| HS Code | 566078 |
| Density | 0.954 g/cm3 |
| Melt Flow Rate 190 C 2 16 Kg | 0.9 g/10 min |
| Tensile Stress At Yield | 26 MPa |
| Tensile Strain At Break | >600% |
| Flexural Modulus | 1300 MPa |
| Charpy Notched Impact Strength 23 C | 10 kJ/m2 |
| Charpy Notched Impact Strength 30 C | 4 kJ/m2 |
| Vicat Softening Temperature | 125°C |
| Shore D Hardness | 60 |
| Environmental Stress Cracking Resistance Escr 10 Igepal | >1000 h |
| Melting Temperature | 133°C |
| Thermal Conductivity | 0.45 W/m·K |
| Water Absorption | <0.01% |
| Dielectric Constant 1 Mhz | 2.3 |
| Volume Resistivity | >10^15 ohm·cm |
| Dielectric Strength | 20 kV/mm |
| Brittleness Temperature | -70°C |
| Oxygen Induction Time | >20 min |
As an accredited Versalis HDPE MP90C factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis HDPE MP90C is packaged in 25 kg bags, stacked on pallets and stretch-wrapped, with 1,000 kg bulk bags available. |
| Container Loading (20′ FCL) | 20′ FCL: 25 kg bags, 55 bags/pallet, 18 pallets, total 24.75 MT Versalis HDPE MP90C, securely stowed and lashed. |
| Shipping | Versalis HDPE MP90C is supplied as non-hazardous polyethylene pellets. It is typically shipped in 25 kg bags, octabins, or bulk trucks/containers under ambient conditions. Keep packages dry, sealed, and away from heat, sunlight, and contamination. No dangerous goods classification or special transport requirements apply. Standard freight handling is recommended. |
| Storage | Store Versalis HDPE MP90C in original, closed packaging in a cool, dry, well-ventilated area. Protect from direct sunlight, heat, moisture, and contamination. Keep away from ignition sources, oxidizers, and incompatible substances. Use pallets and stack securely to prevent damage. Maintain normal warehouse temperatures. For safety, refer to the Safety Data Sheet before handling or storage. |
| Shelf Life | Versalis HDPE MP90C shelf life: 24 months when stored unopened in a cool, dry, ventilated place, away from direct sunlight. |
In a 32-cavity thin-wall container tool mounted on a 2,500 kN accumulator-assisted hydraulic injection machine, Versalis HDPE MP90C fills a 0.45–0.80 mm sidewall only when the gate-to-weld-line path is kept below approximately 180:1 at the nominal melt flow rate of 8 g/10 min under ISO 1133-1:2022 conditions at 190 °C/2.16 kg. For a 125 mL dairy cup with a 0.55 mm nominal wall, barrel temperatures set to 180–200 °C in the feed zone, 210–230 °C in the compression zone, and 220–240 °C at the nozzle prevent both short shots and localised shear heating. Chilled mould water at 12–18 °C maintains cavity wall temperature, while injection speed between 180 mm/s and 250 mm/s is required to prevent flow-front hesitation before the weld line and to keep frozen-layer growth below the critical thickness that would produce tiger-stripe surface defects. Holding pressure is set to 500–750 bar hydraulic, corresponding to cavity pressure 350–500 bar measured with a 1 mm flush-face pressure transducer; hold time is terminated after gate freeze at 0.8–1.2 s, because longer packing in a thin sidewall creates gate-area sink marks and increases cycle time without improving sidewall thickness uniformity beyond ±0.04 mm.
Compliance for food contact is governed by EU 10/2011 with an overall migration limit of 10 mg/dm² and by FDA 21 CFR 177.1520(c) olefin polymer clearance. The pigment package is restricted to a 3–5 wt% PE-based white masterbatch; titanium dioxide loading in the masterbatch must not exceed 60 wt% if the container is intended for acidic dairy products stored at 4 °C for 60 d. A process aid or external lubricant is not added unless justified by mould release trials, since low-molecular-weight additives can increase fatty-food migration values above the specified limit. Stacking performance after filling is measured according to ASTM D2659-16; at 2 mm compression, a 125 mL cup generally fails below 240 N, a value that indicates sidewall ovality exceeding 0.5 mm or uneven gate orientation. Published data for this specific MP90C configuration under all cavity layouts is limited, and mould trials with strain gauges at the four corner cavities are required before committing to a 100,000-cavity production campaign.
