| HS Code | 175292 |
| Productname | Versalis HDPE MP94 |
| Polymertype | High Density Polyethylene |
| Density | 0.960 g/cm³ |
| Meltflowrate | 8 g/10 min (190°C/2.16 kg) |
| Tensilemodulus | 1400 MPa |
| Tensilestrengthatyield | 30 MPa |
| Tensilestrainatyield | 9% |
| Tensilestrengthatbreak | 25 MPa |
| Tensilestrainatbreak | >600% |
| Flexuralmodulus | 1400 MPa |
| Notchedizodimpactstrengthat23c | 8 kJ/m² |
| Notchedizodimpactstrengthatminus30c | 4 kJ/m² |
| Shoredhardness | 64 |
| Vicatsofteningtemperature | 80°C |
| Heatdeflectiontemperature | 75°C |
| Waterabsorption | <0.01% |
| Meltingtemperature | 135°C |
As an accredited Versalis HDPE MP94 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis HDPE MP94 is packaged in 25 kg polyethylene bags, palletized and stretch-wrapped for secure handling and transport. |
| Container Loading (20′ FCL) | Versalis HDPE MP94 loaded in 20′ FCL: 25 kg bags, palletized, shrink-wrapped, evenly distributed, secured in dry container. |
| Shipping | Versalis HDPE MP94 ships as a non-hazardous, solid high-density polyethylene resin in pellet form. Standard packaging includes 25 kg bags, octabins, or bulk containers, palletized and stretch-wrapped. It is not classified as dangerous goods for transport. Store dry, away from heat and direct sunlight, avoiding moisture and contamination. |
| Storage | Store Versalis HDPE MP94 in a cool, dry, well-ventilated area, away from direct sunlight, heat, flames, and strong oxidizing agents. Keep original bags closed and palletized to prevent moisture, dust, and contamination. Avoid prolonged high temperatures and UV exposure. Maintain good housekeeping; follow the manufacturer’s SDS and local regulations. Handle carefully to prevent bag damage. |
| Shelf Life | Store dry, cool, ventilated, away from sunlight; shelf life typically 24 months from production in unopened original packaging. |
In high-speed injection moulding of 28 mm PCO 1881/1810 beverage closures, Versalis HDPE MP94 is processed on 48- to 96-cavity hot-runner closure presses with clamp forces between 1,800 kN and 4,500 kN. The resin is dosed with a let-down ratio of 98.0–99.5 wt% MP94, 0.05–0.10 wt% erucamide slip masterbatch, 0.10–0.20 wt% primary antioxidant masterbatch, and 1.0–2.0 wt% colour concentrate. Melt temperature is maintained at 210–235°C, mould cooling water at 10–18°C, and cycle time at 4.5–7.5 s. If the valve-pin temperature differential across cavities exceeds ±1.2°C, differential shrinkage across the closure skirt produces ovality greater than the tolerance band of ±0.15 mm; this is measured on a coordinate measuring machine after conditioned storage at 23°C and 50% RH for 24 h. Subgate diameters below 0.8 mm induce shear orientation that further increases top-load ovality. Compliance for food-contact closures requires reference to Food and Drug Administration 21 CFR 177.1520 for olefin polymers and Commission Regulation (EU) No 10/2011 as amended, with overall migration testing per EN 1186-2:2022. Tensile yield strength is verified per ASTM D638-14 and melt mass-flow rate per ISO 1133-1:2022 at 190°C and 2.16 kg. Terminal parts are 28 mm beverage closures with tamper-evident bands for carbonated soft drinks, bottled water, and isotonic drinks; site-specific validation on the actual closure press is required for ovality and top-load control.
