    Specifications
    HS Code 360796
    Density 0.970 g/cm3
    Melt Flow Rate 190 C 21 6 Kg 7.0 g/10 min
    Melt Flow Rate 190 C 2 16 Kg 0.2 g/10 min
    Tensile Stress At Yield 28 MPa
    Tensile Strain At Yield 9 %
    Tensile Stress At Break 30 MPa
    Tensile Strain At Break >600 %
    Flexural Modulus 1500 MPa
    Izod Notched Impact Strength At 23 C 15 kJ/m2
    Izod Notched Impact Strength At 30 C 5 kJ/m2
    Shore D Hardness 65
    Vicat Softening Temperature 128 °C
    Melting Temperature 135 °C
    Crystallization Temperature 115 °C
    Thermal Conductivity 0.45 W/mK
    Coefficient Of Linear Thermal Expansion 1.2E-4 /°C
    Specific Heat Capacity 1.9 J/g°C
    Escr 10 Igepal >1000 h
    Water Absorption <0.01 %
    Volume Resistivity >1E15 ohm cm
    Dielectric Constant At 1 Mhz 2.3
    Dissipation Factor At 1 Mhz 0.0002
    Oxygen Index 17 %
    Ul Flammability HB
    Bulk Density 0.58 g/cm3

    As an accredited Versalis HDPE MQ70 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis HDPE MQ70 is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped, or in bulk containers.
    Container Loading (20′ FCL) Container loading: Versalis HDPE MQ70 in 20′ FCL—palletized 25 kg bags, shrink-wrapped, strapped, evenly secured for safe marine transport.
    Shipping Versalis HDPE MQ70 is a non-hazardous high-density polyethylene supplied as pellets. It is shipped in 25 kg bags, octabins, or bulk containers/trucks under standard industrial cargo conditions. No UN number, transport class, or packing group applies. Keep dry, cool, and free from contamination, heat, and direct sunlight.
    Storage Versalis HDPE MQ70 should be stored in a cool, dry, well-ventilated warehouse. Keep in original sealed bags or packaging, on pallets, off the floor. Protect from direct sunlight, moisture, dust, and contamination. Avoid prolonged heat, open flames, and strong oxidizers. Maintain stable ambient temperature, do not stack excessively to prevent deformation, keep containers closed and labeled, and follow FIFO stock rotation.
    Shelf Life No fixed shelf life; stable if stored cool, dry, and away from direct sunlight. Consult supplier for exact retest date.
    Application of Versalis HDPE MQ70

    Versalis HDPE MQ70 is an injection-moulding high-density polyethylene grade with a nominal melt flow rate of 7.0 g/10 min at 190 °C/2.16 kg and a nominal density of 0.960 g/cm³ when tested to ISO 1133-1:2022 and ISO 1183-1:2019. The scenarios below are restricted to production sectors in which the grade is employed as a primary moulding resin, including rigid food-contact packaging, closure systems, returnable logistics articles, industrial pails, institutional housewares, and personal care dispensing components. Each scenario states the applicable regulatory references, quantified addition ratios, process parameters that control mould filling and post-mould dimensional stability, and the terminal article categories produced on industrial lines.

    Thin-Wall Dairy Packaging and Flow-Length Limits at 0.45 mm Nominal Wall

    Dairy cups and tubs are injection-moulded from HDPE MQ70 at a melt temperature of 220–240 °C and a mould-surface temperature of 10–25 °C, with hydraulic accumulator injection speeds maintained in the range of 150–250 mm/s to prevent short shots and jetting in 0.40–0.65 mm wall sections. The governing compliance requirements for direct dairy contact are Commission Regulation (EU) No 10/2011, where overall migration must remain below 10 mg/dm² under the assigned aqueous and acidic simulant conditions, and FDA 21 CFR §177.1520(c) 2.2 for olefin polymers used with food types III, IV, and VII. In the moulding cell, the formulation is maintained at 100 parts by weight virgin HDPE MQ70; white or tinted color masterbatch based on a polyethylene carrier is metered at 1.5–2.5 wt%, and process-lubricant masterbatch is added at 0.3–0.7 wt% only when required for demoulding. Sprues, runners, and edge trim produced from the same compliant lot are reintroduced at up to 20 wt% of total shot mass under a closed-loop recycling programme validated to EC No 2023/2006. Production-scale tools are normally hot-runner systems with 8–24 cavities, valve-gate actuation, and venting gaps of 0.02–0.05 mm; clamping force is sized at 4–6 kN/cm² of projected area and cooling time is set to achieve part ejection below 65 °C. Terminal products include yogurt cups, dairy dessert cups, single-serve drink cups, and margarine tubs with sidewall thicknesses of 0.40–0.65 mm, and the moulded articles are not considered suitable for hot-fill temperatures above 65 °C or for extended freezer use below −20 °C without additional impact modification.