For a 26 mm or 28 mm single-piece beverage closure injection moulded from MP90C, gate vestige height is set by the interaction between hot-runner valve pin retraction, the 0.5–0.7 mm gate diameter, and the melt temperature at the nozzle of 230–245 °C. A valve-gate hot runner with thermal gate insert maintains a vestige below 0.15 mm on the closure top panel when holding pressure is transferred through the gate for 0.6–1.0 s before the pin closes. Short valve-pin delay below 0.4 s freezes the gate too early and leaves a void at the centre of the top panel, while delay above 1.2 s creates stringing and increases cycle time to 8–12 s on a 48-cavity high-speed injection press. The tamper-evident band, with a web thickness of 0.22–0.30 mm, requires an injection speed above 200 mm/s to prevent cold-flow ripples in the bridge segments; the tool is typically run with mould coolant at 8–15 °C to reduce warpage of the band after demoulding.
Linerless closures from MP90C use a moulded elastomeric seal ring whose contact force is evaluated by torque retention under ASTM D2063-12; failure is defined as a retained removal torque below 0.8 N·m after 24 h at 23±2 °C. For still-water and juice applications, organoleptic compliance is assessed according to EU 10/2011, and the base resin must satisfy FDA 21 CFR 177.1520 without a functional barrier. Colour concentrate level is held to 1–3 wt% in a PE carrier; pigments with heavy-metal content above the REACH Annex XVII entry 23 limits are excluded. A processing limitation applies to any programme using acetaldehyde-scavenging or oxygen-scavenging masterbatches: the admixture level must remain below 0.5 wt% because the scavenger particle dispersion in a high-speed screw can agglomerate at the valve pin and raise gate vestige variation from ±0.05 mm to ±0.10 mm.
Household storage boxes and utility receptacles moulded from MP90C with a nominal wall of 2.5 mm shift the quality risk from short-shot instability to differential skin-core orientation and sink development at boss junctions. The melt temperature is set lower than thin-wall packaging, at 190–220 °C, to limit crystallisation shrinkage and reduce cooling time, while the mould temperature is held at 20–35 °C using turbulent water at 8–12 L/min per circuit. A holding pressure of 350–500 bar applied for 6–10 s is adequate only if the gate seal time is confirmed by cavity-pressure decay; packing pressure released below 6 s leaves sink marks near bosses with wall junctions above 1.6:1. Living hinges in houseware lids, typically 0.25–0.45 mm thick, are gated so that flow passes across the hinge in the same direction as flexure; a perpendicular flow front creates a weld-like orientation that fails in less than 5,000 flex cycles at 2.5 Hz.
Formulation for this segment uses 2–4 wt% of a PE-based colour masterbatch and, where UV stability is required for outdoor storage, 0.3–0.6 wt% of a HALS package is added; PP-based or EVA-based masterbatch carriers are excluded above 0.5 wt% because they reduce hinge flex life and cause delamination at the handle insert. Dimensional control follows ISO 294-4 for moulding shrinkage, and the mould allowance is set at 1.6–2.2% in the flow direction and 1.4–1.8% transverse to flow; failure to separate shrinkage axes causes bottom bowing greater than 1.5 mm across a 400 mm box footprint. Recycled content can be introduced at 20 wt% when the regrind is hot-batch, closed-loop and free of adhesive labels; higher fractions reduce the Izod notched impact below the 4.0 kJ/m² value measured under ISO 179-1/1eA at 23 °C. Published data for MP90C in multi-cycle regrind beyond 20 wt% is limited, and converter-specific validation is required.
Open-top pails and industrial containers with a capacity of 20–45 L are moulded from MP90C at a melt temperature of 210–240 °C, a mould temperature of 15–25 °C, and a filling speed of 80–160 mm/s to avoid jetting at the handle bosses. The injection machine must be selected for projected shot weight and clamp force: a 45 L pail with a 2.8–3.2 mm wall requires a clamp force above 5,500 kN when cavity pressure reaches 250–350 bar. Stacking top-load is measured after 14 d conditioning at 40 °C and 90% relative humidity under ASTM D2659-16; a pail with a 280 mm top opening generally must sustain 1,500 N to pass a 3-high warehouse stack without lid deflection exceeding 2 mm.
