Versalis Hdpe Mq74

Versalis HDPE MQ74

    • Product Name: Versalis HDPE MQ74
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 323564
    Density 0.954 g/cm3
    Melt Flow Rate 190 C 2 16 Kg 0.35 g/10 min
    Tensile Modulus 1300 MPa
    Tensile Stress At Yield 27 MPa
    Tensile Strain At Break >600%
    Flexural Modulus 1300 MPa
    Shore D Hardness 65
    Vicat Softening Temperature 125 °C
    Heat Deflection Temperature 0 45 Mpa 75 °C
    Charpy Notched Impact Strength At 23 C 15 kJ/m2
    Charpy Notched Impact Strength At 30 C 8 kJ/m2
    Environmental Stress Cracking Resistance >1000 h
    Melting Temperature 133 °C
    Water Absorption <0.01%

    As an accredited Versalis HDPE MQ74 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis HDPE MQ74 comes in 25 kg polyethylene bags, with 55 bags per pallet, totaling 1,375 kg per pallet.
    Container Loading (20′ FCL) 20′ FCL loading of Versalis HDPE MQ74 high-density polyethylene resin: 25 kg bags, palletized, stretch-wrapped, securely stowed for ocean shipment.
    Shipping Versalis HDPE MQ74 is a non-hazardous high-density polyethylene resin. It is typically shipped in 25 kg moisture-resistant bags, palletized and stretch-wrapped, or in bulk trucks/containers with liners. Transport in clean, dry conditions; avoid moisture, direct sunlight, and excessive heat. No special dangerous-goods classification required.
    Storage Store Versalis HDPE MQ74 in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and strong oxidizing agents. Keep containers closed to prevent moisture and contamination. Avoid prolonged UV exposure. Maintain ambient temperatures, use FIFO rotation, and keep pallets off floors/walls to allow air circulation. Do not stack excessively; protect from physical damage. Follow local regulations.
    Shelf Life Recommended shelf life is 12 months when stored in original unopened packaging, cool, dry, away from direct sunlight and heat.
    Application of Versalis HDPE MQ74
    In the production of 5 L to 30 L tight-head and open-head jerrycans intended for UN 3H1 dangerous goods packaging, the selection of Versalis HDPE MQ74 is driven by a combination of high-load melt flow rate, stress crack resistance, and parison stability during extrusion blow molding. Container wall thickness distribution is mapped around the handle, pinch-off, and sidewall-to-bottom transition, because wall thinning below 1.2 mm on a 20 L jerrycan can compromise the hydraulic pressure retention test under ISO 16104. Melt temperature at the die is maintained between 190 °C and 210 °C, while the accumulator head or continuous extruder screw is operated with a length-to-diameter ratio of 24:1 to 30:1 and a barrel profile from 180 °C to 220 °C to control shear heating. A die gap of 2.0 mm to 3.5 mm is set for a 20 L parison; parison swell is expected to remain in the 25% to 40% range for this grade when the certificate of analysis reports a high-load MFR of 6.0 g/10 min to 8.0 g/10 min at 190 °C and 21.6 kg under ISO 1133-1:2022, with density in the 0.956 g/cm³ to 0.960 g/cm³ range under ISO 1183-1:2019. The pinch-off weld at the container bottom is the most common failure location when regrind addition exceeds 30 wt%, because high-molecular-weight gel particles and oxidative degradation shift the ductile-to-brittle transition and reduce weld-line toughness under impact at -18 °C.Compliance for this segment is governed by UN Model Regulations Chapter 6.1 for 3H1 packages, ADR 6.1.5, and the IMDG Code for sea transport. Qualification includes drop testing from a packing-group-dependent height after conditioning at -18 °C for at least 24 h, leakproofness testing at 30 kPa for 5 min, hydraulic internal pressure testing to 100 kPa, and stacking tests at 40 °C for 28 days. Formulation practice for non-food jerrycan production uses 1.5 wt% to 2.5 wt% carbon black masterbatch for UV stabilization and 15 wt% to 25 wt% clean post-industrial regrind from the same production line. For outdoor storage of hypochlorite or detergent concentrates, a hindered amine light stabilizer is added at 0.2 wt% to 0.5 wt%, but the package must be re-qualified because some stabilizers migrate to the surface and alter weld-line friction during hot-tool pinch-off. End products are 10 L, 20 L, and 25 L tight-head containers for automotive lubricants, light paraffinic solvents, and 5% to 10% sodium hypochlorite solutions, with the external surface marked in accordance with the 3H1 design type certificate.
    Regulatory or test domainStandard or codeTest methodControlled variable in MQ74 containers
    UN dangerous goods packagingUN Model Regulations Chapter 6.1; ADR 6.1.5Drop, leakproofness, hydraulic, stackSidewall thickness ≥ 1.2 mm; pinch-off weld integrity
    Environmental stress crackingASTM D1693-B10% Igepal CO-630 at 50 °CESCR retention after 25 wt% regrind
    Melt flow rateISO 1133-1:2022190 °C, 21.6 kgHigh-load MFR range for parison control
    DensityISO 1183-1:2019Immersion methodDensity specification for rigid container stack strength

