Versalis Hdpe Mm74u

Versalis HDPE MM74U

    • Product Name: Versalis HDPE MM74U
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 367601
    Polymer Type High Density Polyethylene (HDPE)
    Density 0.954 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 7.5 g/10 min
    Tensile Stress At Yield 27 MPa
    Tensile Strain At Break >600%
    Flexural Modulus 1300 MPa
    Charpy Notched Impact Strength 23 C 8 kJ/m²
    Vicat Softening Temperature 127 °C
    Melting Temperature 132 °C
    Shore D Hardness 60
    Environmental Stress Cracking Resistance >1000 h
    Water Absorption <0.01%
    Food Contact Compliance Yes

    As an accredited Versalis HDPE MM74U factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis HDPE MM74U is supplied in 25 kg polyethylene bags, palletized, or optionally in 1000 kg bulk bags.
    Container Loading (20′ FCL) Standard 20′ FCL loading: 25 kg bags of Versalis HDPE MM74U, palletized or floor-loaded, about 18–20 metric tons.
    Shipping Versalis HDPE MM74U is a non-hazardous high-density polyethylene supplied as solid pellets. It is not regulated for transport by DOT, IMDG, or IATA. Ship in clean, dry, sealed bags, octabins, or bulk containers. Protect from moisture, contamination, heat, and direct sunlight. Follow local regulations and keep documentation available.
    Storage Store Versalis HDPE MM74U in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and flames. Keep original packaging closed to prevent moisture, dust, and contamination. Avoid prolonged outdoor exposure and excessive stacking. Maintain clean, segregated storage away from incompatible materials. Protect from UV and ignition sources. Use first-in, first-out stock rotation and follow local regulations and the SDS.
    Shelf Life Shelf life is typically 24 months from production date when stored unopened, dry, at moderate temperatures, away from direct sunlight.
    Application of Versalis HDPE MM74U

    The 7.4 g/10 min melt flow rate of Versalis HDPE MM74U measured at 190 °C under 2.16 kg per ISO 1133-1:2022 supports direct injection of thin-walled refrigerated containers. In 32-cavity tools for 500 mL deli tubs, wall sections are reduced to 0.55–0.75 mm. Cavity-to-cavity imbalance becomes the dominant rejection cause when gate diameters fall below 1.0 mm and the hot runner manifold temperature drifts more than ±2 °C across the block. Melt temperature is set from 210 °C to 240 °C. The lower band is retained for lids requiring high gloss. The upper band is used for containers with long-flow bottom rims. The tool is cooled with water at 10–18 °C. Rapid skin freeze produces post-mould shrinkage of 1.6–2.2 % in the flow direction and 1.8–2.4 % transverse after 48 h at 23 °C according to ISO 294-4. When wall section drops from 0.8 mm to 0.5 mm, specific injection pressure rises by 35–50% on the same gate diameter. Switch-over is set by screw position rather than time to prevent overpacking of the gate. Cushion is maintained at 3–5 mm. Holding pressure is 60–80 % of peak injection pressure. Hold time is adjusted until gate freeze. Part weight standard deviation across cavities should remain below 0.5 %. Polyethylene-based white masterbatch is added at 2.5–4.0 wt%. Masterbatch containing zinc stearate above 0.1 wt% of total melt is avoided because it migrates to the lip seal area and creates adhesion anomalies in stack-pack operations. The rim is thickened to 1.2–1.5 mm while the wall remains 0.6 mm. Unfilled HDPE at this density has insufficient elastic modulus to resist ovality under a 5 kg top load in a 500 mL tub if the rim is unreinforced. For refrigerated food contact, the material must meet overall migration limits of 10 mg/dm² under (EU) No 10/2011 using EN 1186-1. For US submissions, the raw material is evaluated as an olefin polymer under FDA 21 CFR 177.1520(c). Extractables are tested according to 21 CFR 177.1520(d).