Environmental stress-crack resistance is assessed with ASTM D1693-21 condition B in 10% Igepal CO-630 at 50 °C; pail converters commonly require no F50 failure before 120 h. Process-induced ESCR loss is observed when melt temperature exceeds 260 °C for more than 8 min residence time, and when regrind above 30 wt% is blended with insufficient homogenisation. For outdoor exposure, 2–4 wt% carbon black masterbatch provides UV stabilisation, and the black masterbatch carrier must be an HDPE or LLDPE grade with melt-flow ratio within 0.7–1.3 of MP90C; a mismatched high-flow carrier produces streaking at the pail bottom. Dangerous-goods packaging requires additional UN certification of the finished pail assembly, not merely the resin, and must be tested under the applicable ADR/RID/IMDG performance tests at the wall thickness and closure type used in production.
The following table provides indicative processing windows for three conversion routes using MP90C on general-purpose injection machines with 22:1 to 25:1 L/D ratio screws and non-return valve tips.
| Parameter | Thin-wall cup | Closure | Industrial pail |
| Melt temperature at nozzle (°C) | 220–240 | 230–245 | 210–240 |
| Mould temperature (°C) | 12–18 | 8–15 | 15–25 |
| Injection speed (mm/s) | 180–250 | 200–260 | 80–160 |
| Holding pressure (bar) | 500–750 | 350–600 | 450–700 |
| Back pressure (bar) | 5–10 | 3–8 | 5–12 |
| Screw recovery speed (rpm) | 100–150 | 80–120 | 60–100 |
When a 50 mL jar and overcap are specified for cosmetic cream packaging, the wall section of 3.5–5.0 mm places MP90C in a cooling-dominated cycle rather than a flow-dominated cycle. Melt temperature is reduced to 200–220 °C to limit discoloration and to shorten the post-fill cooling stage, while mould temperature is held between 15 °C and 25 °C with conformal cooling channels in the thread ring to prevent ovality. Holding pressure of 400–600 bar is applied for 2–4 s per mm of nominal wall; pressure release below the gate-seal time produces internal voids at the thread root and reduces the ISO 527-2 tensile yield below 25 MPa at 23 °C. Mould shrinkage allowance follows ISO 294-4 at 1.8–2.2% in the flow direction and 1.5–2.0% transverse, with the larger value used in the thread core to avoid cap stripping torque above 1.2 N·m after three days at 40 °C.
Surface gloss for personal-care closures and overcaps is measured at 60° under ASTM D523-14; values above 60 GU require a cavity polish of 0.05 µm Ra or better, and any texture insert must be vented to prevent gas-burn streaks at the rim. Colour concentrate addition is limited to 2–3 wt% of an HDPE-carrier masterbatch with inorganic pigments, while organic pigments that migrate into semi-solid cream media are excluded under EU 10/2011 if the pack is used for leave-on formulations. Regrind is limited to 20 wt% of the same colour family; higher fractions shift the L* a* b* coordinates by more than 0.5 ΔE against the master reference standard and reduce the assembly thread-holding torque below 0.9 N·m.
Returnable logistics trays, ventilation crates and dunnage platforms made from MP90C are injection moulded with a nominal wall of 2.2–3.5 mm, a melt temperature of 210–240 °C, and a mould temperature of 15–25 °C. The gate positions are placed at the base intersections, not at the sidewall corners, to avoid jetting around the ventilation slots and to shift the weld line away from stack bosses. A 600 mm × 400 mm ventilated crate weighing 280–350 g requires a clamp force above 4,000 kN; injection speed is set to 120–200 mm/s and holding pressure 400–600 bar. Stacking restraint is evaluated by an equivalent top load of 2,000 N after conditioning at 40 °C and 90% RH for 14 d using ASTM D2659-16, and flatness of the stack interlock must remain within ±0.8 mm to prevent pallet hang-up.