    What Limits Continuous Extrusion Output in 60 L Tight-Head Drum Production?

    Continuous extrusion of 60 L tight-head drums places two competing demands on the resin: high shear thinning for high output, and high melt strength to prevent parison sag on a 600 mm to 900 mm parison length. When MQ74 is run on a 90 mm extruder with a grooved feed zone and a 30:1 L/D ratio, melt pressure at the die is held between 25 MPa and 35 MPa, while die temperature is kept at 195 °C to 210 °C. Accumulator head machines are preferred above 60 L because they discharge the shot rapidly and reduce residence time; however, continuous extrusion with a 100-point radial wall thickness programmer is used for lower-output operations, where the programmed die gap is narrowed to 1.5 mm at the top and bottom pinch-off zones and opened to 3.0 mm at the sidewall centre to compensate for sag. The grade’s high-load MFR is a primary input for setting extruder screw speed because a shift of more than 0.5 g/10 min between lots can move die swell and alter the final top-load capacity under stack testing.Cooling time becomes the bottleneck at 60 L scale. With a 3.5 mm to 4.5 mm sidewall thickness, cycle times typically extend to 55 s to 75 s depending on mold temperature and water circuit pressure. Mold cooling is maintained at 12 °C to 25 °C, and internal blow air pressure is set at 0.6 MPa to 0.8 MPa. Inadequate cooling leads to post-mold shrinkage above the 2.5% linear shrinkage threshold and changes in the UN stack test result after 28 days at 40 °C. Regrind incorporation for 60 L drums is typically limited to 20 wt% to 30 wt% of the same production stream. The use of 100% virgin MQ74 is specified for drums intended for high-purity solvents or for customers requiring low odour. At 30 wt% regrind, the ESCR value measured on a notched specimen under ASTM D1693-B can retain above 70% of the virgin value; qualification tests on the finished drum should include a 1.2 m drop test at -18 °C and hydraulic internal pressure at 100 kPa for 5 min. End products are 60 L and 120 L tight-head drums for lubricating oils, oil-based agrochemical intermediates, and construction chemicals, where the top and bottom chime areas must withstand repeated fork-lift handling without environmental stress cracking.Agricultural pesticide and adjuvant packaging increasingly uses three-layer blow molded bottles with a thin polyamide barrier layer, because solvent-borne formulations contain xylene, cyclohexanone, or butyl acetate that can penetrate monolayer HDPE at rates that become measurable in container weight-loss tests at 54 °C over 14 days. A three-layer structure of outer HDPE / tie / polyamide / tie / inner HDPE is applied, with layer ratios of 35 wt% / 2 wt% / 6 wt% / 2 wt% / 55 wt% for aggressive organophosphate concentrates. The tie layer is maleic anhydride grafted PE and must ensure interlayer adhesion above 15 N/15 mm when tested after peel conditioning at 23 °C. If the polyamide layer falls below 4 wt% of total structure, pinhole defects and layer break-up occur during parison programming, especially at the bottle shoulder where the parison is stretched beyond 300% local elongation.Coextrusion blow molding of 1 L to 10 L containers uses a multi-layer die with separate extruders of 45 mm, 25 mm, and 65 mm respectively for HDPE, tie, and polyamide. Melt temperatures are 210 °C for HDPE, 220 °C for tie, and 245 °C for PA6; the lower HDPE temperature prevents edge melt fracture at the die exit. A 16-point parison programmer is used to shift the wall thickness profile, with the PA layer being more sensitive to shear stress, so die gaps below 1.2 mm in the pinch-off zone can cause layer break-up and barrier loss. Registration for crop protection packaging may include national pesticide container design type tests, followed by storage stability of the filled package at 54 °C for 14 days. The finished container is checked for closure torque retention after exposure to the product, because gasket compression set and HDPE relaxation can reduce torque retention below the specified limit. End products are 1 L, 2 L, and 5 L narrow-neck bottles for emulsifiable concentrates, suspension concentrates, and adjuvants, with a recyclability preference for all-polyolefin structures when barrier layers are below 5 wt% to avoid sorting rejection.

