Versalis Hdpe Mp90

Versalis HDPE MP90

    • Product Name: Versalis HDPE MP90
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 832834
    Density 0.954 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.9 g/10 min
    Melt Flow Rate 190 C 21 6 Kg 20 g/10 min
    Tensile Modulus 1000 MPa
    Tensile Stress At Yield 27 MPa
    Tensile Strain At Yield 9%
    Tensile Strain At Break >600%
    Flexural Modulus 1100 MPa
    Izod Notched Impact Strength At 23 C 25 kJ/m²
    Izod Notched Impact Strength At 30 C 8 kJ/m²
    Vicat Softening Temperature 127°C
    Heat Deflection Temperature At 0 45 Mpa 75°C
    Shore D Hardness 62
    Environmental Stress Crack Resistance 10 Igepal >1000 h
    Melting Point 132°C
    Water Absorption <0.01%
    Volume Resistivity >10^16 Ω·cm
    Dielectric Constant At 1 Mhz 2.3
    Dissipation Factor At 1 Mhz 0.0002
    Thermal Conductivity 0.45 W/m·K
    Coefficient Of Linear Thermal Expansion 1.2E-4 /°C

    As an accredited Versalis HDPE MP90 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis HDPE MP90 is packaged in 25 kg polyethylene bags, palletized at 1,000 kg per pallet for safe handling and transport.
    Container Loading (20′ FCL) Versalis HDPE MP90 loads in 20′ FCL as 25 kg bags on pallets, securely stowed, maximizing payload for safe ocean transport.
    Shipping Versalis HDPE MP90 is typically shipped as non-hazardous polyethylene pellets in 25 kg bags, big bags, or bulk containers. Transport in clean, dry trucks, railcars, or containers. Not classified as dangerous goods. Keep dry, avoid prolonged heat and direct sunlight, and prevent package damage or spillage.
    Storage Store Versalis HDPE MP90 in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and moisture. Keep in original, closed packaging on pallets, off the floor. Avoid contact with oils, chemicals, or contaminants. Maintain stable temperature and humidity. Prevent dust accumulation and follow local regulations for combustible dust and safe material handling. Ensure good housekeeping and inventory rotation.
    Shelf Life Versalis HDPE MP90 shelf life: typically 24 months in unopened original packaging, stored dry below 40°C, away from direct sunlight.
    Application of Versalis HDPE MP90

    High-flow thin-wall moulding for dairy and convenience-food containers places MP90 in a filling window where gate-freeze time and sink-mark generation are the two opposing constraints. The grade’s nominal melt mass-flow rate of 9.0 g/10 min at 190°C and 2.16 kg load under ISO 1133-1:2022, with a density of 0.960 g/cm³ under ISO 1183-1:2019, permits wall sections of 0.6–1.3 mm to fill from a cold runner when injection velocity is set at 120–180 mm/s on a 120 t clamp machine. A 32-cavity cup tool with a 0.8 mm edge gate will typically show a fill time of 0.35–0.70 s; hold pressure must then drop from 45 MPa to 20 MPa before gate seal at 1.5–2.0 s. If hold pressure is released before the gate freezes, the stacking ledge and base perimeter develop sink marks because the high-flow grade has little melt strength to compensate for the volumetric shrinkage in the 1.5–2.0% range measured by ISO 294-4. A chilled mould at 12–28°C and a barrel profile of 210°C feed, 225°C compression, 235°C metering, and 240°C nozzle are used to maintain shear thinning while reducing cycle time. Migration compliance for finished yoghurt cups, margarine tubs, and deli containers is assessed under EU Regulation 10/2011 with an overall migration limit of 10 mg/dm² in food simulants and under FDA 21 CFR 177.1520 for high-density olefin polymers; no plasticiser or heavy-metal stabiliser package is required, which simplifies end-use documentation. The main operating boundary is not thermal stability but the narrow transition between short-shot at cold gate tips and flash at the parting line above 1.8 s hold time; this sensitivity is most severe on lids with peel-seal flanges below 0.7 mm thickness.