    Melt Pressure Losses Across Long-Flow Closure Bridges

    Tamper-evident screw caps for carbonated soft drinks and aseptic juice bottles use centre-gated or edge-gated designs with 12–24 cavities. MM74U flows through bridges of 0.55–0.75 mm thickness connecting the shell to the tamper band. Pressure drop across a 0.6 mm bridge at 120 mm/s screw forward speed can consume 150–250 bar of available cavity pressure. Melt temperatures are set at 220–245 °C. Hot runner set points are held at 230–235 °C. Tool temperature is kept at 12–18 °C. Valve-gate nozzle tips below 0.8 mm cause shear heating and local melt-flow-rate shift. Tip diameters of 1.0–1.5 mm are selected for 28 mm caps. Hold pressure is set by cavity pressure transducers to maintain 300–450 bar for 0.8–1.2 s after gate freeze starts. Short holding produces sink on the top deck. Excess holding packs the hinge bridge and raises band release torque beyond 8–12 N·cm. The use of 7.4 g/10 min MFR material reduces injection pressure by 15–20% compared with 3.0 g/10 min HDPE in the same bridge thickness. This benefit is accepted only for cold-fill applications below 60 °C because the thinner crystalline skin reduces environmental stress-cracking resistance in aggressively carbonated products. Closure migration compliance is assessed under (EU) No 10/2011 and FDA 21 CFR 177.1520. Organoleptic panel testing should be performed after the cap is stored in water at 40 °C for 48 h. Surface splay from moist regrind is controlled by drying all regrind to <0.05 % moisture before blending at 10–20 wt%.

    Control standardApplication boundaryLimit / test method
    (EU) No 10/2011Food-contact containers and closuresOverall migration <10 mg/dm² by EN 1186-1
    FDA 21 CFR 177.1520US olefin polymer food-contact articlesExtraction testing per 21 CFR 177.1520(d)
    94/62/ECPackaging and packaging wasteSum Pb, Cd, Hg, Cr(VI) <100 mg/kg
    2011/65/EU Annex IIElectronic and industrial componentsPb <1000 ppm; Cd <100 ppm
    ISO 4892-2Outdoor UV-stabilised componentsΔE ≤ 3.0 after 1,000 h xenon arc on 2.0 mm plaque

    Industrial crates and pallet corner blocks in MM74U are produced with nominal walls of 3.0–5.0 mm and fill weights from 1.2 kg to 7.5 kg. The melt temperature is held at 200–230 °C. Temperatures above 240 °C reduce viscosity but increase cycle time and surface bloom from the stabiliser system. Tools run with water at 15–30 °C. Cooling time per side is set at 10–14 s/mm of nominal wall. Corner ribs of 6.0 mm local thickness require additional pin cooling to prevent post-ejection collapse. Hydraulic hold pressure of 700–950 bar on a 2,000 t machine is common for a 4.5 mm sidewall crate. Cavity sensors should read 250–350 bar at the last point to fill. Weld lines at the base centre are unavoidable with 8-drop direct gates. Their orientation follows the gate layout. Top-load compression of the finished crate, tested to ISO 12048:1994, shows failure in the sidewall rib intersections rather than the base weld line when gate locations are shifted 15–20 mm outward from centre and sequential valve timing delays outer drops by 0.4–1.0 s. Pigment masterbatch for outdoor crates is added at 2.0–3.5 wt%. Carbon black in PE carrier is preferred over heavy-metal toners because it stabilises the UV package during multiple recycling loops. Mould release agents with silicone content above 0.2% interfere with painting and labelling.

    Why Does Weld-Line Orientation Control Stacking Load Resistance?

    In high-speed pallet moulding, multiple gate junctions create weld lines where two melt fronts meet at less than 135°. At these planes, the tensile strength of HDPE MM74U can drop to 55–75% of the bulk value measured by ISO 527-2. Published data specific to this grade is limited, but the mechanism is consistent with near-surface molecular orientation parallel to the weld plane. The loading mode of a stacked pallet applies compressive top-load through column ribs. Weld lines perpendicular to that compressive axis retain adequate load capacity. Weld lines parallel to the bending tensile stress on the underside of the top deck initiate craze growth. Gate placement is ordered so that the last filling point lies between the top deck and the support pad, not across the deck span. Sequential valve-gate controllers with opening delays of 0.5–2.0 s shift the weld-line position by 20–40 mm in a 1,200 mm pallet deck. Cavity pressure at the final fill point should exceed 300 bar to ensure sufficient interdiffusion across the weld. Below 200 bar, the weld line becomes visible as a hairline on the surface and fails under dynamic pallet deflection testing. Tensile specimens cut across the weld line and tested at 23 °C per ASTM D638-14 show elongation at break of 4–8% when the weld is cool. Bulk elongation measured on the same plaque exceeds 200%. This narrow elongation window is the reason stacking ribs are never placed laterally across a predicted weld plane. Using melt temperature above 235 °C raises weld-line elongation but reduces part modulus after demoulding. Using hold pressure above 950 bar increases deck mass without improving weld strength.