Washdown exposure introduces a thermal boundary that is often underestimated. A caustic wash at 80 °C for 120 s with 0.5% NaOH solution relaxes moulded-in stress at gate bosses and can increase sidewall bowing by 0.6–1.2 mm after 20 cycles, so accelerated trials with 20 wash cycles are specified before accepting the crate for returnable service. Formulation includes 2–4 wt% colour or carbon black masterbatch and, when UV resistance is required, 0.3–0.6 wt% HALS/UV package; regrind addition is limited to 25 wt% because higher fractions reduce low-temperature drop impact at −20 °C to less than 3 J under ASTM D2463-15. The returnable packaging application is outside direct food-contact scope except where a specific logistics tray is declared, and compliance is driven by REACH SVHC content and 2011/65/EU RoHS Annex II restricted substances. Published data for MP90C under repeated 80 °C alkaline washdown is limited; converter-specific validation on the actual grid geometry is required.
Competitive Versalis HDPE MP90C prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis HDPE MP90C (also designated Eraclene MP90C in the Versalis polyethylene portfolio) is a high-density polyethylene grade specified for extrusion blow moulding of rigid packaging and technical hollow parts. The grade is supplied as pelletised resin with a nominal density of 0.954 g/cm³ measured by ISO 1183-1:2019 and a melt flow rate of 0.80 g/10 min determined at 190°C under 2.16 kg load according to ISO 1133-1:2022. These values place the product in the medium-high molecular weight HDPE blow moulding segment, where melt strength during parison extrusion and resistance to slow crack growth are the controlling design parameters. The resin is used in monolayer and multi-layer extrusion blow moulding lines for containers typically between 0.5 L and 30 L, including detergent, agrochemical, lubricant, and auxiliary fluid packaging. It is not intended for injection moulding, blown film, pipe extrusion, or rotational moulding, where the required flow behaviour and molecular architecture differ. Published technical data for this specific configuration is limited, and conversion trials should be based on the certificate of analysis for the supplied lot.
The values below represent typical material characterisation data associated with Versalis HDPE MP90C. They should not be read as guaranteed specification limits because lot-to-lot variation and sample preparation can shift some measurements. Where a property is critical to container qualification, the corresponding test method should be repeated on plaques or containers taken from the production line under the same thermal history.
| Property | Test method | Typical value | Unit |
|---|---|---|---|
| Density | ISO 1183-1:2019 | 0.954 | g/cm³ |
| Melt flow rate | ISO 1133-1:2022 | 0.80 | g/10 min |
| Tensile stress at yield | ISO 527-2:2012 | 26 | MPa |
| Elongation at break | ISO 527-2:2012 | >600 | % |
| Flexural modulus | ISO 178:2019 | 1050 | MPa |
| Charpy notched impact at 23°C | ISO 179-1:2023 | 9 | kJ/m² |
| Vicat softening temperature | ISO 306:2022 A50 | 126 | °C |
| Shore hardness | ISO 868:2003 | 61 | Shore D |
| Environmental stress crack resistance | ASTM D1693-21 | >120 | h |
The combination of 26 MPa yield stress and 1050 MPa flexural modulus provides stack-load bearing capacity in large containers, while the notched impact of 9 kJ/m² at 23°C contributes to drop resistance after filling. The ESCR value above 120 h under 100% Igepal is relevant because detergent and agrochemical formulations often contain non-ionic surfactants that accelerate crack propagation in lower-molecular-weight HDPE grades.
For incoming lot acceptance, the quality control protocol should include melt flow rate, density, and visual gel count on a laboratory cast film line according to ASTM D7310-20. Gel count above 20 particles/1000 cm² larger than 0.5 mm indicates thermal degradation or contamination and predicts poor parison surface quality. Moisture content by Karl Fischer titration should be below 0.05% before processing. Batch-to-batch variation in molecular weight distribution can be monitored by dynamic oscillatory rheometry at 190°C; the shear storage modulus at 0.1 rad/s and the crossover frequency are sensitive indicators of parison sag. Published data for this specific configuration is limited, so incoming QC limits should be built from at least 10 production lots.