    In closure manufacturing cells configured with 96- to 128-cavity hot-runner tools, HDPE MQ70 is selected for still-water, dairy, and non-carbonated beverage closures because its melt-flow-rate stability at 7.0 g/10 min supports cavity-to-cavity filling repeatability across multi-drop manifolds and reduces gate-stringing in negative-angle bridge seals. The applicable compliance framework includes FDA 21 CFR §177.1520(c) 2.2, Commission Regulation (EU) No 10/2011, and current good manufacturing practice under EC No 2023/2006 for food-contact plastic articles. Formulation for tamper-evident beverage closures consists of 96.0–98.0 wt% HDPE MQ70, slip-agent masterbatch at 1.0–2.0 wt% to reduce cap-application torque without exceeding the migration budget of the food-contact declaration, and color masterbatch at 1.0–3.0 wt%; process-generated trimmings and reject caps are re-ground and metered into the feed throat at 10–20 wt% after metal separation and melt filtration through a 60–100 mesh screen pack. Moulding is performed at a barrel profile of 190–240 °C, mould temperature of 10–25 °C, injection pressure of 80–120 MPa, and clamping-force availability of 3–5 kN/cm² of projected area. Dimensional control of the tamper-evident band and bridge webs requires holding pressure and cooling time to limit post-mould shrinkage to 2.0–2.5% across the cap diameter; ejection is normally interrupted if part temperature exceeds 60 °C. Terminal products include 28 mm and 30 mm still-water closures, dairy-cap push-pull fitments, tamper-evident bands, and screw caps for non-carbonated beverages, all of which are subject to application-torque testing according to ASTM D2063 and leakage testing after capping.

    When Load-Bearing Crates Are Moulded with 30% Closed-Loop Regrind

    Load-bearing returnable crates for beverage distribution are produced from HDPE MQ70 with closed-loop regrind contents up to 30 wt% only when the regrind stream is monitored for melt-flow-rate shift, ash content, and oxidative degradation; the virgin fraction remains 70–80 wt%, and the combined formulation includes UV-stabilizer masterbatch at 1.5–3.0 wt% and antioxidant masterbatch at 0.2–0.5 wt%. The governing compliance references are REACH Regulation (EC) No 1907/2006 and RoHS Directive 2011/65/EU for heavy-metal restrictions, while mechanical acceptance testing follows ISO 12048 compression testing of filled crates and ISO 6603-2 instrumented puncture impact at −20 °C. In production, thick-section crate tools with wall thicknesses of 2.5–4.0 mm are run on injection moulding machines with clamping force from 600 to 1,200 tonnes, barrel temperatures of 230–250 °C, and mould temperatures of 15–30 °C; multiple submarine or hot-tip gates are balanced to maintain a flow-length-to-thickness ratio below 150:1. The addition of regrind above 30 wt% is not recommended for crates with load-rated bottom grids because the corresponding loss in environmental stress-cracking resistance can reduce the number of return trips before webbing cracks initiate between ventilation slots. Published data for this specific crate-tool configuration is limited above that regrind loading; therefore, production validation requires instrumented puncture testing on moulded specimens according to ISO 6603-2. Terminal products comprise beer-crate bottom shells, dairy-crate frames, ventilated produce crates, and returnable logistics totes with load ratings up to 25 kg in stacked configurations, and outdoor service life is dependent on stabilizer package retention rather than on the polymer base alone.

    What Limits Injection Speed in 10–25 L Open-Top Pail Production?