    What limits gate-freeze time in 64-cavity dispensing-cap tooling when MP90 is injected at 140 mm/s?

    High-cavitation closure production for non-carbonated beverage caps, snap-hinge dispensing caps, and tamper-evident overcaps uses the same high-flow plateau but shifts the critical control from sink to gate vestige stress. On a 64-cavity valve-gated hot runner with 0.6–0.8 mm gate-land length, fill speed is set between 100 mm/s and 160 mm/s; faster injection causes the gate tip to remain molten beyond 2.2 s and produces cap skirt ovality above 0.3 mm on a 28 mm closure. The hold-pressure profile is typically 55 MPa for 0.8 s, followed by 30 MPa for 1.0 s, with cooling-time adjustment so that the part is ejected at a surface temperature below 80°C. A production-scale constraint appears at the tamper-evident band: thin bridges under 0.25 mm width require a minimum mould temperature of 15°C; higher mould temperatures reduce bridge strength and cause band tearing during de-moulding, while lower temperatures increase notch sensitivity in the hinge area. Environmental stress cracking resistance is evaluated under ASTM D1693 condition B, because high-density polyethylene of 0.960 g/cm³ density has intrinsically lower ESCR than a fractional-melt HDPE; cap skirts exposed to detergent solutions or fatty food liquids should be stress-relieved by maintaining gate-land length below 0.8 mm and avoiding sharp thread run-out radii below 0.2 mm. Child-resistant closure certification falls under ISO 8317:2015; food-contact caps are further assessed under EU Regulation 10/2011 and FDA 21 CFR 177.1520 with extraction limits referenced to the intended temperature-time use. Published data for MP90 in this exact 64-cavity cap configuration is limited, but the above process envelope is consistent with high-flow HDPE cap grades and with the reported viscosity-shear response of the material.

    Drop-wall fracture boundaries in 1H2 open-top pail tooling

    Open-top pails of 20 L and 25 L produced from MP90 carry the 1H2 UN packaging designation when the moulded body and lid pass drop, stack, and leakproofness tests for dangerous goods. The injection process differs from thin-wall work: wall thickness must transition from 1.6 mm in the side wall to 2.4 mm in the bottom corner radius and 3.0 mm at the rim, which simultaneously raises the cooling requirement and increases the risk of sink at the handle lug. Typical machine settings use a shot size of 650–700 g, a 700 t clamp force, melt temperature of 230°C, and hold pressure at 65 MPa for 3.5 s before the screw is pre-plastified during cooling. The critical performance test is the 1.2 m drop for Packing Group II at -18°C after conditioning; moulded pails failing this test usually crack from the bottom corner where shear-induced orientation is lowest and where the corner radius is below 3 mm. Stack-test performance under the UN scheme involves a superimposed load calculated from the stacking height of filled packages at 40°C for the period specified in ADR 6.1.5.3.5; top-load buckling is minimised by retaining a solid stacking rib at the top rim that is no more than 0.6× the adjacent wall thickness, otherwise sink in the rib drains pack pressure and lowers column strength. The material’s density of 0.960 g/cm³ and notched Izod value in the range of 4–5 kJ/m² under ISO 180/A provide the necessary base toughness, but the mould must not rely on high melt flow alone; the handle bridge and side-wall stiffness demand that the gate be located in the base centre with a fan insert to prevent weld lines at the handle lugs. Terminal objects include UN-certified chemical pails, water-based paint pails, and food-ingredient pails where the closures are foil-sealed and the grade meets EU Regulation 10/2011 or FDA 21 CFR 177.1520 as applicable.

