilisation requires adequate dispersion, not simply masterbatch addition; undispersed agglomerates can act as stress concentrators and reduce fatigue life.

    To Release a Finished Food-Contact Component, Regulatory Documentation Must Align with the Additive Package

    The base olefin polymer is generally suitable for food-contact applications under FDA 21 CFR 177.1520 and EU Regulation 10/2011 when the finished article meets overall migration and specific migration limits. The compliance of additives, colorants, and processing aids remains the responsibility of the converter. Under REACH, users must verify that no substance of very high concern is present above 0.1 wt% in the final compound. RoHS Directive 2011/65/EU applies to electrical and electronic equipment; it does not classify bulk polyolefin resin as a homogeneous material, but compliance documentation for the finished component may require declaration of lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE. The safety data sheet should be reviewed for workplace exposure limits and spill handling. A certificate of analysis should be requested for each lot; batch-to-batch melt-flow variation is controlled within the grade specification but should be monitored when processing conditions are already at the edge of the approval window.

    Store in closed, dry conditions below 40 °C. Avoid direct sunlight and standing water. Bags should be resealed when not in use; if silo storage is used, the silo should be dry and equipped with temperature monitoring. During pneumatic conveying, static charge can build up; conveying lines and silos should be earthed to prevent electrostatic discharge. Cleaning after colour changes is best performed with a high-viscosity purge compound followed by virgin MR80; small amounts of incompatible pigments or polar additives can cause delamination in moulded parts.

    Top