    Automotive Fluid Reservoir Welding and Heat-Aging Behaviour

    Automotive windshield washer reservoirs, coolant expansion tanks, and headlamp washer bottles are blow molded from high-molecular-weight HDPE because the part must survive vibration and under-hood temperatures while retaining weld integrity. For MQ74, the resin is run at die temperatures between 200 °C and 215 °C with a die gap of 2.0 mm to 2.8 mm for 2.5 mm to 3.5 mm nominal wall thickness. Weld lines at filler neck and bracket attachments are produced by hot-plate welding or spin welding; weld tensile failure stress should be measured according to ISO 527-2 and should maintain at least 80% of the base material yield stress when tested at 23 °C, but at 80 °C the value can fall to 60% because the polymer is closer to its Vicat softening point. Thermal cycling for engine compartment components is derived from ISO 16750-4, with cycling from -40 °C to 120 °C for 150 cycles.Heat aging for coolant expansion tanks is typically conducted at 121 °C in a 50/50 ethylene glycol-water mixture for 1,000 h. The acceptance criterion includes no visual delamination, no loss of fluid weight above 0.5 g, and no crack formation at weld zones after thermal cycling. HDPE grades in this class can show oxidation-induced embrittlement at the inner wall unless the coolant additive package is compatible with the polymer; acidic coolant degradation products accelerate molecular weight reduction at the tank wall. Reservoir formulations use 0.3 wt% to 0.5 wt% primary antioxidant and 0.2 wt% phosphorus stabilizer to survive multiple heat histories. Post-industrial regrind is limited to 15 wt% for coolant tanks because higher levels reduce hot-plate weld strength below OEM specification. The use of 2 wt% carbon black masterbatch is standard for UV resistance in visible fluid reservoirs. End products include washer bottles from 3 L to 7 L capacity, coolant expansion reservoirs from 1 L to 3 L, and auxiliary fluid reservoirs where the tank must pass an accelerated environmental stress cracking test with 5% surfactant at 60 °C.Sheet extrusion of Versalis HDPE MQ74 into 2.0 mm to 3.0 mm monolayer sheet for thermoformed food distribution trays requires a flat die temperature of 220 °C to 230 °C and a three-roll polishing stack set at 40 °C to 80 °C. The melt curtain is drawn down to the roll stack at a rate that controls machine-direction orientation, because orientation above 10% in the machine direction produces non-uniform shrinkage during thermoforming at 150 °C to 170 °C. The sheet is formed into defined-depth trays with plug-assisted vacuum forming; female cavity temperature is held at 20 °C to 40 °C, and the plug temperature is set to 90 °C to 110 °C to avoid premature cooling streaks. Food-contact compliance for the monolayer sheet is based on Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520 for olefin polymers. For structures with post-consumer recycled content, a three-layer A/B/A sheet is used with virgin MQ74 on both food-contact surfaces and 30 wt% to 50 wt% recycled HDPE in the core layer. Overall migration into 10% ethanol, 3% acetic acid, and iso-octane is tested according to the test conditions specified in Regulation (EU) No 10/2011 Annexes III and V. The end products are reusable dairy distribution trays, meat transport trays, and cold-chain boxes; the tray bottom must retain local wall thickness above 0.8 mm to survive repeated freezing and washing with alkaline detergents at 60 °C. At -20 °C, the material may exhibit reduced ductility; therefore, tray design must avoid sharp corners with radius below 2 mm to reduce stress concentration.