    Injection speed in 10–25 L open-top pail production is limited by gate blush, weld-line strength at the handle lugs, and the onset of flow hesitation along the pail sidewall when the melt pressure at the end of fill falls below 35 MPa. HDPE MQ70 is processed at a melt temperature of 220–250 °C and a mould temperature of 15–30 °C, with injection speeds typically capped between 80 and 150 mm/s for single-cavity or two-cavity pail tools. The applicable compliance framework for pails used to transport non-hazardous liquid foods is Commission Regulation (EU) No 10/2011 and FDA 21 CFR §177.1520(c) 2.2; pails intended for dangerous goods must additionally pass UN type-approval drop and stacking tests under ADR/RID/IMDG packaging instructions, including drop impact at −18 °C and hydraulic pressure retention of side seams. Formulation for industrial pails is normally 97.0–99.0 wt% HDPE MQ70, with color masterbatch at 1.0–3.0 wt%; clean in-house regrind from rejected pails may replace up to 20 wt% of virgin material only after sustained pressure and leakage testing confirms equivalent weld-line integrity. The production equipment includes two-platen machines with clamp force between 500 and 1,600 tonnes, cold or hot runner systems with a central sprue and four to eight hot drops, and core cooling circuits that maintain part ejection below 60 °C. Terminal products include 10 L, 15 L, and 25 L open-top pails, lid-seating rims, and tamper-evident pail handles for non-carbonated liquid and powder filling.

    For industrial and institutional houseware lines operating two-platen injection moulding machines with clamp force between 250 and 800 tonnes, the grade is dispensed into open storage container moulds at a melt temperature of 210–240 °C and a mould temperature of 15–30 °C, producing opaque rigid articles with sidewall thicknesses between 1.5 and 3.0 mm. The relevant conformity framework is REACH Regulation (EC) No 1907/2006 and, where the container is intended for repeated kitchen use, FDA 21 CFR §177.1520(c) 2.2 and Commission Regulation (EU) No 10/2011. The dry-blend formulation is kept at 100 parts by weight HDPE MQ70 plus color masterbatch at 2.0–4.0 wt%; process regrind from shredded gates and side walls is added at up to 25 wt% for opaque houseware grades, provided that the regrind is dried below 0.05% surface moisture and pneumatically conveyed through metal separation. Processing uses single-cavity or multi-cavity cold-runner tools with edge gates, injection pressure of 80–110 MPa, and cooling times of 12–30 s depending on wall thickness. Terminal products include institutional storage boxes, tote bins for healthcare linen handling, stackable utility containers, and non-food drawer organisers, all of which are subject to dimensional stability checks after 48 h atmospheric conditioning at 23 °C/50% RH according to ISO 291.

    Application SectorGoverning Standard or DirectiveTest Method or ClauseCritical Requirement or Acceptance Range
    Thin-wall dairy packagingEU 10/2011, FDA 21 CFR §177.1520(c) 2.2EN 1186-1, ISO 1133-1:2022Overall migration below 10 mg/dm²; wall thickness 0.40–0.65 mm
    Beverage closure mouldingEU 10/2011, FDA 21 CFR §177.1520ASTM D2063, ISO 1133-1:2022Screw-cap torque retention after capping; post-mould shrinkage 2.0–2.5%
    Returnable logistics cratesREACH 1907/2006, RoHS 2011/65/EUISO 12048, ISO 6603-2Instrumented puncture impact at −20 °C; stacked load up to 25 kg
    Open-top industrial pailsADR/RID/IMDG, FDA 21 CFR §177.1520UN drop and stacking testsDrop impact at −18 °C without leakage; side-seam hydraulic retention
    Institutional housewaresREACH 1907/2006, EU 10/2011ISO 291Dimensional stability after 48 h at 23 °C/50% RH
    Personal care dispensing closuresEU 1223/2009, REACH 1907/2006FDA 21 CFR §177.1520Organoleptic neutrality; mold shrinkage consistent with hinge flex fatigue

