Versalis Hdpe Mm 80 U

Versalis HDPE MM 80 U

    • Product Name: Versalis HDPE MM 80 U
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 214259
    Density 0.960 g/cm³
    Melt Flow Rate 190c 2 16kg 8.0 g/10 min
    Tensile Modulus 1500 MPa
    Tensile Stress At Yield 30 MPa
    Tensile Strain At Yield 9%
    Tensile Strain At Break 100%
    Charpy Notched Impact Strength 23c 5 kJ/m²
    Charpy Notched Impact Strength Minus30c 3 kJ/m²
    Shore D Hardness 65
    Vicat Softening Temperature 125 °C
    Heat Deflection Temperature 0 45mpa 80 °C
    Brittleness Temperature -70 °C
    Melting Temperature 135 °C
    Water Absorption <0.01%
    Volume Resistivity >10^16 ohm·cm
    Dielectric Constant 1mhz 2.3
    Uv Stabilization Yes
    Thermal Conductivity 0.40 W/m·K
    Specific Heat 1.9 J/g·°C

    As an accredited Versalis HDPE MM 80 U factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis HDPE MM 80 U is supplied in 25 kg polyethylene bags, palletized and shrink-wrapped, 40 bags per 1,000 kg pallet.
    Container Loading (20′ FCL) Versalis HDPE MM 80 U, bagged/palletized, shrink-wrapped, evenly loaded and secured in 20′ FCL containers; typical net load approximately 18–20 MT.
    Shipping Versalis HDPE MM 80 U is shipped as non-hazardous solid polyethylene pellets, typically in 25 kg PE bags on pallets, stretch-wrapped. Use clean, dry, covered trucks or containers. Protect from moisture, heat, direct sunlight, and contamination. No dangerous goods classification, UN number, or special shipping labels required.
    Storage Store Versalis HDPE MM 80 U in a cool, dry, well-ventilated area, away from direct sunlight, heat, and ignition sources. Keep original bags or containers closed, clean, and palletized off the floor. Protect from moisture and contamination. Segregate from strong oxidizers. Avoid dust accumulation. Do not expose to open flames or excessive temperatures. Follow the manufacturer’s safety data sheet and local regulations.
    Shelf Life Versalis HDPE MM 80 U shelf life: typically 12 months in original sealed packaging, away from heat, moisture, and direct sunlight.
    Application of Versalis HDPE MM 80 U

    On accumulator-head extrusion blow-moulding lines for 60–220 L tight-head drums, Versalis HDPE MM 80 U is processed with a 24:1 to 30:1 L/D barrier screw and a grooved feed section. Melt temperature measured at the die head is maintained from 185 °C to 205 °C; the mould shell is held at 10 °C to 20 °C. Shot weight is adjusted for part weight plus pinch-off and dome flash. Parison programming is configured with 10 to 20 axial points to control wall thickness from 1.8 mm at the top to 4.5 mm at the chime. Blow air pressure is set at 0.6 MPa to 0.8 MPa, and part surface temperature prior to demoulding is verified below 70 °C to prevent post-mould shrinkage outside the tolerance band. For dangerous goods packaging, the finished drum is subjected to UN Manual of Tests and Criteria Part III performance qualification, including leakproofness, hydraulic pressure, and stacking. Hydraulic test pressure is derived from the vapour pressure of the filling substance at 55 °C; stack load testing is carried out per ISO 2234 for 28 days at 40 °C after conditioning. Wall-thickness distribution is mapped by ultrasonic thickness measurement, and stress-crack resistance is assessed in 100 % Igepal CO-630 at 50 °C under ASTM D1693-15e1. Because high-molecular-weight HDPE exhibits batch-to-batch ESCR variance, the certificate of analysis should be checked for melt-flow-rate ratio and density; published data for this specific configuration is limited where recycled scrap layers exceed 15 wt% of the total shot. For food-contact liner applications, EU Regulation (EU) No 10/2011 Annex I total migration limit of 10 mg/dm² and FDA 21 CFR 177.1520(c) apply depending on food type and temperature. Regrind from dome and flash is reintroduced up to 30 wt% where type-approval permits; above this level, sidewall gloss and ESCR shift and must be revalidated on production-scale moulds.

