Versalis Hdpe Mm74

Versalis HDPE MM74

    • Product Name: Versalis HDPE MM74
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 508195
    Density 0.960 g/cm3
    Melt Flow Rate 190 C 2 16 Kg 7.5 g/10 min
    Tensile Stress At Yield 28 MPa
    Tensile Strain At Yield 9%
    Tensile Strain At Break >600%
    Flexural Modulus 1400 MPa
    Charpy Notched Impact Strength 23 C 6 kJ/m2
    Charpy Notched Impact Strength 20 C 4 kJ/m2
    Vicat Softening Temperature 125°C
    Heat Deflection Temperature 0 45 Mpa 75°C
    Shore D Hardness 65
    Melting Temperature 130°C
    Mold Shrinkage 2.0%
    Water Absorption <0.01%
    Volume Resistivity >10^15 ohm·cm
    Dielectric Constant 1 Mhz 2.3
    Dissipation Factor 1 Mhz 0.0002
    Thermal Conductivity 0.4 W/m·K
    Coefficient Of Linear Thermal Expansion 1.2E-4 /°C
    Specific Heat Capacity 1.9 kJ/kg·K

    As an accredited Versalis HDPE MM74 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis HDPE MM74 is supplied in 25 kg polyethylene bags, palletized, or 1,000 kg bulk bags for industrial handling.
    Container Loading (20′ FCL) 20' FCL loaded with Versalis HDPE MM74 in 25 kg PE bags on pallets, shrink-wrapped and securely stowed for ocean transport.
    Shipping Versalis HDPE MM74 is shipped as a non-hazardous polymer in 25 kg polyethylene bags, palletized and stretch-wrapped, or in bulk bags/octabins. It is transported in clean, dry, covered trucks or containers. No UN number or dangerous-goods labels are required. Store away from heat, direct sunlight, moisture, and contamination.
    Storage Store Versalis HDPE MM74 polyethylene resin in a clean, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep bags or containers sealed and palletized to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and extreme temperatures. Use first-in, first-out stock rotation, and follow manufacturer and SDS storage guidance.
    Shelf Life Versalis HDPE MM74: approximately 24 months from production date when stored dry, cool, away from direct sunlight and heat.
    Application of Versalis HDPE MM74

    In beverage cap manufacturing, MM74 is introduced at 95–98 wt% of total compound mass, with 2–5 wt% of a polyethylene-based color masterbatch and, for carbonated soft drink closures, 0.05–0.15 wt% of an erucamide slip masterbatch selected to bring cap removal torque into the 0.8–2.4 N·m band after 24 h on filled bottles. Grade acceptance on high-speed cap lines includes melt flow rate testing under ISO 1133-1:2022 at 190 °C/2.16 kg, with production-lot variation typically between 7.0 g/10 min and 8.0 g/10 min, and density verification under ISO 1183-1 at 0.960–0.965 g/cm³. Processing is carried out on injection moulding machines with 48–96 valve-gated cavities, screw L/D ratio of 22:1, melt temperature 220–240 °C, and chilled water at 8–12 °C; cycle times below 6 s are reported in 96-cavity lines, but cavity-to-cavity fill imbalance can reach 0.3–0.6 wt% when valve-gate stem wear is not corrected. The grade conforms to food-contact requirements under FDA 21 CFR 177.1520 for olefin polymers and EU Regulation 10/2011, with overall migration below 10 mg/dm² when tested under EN 1186-1; converters additionally verify organoleptic neutrality for water-contact closures under EN 1622. Finished articles include tamper-evident closures for carbonated soft drinks, flat caps for bottled water, and aseptic dairy closures.

    What Melt Temperature Window Minimizes Warpage in Thin-Walled Dairy Spread Containers?