    Personal Care Dispensing Closure Moulding and Organoleptic Boundary Conditions

    Dispensing closures for personal care formulations are moulded from HDPE MQ70 when the brand specification demands a low residual odor, low extractables profile, and consistent hinge flex in flip-top caps. The governing compliance references are EU Regulation (EC) No 1223/2009 for cosmetic product packaging compatibility, REACH Regulation (EC) No 1907/2006 for substances in articles, and FDA 21 CFR §177.1520 if the same closure family is used in contact with aqueous cosmetic emulsions. The formulation is 96.0–98.5 wt% HDPE MQ70, with color masterbatch at 0.8–2.0 wt% and an external lubricant masterbatch at 0.5–1.5 wt%; process regrind from runner systems and rejected caps is limited to 15 wt% of shot mass to avoid batch-to-batch variation in hinge stress-whitening. Moulding is performed on high-cavitation injection machines with 32–64 cavities, hot-runner valve gates, melt temperature of 210–240 °C, mould temperature of 15–30 °C, and clamp force of 3–5 kN/cm² of projected area. The critical boundary condition is organoleptic neutrality: the use of external post-consumer recycled material is excluded, and masterbatch carriers must be based on polyethylene that conforms to the same food-contact or cosmetic-contact declaration as the base resin. Terminal products include flip-top dispensing caps for shampoos and lotion tubes, screw overcaps for bottle pumps, and hinge-cap assemblies for personal care tubes.

    Free Quote

    Competitive Versalis HDPE MQ70 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis HDPE MQ70, also designated Eraclene MQ 70 U in supplier technical literature, is a pelletised high-density polyethylene injection moulding grade. The nominal melt mass-flow rate is 7.0 g/10 min when measured at 190 °C under a 2.16 kg load according to ISO 1133-1:2022, and the density is 0.960 g/cm³ at 23 °C according to ISO 1183-1:2019. The intended application field covers injection-moulded crates, caps, thin-wall containers and housewares where the 7.0 g/10 min melt flow supports filling of wall sections between 1.0 mm and 2.5 mm. Published mechanical data for the exact product configuration is limited; tensile yield, flexural modulus and impact strength must be taken from the current Versalis certificate of analysis or supplier datasheet rather than assumed from generic HDPE tables.

    What Distinguishes MQ70 from Lower-Flow HDPE Extrusion and Blow Moulding Resins?

    The principal distinction is rheological. Blow moulding HDPE grades commonly show MFR values from 0.2 g/10 min to 1.2 g/10 min, and many extrusion grades fall below 2.0 g/10 min. MQ70 at 7.0 g/10 min reduces injection pressure and permits shorter hold-pressure time in thin-wall tools, but the lower molecular weight associated with higher MFR reduces environmental stress crack resistance. ESCR measured under ASTM D1693-15 condition B is therefore expected to be lower than that of fractional-MFR blow moulding resin. Published ESCR values for MQ70 are not available in the present source; detergent containers, oil-contact parts, and solvent-bearing packages require lot-specific ESCR validation on the finished article.

    Compared with HDPE injection grades above 20 g/10 min, MQ70 retains higher impact resistance and lower shrinkage anisotropy, but it is less suited to wall sections below 0.6 mm where ultra-high-flow grades maintain fill pressure. Compared with impact-modified polypropylene, MQ70 offers lower density and different post-mould shrinkage but has a narrower continuous-use temperature window; continuous exposure above 80 °C should be reviewed for antioxidant depletion.

    Nominal grade data and processing reference values
    PropertyNominal valueStandard or source
    Melt mass-flow rate7.0 g/10 minISO 1133-1:2022
    Density0.960 g/cm³ISO 1183-1:2019
    Melt temperature200–250 °CSupplier processing guideline
    Mould temperature15–40 °CSupplier processing guideline
    PredryingNot normally required below 50 % RH; if condensation occurs, 80 °C for 2 h in desiccant dryerSupplier handling guideline

    On reciprocating-screw injection moulding machines with screw L/D ratios of 20:1 to 25:1 and compression ratios from 2.0:1 to 2.8:1, the barrel temperature profile is typically set with rear zone at 180–200 °C, centre zone at 210–230 °C, front zone at 220–240 °C, and nozzle at 230–250 °C. Mould surface temperature is maintained between 15 °C and 40 °C to control shrinkage and ejection distortion. For multi-cavity crates with projected area above 400 cm², clamp force requirements generally fall between 3500 kN and 8000 kN. When wall stock drops below 1.0 mm, shot-to-shot fill variation increases if the melt cushion is less than 3 mm, and short shots become significant below 1.0 mm without high injection speed and adequate venting.