Stackable crate and distribution pallet mouldings produced with Versalis HDPE MP94 on 1,000–1,400 t toggle-clamp injection machines expose a different defect signature: the base rib intersection, not the side wall, is the primary stress concentration. A production-scale line tends to exhibit short shots when the melt cushion drops below 4 mm or when the screw switch-over point moves beyond 95% of filling volume, while over-packing above 1,100 bar specific pressure causes ejection pin push marks on the flat panel. The compounding regime for heavy-duty crates comprises 88–95 wt% MP94, 5–12 wt% post-consumer recycle flake from closed-loop distribution crates, 0.10–0.25 wt% hindered amine light stabilizer masterbatch, and 1.0–2.5 wt% colorant. Wall thickness in the rib grid ranges from 3.0 mm to 6.5 mm; cooling time is therefore set between 25 s and 45 s, with mould temperature at 20–35°C. Compliance for industrial pallets can be verified according to ISO 8611-1:2021 for racking and stacking load performance, while tensile and flexural data follow ISO 527-2:2012 and ISO 178:2019. The terminal parts are stack-and-nest crates, vented distribution containers, and four-way entry Euro pallets. Pre-drying is not required if resin has been stored sealed; if exposed to relative humidity above 60% for more than 48 h, pre-drying at 80°C for 2 h prevents surface splay on thick ribs.
The thin-wall margarine tub segment imposes a flow-length-to-wall-thickness ratio of 150:1 to 220:1, which is achieved on high-speed injection machines with injection velocities from 150 mm/s to 300 mm/s, a 22:1 L/D barrier screw, and hydraulic accumulator control. Versalis HDPE MP94 is processed at melt temperatures of 235–250°C and mould temperatures of 15–30°C, with cycle times of 2.5–4.0 s. Formulation consists of 96.0–98.0 wt% MP94, 0.08–0.15 wt% slip additive masterbatch, 0.15–0.25 wt% antioxidant masterbatch, 0.05–0.10 wt% nucleating agent masterbatch, and 1.0–2.0 wt% titanium dioxide white concentrate. The critical processing conflict is gate blush at valve-gate diameters below 0.5 mm and flow hesitation when injection speed falls below 120 mm/s; both defects are measured by visual inspection under 1,000 lux illumination and confirmed by scanning electron microscopy. Compliance for fatty food contact uses Commission Regulation (EU) No 10/2011 and 21 CFR 177.1520, with overall migration evaluated according to EN 1186-2:2022 and sensory panel residual taint. Terminal products are round 250–500 ml spreadable margarine tubs and dairy snack cups with snap-fit lids. Published processing data for this specific MP94 thin-wall configuration are limited; validation on the target press and mould is required to establish adequate part mass consistency and gate blush control.
Household modular storage boxes and lidded under-bed containers moulded from Versalis HDPE MP94 have wall sections from 1.4 mm to 2.8 mm, placing them outside the high-flow thin-wall window but inside the easy-fill range of a standard 22:1 L/D screw with back pressure between 6 bar and 12 bar. The formulation uses 94–96 wt% MP94, 4–6 wt% talc masterbatch for dimensional consistency, 0.05–0.10 wt% antistatic concentrate, and 1–2 wt% colour concentrate. Melt temperature is set at 210–230°C, mould temperature at 25–40°C, and cooling time at 18–28 s depending on rib depth. Food-contact storage applications require 21 CFR 177.1520 and Regulation (EU) 10/2011; non-food applications require REACH SVHC screening under Article 33. Terminal parts include stackable shoe boxes, archive boxes, and lidded storage totes with integral handle hinges. If moulding at ambient relative humidity above 60%, pre-drying at 80°C for 2 h is recommended to avoid surface splay on the textured lid surface.
For 20-L open-head industrial pails manufactured with Versalis HDPE MP94, the handle-to-pail body junction is the dominant failure point when stacked three-high in warehouse storage at 40°C. The injection moulding process uses 400–700 t hydraulic machines with a melt temperature of 210–240°C, mould temperature of 15–30°C, and cycle time of 22–35 s. The handle is moulded as an integrally hinged structural ring or as a separate component insert-moulded in the same cycle. Formulation consists of 95–98 wt% MP94, 2–5 wt% metallocene LLDPE letdown for ESCR improvement, 0.10–0.20 wt% antioxidant masterbatch, 0.10–0.30 wt% hindered amine light stabilizer masterbatch, and 1.0–2.0 wt% colour concentrate. Compliance for dangerous goods packaging follows the UN Model Regulations, specifically Chapter 6.1.4 and 6.1.5, with road and rail carriage conformity assessed under ADR/RID. Environmental stress crack resistance is verified per ASTM D1693-15 Condition B, and tensile properties per ASTM D638-14. Terminal parts are 5 L, 10 L, and 20 L open-head pails with gasketed lids for water-based chemicals, detergents, and food ingredients. The resin should not be used with concentrated oxidizing acids or aromatic hydrocarbon solvents above 40°C because environmental stress cracking accelerates sharply under those conditions.
