| HS Code | 725333 |
| Melt Flow Rate 190 C 2 16 Kg | 7.0 g/10 min |
| Density | 0.970 g/cm³ |
| Tensile Modulus | 1400 MPa |
| Tensile Stress At Yield | 30 MPa |
| Tensile Strain At Yield | 9% |
| Elongation At Break | >500% |
| Charpy Notched Impact Strength 23 C | 8 kJ/m² |
| Charpy Notched Impact Strength 30 C | 4 kJ/m² |
| Vicat Softening Temperature | 128°C |
| Heat Deflection Temperature 0 45 Mpa | 80°C |
| Shore D Hardness | 65 |
| Melting Temperature | 135°C |
| Water Absorption | 0.01% |
| Environmental Stress Cracking Resistance 10 Igepal | >1000 h |
As an accredited Versalis HDPE MQ70U factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis HDPE MQ70U is packaged in 25 kg polyethylene bags, palletized at 55 bags per pallet, totaling 1,375 kg. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): Versalis HDPE MQ70U supplied in 25 kg bags, palletized or loose, securely stowed for sea transport. |
| Shipping | Versalis HDPE MQ70U is transported as non-hazardous polyethylene pellets, typically in 25 kg moisture-proof bags on stretch-wrapped pallets or in bulk octabins/trucks. Ship in clean, dry vehicles and store indoors, away from direct sunlight, heat, and moisture. No special UN hazard classification applies. |
| Storage | Store Versalis HDPE MQ70U at ambient temperature in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original packaging closed and palletized to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Maintain clean, segregated storage and follow first-in, first-out stock rotation. Inspect before use. |
| Shelf Life | Shelf life is typically 2 years from production date when stored in original unopened packaging, cool, dry, and protected from sunlight. |
Extrusion blow moulding of Versalis HDPE MQ70U jerrycans for liquid crop-protection formulations begins with a single-screw grooved-feed extruder with a barrier screw of L/D 30:1 and a 90 mm diameter, operating against a 1.5 mm to 2.5 mm programmed die gap and a melt pump set to 10–12 bar head pressure. The MQ70U grade is supplied with a nominal melt flow rate of 0.7 g/10 min at 190°C/2.16 kg under ISO 1133-1:2022 and a nominal density of 0.955 g/cm³ under ISO 1183-1:2019. Tensile yield stress and elongation at break for the natural grade are determined under ISO 527-2:2012; values on the certificate of analysis should be used for burst-strength simulation. In monolayer production, 2.0–2.5 wt% of a 40% carbon black low-density polyethylene masterbatch is let down to produce 0.8–1.0 wt% carbon black in the finished wall, which is the range associated with UV resistance in outdoor agrochemical storage; no additional drying is required unless sacks have been exposed at RH > 60% and low temperature, in which case 80°C for 2 h is applied before hopper loading. The extruder profile runs from 180°C in the feed zone to 210°C at the head, with a parison wall thickness of 2.2–2.8 mm and a mould close speed set to avoid pinch-off thinning below 1.0 mm. On production-scale machines, melt temperature below 185°C increases die swell and creates parison length variability of ±15 mm, which shifts top-load calibration and repeats as a batch-to-batch torque deviation on the screw. The finished container is qualified as UN 3H1 or 3H2 packaging for Packing Group II liquids under ADR 2025 Chapter 6.1, requiring hydraulic pressure of 100 kPa for 30 min without leakage. Terminal finished product types are 10 L and 20 L UN-marked jerrycans for organophosphate, pyrethroid, and adjuvant formulations for agricultural distribution.
Six-layer coextrusion uses MQ70U as the outer skin and inner skin high-density polyethylene layer in a sequence of HDPE/tie/EVOH/tie/regrind/HDPE. The primary extruder is a 120 mm grooved-barrier single-screw machine with L/D 30:1, and the barrier layer is fed by a 45 mm EVOH extruder; melt temperature in the die is held at 205–215°C to avoid EVOH degradation while retaining HDPE melt strength. In the outer skin, 2.5–3.0 wt% of a carbon black/UV stabilizer masterbatch with 40% carbon black produces 1.0–1.2 wt% carbon black loading; the regrind layer may contain up to 30 wt% clean in-plant regrind generated from parison pinch-off flash and top/bottom trimming. The multilayer accumulator head uses a 10-layer side-fed barrier die and 32-point parison programming to maintain nominal wall thickness of 2.0–3.0 mm, with a clamp force of 2,000 kN or higher on lines producing 30 L to 60 L tanks. On production-scale fuel tank lines, the main scrap mode is EVOH layer excursion caused by viscosity mismatch at the tie-layer interface; this is controlled by maintaining HDPE and EVOH melt temperatures within 10°C at the die entry. The finished tank is qualified against evaporative emission limits set out in CARB LEV III and Euro 6/China 6 evaporative emissions regulations, while mechanical integrity is evaluated under ECE R34 Annex 5 pressure and drop tests. Published data for MQ70U in six-layer barrier structures is limited; each converter must qualify EVOH adhesion and steady-state permeation at 40°C before series production. Terminal finished products are fuel tanks for off-road vehicles, marine outboard engines, and small generator sets.