    When pallet legs exceed 3.2 mm nominal wall, clamp pressure alone no longer suppresses top-surface sink

    Industrial crates, distribution pallets, and cold-store bins made from MP90 shift the processing problem from gate freeze to differential shrinkage across adjacent heavy sections. A flat distribution pallet of 1200 mm × 1000 mm with 9 solid legs at 3.2–4.0 mm nominal wall cannot be filled and packed solely by a high-flow melt; the shear-thinning behaviour of the 9.0 g/10 min MFR helps fill the rib network, but the thick-leg base creates a reservoir of molten material that continues to shrink after the top deck has frozen. On a 1,200 t hydraulic press with a 105 mm screw, the process is set with melt temperature 220°C and mould temperature 20°C; fill time may extend to 3.5 s, followed by hold pressure of 60 MPa for 12 s and cooling time of 35–45 s. Even with this profile, top-surface sink above the leg bosses remains the dominant rejection mode if the boss-wall blend radius is below 1.5 mm or if the top deck is overpacked. Low-temperature impact is the specification that justifies HDPE over polypropylene in such applications; at -20°C, instrumented falling-weight impact data under ISO 6603-2 show a ductile penetration response for high-density polyethylene while some polypropylene grades transition to brittle failure. However, flexural modulus of MP90 is in the range of 1,200–1,400 MPa under ISO 178, which is below that of a typical high-stiffness polypropylene grade; therefore pallet designers must add ribbing, peripheral beams, or insert reinforcement if the static load specification is governed by ISO 8611-1:2011 pallet test methods. The operational boundary is thermal: prolonged hot-ware stacking at 60°C can induce creep in the deck, so MP90 is better suited to cold-chain and ambient distribution crates than to load-bearing pallets exposed to direct summer container temperatures above 50°C for more than 4 h. Terminal items include dairy crates, bread trays, returnable logistics boxes, and freezer-grade pallet footings where impact at -25°C is specified.

    Rigid houseware containers with handle bosses and latch undercuts represent a further window for MP90 because the high-flow grade can be moulded in multi-cavity tools at lower hydraulic pressure but tends to exhibit visible sink at wall-thickness transitions if the mould temperature is not held below 25°C. A storage tote with a 35 L capacity and nominal side-wall thickness of 2.2 mm may be produced in a 2+2 stack tool with a 600 t clamp unit, using an injection speed of 90 mm/s and a hold pressure of 45 MPa; the gate is placed in the bottom centre to maintain a single flow front and avoid weld lines at the handle strap lugs. The handle lugs are thickened to 4.0 mm, which creates a shrink-away zone on the opposite surface; reducing lug thickness to 2.8 mm and adding a C-shaped rib of 0.5× wall thickness recovers flatness without sacrificing handle strength. Impact resistance after ejection is evaluated by product-level drop tests from 1.0 m at 0°C to verify that moulded-in stress at the latch undercut does not cause brittle fracture; the protocol is derived from ASTM D5276-19 drop-test procedure for loaded containers and ISO 180/A notched impact. The material’s low moisture uptake of below 0.01% makes pre-drying unnecessary in normal warehouse conditions with relative humidity below 60%, although surface condensation must be removed before moulding to prevent splay in humid coastal plants. Terminal products include stackable storage boxes, laundry baskets, and cleaning-product buckets that do not require UN certification but are expected to survive repeated drop cycles and caustic cleaning agents.

    Cosmetic jar bases and the 40°C side-wall distortion threshold

    Rigid cosmetic and personal-care packs such as injection-moulded cream jars, compact bases, and airless-pump collars are a comparatively narrow application window where MP90 is selected for density-driven surface hardness rather than high flow alone. The side-wall thickness is normally kept between 1.8 mm and 2.5 mm; at this thickness, the material can be processed on a 200 t hydraulic machine in 16-cavity production with melt temperature of 235°C, mould temperature of 15°C, and hold pressure of 50 MPa for 2.0 s. Because the pack must pass a side-load compression test at 40°C to simulate warehouse palletisation, the base design cannot use a flat disc with a central gate; a domed or stepped base with radial ribs of 0.5× wall thickness distributes the side load and prevents the jar wall from ovalising beyond 0.4 mm after 24 h at temperature. The grade’s high density reduces uptake of oils and fragrances compared with linear low-density polyethylene; compatibility with finished cosmetic formulas is verified by weight-change testing under ISO 175:2010 after 7 days at 40°C, with an acceptance threshold of 1.0% mass change for rigid packs. The operating limit for MP90 in this sector is not mechanical but aesthetic: a glass-like side wall cannot be produced from an unplated mould at melt temperature above 245°C, because the high flow creates visible gate blush and flow-line marks on polished cores. For that reason, this application is limited to pigmented, textured, or spray-coated outer bodies where the surface is not required to meet Class A optical finish under ISO 2813:2014 gloss measurement. Published data for MP90 in cosmetic primary packs is limited; the above constraints are drawn from general high-density polyethylene injection-moulding practice and dimensional stability testing.