Competitive Versalis HDPE MP94 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis HDPE MP94 is a high-density polyethylene grade supplied by Versalis for injection-molding conversion of thin-wall packaging, caps, closures, crates, and industrial containers. The product is positioned in the high-flow segment of the HDPE portfolio, meaning its melt flow rate under ISO 1133-1:2022 at 190 °C with 2.16 kg nominal load is designed for shorter filling times than fractional-melt HDPE grades used in extrusion blow molding. Public technical literature differentiates MP94 from general-purpose HDPE by its balance of flow length, stiffness, and rapid set-up behavior in multi-cavity tools; however, exact lot-release values are governed by the certificate of analysis and should not be assumed from summary datasheets. Typical conversion applications include containers with nominal wall thickness from 0.8 mm to 2.5 mm, closures requiring short gate-freeze time, and housewares or crates where fast cycles and repeatable dimensional stability are primary production requirements.
The grade is normally specified by density and melt-flow rate rather than by a single proprietary value. Density is measured under ISO 1183-1, and the material class is typically near 0.960 g/cm³. HDPE materials in this density range generally exhibit tensile yield stress from 25 MPa to 30 MPa when tested according to ISO 527-2 using Type 1A specimens at 50 mm/min. Flexural modulus, measured under ISO 178 at 2 mm/min, commonly falls between 1100 MPa and 1500 MPa, which is relevant to top-load resistance in closures and stacking strength in thin-wall containers. Charpy notched impact resistance under ISO 179-1/1eA at 23 °C for this melt-flow class is normally below 6 kJ/m²; therefore, the grade is not selected for cryogenic impact service. Thermal boundaries include a Vicat softening temperature typically in the 125–130 °C band under ISO 306 method A50 and a heat deflection temperature under ISO 75-2 method B at 0.45 MPa typically in the 65–80 °C range. These property windows are class ranges derived from published HDPE injection-molding data; they are not lot-certified MP94 values. For any production system, the certificate of analysis for the specific lot must be matched to the tool and end-use specification before release.
Virgin HDPE pellets do not hydrolyze, but surface condensation can introduce moisture that causes splay, silver streaks, and gate blush at high injection velocities. When pellets are transferred from cold storage into a warm molding area above 60% relative humidity, a drying step is advisable. A desiccant dryer set at 80 °C for 2–4 h typically reduces pellet moisture to below 0.02 wt%; hopper hot-air dryers are effective only if residence time is sufficient and inlet air dew point is below -20 °C. Moisture above approximately 0.05 wt% can produce visible splay in rapid filling of thin-wall containers because entrained water vapor acts as a physical blowing agent. Karl Fischer titration to ISO 15512 is the accepted method for certifying resin dryness in dispute cases. The same caution applies to post-industrial regrind stored in outdoor silos or open bins; regrind may contain fines and additive residues that retain surface water more strongly than virgin pellets. Published MP94-specific moisture thresholds are limited, and the above envelope reflects general HDPE injection-molding practice.
On high-speed closure tools with valve-gated hot-runner systems, the relevant processing limit is not melt temperature alone but shear-rate-dependent viscosity and gate-freeze time. Capillary rheometry under ISO 11443 can be used to compare lots; high-flow HDPE grades in the MP94 melt-flow class typically show apparent viscosity from 200 Pa·s to 400 Pa·s at 1000 s⁻¹ and 190 °C. Published MP94-specific capillary viscosity data is limited, so lot certification should be used for simulation input. In production, electric injection molding machines with clamp force from 80 tonnes to 150 tonnes are generally applied to 16- to 64-cavity closure tools, where the critical parameters are injection pressure, pack pressure, and cavity-pressure integrals. Gate diameters below 0.6 mm may freeze before pack transfer in parts with wall thickness below 0.8 mm, causing sink marks near the gate. Mold temperature is commonly held at 10–20 °C for fast cooling, but this lowers surface gloss and increases internal stress in deep-draw parts; raising mold temperature to 25–40 °C improves dimensional stability at the cost of longer cycle time. Three-zone polyolefin screws with compression ratios from 2.5:1 to 3.0:1 and L/D ratios between 20:1 and 25:1 are typically sufficient for MP94; excessive shear heating from high-compression PVC screws is unnecessary and may accelerate molecular weight loss. These are operational boundaries based on general HDPE injection-molding behavior, not on a single MP94 datasheet curve.