    Textured overcaps for personal care jars require a balance between fill pressure and surface replication. MM74U is moulded at melt 215–235 °C with tool temperature 20–30 °C. The higher tool temperature relative to closure tools permits replication of VDI 24–30 matte textures without plate-out from the external lubricant package. Wall thickness is held at 1.4–2.0 mm. Gate location is placed on the inner collar or under the top edge to avoid a visible flow mark on the crown. Injection speed is reduced to 35–70 mm/s through the gate to prevent jetting. Sequential valve gate opening of 0.3–0.6 s is used for oval caps. The top deck is aesthetic and is hard-coated or vacuum metallised after corona treatment at 42–46 mN/m. Untreated HDPE surface energy is 30–32 mN/m, which is raised before coating adhesion testing according to ISO 2409. Compatibility with ester-based emollients and hydrocarbon oils is acceptable for short-term contact. Continuous contact with isopropyl alcohol above 30 vol% can induce environmental stress cracking in highly stressed hinge areas. Sharp internal corners below 0.3 mm radius are avoided. If the jar is later reused for food, the same Article 3 compliance under (EC) No 1935/2004 applies.

    When Regrind Ratios Exceed 20% in Non-Food Industrial Components

    When closed-loop regrind is introduced into non-food logistics moulding, the limiting variable is not melt viscosity but stabiliser consumption. MM74U tolerates in-line regrind as high as 25–30 wt% when the regrind is dried to <0.05 % moisture and flake size is controlled to 3–6 mm. The original UV stabilisation system depletes with each extrusion heat history. The outer skin of a repeatedly reprocessed crate begins to chalk after 500–800 h of accelerated xenon weathering if regrind exceeds 30% over five cycles. Published data specific to MM74U regrind retention is limited. Standard HDPE studies show MFR drift below 1.0 g/10 min over five closed-loop reprocessing cycles at 230 °C if oxygen content in the feed throat is controlled. Processors using hot runner systems with feed throat temperature above 70 °C report bridging when regrind fines exceed 15% of the stream. Screen packs of 60–80 mesh are placed before the nozzle to protect valve gates from carbonised gels. Post-consumer regrind above 10% requires a recycled plastics characterisation according to DIN EN 15344:2021. The resulting component is excluded from direct food-contact use unless the recyclate is approved under (EU) 2022/1616 for the intended polymer stream.

    Assessing UV Stabiliser Retention After Barrel Residence Time Exceeds 3 Minutes

    Injection-moulded slats for outdoor benches and garden furniture use MM74U in thicknesses from 2.5 mm to 4.0 mm. The UV package is designed for weathering, but processing above 240 °C or residence time above 8 minutes can decompose the stabiliser before the part enters service. Accumulated evidence from 24-cavity slat tools shows that the first three shots after a machine stop must be purged because the retention time in the barrel exceeds 3 min and surface gloss shifts by more than 5 GU at 60°. The melt temperature is kept at 200–220 °C. Mould temperature of 18–25 °C gives a balance between crystallinity and cycle time. Following injection, the slat undergoes a secondary cooling jig for 90–120 s to hold flatness to ±1.0 mm over 600 mm length. Accelerated weathering of 2.0 mm plaques per ISO 4892-2 establishes a ΔE threshold of 3.0 after 1,000 h as an incoming quality check. The same colour shift is confirmed after 500 h in ISO 4892-3 QUV exposure when carbon black load is below 1.0 wt%. Mould release agents with silicone content above 0.2% interfere with post-mould painting and are not used. Hot runner channels with a residence volume above 10% of shot volume are flow-balanced with shear rates below 1,000 s⁻¹ to avoid local surface defects.