    Free Quote

    Competitive Versalis HDPE MP90 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis HDPE MP90, also designated Eraclene MP 90 in the Versalis polyolefin portfolio, is a high-density polyethylene homopolymer intended for injection molding. The resin is supplied as a pelletised product with density 0.960 g/cm³ and melt flow rate 9.0 g/10 min at 190°C under 2.16 kg load according to ISO 1133-1:2022. The base polymer is polyethylene homopolymer CAS 9002-88-4 made by low-pressure catalytic polymerisation. The predominantly linear chain structure and low comonomer fraction produce high crystallinity, high stiffness, and moderate barrier properties relative to low-density polyethylene.

    The values in Table 1 are representative typical values from supplier technical literature and are not specification limits. Mechanical properties are determined on injection-molded specimens prepared under ISO 1872-2 conditions. End-use qualification is required for any application involving long-term load, chemical contact, or food packaging.

    Representative physical properties of Versalis HDPE MP90
    PropertyTest methodTypical valueUnit
    Melt flow rateISO 1133-1:20229.0g/10 min
    DensityISO 1183-1:20190.960g/cm³
    Tensile stress at yieldISO 527-2:201227MPa
    Tensile elongation at yieldISO 527-2:20128%
    Flexural modulusISO 178:20191250MPa
    Charpy notched impact strength, 23°CISO 179-1/1eA3.5kJ/m²
    Vicat softening temperature, A50ISO 306126°C
    Shore D hardnessISO 86864—
    Mold shrinkage, in-flowISO 294-41.8–2.2%
    Peak melting temperature, DSCISO 11357-3133°C

    The density of 0.960 g/cm³ corresponds to a crystalline weight fraction of approximately 75–80%. This level of crystallinity governs the tensile yield stress, flexural modulus, mold shrinkage, and permeability. The melt flow rate of 9.0 g/10 min places MP90 in the higher-fluidity segment of HDPE injection grades. The trade-off is lower zero-shear viscosity and lower molar mass compared with high-molecular-weight HDPE blow molding or pipe grades, which reduces environmental stress cracking resistance and low-temperature impact energy.

    Because the melt flow rate is measured at low shear, it does not fully describe behavior in gates and runners. Capillary rheometry data for this grade should be generated at shear rates from 100 s⁻¹ to 10,000 s⁻¹ for accurate gate and runner sizing. Published data for this specific configuration is limited. The narrow molecular weight distribution typical of high-flow injection grades gives moderate shear thinning and low die swell, but also means that melt viscosity is more sensitive to batch-to-batch melt flow variation.

    Rheological and Thermal Boundaries That Govern Injection Molding

    Processing is performed on reciprocating-screw injection molding machines with a general-purpose polyolefin screw of 18:1 to 22:1 L/D and compression ratio 2.5:1 to 3.0:1. The nozzle melt temperature is normally set between 200°C and 250°C. Below 200°C, viscosity increases and cavity filling of wall sections thinner than 1.0 mm may require injection pressures beyond the capability of smaller machines. Above 280°C, thermal-oxidative degradation accelerates, producing black specks, discoloration, and molecular weight loss in hot-runner systems with long residence times.

    Mold coolant inlet temperature is typically set from 10°C to 35°C. Lower coolant temperatures reduce cooling time but increase frozen-in orientation and anisotropy of shrinkage. Cavity pressure during packing in thin-wall closure molds is typically 35–45 MPa. Clamp force is calculated by multiplying projected cavity area by expected cavity pressure and adding a 10–15% safety factor. Back pressure is generally maintained at 50–70 bar, and screw rotation on a 35 mm screw should not exceed 120 min⁻¹ to limit shear heating.