    How Does EVOH Layer Distribution Constrain HDPE MM 80 U in Multi-Layer Fuel Tank Blow Moulding?

    Multi-layer fuel tank production uses HDPE MM 80 U as the outer skin, inner skin, and regrind carrier in six-layer coextrusion. The layer stack typically allocates 35 % to 40 % of total wall thickness to HDPE skins, 2 % to 4 % to ethylene-vinyl alcohol copolymer, and 3 % to 5 % to maleic anhydride-grafted LLDPE tie layers. Die head temperatures are set between 200 °C and 230 °C; parison die gap is controlled from 1.2 mm to 2.5 mm to maintain layer stability. If EVOH thickness falls below 2.5 % of total wall, gravimetric fuel-loss testing shows non-linear permeation increase, and compliance with evaporative emission constraints under US EPA 40 CFR Part 86 or CARB LEV III requires barrier-layer redesign or multilayer parison programming correction. The barrier layer is dried in a desiccant dryer to a dew point of −40 °C or lower because EVOH moisture uptake above 0.1 wt% generates microbubbles at the tie-layer interface and reduces interlayer adhesion. Post-moulding wall-thickness distribution is scanned by X-ray or ultrasonic systems, and T-peel adhesion between HDPE and tie layers is evaluated under ASTM D1876. Drop-impact tests at −40 °C on filled tanks follow OEM specifications that require no leakage and no structural crack at the pinch-off area; published data for this specific configuration is limited where regrind content exceeds 50 wt% of the core layer.

    Accumulator-head machines with shot capacities between 30 kg and 45 kg are used for blow-moulded 1,000 L IBC inner containers from HDPE MM 80 U. The die head is operated at 195 °C to 215 °C, and mould cooling water is maintained at 8 °C to 15 °C to control cycle time between 240 s and 360 s. A 100-point parison programmer shifts wall thickness from 4.0 mm at the top manway flange to 6.5 mm in the base transition, compensating for parison sag over shot lengths of 2.0 m to 2.5 m. The IBC inner bottle must pass the UN 31H1 qualification, including bottom lift, top lift, stack load, and drop tests at the packing-group prescribed drop height. Stack load is evaluated per ISO 12048 at 40 °C for 28 days; drop tests are performed after conditioning at −18 °C for 24 h. In service, the bottle is supported by a steel cage, so the HDPE structure must retain enough creep resistance to avoid deformation at the top valve connection under a torque of 40 N·m to 80 N·m. Weld-line strength is checked by sectioning the base pinch-off flash and performing tensile tests at 23 °C and −20 °C under ISO 527-2. When conductive or static-dissipative IBC liners are required for flammable solvent service, surface resistance of the inner wall is controlled below 10^9 Ω per IEC 61340-2-3 by addition of conductive carbon black masterbatch at 5 wt% to 8 wt%; low-temperature impact strength is then reduced and must be revalidated against the drop test requirement.

    Application segmentCritical propertyTest methodEquipment or process parameter
    Tight-head drumsStress-crack resistanceASTM D1693-15e1100 % Igepal, 50 °C
    Multi-layer fuel tanksBarrier layer distributionGravimetric fuel-loss, X-ray scanning2.5 % EVOH threshold
    IBC inner containersStack load and creepISO 1204840 °C, 28 days
    Agrochemical containersLow-temperature impactISO 2248, UN Part III−18 °C, 24 h conditioning
    Antistatic linersSurface resistanceIEC 61340-2-312 % RH, 23 °C
    Hot-fill containersCreep modulusISO 899-180 °C loading