    For thin-walled injection-moulded dairy spread containers and deli lids, MM74 is dry-blended at 97.0–99.5 wt% of total compound mass with 0.1–0.3 wt% external polyolefin processing aid and 1.5–3.0 wt% titanium dioxide white masterbatch; LLDPE impact modification is limited to 2–4 wt% when hinge-flexural fatigue resistance is required, but is excluded from stackable tub bodies because it reduces side-wall crush stiffness. The downstream process uses a 2+2 stack mould with mould coolant at 12–18 °C and melt temperature 190–215 °C; the threshold for dimensional control is the maximum temperature difference between mould surface and cooling water inlet, which should not exceed 6 °C across the cavity block. Exceeding this range produces corner warpage and rim ovality above 0.8 mm on a 500 ml tub, while lower melt temperatures reduce sink marks but increase moulded-in stress at the rim. Food-contact compliance is maintained under EU 1935/2004, EU 10/2011, and FDA 21 CFR 177.1520, with specific migration testing conducted according to EN 1186-2 and overall migration below 10 mg/dm². Terminal products include one-piece cylindrical margarine tubs, round dairy spread containers, delicatessen lids, and tamper-evident food boxes.

    When Returnable Industrial Pallets Are Moulded from MM74 with Post-Industrial Regrind

    Returnable pallets and distribution trays are formulated from 60–80 wt% virgin MM74, 20–40 wt% post-industrial HDPE regrind sourced from the same pallet production line, 0.15–0.30 wt% hindered phenolic antioxidant masterbatch, and 0.05–0.15 wt% phosphite process stabilizer to inhibit gel formation during barrel residence times up to 35 min at changeovers. The injection moulding process uses large-tonnage machines with clamp forces from 15,000 kN to 30,000 kN and shot capacities from 8 kg to 25 kg; melt temperature is held at 230–250 °C, but the controlling variable is regrind moisture. If moisture exceeds 0.05 wt%, steam expansion at melt temperatures above 230 °C creates splay and internal voids at rib intersections, so pre-drying at 80 °C for 2 h is used when regrind has been stored at relative humidity above 60 % RH. Physical durability is verified under ISO 8611-1:2011 for flat pallets, ISO 8256 for tensile impact, and ASTM D638-22 for weld-line tensile strength; food-contact pallets for dry grocery logistics are evaluated under EU 10/2011 and FDA 21 CFR 177.1520. Finished articles include 1,200 mm × 1,000 mm returnable pallets, nestable distribution trays, and folding dairy crates.

    In agricultural compression fittings for low-pressure drip and micro-irrigation laterals, MM74 is used at 88–94 wt% of total compound mass together with 2.0–2.5 wt% carbon black masterbatch for UV stabilisation, 0.1–0.3 wt% high-molecular-weight hindered amine light stabilizer, and 4–8 wt% PE100-grade HDPE to increase slow crack growth resistance under hoop stress. The parts are injection moulded on multi-cavity family tools with hydraulic gate systems, melt temperature 210–230 °C, mould temperature 20–30 °C, and screw back pressure 0.5–1.0 MPa; the main production defect is a weak knit line where melt fronts reunite downstream of spigot cores, and moulders raise the core temperature to 40 °C to delay flow-front freezing. Compliance is referenced to ISO 4427-3:2019 for polyethylene pressure fittings, EN 12201-3 for water supply systems, and ISO 10508 for service temperature and pressure classification; potable-water contact formulations are tested under EN 12873-1 for influence on water quality. Terminal products include 16–32 mm compression couplings, barbed fittings for porous hose, and end-stop plugs for lateral irrigation lines.

    Insulated Cable Duct Joints and HDPE Junction Box Bodies

    For non-current-carrying electrical accessories such as junction box bodies and cable duct joints, MM74 is processed at 90–95 wt% of total compound mass with 5–10 wt% mineral-filled HDPE masterbatch to control linear shrinkage to 0.8–1.2 % in wall thicknesses from 2.0 mm to 4.0 mm; flame-retardant masterbatches are not added unless the application requires glowing-wire testing, because halogen-free FR packages reduce Charpy notched impact strength and may move the formulation outside the producer’s narrow molar mass distribution tolerance. Processing on small to medium injection moulding machines with screw L/D ratios of 20:1–25:1, melt temperature 220–240 °C, and mould temperature 15–25 °C requires rib-to-wall thickness ratios below 0.6 to prevent sink marks at screw bosses; the observed failure mode in production is cracking at thin-walled snap-fit tabs when mould release draft angle is less than 1°. Electrical enclosure compliance is assessed under IEC 62208 for empty low-voltage switchgear housings, with flammability rated at UL 94 HB at 1.5 mm; material conformance includes RoHS Directive 2011/65/EU and REACH Regulation (EC) No 1907/2006. Terminal articles include cable duct junction boxes, terminal block enclosures, and conduit inspection elbows.