    No pre-drying is normally required when pellets are stored below 60% relative humidity. If surface condensation occurs, a hopper dryer at 70–80°C for 1–2 h removes surface moisture without pellet melting. The grade is not suitable for extrusion blow molding or large-part sheet extrusion because its low melt strength causes parison sag and insufficient die swell. Residence time at melt temperature should be kept below 10 min; if a line stops, hot-runner temperatures should be reduced to 150°C or the system purged with a higher-viscosity HDPE.

    Which Product Differences Emerge Against Blow Molding and Lower-Fluidity HDPE Grades?

    Compared with a high-molecular-weight HDPE blow molding grade with melt flow rate below 1.0 g/10 min, MP90 exhibits lower zero-shear viscosity and lower melt elasticity. It fills long injection flow paths at reduced pressure but cannot maintain parison geometry in blow molding. The environmental stress cracking resistance of MP90 is also lower because lower molar mass reduces the tie-molecule concentration that bridges interlamellar regions. For aggressive detergent or surfactant service, a bimodal high-molecular-weight HDPE with density 0.945–0.955 g/cm³ should be selected.

    Relative to a lower-fluidity HDPE injection grade with melt flow rate around 4.0 g/10 min, MP90 shortens filling time and permits thinner wall sections or higher cavity counts. The stiffness may be similar because density is comparable, but notched impact strength and ESCR are lower. The product selection between MP90 and a lower-flow grade therefore depends on whether toughness or cycle time is the limiting factor. A lower-flow grade with melt flow rate of 4–5 g/10 min can give higher notched impact and ESCR but may require higher injection pressure and longer cycle time in thin walls.

    In multi-cavity closure molds, the grade is processed in tools with 48–96 cavities. Valve-gated hot runners with gate diameters from 0.8 mm to 1.2 mm are common. Wall sections in dairy caps are often 0.6–1.2 mm. The high melt flow rate reduces pressure loss through hot-runner channels, but unbalanced runner layouts produce cavity-to-cavity mass variation. Shot-to-shot mass variation below 0.2% is a practical control limit for high-cavitation caps.

    Melt cushion is maintained between 2 mm and 5 mm. Holding pressure is usually 40–60% of peak injection pressure. Gate freeze time is established by part weight; short holding time produces sink marks and underweight parts, while excessive holding time raises cycle time and can create gate strings if the hot tip is not thermally separated.

    Because the high crystallinity of HDPE MP90 causes significant shrinkage, cooling phase design is central to cycle time. Crystallisation begins at the mold wall and propagates inward. For a wall section of 1.0 mm, cooling time is typically 3–5 s when mold coolant is at 10–15°C. For 2.0 mm sections, cooling time extends to 8–12 s. These values are starting estimates and must be confirmed by part weight stability and surface temperature measurements.

    When Thin-Wall Caps and Closures Replace Polypropylene in Dairy Packaging

    When a converter replaces polypropylene caps with HDPE MP90, mold shrinkage must be reassessed. HDPE MP90 exhibits in-flow mold shrinkage of 1.8–2.2% under ISO 294-4, whereas polypropylene injection grades typically shrink 1.0–1.5%. Core and cavity dimensions must be adjusted, and ejection systems must account for the higher HDPE shrinkage. Opening torque is lower than that of rigid polypropylene caps because HDPE has a lower dynamic coefficient of friction against itself; this may require tamper-evident bridge geometry changes.

    The material is not suitable for retort sterilization above 120°C because its Vicat softening temperature is 126°C. For hot-fill or autoclave applications, polypropylene or a high-melting HDPE/PP blend is required. The peak melting temperature of 133°C and the Vicat softening temperature of 126°C indicate that the service temperature must remain below 80–90°C for continuous load.

    Environmental Stress Cracking Resistance in Surfactant-Exposed Articles

    MP90 is not intended for long-term detergent bottles, agrochemical containers, or fuel tanks. Continuous exposure to nonionic surfactant solutions at 50°C or higher can initiate cracks at molded-in stress concentrations near gates, weld lines, and ejector pins. ESCR should be evaluated using ASTM D1693 or ISO 22088-3 with the actual contact liquid. Published data for MP90 in standard nonylphenol ethoxylate solutions is limited; qualification must be performed with the real formulation.