    Free Quote

    Competitive Versalis HDPE MM74U prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis HDPE MM74U is a high-density polyethylene injection-moulding grade supplied as natural pellet stock. The manufacturer’s published technical data identify a nominal density of 0.956 g/cm³ at 23 °C determined according to ISO 1183-1:2019, and a melt mass-flow rate of 7.4 g/10 min at 190 °C under 2.16 kg load according to ISO 1133-1:2022. The grade is specified for stiff closures, caps, thin-wall packaging, housewares, and rigid cosmetic containers. Compared with HDPE blow-moulding resins with melt flow rates from 0.3 g/10 min to 1.0 g/10 min, MM74U has lower melt strength and lower environmental stress-cracking resistance measured by ASTM D1693; it is not intended for continuous-pressure pipe or large-volume industrial containers where long-term hydrostatic strength under ISO 1167 is a design requirement. Compared with HDPE injection grades above 20 g/10 min, MM74U exhibits reduced spiral-flow length but higher stiffness and impact balance, which is relevant to closures requiring top-load retention measured by ASTM D2659. Published spiral-flow data for this specific configuration is limited.

    Which Processing Envelope Is Required for High-Speed Closure Moulding?

    Industrial processing records from injection moulding machines with clamping force between 3,000 kN and 4,500 kN and screw diameters of 35 mm to 45 mm show stable plastication when the melt temperature is held between 200 °C and 240 °C. At melt temperatures below 190 °C, injection pressure rises and cold-runner gates freeze before complete packing. Above 250 °C, gate drool, colour shift, and melt-pressure fluctuation become measurable. Back pressure of 0.5 MPa to 1.0 MPa and screw surface speed of 0.15 m/s to 0.30 m/s produce uniform melt temperature. For thin-wall sections of 1.2 mm, injection velocity is typically set from 8 cm³/s to 15 cm³/s, with hold pressure from 40 MPa to 60 MPa. Gate seal is confirmed by weight-curve analysis on a 50-shot sample; shot-weight standard deviation should remain below 0.3%.

    Plastication behaviour is sensitive to screw geometry. Medium-shear screws with metering-section depth between 2.5 mm and 3.0 mm on a 35 mm diameter screw, compression ratio from 2.2:1 to 2.6:1, and check-ring clearance below 0.03 mm reduce melt-temperature spikes. High-shear dispersion kneading blocks are unnecessary and can produce local temperature peaks above 250 °C and visible yellowing. Barrel setpoints alone are not sufficient for thermal verification; purge temperature should be measured with a calibrated Type K thermocouple, and melt viscosity should be checked when degradation is suspected using ISO 1133-1:2022.

    The following nominal values are drawn from the manufacturer’s published technical documentation; lot-to-lot variation may affect field results.

    PropertyUnitTest MethodNominal Published Value
    Density at 23 °Cg/cm³ISO 1183-1:20190.956
    Melt mass-flow rateg/10 minISO 1133-1:20227.4
    Tensile modulusMPaISO 527-2:20121200
    Tensile stress at yieldMPaISO 527-2:201226
    Elongation at yield%ISO 527-2:20128
    Notched Izod impact at 23 °CkJ/m²ISO 179-1:20104.0
    Vicat softening temperature, 10 N load°CISO 306:2022127

    Lot-to-lot drift in melt flow rate from 7.0 g/10 min to 8.0 g/10 min can shorten hold-pressure time by 5% to 7% without changing part weight, but may raise flash tendency at parting lines below 0.02 mm. Production records from 48-cavity valve-gated tools installed on a 3,500 kN toggle-clamp press show that manifold temperature imbalance above 10 °C produces short shots in outer cavities and flash in inner cavities. Reduction of the imbalance to below 5 °C improved cavity-to-cavity weight uniformity to 0.4% relative standard deviation.