    The injection moulding of institutional and light industrial containers from MM74 uses a formulation of 85–95 wt% virgin MM74, 5–15 wt% cleaned post-consumer HDPE recyclate, 0.2–0.5 wt% masterbatch lubricant/dispersant, and color masterbatch at 1.5–3.0 wt%. Medium-tonnage injection moulding machines supply clamp force sufficient to provide 3.0–4.5 kN/cm² of projected area, melt temperature 210–240 °C, and mould coolant temperature 10–20 °C; cooling time for a 20 L pail with sidewall thickness 2.5 mm is 18–25 s, and insufficient mould breathing causes vacuum drag marks on the bucket floor due to poor air evacuation at the end of fill. Drop impact is checked at -20 °C under ASTM D5276, and stacking performance is verified under ISO 2234 for static compression. For containers intended for dangerous goods, UN certification is carried out under ADR 6.5.2; food-contact buckets comply with EU 10/2011 and FDA 21 CFR 177.1520. Terminal products include 5–25 L pails with tear-tab lids, industrial waste bins, and institutional storage buckets.

    Free Quote

    Competitive Versalis HDPE MM74 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis HDPE MM74 is a high-density polyethylene injection-molding grade supplied by Versalis S.p.A. The published technical data for the grade list a nominal density of 0.964 g/cm³ determined according to ISO 1183-1 and a melt mass-flow rate of 8 g/10 min at 190°C with a 2.16 kg load according to ISO 1133-1. The resin is characterized by a narrow molecular weight distribution and is intended for rigid injection-molded articles in which high stiffness, low cycle time, and consistent mold filling are the controlling design requirements. Typical application areas include thin-wall packaging, caps and overcaps, household articles, toys, pails, and small industrial components. The comparatively high melt flow permits short injection times and multi-cavity filling, but it also places limits on environmental stress-cracking resistance and notched impact strength relative to high-molecular-weight HDPE grades used in blow molding.

    The primary mechanical values are determined on injection-molded or compression-molded specimens. Tensile stress at yield is reported as 28 MPa when tested on ISO 527-2 Type 1A specimens at 23°C and 50 mm/min. Tensile strain at yield is 9%. Flexural modulus according to ISO 178 is 1300 MPa at 2 mm/min. The Vicat softening temperature under ISO 306/A50 is 126°C, and Shore D hardness under ISO 868 is 65. The density of 0.964 g/cm³ indicates high crystallinity, which contributes to the elevated modulus but also increases the tendency for post-mold shrinkage and anisotropic dimensional change in thick sections. Published capillary rheometry data for this specific grade are limited; mold-filling simulation should therefore use viscosity curves generated under ISO 11443 at melt temperatures of 220°C, 240°C, and 260°C rather than relying on a single-point melt flow value.

    What Distinguishes MM74 from High-Molecular-Weight Blow-Molding Grades?

    The principal differentiation is melt flow. High-molecular-weight blow-molding HDPE grades are commonly specified with melt mass-flow rates below 1 g/10 min to provide parison melt strength and impact toughness. MM74, with an MFR of 8 g/10 min, exhibits significantly lower melt viscosity and can fill thin sections at reduced injection pressure. This process advantage is offset by lower environmental stress-cracking resistance and reduced notched impact strength. High-molecular-weight blow-molding grades often show notched Charpy impact values above 15 kJ/m² at 23°C under ISO 179-1/1eA because their higher molecular weight increases the density of load-bearing tie molecules. MM74 is therefore suited to rigid packaging and closures but is not appropriate for large drums, fuel tanks, or pressure vessels where long-term ductility and slow-crack-growth resistance are critical. The grade also differs from lower-density HDPE copolymers: its higher density of 0.964 g/cm³ raises flexural modulus to 1300 MPa, whereas many 0.950 g/cm³ HDPE copolymer grades exhibit lower modulus and better environmental stress-cracking resistance.