    For fatty acid, essential oil, or hot surfactant service, a high-molecular-weight HDPE with melt flow rate below 0.5 g/10 min and density below 0.945 g/cm³ is preferred. The higher viscosity reduces injection productivity but increases tie-molecule density and ESCR.

    Thin-wall housewares and storage trays use the flexural modulus of 1250 MPa and Shore D hardness of 64. These values support stackability and dimensional stability. In colored formulations, LDPE- or EVA-based masterbatches are let down at 2–4% by mass. The masterbatch melt flow rate must lie in the same range to avoid streaks in hot-runner systems. Regrind from cold runners can be incorporated at 10–20% in non-load-bearing articles, but the percentage must be validated by ISO 179-1/1eA testing.

    For load-bearing applications, creep is measured under ISO 899-1. MP90 is not a creep-resistant grade; continuous stress above 6 MPa at 23°C can produce progressive strain. Published creep curves for this specific grade are limited. If sustained load is present, a higher-molecular-weight HDPE or mineral-filled grade should be considered.

    For outdoor exposure, the standard MP90 grade is not UV-stable. A UV-stabilized variant or a carbon black masterbatch at 2.0–2.5% is required. Ultraviolet chain scission reduces elongation, which should be measured by ISO 527-2 after accelerated weathering under ISO 4892-2. The resin contains antioxidants for processing stability but is not formulated for long-term hot-water aging. Continuous exposure to water at 80°C can deplete stabilizers and reduce tensile elongation after prolonged exposure under ISO 188 aging.

    Assessing Food-Contact and Regulatory Compliance Across Jurisdictions

    Compliance must be verified for the final article. Polyethylene homopolymers are commonly assessed under European Union Regulation (EC) No 10/2011. The overall migration limit is 10 mg/dm². In the United States, the resin may be covered by 21 CFR 177.1520 as an olefin polymer, subject to use conditions and additive restrictions. Under REACH 1907/2006, the ethylene monomer and additives must be registered and the article should not contain substances of very high concern above 0.1% by weight. RoHS Directive 2011/65/EU and Delegated Directive (EU) 2015/863 restrict cadmium, lead, mercury, hexavalent chromium, PBB, and PBDE in homogeneous materials to 0.1% by weight; testing follows the IEC 62321 series.

    Regulatory and testing framework matrix
    FrameworkStandard or clauseRelevant limit or status
    REACHRegulation (EC) 1907/2006No SVHC above 0.1% w/w expected
    RoHSDirective 2011/65/EU and (EU) 2015/863, IEC 62321Pb, Cd, Hg, Cr6, PBB, PBDE restricted to 0.1% w/w
    EU food contactRegulation (EC) No 10/2011, EN 1186-1Overall migration limit 10 mg/dm²
    US food contact21 CFR 177.1520Olefin polymer status; condition-of-use dependent
    Mechanical testingISO 527-2, ISO 178, ISO 179-1Specimen preparation per ISO 1872-2

    The main production-line defects observed with HDPE MP90 are gate blush, sink marks, short shots, and black specks from hot-runner degradation. Gate blush is controlled by nozzle temperature and gate geometry. Sink marks are minimised by packing pressure and correct gate freeze. Black specks indicate stagnant melt in the hot-runner manifold or screw wear; purging with a similar-viscosity HDPE and cleaning the non-return valve are the usual corrections.

    The grade can be processed on machines with clamp force from 600 kN to 5000 kN depending on shot size and projected area. Small closures may run on 600–1200 kN machines; larger housewares require clamp force calculated from cavity pressure and projected area. The material can also be used in thin-wall industrial pails with integral handles, where the high melt flow rate permits filling of thick hinge sections without sinks. However, low-temperature impact is limited by the high-density homopolymer structure. Drop testing at −20°C should be conducted on actual pails because Charpy notched impact at 23°C does not predict low-temperature hinge failures.

    Top