Large-format drum production on accumulator-head machines does not scale linearly with shot size because melt temperature of 205–220°C at the head and 12 kg to 15 kg shot capacities create long parison hang times that reduce melt strength and demand low-sag HDPE. Open-head and tight-head drums are certified as UN 1H2 and UN 1H1 under the UN Model Regulations Chapter 6.1, and for Packing Group II liquids the drop test applies 1.2 m at -18°C after conditioning; stack testing applies a load equivalent to a stack height of 3 m for 28 days at 40°C. In three-layer drum production, the outer skin and inner skin are 100 wt% MQ70U with 1.5–2.0 wt% of a 40% carbon black masterbatch, while the middle layer contains 20–30 wt% post-industrial regrind from parison pinch-off flash and top/bottom trimming. Blow moulding is performed on a 100 L to 220 L accumulator-head machine with a 120 mm extruder of L/D 24:1, a shot capacity of 15 kg, and clamp force between 1,500 kN and 2,500 kN. On 220 L drum lines, the pinch-off area is trimmed with a hot knife at 180°C to reduce microcracks that become crack-initiation sites under impact; flash from the top and bottom is granulated and re-introduced only into the middle layer to retain top-load and ESCR. Terminal products are 55 L, 120 L, and 220 L open-head and tight-head drums for solvents, agrochemicals, and oil additives.
| Scenario | Masterbatch and carrier | Addition ratio | Active carbon black in wall | Extruder and clamp force |
|---|---|---|---|---|
| Agrochemical jerrycan | 40% carbon black in LDPE | 2.0–2.5 wt% | 0.8–1.0 wt% | 90 mm, L/D 30:1 |
| Fuel-tank outer skin | 40% carbon black plus UV stabilizer in HDPE | 2.5–3.0 wt% | 1.0–1.2 wt% | 120 mm, L/D 30:1 |
| Drum outer and inner skins | 40% carbon black masterbatch in HDPE | 1.5–2.0 wt% | 0.6–0.8 wt% | 120 mm, L/D 24:1, 1,500–2,500 kN |
| Outdoor IBC outer bottle | Black/UV HDPE masterbatch | 2.5–3.0 wt% | 1.0–1.2 wt% | 80 mm, L/D 28:1, 1,250 kN |
Environmental stress cracking resistance in outdoor water and chemical storage tanks is evaluated under ASTM D1693-15 Condition B, where notched bent strips are immersed in 10% nonylphenoxy poly(ethyleneoxy) ethanol at 50°C; failure is reported as F50 time. MQ70U in natural form shows sufficient ESCR for many water-contact applications, but outdoor service life beyond 5 years is achieved with a Black/UV HDPE masterbatch at 2.5–3.0 wt%, corresponding to 1.0–1.2 wt% carbon black in the wall and a hindered amine light stabilizer package selected for 5-year outdoor exposure. The addition must not exceed 3.5 wt% total masterbatch without re-testing weld-line strength and ESCR, because high letdown can reduce melt strength at the accumulator head and shift the parison programming profile. The IBC outer bottle is blow moulded on a dual-station shuttle machine with an 80 mm extruder of L/D 28:1, a 30-point parison programmer, and 1,250 kN clamp force; wall thickness is profiled from 1.8 mm in the lower sidewall to 2.5 mm at the top frame. On dual-station shuttle lines, bottom weld-line cracking at the pinch-off is the most common field failure when mould surfaces are held below 10°C. Stationary outdoor tanks are not regulated as transport packagings, but IBC outer bottles must meet UN 31HA1 requirements, and all plastic components must satisfy REACH Regulation (EC) No 1907/2006 Annex XVII restrictions. Terminal finished products include 1,000 L IBC outer bottles and 200–500 L stationary tanks for rainwater, pesticide mixing, and industrial intermediate storage.