    Compared with polypropylene homopolymers of similar melt flow, MM74 has a lower Vicat softening temperature of 126°C and lower room-temperature flexural modulus than some high-crystallinity PP grades. In exchange, high-density polyethylene typically retains better low-temperature ductility and more predictable behavior in aqueous detergent environments. For hot-fill packaging or autoclave sterilization above 121°C, MM74 is not recommended because stiffness declines as the temperature approaches the Vicat boundary. The product should not be used as a pressure-pipe material: no long-term hydrostatic strength classification under ISO 9080 is published for this grade.

    In the broader HDPE injection-molding range, higher-flow grades with MFR values above 20 g/10 min improve thin-wall filling but sacrifice stiffness and environmental stress-cracking resistance further. Lower-flow grades with MFR values below 4 g/10 min provide better impact behavior but require higher injection pressure and longer cycle times. MM74 occupies an intermediate position, providing a balance between processability and rigidity for general-purpose thin-wall injection molding. For molders running multi-cavity tools with long flow paths, the difference between MM74 and a low-flow HDPE appears on the injection pressure curve: the lower melt viscosity reduces hydraulic pressure demand but also shortens the packing window because the gate freezes more quickly.

    Batch-to-batch variation in melt flow rate is controlled within the normal repeatability limits of ISO 1133-1 for this material class. However, switching between lots may require adjustment of switch-over position or hold pressure because minor shifts in melt flow alter packing behavior in thin-wall tools. Processors should record melt temperature at the nozzle rather than relying solely on barrel set points. Nozzle melt-temperature variation above ±5°C can produce visible dimensional drift in thin-wall containers, even when the part weight remains within a narrow control band.

    When Thin-Wall Injection Molding Dictates Cooling and Dimensional Stability

    For parts with nominal wall stock at or below 1.2 mm, melt temperature and mold temperature must be controlled together. The recommended melt temperature range is 220°C to 250°C. Below 210°C, injection pressure rises and short shots may appear in high-cavitation tools. Above 260°C, oxidative degradation may shift the melt flow rate and produce yellowing, odor, or surface splay. A mold temperature between 30°C and 50°C generally balances surface quality, shrinkage, and cycle time. Lower mold temperatures reduce cooling time but freeze weld lines more aggressively, increasing the probability of brittle failure at knit lines. Higher mold temperatures improve dimensional repeatability but can extend cycle time beyond practical limits for thin-wall packaging. The cooling time requirement is controlled by part thickness and the thermal diffusivity of HDPE; in 2 mm wall sections, cooling times are typically in the range of 8 s to 15 s depending on mold temperature and coolant flow.

    Pre-drying is not routinely required. If pellets are stored in outdoor silos or exposed to condensation, surface moisture can cause splay and should be removed by drying at 70°C to 80°C for 1 h to 2 h in a desiccant dryer. Processors operating 1000 kN to 1500 kN hydraulic injection machines with general-purpose polyolefin screws of 20:1 to 24:1 L/D have observed that screw-recovery interruptions and excessive barrel residence time cause melt-temperature variation and dimensional drift. If the machine is stopped for more than 5 min at a melt set point of 240°C, purging before restart is recommended. The barrel should be kept moving during routine interruptions, and the rear zone should be maintained below 160°C to prevent premature melting and bridging in the feed throat.

    The processing window for this grade is not a narrow thermal plateau of a few degrees; the critical constraints are residence time, moisture, and shear heating. High screw speeds and high back pressure can raise melt temperature above the set point by 10°C or more. For a 22:1 L/D general-purpose polyolefin screw, screw surface speed is commonly maintained in the range of 0.3 m/s to 0.6 m/s. Back pressure is typically set between 0.5 MPa and 1.5 MPa. Excessive back pressure increases melt temperature and reduces plasticating capacity. Injection velocity should be set to produce a fill time of 0.3 s to 0.8 s for wall thicknesses near 1.2 mm; fill times above 1.5 s can cause flow marks and premature ice formation in the gate area.