    When Vibration-Welded Marine Battery Boxes Require Impact Strength Retention at -20 °C

    Marine battery boxes and acid-bath housings are blow molded from HDPE with wall thickness of 3.0 mm to 5.0 mm, because the component must retain impact strength at sub-zero temperatures while resisting sulfuric acid electrolyte. For this application, MQ74 is processed at die temperatures of 205 °C to 215 °C with a die gap of 2.5 mm to 3.5 mm. The blow mold is chilled to 15 °C to 25 °C, but not below 10 °C, because rapid quenching at the mold surface increases frozen-in orientation and can reduce low-temperature impact at the pinch-off weld. Vibration-welded cover joints are produced at a frequency of 200 Hz to 240 Hz with a peak-to-peak amplitude of 1.0 mm to 1.8 mm, and weld pressure is set between 0.5 MPa and 1.5 MPa depending on the melt-down distance.Qualification for the application includes notched Charpy impact per ISO 179-1/1eA at -20 °C, a chemical immersion test in 37% sulfuric acid at 23 °C for 7 days under ISO 175, and a leakage test after 1.0 m drop at -20 °C. The pinch-off weld is the primary failure mode if the parison temperature drops below 195 °C or if the mold closes too slowly, because the cold weld-line becomes brittle under impact. Carbon black loading is kept at 2.0 wt% to 2.5 wt% for UV stability, and regrind is limited to 10 wt% because marine battery boxes are subjected to repeated impact loads during removal and replacement. End products include blow molded marine battery boxes, acid-drip troughs, and electrolyte handling trays for marine and off-grid storage applications.
    Free Quote

    Competitive Versalis HDPE MQ74 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis HDPE MQ74 is an injection moulding grade of high-density polyethylene supplied in pellet form. Public material databases describe the grade as having a melt flow rate in the 7–8 g/10 min range at 190 °C with 2.16 kg load and a density in the 0.956–0.960 g/cm³ range at 23 °C. These values place MQ74 in the medium-flow high-density injection moulding band used for rigid articles such as caps, closures, thin-wall containers, crates, pallets, housewares, and small industrial components. The melt flow rate is determined in accordance with ISO 1133-1; density is measured according to ISO 1183-1. The resin is not formulated for large-part blow moulding, blown film, or rotational moulding, where high melt strength, bubble stability, or long oven stabilisation are controlling.

    Which test standards constrain MQ74 component design?

    Design data for MQ74 are generated on injection-moulded specimens rather than compression-moulded sheets because flow orientation and frozen-in stress influence mechanical response. Tensile yield stress and elongation at break are evaluated according to ISO 527-2 or ASTM D638-14. Flexural modulus is determined under ISO 178 or ASTM D790. Notched Izod impact strength is measured by ISO 180/A or ASTM D256; comparisons must be made at identical specimen thickness and notch radius because energy absorption scales with ligament area. Vicat softening temperature is determined according to ISO 306/A120 or ASTM D1525; it is a short-term thermal resistance index and not a continuous-use temperature. Heat deflection temperature at 0.45 MPa is measured according to ISO 75-2/B or ASTM D648. Environmental stress crack resistance is assessed by ASTM D1693, but field performance is strongly influenced by moulded-in stress, processing orientation, and chemical concentration. Published data for this specific configuration is limited when laboratory ESCR values from plaques are applied to thin-wall closures with sharp corners.