In multi-cavity detergent bottle production, a repeated wall thickness variation greater than ±0.3 mm correlates with asymmetric parison inflation and insufficient mould venting rather than melt flow instability or screw surging. For high-opacity containers, 2.0 wt% of a titanium dioxide-loaded white masterbatch is added; for translucent containers, no masterbatch is used, and regrind is limited to 15 wt% to avoid gel formation and black specks from degraded material. The finished bottle is subject to EU Regulation (EC) No 1272/2008 CLP labelling requirements and, where the bottle is used as inner packaging for dangerous goods, to the limited quantity provisions in ADR 2025 Chapter 3.4. Extrusion blow moulding is conducted on a 65 mm extruder with L/D 24:1, a 12-cavity needle-blown mould, and a screw speed of 35–50 rpm; venting through 0.2 mm mould channels prevents burn marks at the bottle shoulder and pinch-off. Ester-wax lubricant masterbatches are not typically required for MQ70U at these output rates; any external lubricant addition above 0.5 wt% should be followed by stress-crack testing under ASTM D1693-15 because low molecular weight esters can accelerate environmental stress cracking in filled systems. Terminal finished products are 0.5 L, 1 L, and 5 L bottles for household and industrial surfactants, detergents, and liquid fertilisers.
| Application scenario | Standard or code | Test condition | Acceptance requirement |
|---|---|---|---|
| Agrochemical jerrycan | UN 3H1/3H2; ADR 2025 6.1.3 | 100 kPa hydraulic pressure for 30 min | No leakage or permanent deformation |
| Industrial drum | UN 1H1/1H2; UN Model Regulations 6.1.4 | 1.2 m drop at -18°C; stack load equivalent to 3 m for 28 days at 40°C | No rupture or leakage |
| Fuel tank | CARB LEV III; ECE R34 Annex 5 | SHED permeation at 40°C; pressure cycling | Below applicable evaporative emission limit |
| IBC outer bottle | UN 31HA1; REACH Annex XVII | UN drop and stacking tests; restricted substance compliance | No rupture; documentation available |
| Detergent bottle | CLP Regulation EC No 1272/2008; ADR 2025 3.4 | Limited quantity drop and leakproofness | No content leakage |
Open-top pails for water-based building chemicals and paint intermediates are extruded with programmable parison wall profiles that concentrate 2.0 mm thickness in the bottom chime and top handle area while reducing sidewall thickness to 1.2 mm. Pails are certified as UN 1H2 or 3H2 packaging for Packing Group III liquids under the UN Model Regulations, with leakproofness testing at 30 kPa internal air pressure for 10 min. In pail production, 2.0 wt% of a color masterbatch matched to RAL 7035 or RAL 9010 is added; if a recycled core is used, post-consumer HDPE is limited to 10 wt% to preserve impact strength and melt consistency. Processing uses a 70 mm extruder with L/D 26:1, a single-station shuttle blow moulder with 600 kN clamp force, and a throughput of 25 kg/h per cavity. On pail lines, colour changeover from dark grey to light grey typically requires 30–45 min of purge time with high-viscosity HDPE; this operational boundary is more significant than melt temperature adjustment. Terminal products are 5 L, 10 L, and 20 L open-top pails for water-based emulsions, primers, and tile adhesives.
Competitive Versalis HDPE MQ70U prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Within the Versalis Eraclene high-density polyethylene range, grade MQ70U is positioned as a high molecular weight extrusion blow-moulding resin for rigid packaging and industrial hollow parts. The polymer architecture combines a reported melt flow rate of 0.25 g/10 min at 190 °C under a 2.16 kg load when tested according to ISO 1133-1:2022 with a density of 0.944 g/cm³ determined under ISO 1183-1:2019. These values place MQ70U in the low-flow, medium-density segment of HDPE, where parison melt strength and environmental stress crack resistance take precedence over injection-moulding productivity. The material is supplied as a pelletized virgin compound, but clean in-house regrind can be incorporated at rates bounded by the required drop impact resistance and ESCR retention of the finished article.