Processing MP90C on a production blow moulder requires a single-screw extruder with 24:1 to 30:1 L/D and compression ratios between 2.5:1 and 3.5:1. Barrel temperature profiles from feed to metering zone commonly range from 180°C to 220°C, while the head and die zones are held between 190°C and 210°C. Sustained melt temperatures above 220°C increase thermo-oxidative chain scission, leading to gel formation, die lip staining, and loss of parison melt strength. The die gap is usually set to 0.8–1.2 times the intended wall thickness to offset die swell, which for MP90C is observed as 35%–65% weight swell on accumulator-head lines. On production-scale machines, the parison programmer should be adjusted for containers with length-to-diameter ratios above 2:1 to prevent thinning at the parting line and excessive flash at the pinch-off. Clamp force requirements are tied to projected area and blowing pressure: 0.5–5 L containers are frequently moulded on presses with 10–30 t clamp force, while 20–30 L jerry cans require 80–150 t depending on blow-up ratio and mould cooling geometry. Pellet surface moisture is not typically an issue below 60% relative humidity; if resin is stored in open silos or feed hoppers above 60% relative humidity, hopper drying at 60°C for 1 h reduces melt splay and void formation in thick parison sections. On shuttle blow moulding machines with 2–6 stations, parison consistency across moulds is controlled by accumulator head pressure and die gap rather than by screw speed alone.
If colouring is required, MP90C is usually run with polyolefin-based masterbatches at let-down ratios from 2% to 4%. Carbon black or iron oxide pigments can nucleate HDPE and alter shrinkage and ESCR; therefore, masterbatch lot changes should be revalidated with drop impact and ESCR tests. Liquid pigments are generally avoided in blow moulding because they reduce viscosity locally and can create streaks at the die lip. The use of calcium carbonate filler is not recommended for thin-wall containers because it lowers tensile impact and ESCR at loadings above 5%. Published data for this specific configuration is limited for high-load pigmented systems.
Blow-up ratio in extrusion blow moulding is calculated as the ratio of the mould cavity diameter to the parison diameter. In container lines running MP90C with blow-up ratios above 2.5:1, the radial wall-thickness distribution becomes the critical process output. If the die head temperature is not maintained within ±5°C of the setpoint, the parison sag rate changes and the upper wall of the container thins before the mould closes. A drift of +5°C increases sag and produces top-wall thinning; a drift of −5°C creates cold welds at the tail pinch-off and lower burst strength because insufficient intermolecular diffusion occurs at the weld line. The grade is therefore run on machines with closed-loop die temperature control and separate body, foot, and pinch-off zones. When the BUR exceeds 3:1, a diverging die tool and parison profiling with 10–100 point axial wall-thickness control are used to compensate for the difference between the parison length and the cavity length. Mould cooling at 10–40°C with turbulent water flow is required to remove heat through the wall; insufficient cooling increases crystallinity and can reduce drop impact at −20°C. Production-scale experience on 60–90 mm screw diameters indicates that throughput and weight distribution are more sensitive to die gap variation than to screw speed when the melt is in the Newtonian plateau of MP90C.
The design of blow-moulded containers with MP90C must account for mould shrinkage after demoulding. HDPE of density 0.954 g/cm³ typically exhibits mould shrinkage of 1.5%–2.5% depending on wall thickness and cooling rate. Thick sections cool more slowly and develop higher crystallinity, which increases local density and can cause sink marks or warpage. Handles, ribs, and foot sections should be radiused and gated for uniform flow; sharp corners act as stress concentrators and reduce environmental stress crack resistance. The pinch-off weld at the bottom of the container is a critical stress raiser. In drop tests, containers made from MP90C generally fail at the pinch-off or at the sidewall area adjacent to the mould parting line if the wall distribution is below the design threshold. Finite element analysis for wall-thickness optimisation uses input data such as the 26 MPa yield stress and 9 kJ/m² Charpy impact measured by the methods listed above.
In rigid containers made from MP90C, chemical resistance is controlled by the semi-crystalline morphology and the continuity of tie molecules between lamellae. The ESCR test under ASTM D1693-21 uses bent strips immersed in 100% Igepal CO-630 at 50°C; failure is recorded as slow crack propagation from surface defects. The mechanism is not bulk dissolution but environmental stress cracking, in which the surface-active agent reduces the energy required for fibril breakage at crack tips. Containers made from MP90C are used for many detergent, mild oxidiser, and aliphatic hydrocarbon products, but they are not recommended for strong oxidising acids at elevated temperature, aromatic solvents, or chlorinated hydrocarbons, which swell or degrade the polymer. Permeation of non-polar solvents through the container wall increases with storage temperature and should be assessed by weight loss or pressure rise methods in accordance with ISO 62:2008 or equivalent. Published data for this specific configuration is limited for aggressive solvent mixtures, and testing on production bottles is required before commercial use.