    Property-test matrix for Versalis HDPE MQ74
    PropertyStandard methodApplication relevance
    DensityISO 1183-1Controls part mass, shrinkage, and stiffness per unit wall thickness
    Melt flow rateISO 1133-1Indicates mould filling behaviour and cycle time class
    Tensile yield stressISO 527-2 / ASTM D638-14Sets short-term load-bearing limits for crates and pails
    Flexural modulusISO 178 / ASTM D790Predicts resistance to bending deformation in thin-wall panels
    Notched Izod impactISO 180/A / ASTM D256Screens toughness at gates, weld lines, and rib roots
    Vicat softening pointISO 306/A120Short-term thermal resistance for hot-fill packaging checks
    ESCRASTM D1693Relevant for detergent, lubricant, and chemical container performance

    Rheological characterisation beyond melt flow rate is performed by capillary rheometry according to ISO 11443. Apparent viscosity is measured at shear rates from 100 s⁻¹ to 10,000 s⁻¹ to build a viscosity curve for mould filling simulation. MQ74 exhibits shear-thinning behaviour: viscosity decreases as shear rate increases, which supports thin-wall filling, while higher viscosity at low shear supports packing and dimensional stability. The crystallisation kinetics of high-density polyethylene are controlled by mould temperature and cooling rate. Rapid cooling at mould temperatures below 20 °C creates smaller spherulites and can improve toughness but increases differential shrinkage. Slow cooling at mould temperatures above 40 °C raises stiffness and reduces warpage but lengthens cycle time.

    Differentiation from blow moulding, film, and rotomoulding polyethylenes

    Blow moulding HDPE grades are typically formulated with melt flow rates below 1 g/10 min at 190 °C/2.16 kg. Their higher molecular weight generates the melt strength needed for parison hang time and bottle pinch-off integrity. MQ74 is positioned in a higher-flow injection moulding band; it has lower zero-shear viscosity, faster stress relaxation, and shorter hold time than those blow moulding grades. These features are advantageous in thin-wall injection moulding but make MQ74 unsuitable for large-part blow moulding because the parison would draw down excessively. Blown film grades, especially high-molecular-weight HDPE, are designed for bubble stability and dart impact resistance under rapid drawing; MQ74 lacks the molecular weight and melt strength for blown film processes. Rotomoulding grades are ground to fine powders, stabilised for long oven cycles at 250–320 °C, and selected for low melt index to avoid pinholes and bubble entrapment during densification. MQ74 is pelletised and not formulated for the oxidative conditions of rotational moulding ovens. Compared with polypropylene injection grades, MQ74 has lower melting temperature and lower stiffness but better low-temperature impact and stress crack resistance in many nonoxidising chemical environments. Compared with linear low-density polyethylene, MQ74 has higher density, higher crystallinity, lower elongation at break, and greater hard-shell rigidity.

    When processing boundaries control quality in thin-wall moulds

    Control of temperature, screw speed, and hold pressure determines whether MQ74 produces void-free parts with acceptable weld lines. Barrel set points should follow a rising profile from 180 °C near the feed throat to 240 °C at the nozzle; these set points are adjusted for shot weight and flow length. Mould temperatures between 10 °C and 40 °C are common; the lower end shortens cycle time but increases residual stress, while the upper end improves gloss and knit-line strength at the expense of cooling time. Back pressure in the range 0.5–1.0 MPa improves melt homogenisation and eliminates colour streaks. Hold pressure is set at 50–70% of injection peak pressure and maintained until gate freeze. Screw speed above 150 rpm can induce frictional heating, lower melt viscosity, and promote flash in multi-cavity tools. Hot runner manifolds should not exceed 260 °C; melt residence time above 230 °C should remain below 10 min to limit thermal degradation and mould deposit formation. Pre-drying is not normally required, but condensation on pellets stored at relative humidity above 60% can cause splay and voids. In that condition, pre-drying at 70 °C for 1–2 h in a desiccant dryer is recommended.