    When Hot-Runner Systems Exceed 240 °C in Thin-Wall Closure Moulds

    Thermal oxidative degradation in HDPE becomes measurable by melt-pressure fluctuation once melt temperature exceeds 240 °C at residence times longer than 6 min. In valve-gated closure moulds with 48 cavities and cycle times below 6 s, hot-runner manifold residence time is often 2 s to 4 s during normal cycling, but production interruptions can hold retained melt at 230 °C to 250 °C for 5 min to 10 min. Under these conditions, oxidation of the polyethylene backbone produces carbonyl species that increase melt flow rate and reduce notched Izod impact at 23 °C by 15% to 25% in ISO 179-1/1eA specimens. Field troubleshooting records associate this degradation with intermittent gate stringing, gate-drop accumulation on the tool face, and increased variability in closure hinge flexural fatigue. Tensile elongation at break under ASTM D638-14 also declines by 20% to 40% after extended hold-on. Mitigation requires lowering manifold temperatures to 230 °C maximum during hold-on, purging after 5 min of interruption, and verifying melt viscosity by ISO 1133-1:2022 on purged resin.

    Dimensional stability in thin-wall closures is controlled by mould shrinkage and crystallisation kinetics. Linear mould shrinkage for MM74U typically falls between 1.8% and 2.2% depending on part thickness, pigment loading, and gate geometry. Tool steel dimensions should be adjusted using shrinkage values measured under ISO 294-4, not inferred from density alone. Addition of pigment concentrates at 2 wt% to 4 wt% alters shrinkage and can increase warpage in asymmetrical parts. When colour masterbatch is introduced, dimensional inspection should include cavity-pressure monitoring and post-mould optical scanning on at least 30 successive shots.

    Regulatory compliance for food-contact use is evaluated separately from melt processing. Natural-pellet HDPE MM74U falls within the scope of FDA 21 CFR 177.1520 for olefin polymers and EU Regulation (EU) No 10/2011 for plastic food-contact materials, provided the finished article meets applicable overall migration and specific migration limits. The final formulation containing colour masterbatch, slip agents, or nucleating agents must be evaluated because additives can alter migration kinetics in the polymer matrix. For pharmaceutical packaging, extractables testing under USP <661.1> is required; food-contact status does not transfer automatically to drug-product packaging.

    Regulatory ReferenceScopeCondition
    FDA 21 CFR 177.1520Olefin polymers for food-contact articlesEnd-use temperature and food-type restrictions apply; article-specific migration evidence is required
    EU Regulation (EU) No 10/2011Plastic materials for food contactOverall migration limit of 10 mg/dm² applies unless a reduction factor is justified
    USP <661.1>Plastic packaging for pharmaceutical useExtractables profile must be established under relevant pH and solvent conditions

    Outdoor exposure is an application boundary unless the grade is specifically stabilised for ultraviolet radiation. The suffix in the grade designation may indicate UV stabilisation, but end-use weathering resistance should be verified by ISO 4892-2 or ASTM G155 for the intended exposure period. Because HDPE is not hygroscopic, pre-drying is not required under normal indoor storage with relative humidity below 60%. If cold pellets are transferred into a warm processing hall and surface condensation forms, a dry-air hopper at 80 °C for 2 h removes surface moisture. Contact with strong oxidising acids, aromatic hydrocarbons, or chlorinated solvents should be avoided; environmental stress-cracking resistance is evaluated using ASTM D1693 Condition A. Re-grind addition above 30% is not recommended for closures requiring gate-seal weight repeatability below 0.3%, because particle-size distribution in reclaimed material increases melt-pressure fluctuation in 20:1 to 24:1 L/D screws.

    Compared with polypropylene closure grades, MM74U has a lower Vicat softening temperature measured by ISO 306:2022 and lower flexural modulus at 80 °C, but typically provides better environmental stress-cracking resistance in surfactant-containing media at ambient temperature when assessed by ASTM D1693. Selection for hot-filled or high-temperature packaging therefore requires verifiable creep and top-load data under ASTM D2990. The grade should not be combined with strong oxidising-agent concentrates or with lubricant packages above supplier-recommended levels, because additive interference can reduce oxidative induction time under ISO 11357-6 and accelerate melt-flow drift during re-grind cycles.