    Mold shrinkage for HDPE of this density class is geometry-dependent and is typically 1.5% to 2.5% in the flow direction and 1.8% to 2.8% transverse. Dimensional inspection should be delayed 24 h to 48 h after molding because post-molding crystallization continues at ambient temperature. Warpage in rectangular containers is commonly driven by differential shrinkage between flow and transverse directions. Gate placement at the thickest section, uniform cooling circuits, and balanced runner systems reduce this distortion. For parts with multiple gates, weld lines should be located away from load-bearing areas; high-flow HDPE grades develop lower weld-line strength because short relaxation times reduce molecular interdiffusion across the flow front.

    Published typical property data for Versalis HDPE MM74
    PropertyTest methodUnitValue
    DensityISO 1183-1g/cm³0.964
    Melt mass-flow rate, 190°C/2.16 kgISO 1133-1g/10 min8
    Tensile stress at yieldISO 527-2MPa28
    Tensile strain at yieldISO 527-2%9
    Flexural modulusISO 178MPa1300
    Charpy notched impact strength, 23°CISO 179-1/1eAkJ/m²4
    Vicat softening temperature, A50ISO 306/A50°C126
    Shore D hardnessISO 868—65

    Environmental Stress-Cracking and Chemical Exposure Constraints

    Environmental stress-cracking resistance in high-density polyethylene is governed by molecular weight, short-chain branching, and cooling-induced crystallinity. Because MM74 is a high-flow grade with a density of 0.964 g/cm³, its environmental stress-cracking resistance is lower than that of medium-molecular-weight HDPE copolymers. Applications involving continuous contact with aggressive surfactants, alcohols, fats, or stressed closures should be validated under end-use conditions using ASTM D1693 or a notched constant-strain method. Published ESCR values for this grade under all specified test conditions are not available in every supplier document; users should request test data or commission comparative testing before specifying the material for detergent bottles, high-hoop-stress closures, or chemical packaging. The material is not recommended for sustained pressure service because no long-term hydrostatic strength data under ISO 9080 are published.

    Chemical resistance follows general high-density polyethylene behavior. At room temperature, the resin resists dilute acids, alkalis, and many polar solvents, but it is swollen or softened by non-polar aromatic and chlorinated solvents. Certain essential oils can induce swelling and stress cracking in thin-walled containers. Oxygen, carbon dioxide, and water-vapor transmission are lower than in low-density polyethylene but higher than in polyamide or EVOH barrier layers. For oxygen-sensitive food packaging, MM74 should function as the structural layer rather than as the sole barrier. Migration of low-molecular-weight fractions into food simulants must be evaluated for the specific conversion conditions. Under EU Regulation (EU) No 10/2011, the overall migration limit is 10 mg/dm²; specific migration limits for additives and monomers apply according to the formulation. Under 21 CFR 177.1520, olefin polymers are regulated by density and condition-of-use restrictions. The current supplier regulatory data sheet should be consulted for food-contact statements, because compliance depends on the grade formulation and pigment masterbatch used.

    Regulatory and safety references applicable to HDPE MM74 when supplied for food-contact or general-purpose use
    InstrumentScopeRelevant limit or condition
    21 CFR 177.1520Olefin polymers in food contactDensity and condition-of-use restrictions apply
    EU Regulation (EU) No 10/2011Plastic food-contact materialsOverall migration limit 10 mg/dm²; specific migration limits for additives apply
    Regulation (EC) No 1907/2006 (REACH)Registration and SVHC controlSVHC content below 0.1% w/w per candidate list
    Directive 2011/65/EU (RoHS)Electrical and electronic equipmentPb, Hg, Cr(VI), PBB, PBDE each 0.1% w/w maximum; Cd 0.01% w/w maximum

    In production, the melt should not remain at 260°C or above for more than 10 min. If a tool change interrupts production, barrel temperatures should be reduced to 150°C or the barrel should be purged with a lower-temperature polyolefin. Regrind use is permissible only when the material is clean, dry, and free of oil or grease. The regrind ratio and thermal history must be validated for the specific part because repeated heat input shifts the molecular weight distribution and reduces notched impact strength. For critical dimensions, the injection pressure profile should avoid overpacking: excessive packing can increase part weight and differential shrinkage, while insufficient packing can generate sink marks above ribs and bosses. Color and additive masterbatches should be polyethylene-compatible and evaluated for migration when the finished article is intended for food contact. If the grade is used outside the documented processing window, the resulting changes in melt flow and molecular weight may move the product outside its published specification profile.