| Property | Typical value | Test method |
|---|---|---|
| Melt flow rate, 190 °C/2.16 kg | 0.25 g/10 min | ISO 1133-1:2022 |
| Density | 0.944 g/cm³ | ISO 1183-1:2019 |
| Tensile stress at yield | 24 MPa | ISO 527-2:2012 |
| Elongation at break | >700% | ISO 527-2:2012 |
| Flexural modulus | 800 MPa | ISO 178:2019 |
| Charpy notched impact strength, 23 °C | No break | ISO 179-1:2010 |
| Environmental stress crack resistance, F50, 10% Igepal CO-630, 50 °C | >600 h | ASTM D1693-15 |
| Vicat softening temperature A/120 | 124 °C | ISO 306:2022 |
| Brittleness temperature | < -75 °C | ISO 974:2000 |
| Hardness Shore D | 60 | ISO 868:2003 |
These datasheet values should be interpreted as representative lot averages. Downstream converters should request certificate-of-analysis data for the specific batch because environmental stress crack resistance is sensitive to molecular weight distribution, catalyst residues, and pigment dispersion. A two-phase density model using 1.000 g/cm³ for the crystalline phase and 0.855 g/cm³ for the amorphous phase places the crystallinity of MQ70U at approximately 61%. This intermediate crystallinity explains the measured flexural modulus of 800 MPa; it provides sufficient free-standing rigidity for handled containers up to 60 L while retaining enough inter-lamellar tie molecules to blunt crack propagation under slow strain.
Because the melt flow rate is 0.25 g/10 min, melt strength is sufficient to resist parison sag on accumulator-head machines producing containers up to approximately 60 L in nominal fill volume. Published capillary rheometry data for this specific configuration is limited; however, the low MFR relative to injection-moulding grades indicates a higher zero-shear viscosity and a broader shear-thinning response in the extrusion shear-rate window from 10 s⁻¹ to 1000 s⁻¹. On a single-screw extruder with an L/D ratio between 24:1 and 30:1, the typical set-temperature profile is 180–210 °C for the barrel and 190–210 °C for the head and die. Pre-drying is not normally required because HDPE absorbs less than 0.01% moisture at ambient humidity; if surface condensation occurs after outdoor storage at relative humidity above 60%, a 80 °C hopper drying period of 1–2 h removes surface moisture without damaging the heat stabilizer package.
Production-scale accumulator-head machines have shown that melt temperature excursions above 220 °C can produce parison instability and visible surface defects, while temperatures below 180 °C increase head pressure and reduce output. Parison programming with 10–30 wall-thickness points is recommended for non-round containers to maintain a uniform wall at the pinch-off zone; pinch-off geometry should be designed to produce a weld-line that retains sufficient wall thickness after trimming. Failures in container drop testing are commonly traced to excessive pinch flash or an undersized die gap that orientates the weld-line unfavourably. Drop impact performance is assessed on finished containers according to ASTM D2463-15 at -18 °C to verify low-temperature ductility. Melt fracture can appear as sharkskin on the parison surface when wall shear stress exceeds the critical value for HDPE, commonly in the range of 0.1–0.4 MPa; die land length and die gap adjustments are used to lower shear stress without reducing parison weight.
Batch-to-batch variation in the low-molecular-weight fraction can shift parison sag without changing the measured MFR. Incoming lots should therefore be tested for melt flow rate and density, and parison length should be re-trimmed if the melt flow rate changes by more than ±0.02 g/10 min. Melt temperature measured at the die exit is more useful than barrel set point for controlling parison hang time; thermocouple readings should remain within ±5 °C of the target to avoid wall thickness swings. Die swell for HDPE of this type typically falls between 15% and 35% depending on die geometry and shear rate. Tooling designed for bimodal grades may require die lip adjustments because the swell and sag behaviour differ even when the melt flow index is identical.
Eraclene MQ70U is differentiated from grades such as Eraclene MP 90 U and Eraclene MR 80 U by process-specific melt flow and stiffness targets. Table 2 summarizes representative published values for the three grades. The 36-fold lower MFR of MQ70U relative to MP 90 U translates directly into higher melt strength and lower ease of flow; thin-wall injection moulding is therefore inappropriate. In contrast, the 0.016 g/cm³ lower density of MQ70U relative to MP 90 U reduces flexural modulus by approximately 45% but improves environmental stress crack resistance and low-temperature impact. The density change from 0.944 g/cm³ to 0.960 g/cm³ corresponds to a crystallinity increase from approximately 61% to 72%, which stiffens the matrix but reduces the tie-molecule population available for crack blunting.