    Impact-Modified Formulation Design for Agrochemical Containers at −18 °C

    In cold-climate agrochemical distribution, blow-moulded 20 L to 30 L jerry cans made from HDPE MM 80 U are modified with polyolefin elastomer at 2 wt% to 5 wt% when drop-impact resistance at −18 °C is specified. The modifier reduces flexural modulus by approximately 10 % to 20 % depending on comonomer content and crystallinity, so top-load capacity must be re-evaluated under ISO 12048 at 40 °C. UV stabilization for outdoor storage in agricultural depots is achieved with carbon black masterbatch at 2.0 wt% to 2.5 wt%, which raises melt viscosity and requires a die head temperature increase of 5 °C to 10 °C to avoid melt fracture. Hindered amine light stabilizers are added at 0.1 wt% to 0.3 wt% when colour-matching to brand specifications does not permit carbon black. The pinch-off weld at the base is the highest-risk initiation site for brittle fracture; weld strength is assessed by cutting 25 mm strips across the pinch-off seam and pulling them at 10 mm/min under ISO 527-3. When filled with emulsifiable concentrate formulations, stress-crack resistance is tested with 10 % nonylphenol ethoxylate or the actual formulation at 50 °C because solvent composition shifts the ESCR ranking of the base resin; published data for this specific configuration is limited where custom pesticide formulations exceed 30 % aromatic hydrocarbon content. Screw speed on a 25:1 L/D extruder should be limited to maintain melt temperature below 210 °C because additive degradation can produce surface pitting and reduce burst strength. The finished can is also subjected to hydraulic pressure testing and closure torque verification under the relevant UN packaging group.

    Surface Resistivity Control in Antistatic Blow-Moulded Drum Liners for Solvent Delivery

    For conductive or static-dissipative blow-moulded liners inserted into 200 L steel drums, HDPE MM 80 U is compounded with conductive carbon black loadings from 8 wt% to 12 wt%, or with carbon nanotube masterbatch at 1 wt% to 2 wt% when lower filler load is required for pinch-off weld integrity. Surface resistance is measured at 23 °C and 12 % relative humidity under IEC 61340-2-3; acceptance for solvent delivery is typically below 10^9 Ω. Carbon black addition raises melt viscosity and reduces parison flare, so die head pressure increases by 10 % to 30 % compared with unfilled HDPE under the same screw speed. The liner is corona-treated on the outer surface to 38 mN/m to 42 mN/m before lamination to the steel drum wall; the inner surface remains untreated to avoid changing surface conductivity. Because conductive carbon black can nucleate crystallinity changes that reduce ESCR, the filled compound is tested under ASTM D1693-15e1 and compared with neat resin; a drop in F50 failure time of more than 20 % is a reject condition for contact with ketones and esters. The liner is produced on a continuous accumulator head, and the parison is programmed to maintain 1.5 mm minimum wall thickness after insertion; below this thickness, static decay time at 5 kV may exceed 2.0 s when measured under IEC 61340-5-1 acceptance limits. Published data for this specific configuration is limited where carbon nanotube dispersion is not verified by optical microscopy at 200×.

    Where High-Temperature Filling Conditions Force HDPE Liner Wall-Thickness Redistribution

    At filling temperatures of 70 °C to 85 °C, hot-fill blow-moulded containers for liquid household chemicals and agricultural adjuvants exhibit a sharp reduction in instantaneous modulus and require time- and temperature-dependent top-load design. Creep modulus is measured under ISO 899-1 at 80 °C to calculate the wall-thickness multiplier needed for a 24 h stack-load condition; the multiplier generally falls between 1.15 and 1.35 relative to ambient design. Parison programming must shift material from the upper and lower pinch-off zones into the body panels, with a minimum sidewall thickness of 2.0 mm for a 5 L container subjected to 300 N top load. The neck thread geometry is modified to a buttress profile when closures are applied at high filling temperatures because polyolefin shrinkage at the finish can reduce removal torque below specification; removal torque after cooling is verified between 1.0 N·m and 1.8 N·m on automated torque testers. Vacuum collapse during cooling is prevented by nitrogen dosing at 0.02 MPa to 0.05 MPa before capping; for products with oxygen sensitivity, headspace oxygen concentration is verified below 2.0 % by electrochemical probe. The mould cooling time is extended by 10 % to 20 % compared with ambient filling because residual heat from the filled product re-softens the pinched-off bottom seam and can cause pallet-load deformation. Accelerated lifetime testing is performed at 60 °C for 14 days with the actual filling formulation; if the container loses more than 5 % of initial top-load capacity, the design wall thickness is revised upward.