The incorporation of post-industrial regrind into MP94-based compounds is routine, but the process window narrows when regrind content exceeds 30 wt%. Multiple heat histories can shift melt flow rate by more than 1.0 g/10 min across a production run, causing variation in filling pressure and part mass. The regrind should be dedusted so that fines smaller than 500 µm remain below 5 wt% of the blend; excessive fines increase gel formation and black-speck generation in high-shear zones. Gravimetric dosing of regrind is preferred over volumetric blending because bulk-density variation in ground containers alters feed rate. A consistent blend should be verified by melt-flow measurement under ISO 1133-1:2022 at 190 °C/2.16 kg every 4 h during long campaigns. Impact retention after regrind is also a constraint: recycled HDPE can lose Charpy notched impact resistance under ISO 179-1/1eA by 20–50% after multiple heat histories, depending on regrind source and stabilizer renewal. In multi-layer barrier packaging, regrind containing EVOH or tie-layer residues is not an acceptable feedstock for MP94 monolayer injection because immiscible domains cause delamination and reduced burst strength. Published MP94-specific regrind retention curves are limited; the stated effects reflect general high-flow HDPE behavior.
Fractional-melt HDPE grades, typically characterized by melt flow rates from 0.3 g/10 min to 1.0 g/10 min, provide high environmental stress crack resistance and are used in blow-molded bottles and large drums. MP94 belongs to the high-flow injection-molding class, reducing injection pressure required to fill a given cavity and allowing shorter cycles through earlier plastication and faster packing. The trade-off is reduced stress-crack performance: under ASTM D1693, high-flow injection-molding grades generally show lower F50 values than fractional-melt grades, especially in 10% Igepal CO-630 solution at 50 °C. Published MP94-specific ESCR data is limited; users should request the lot certificate or run comparative tests before replacing a fractional-melt HDPE in bleach or surfactant packaging. Differences also appear in mold-filling pressure: a grade in the MP94 flow class may fill thin-wall portions at lower hydraulic pressure than a 0.4 g/10 min blow-molding grade, but the high-flow product may also exhibit greater sink-mark sensitivity if insufficient packing pressure is applied. In closure tooling, MP94’s rapid gate freeze is useful for short cycle times, but it can create frozen-in orientation and anisotropic shrinkage that must be compensated in the tool design.
MP94 is not an extrusion blow-molding grade. The high melt flow and relatively narrow molecular weight distribution reduce parison hang strength and increase drawdown sag on continuous shuttle or accumulator-head machines. For monolayer film extrusion, melt-pressure stability and bubble stability are usually inferior to film-grade HDPE with higher melt strength and broader molecular weight distribution. Published MP94-specific extensional viscosity data is limited; conversion on blow-molding or film lines should proceed only after pilot trials on the intended equipment. This operational boundary distinguishes MP94 from high-molecular-weight HDPE grades in the same density class and is a primary selection criterion for converters.
For food-contact injection-molded articles, conformity is established on the final article and conversion process, not by raw-material selection alone. The table below summarizes the regulatory instruments that typically govern HDPE MP94 applications in the European Union and North America; the listed conditions are framework-level and do not replace a specific declaration from the compounder or converter.
| Regulatory instrument | Scope | Clause or test method | Typical control requirement |
|---|---|---|---|
| EU Regulation 10/2011 | Plastic food-contact materials | Annex I and II; migration under EN 1186-1 | Overall migration ≤ 10 mg/dm²; specific migration limits per substance |
| FDA 21 CFR 177.1520 | Olefin polymers in food contact | 177.1520(c) specifications; conditions of use | Conformity depends on end-use temperature and food type |
| REACH Regulation (EC) No 1907/2006 | SVHC and restrictions | Annex XIV, Annex XVII | SVHC content restrictions; article communication duties |
| RoHS Directive 2011/65/EU | Electrical and electronic equipment | Annex II restricted substances | Pb, Hg, Cr(VI), PBB, PBDE ≤ 0.1 wt%; Cd ≤ 0.01 wt% |
| ISO 1133-1:2022 | Melt flow rate of thermoplastics | Method A/B | Lot-release consistency at 190 °C/2.16 kg |