    Injection moulding machines with clamp force from 80 t to 400 t are used for MQ74 caps, closures, and small containers; crates and pallets may require clamp force from 500 t to 1,000 t depending on projected area. The screw should be a general-purpose polyolefin design with L/D ratio from 18:1 to 24:1 and compression ratio in the range 2.2:1–2.8:1. For parts with wall thickness below 0.8 mm, injection speed should be high enough to fill before the flow front freezes, but excessive speed creates shear heating and may degrade additives. Gate position should place weld lines away from sealing surfaces in caps and closures; for crates and pallets, thick rib intersections require extended hold pressure rather than excessive injection speed to reduce sink marks and warpage. Masterbatch addition at 1–3 wt% should be metered with a low-shear mixing screw to avoid pigment agglomerates and uneven colour distribution.

    In multi-cavity closure moulds, cavity-to-cavity flow balance is controlled by runner design rather than by raising melt temperature. Unbalanced runners create differential packing, leading to nonuniform shrinkage and cap fit deviation. Flow length tests using an injection spiral mould are useful for comparing MQ74 lot-to-lot variation, but published data for this specific configuration is limited across different machine sizes and nozzle designs. Mould release from MQ74 parts is generally achieved with standard draft angles of 0.5–1.0° on ribs and 1–2° on sidewalls; lower draft angles require additional release agents, which can interfere with printing or adhesion. For stack moulds, the longer melt path increases pressure loss; hydraulic pressure settings should be verified by pressure transducers inside the cavity rather than by injection unit gauge alone.

    Surface splay in MQ74 parts is often caused by moisture on pellet surfaces or by gas entrapment in the melt. Moisture-derived splay appears as silver streaks from the gate and is corrected by predrying at the conditions stated above. Gas-entrapped splay appears as dark streaks near the end of the fill pattern and is corrected by reducing injection speed or adding vents at the last-fill region. Warpage in thin-wall lids is controlled by uniform cooling and by selecting a low mould temperature differential between fixed and moving halves. Sink marks at rib roots are minimised by maintaining hold pressure until gate freeze and by reducing rib thickness to not more than 60% of the adjoining wall thickness. Dimensional variation in closures is reduced by holding melt temperature within a narrow band of ±5 °C around the optimised set point and by controlling mould temperature within ±3 °C. Lot-to-lot melt flow rate variation should be monitored because changes in viscosity alter fill pressure and packing; incoming raw material control should include melt flow rate by ISO 1133-1 and density by ISO 1183-1.

    Weld-line strength in coloured MQ74 compounds can be lower than in natural resin because pigments orient parallel to the weld line. For coloured versions, masterbatch carrier resins should be selected from the same polyethylene family to avoid knit-line weakness. The use of nucleating agents is not required in MQ74 but may be added at low levels to increase crystallisation temperature and shorten cycle time; such additions should be validated by differential scanning calorimetry according to ISO 11357-3 to quantify crystallisation temperature shifts. Post-industrial regrind from MQ74 sprues and runners can be blended with virgin pellets at levels up to 20 wt% for many non-critical applications. Repeated extrusion reduces molecular weight and raises melt flow rate; regrind ratio should be controlled by measuring melt flow rate and notched Izod impact after each pass. Colour shift and gel formation should be monitored by screen pack pressure rise and by visual inspection of moulded plaques.

    Chemical resistance of MQ74 follows the general behaviour of high-density polyethylene: resistance is good in aqueous, polar, and many nonpolar environments at room temperature, but the resin is not recommended for continuous exposure to strong oxidising agents, aromatic hydrocarbons at elevated temperature, or chlorinated solvents under stress. Stress crack resistance in detergent and lubricant packaging is a function of moulded-in stress, not polymer density alone; local frozen-in stress at gate regions and weld lines can initiate crazing even when the resin passes laboratory ESCR. The grade should not be exposed to sustained load above 60 °C unless supported by application-specific creep data. For food-contact end uses, compliance with EU Regulation 10/2011 and FDA 21 CFR 177.1520 must be confirmed by the converter for the specific additive package and processing conditions. Current supplier certification is authoritative for REACH and RoHS obligations. The use of post-consumer recyclate in MQ74-based parts requires migration and odour testing according to the relevant food-contact regulation if the part is intended for food packaging.

    Top