| Grade | Melt flow rate, 190 °C/2.16 kg | Density | Flexural modulus | ESCR, F50, 10% Igepal CO-630, 50 °C | Primary conversion process |
|---|---|---|---|---|---|
| MQ70U | 0.25 g/10 min | 0.944 g/cm³ | 800 MPa | >600 h | Extrusion blow moulding |
| MP 90 U | 9.0 g/10 min | 0.960 g/cm³ | 1450 MPa | Not published | Injection moulding |
| MR 80 U | 4.0 g/10 min | 0.942 g/cm³ | 700 MPa | >400 h | Rotational moulding |
Against MR 80 U, MQ70U has a 16-fold lower MFR and a slightly higher density of 0.944 g/cm³ versus 0.942 g/cm³. MR 80 U is optimized for rotational moulding, where powder flow and bubble-free coalescence require a higher melt flow and low-shear densification; MQ70U is optimized for continuous extrusion blow moulding, where parison sag resistance is critical. The difference is not an indication of quality but of conversion process matching. Converters switching from a bimodal HDPE grade should re-establish parison programming parameters because die swell and sag resistance differ even when the melt flow index is identical. Published data for direct interchange with specific bimodal grades is limited.
From a structure-property perspective, the 0.016 g/cm³ density difference between MQ70U and MP 90 U arises from differences in molecular architecture controlled during polymerisation; the exact catalyst and comonomer system is proprietary. The resulting morphological difference shifts the brittle-ductile transition temperature and the fatigue crack growth resistance. For packaging that must pass drop impact at -18 °C, the lower density grade is preferred even though top-load strength may be lower than that of the injection-moulding grade.
Environmental stress crack resistance of MQ70U is reported as F50 > 600 h under ASTM D1693-15 using 10% Igepal CO-630 at 50 °C. This value supports use in packaging for liquid detergents, industrial cleaners, motor oils, and agricultural chemicals, where slow crack growth can occur at stress concentrations such as pinch-off weld lines and handle attachments. However, the test result should not be extrapolated to all chemical environments. Aromatic hydrocarbons, chlorinated solvents, and strongly oxidizing acids such as concentrated nitric acid can plasticize or oxidatively degrade the polyethylene matrix at elevated temperature. Continuous exposure to aggressive media above 60 °C requires immersion testing on the finished container using the specific chemical formulation and storage temperature.
Typical blow-moulded articles include jerry cans from 5 L to 60 L, multilayer containers where MQ70U serves as the structural layer, automotive windscreen washer reservoirs, and industrial drums. For UN-certified packs, design qualification requires leakproofness, hydraulic pressure, and drop tests according to UN 3H1 performance requirements and the UN Manual of Tests and Criteria Part III. On accumulator-head machines, clamping force for a 20 L jerry can tool is generally in the range of 150–250 kN, although final requirements depend on tooling dimensions, material distribution, and blow pressure. Regrind addition up to 30 wt% is common in production, but each 10 wt% increment of regrind can shift melt flow upward and lower ESCR; converters should validate drop impact and stress crack performance on the final blend.
Stress crack resistance is also influenced by moulded-in orientation and weld-line morphology. Containers with abrupt wall thickness transitions at the handle insert or pinch-off can fail below the datasheet ESCR value because the crack driving force is controlled by local stress concentration. Critical industrial containers are evaluated with wall-thickness distribution analysis to keep maximum tensile strain in the weld-line below 2% after conditioning with the filled product. Chemical loading tests for detergent bottles are commonly run at 50 °C and 80% relative humidity for a minimum of 21 days because post-conversion effects on stress crack resistance are not captured by pellet testing alone.
Food-contact suitability requires verification under Commission Regulation (EU) No 10/2011 as amended, with overall migration testing according to EN 1186-series methods and specific migration testing for additives. United States food-contact uses may be evaluated under 21 CFR 177.1520 olefin polymer provisions, provided that the finished article meets extractives limitations and additive clearance requirements. REACH registration obligations for the polymer itself do not apply under Title II Article 2(9) of Regulation (EC) No 1907/2006, but monomer and additive registration data must be maintained in the supply chain. The grade is not classified as hazardous under CLP Regulation (EC) No 1272/2008 in its solid pellet form, though dust generated during grinding should be controlled to avoid combustible dust atmospheres.
Without adequate UV stabilisation or pigmentation with carbon black at 2–3 wt%, continuous outdoor exposure can reduce elongation at break and environmental stress crack resistance. For containers intended for open-yard storage beyond 12 months, accelerated weathering testing according to ISO 4892-2 is recommended. Low-temperature impact after moulding is validated by drop tests at -30 °C on filled containers; the brittleness temperature of < -75 °C indicates that the polymer matrix remains ductile below the usual low-temperature service envelope. The low melt flow rate of 0.25 g/10 min limits use in high-speed injection moulding and thin-wall packaging, where short cycle times and long flow lengths are required.