Coextruded containers using MP90C as the structural layer can include an inner or outer polymer layer selected for barrier properties, such as EVOH or polyamide. The melt streams must be thermally matched; MP90C is processed at 190–220°C, while EVOH requires 220–240°C, so appropriate die design and layer separation are required. Adhesive tie layers based on maleic anhydride-grafted polyolefins are mandatory between HDPE and EVOH or polyamide, because HDPE has no polar functionality. The addition of regrind at 30% or higher can introduce mixed-layer contamination and increase gel formation; regrind content should be validated by optical inspection of the parison surface and container burst testing.
The principal difference between MP90C and a general-purpose HDPE injection moulding grade is the molecular weight distribution. MP90C has a higher weight-average molecular weight and a broader distribution, which produces the parison melt strength needed to resist draw-down during the open-mould cycle. Injection grades are controlled for spiral flow and rapid relaxation, typically with MFR values above 10 g/10 min, whereas MP90C is produced at 0.80 g/10 min. A high-load melt index HDPE film grade is typically in the range 0.2–0.5 g/10 min; although such grades have high melt strength, they are not an automatic substitute for MP90C because lower flow can cause excessive die swell, melt fracture, and reduced output on blow moulding extruders designed for medium-molecular-weight HDPE. Compared with high-molecular-weight HDPE blow moulding grades used for 200 L drums, MP90C has lower molecular weight and higher MFR, which allows shorter cycle times but generally lower long-term hydrostatic strength and lower resistance to environmental stress cracking. It also differs from HDPE blow moulding grades with density 0.945 g/cm³ intended for squeezable containers; the higher density of MP90C yields greater stiffness and reduced permeability but lower stress crack resistance in highly constrained geometries. Compared with HDPE pipe grades rated for PE100 slow crack growth under sustained hoop stress, MP90C is not optimised for hydrostatic design basis and should not be substituted in pressure-pipe applications. Compared with polypropylene random copolymer blow moulding grades, MP90C has lower heat distortion temperature and lower stiffness but generally better ESCR in surfactant systems and lower processing temperatures.
Depending on grade version and intended contact use, regulatory status should be confirmed against the current supplier certificate. Polyethylene grades in this density range may be evaluated for food-contact compliance under FDA 21 CFR 177.1520, which covers olefin polymers, but a finished food-contact statement for MP90C must be confirmed for the supplied lot because additive packages and catalyst residues vary by production campaign. Under European Union legislation, the resin falls under REACH registration obligations for polymers and monomers, while electrical and electronic packaging applications are typically assessed under RoHS Directive 2011/65/EU for lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls, and polybrominated diphenyl ethers. Reprocessing of production scrap at levels up to 30% is common but should be validated for ESCR and drop impact because repeated extrusion shifts the molecular weight distribution and raises gel counts.
For warehouse storage, MP90C pellets should be kept away from direct sunlight and prolonged temperatures above 50°C to limit surface oxidation and colour shift. In outdoor silos, temperature stratification can create condensation cycling below 0°C and above 40°C; the resulting surface moisture is re-absorbed slowly and can affect extrusion stability. The grade should not be stored near open sources of volatile organic compounds because polyethylene can absorb odorous species that later appear in blow-moulded containers. Inventory rotation should follow first-in-first-out practice, with shelf-life verification by melt flow stability after extended storage. Published data for this specific configuration is limited beyond typical polyolefin warehouse practice.
When MP90C containers are jointed by hot-plate, ultrasonic, or spin welding, the interface must be heated above the melting temperature to allow chain diffusion. The melting temperature of HDPE with density 0.954 g/cm³ is approximately 130–135°C by differential scanning calorimetry according to ISO 11357-3:2018, but welding tools are set higher to compensate for heat loss. Hot-plate temperatures of 210–230°C are typical for HDPE, with welding pressure from 0.1–0.3 MPa at the joint area. The main risk in welded MP90C containers is cold welding at the pinch zone if the parison tail temperature drops below 160°C before the mould closes. In such cases, the failure mode is brittle fracture at the weld line during drop testing. For laboratory qualification, the burst strength of welded jerry cans can be measured by hydraulic pressurisation at 0.1–0.5 bar/s until failure, with acceptance criteria defined by dangerous goods transport regulations such as ADR 6.1.5.3 for UN packaging.