    Thermal Degradation Boundaries and Residence-Time Constraints

    Melt temperature above 280 °C accelerates oxidative chain scission and produces discoloration and odour. Oxidation induction time measured by ISO 11357-6:2018 is the appropriate lot-release parameter for thermal stability. The practical melt-temperature window is bounded at the upper end by stabilizer depletion and at the lower end by viscosity-related short shots. In hot-runner systems with extended melt residence time, production experience indicates purging with virgin MQ70 after 20 minutes of interruption; longer hold at temperature degrades the antioxidant package. Screw rotation above 150 rpm on small-diameter screws can generate shear heating that exceeds the set barrel temperature and should be verified by melt pyrometry.

    When moulders process masterbatches or regrind, the same thermal limits apply. Regrind content above 20 wt% may raise effective MFR and reduce cavity pressure because prior processing introduces chain scission. Hold-pressure time should be re-established by gate-seal time measurement with cavity pressure transducers. Inorganic pigment masterbatches can nucleate HDPE and raise isothermal crystallization temperature; this reduces cooling time but increases anisotropic shrinkage. A PE-based carrier masterbatch at 2–3 wt% is typical. Higher loadings can shift density above 0.960 g/cm³ and should be confirmed by ISO 1183-1:2019.

    When Moisture Condensation or Additive Interactions Narrow the Moulding Envelope

    HDPE is generally low in moisture sensitivity, but pellet surface condensation can appear when storage humidity exceeds 60 % RH. If splay, internal voids, or gas marks are observed, predrying at 80 °C for 2 h in a desiccant dryer is required. Low-molecular-weight amide slip additives may plate out on mould surfaces and reduce venting; vent grooves in HDPE tools are typically depth-limited to 0.02–0.03 mm. Halogenated flame-retardant systems should be avoided unless specifically approved for the grade, because acid release during processing can accelerate degradation and corrode tool steel. For food-contact applications, only masterbatches listed in the current supplier compliance statement under Regulation (EU) No 10/2011 should be used.

    For applications involving surfactants, bleach solutions, or hydrocarbon emulsions, testing per ASTM D1693-15 condition B is required on the finished article. Published data for this specific configuration is limited; however, constant-strain exposure above 2 % may initiate stress cracks at gate vestiges and weld lines. Hot-fill exposure above 60 °C further reduces ESCR by increasing molecular mobility. Weld lines in multi-gate crates can reduce local tensile strength by 10 % to 30 % relative to neat material when evaluated under ISO 527-2:2012; flow-front temperature above 210 °C and adequate venting reduce this loss.

    Shrinkage Anisotropy and Gate Design Determine Dimensional Stability in Thin-Wall Containers

    Gate freeze-off time is a primary constraint. For edge-gated crates with wall thickness 2.0 mm, gate diameter below 1.0 mm can freeze before packing and produce sink marks. Direct sprue gates or fan gates with land length not exceeding 0.75 mm are preferred for fast filling. Hold pressure is generally 40–60 % of injection pressure, but this must be adjusted by cavity pressure data. If gate-seal time is not reached, sink marks and high shrinkage anisotropy occur. Shrinkage in flow direction is typically 1.5–2.5 % and transverse 1.0–2.0 % depending on wall thickness, mould temperature and holding pressure. Parts ejected above 60 °C may continue to crystallize and warp in stacking.

    Compliance documentation is lot specific. The safety data sheet and product compliance statement should be consulted for REACH (EC) No 1907/2006, Regulation (EU) No 10/2011 and RoHS Directive 2011/65/EU applicability. Food-contact status is not automatically transferable across global jurisdictions; finished articles require migration testing under Regulation (EU) No 10/2011 Annex I and Annex II. Substitution into blow moulding, pipe extrusion, corrugated sheet, or rotational moulding is not supported because the lower melt strength and higher MFR of MQ70 compromise parison stability and extrudate strength. Published process data for these alternative conversion techniques is limited.