    Free Quote

    Competitive Versalis HDPE MM 80 U prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis HDPE MM 80 U is a high-density polyethylene injection moulding grade supplied in pellet form and formulated with a UV-stabiliser package. Manufacturer technical data identify the grade as an intermediate-flow resin: melt mass-flow rate measured at 190°C under 2.16 kg load is reported in the 7.5–8.5 g/10 min range in accordance with ISO 1133-1:2022, and density is reported in the 0.952–0.956 g/cm³ range under ISO 1183-1:2019. The material is directed to thin-wall injection moulding of crates, caps, closures, housewares, and industrial packaging where a balance of rigidity, dimensional stability, and outdoor weathering resistance is required. Against lower-melt-flow blow moulding grades, MM 80 U offers reduced injection pressure and shorter cycle times; against high-flow injection moulding grades with MFR above 20 g/10 min, it provides higher environmental stress crack resistance and better top-load performance, but requires higher melt temperature and injection pressure to fill long flow paths.

    What Grade-Specific Rheology Separates MM 80 U from Lower-MFR Blow Moulding Resins?

    The intermediate MFR of 8 g/10 min places MM 80 U in a viscosity range where injection moulding filling behaviour is dominated by shear thinning at gate and runner shear rates above 10,000 s⁻¹. Extrusion blow moulding HDPE grades typically operate at MFR values from 0.2 g/10 min to 0.8 g/10 min because high molecular weight and a broad molecular weight distribution provide parison sag resistance. In a conventional shuttle blow moulder with parison drop lengths above 500 mm, an MFR 8 g/10 min resin such as MM 80 U would generate excessive sag and wall thinning; therefore the grade is excluded from large-container blow moulding. Conversely, high-flow injection moulding grades with MFR above 20 g/10 min fill thin sections at lower pressure but lose stiffness and stress crack resistance. Grade-specific capillary rheometry data for MM 80 U is not published in the current datasheet; process engineers should measure the viscosity curve on a capillary rheometer per ISO 11443:2021 before converting a mould from a 20 g/10 min grade.

    The mechanical property envelope of MM 80 U is based on ISO 527-2:2012 and ISO 178:2019 data. Tensile yield stress is typically reported in the 24–26 MPa range, tensile elongation at break above 500%, flexural modulus in the 900–1100 MPa range, and notched Charpy impact at 23°C in the 4–6 kJ/m² range under ISO 179-1:2010. The Vicat softening point A50 is reported near 124°C under ISO 306:2022. These values position the grade as a stiff, moderately tough HDPE suitable for stacking crates and closure systems requiring top-load resistance. The density of 0.954 g/cm³ corresponds to a crystalline fraction of approximately 62–65% based on the two-phase density method; this crystallinity contributes to hardness and chemical resistance but reduces impact toughness at sub-zero temperatures.

    Published typical property values for Versalis HDPE MM 80 U
    PropertyTest methodTypical range or value
    Melt mass-flow rate (190°C/2.16 kg)ISO 1133-1:20227.5–8.5 g/10 min
    DensityISO 1183-1:20190.952–0.956 g/cm³
    Tensile yield stressISO 527-2:201224–26 MPa
    Tensile elongation at breakISO 527-2:2012>500%
    Flexural modulusISO 178:2019900–1100 MPa
    Charpy notched impact at 23°CISO 179-1:20104–6 kJ/m²
    Vicat softening point A50ISO 306:2022123–125°C

    Machine Settings and Failure Modes on Reciprocating-Screw Injection Moulders

    On a standard reciprocating-screw injection moulding machine with an L/D ratio of 20:1 to 24:1 and a compression screw of 2.5:1 to 3:1, MM 80 U is processed at barrel temperature settings from 180°C at the feed zone to 230°C at the nozzle, with mould temperature controlled between 15°C and 40°C. For a 32-cavity closure mould with hot runner, injection speed is set to achieve a fill time below 0.3 s per shot; insufficient speed produces flow hesitation and weld-line weakness at the closure bridge. Injection pressure normally falls between 70 MPa and 100 MPa, while hold pressure is applied at 60–80% of peak pressure for 1.5–2.5 s. A documented process failure mode involves excessive cushion control: if the cushion drops below 2 mm on a 50 mm screw, unmelted material can enter the shot and cause surface splay. Conversely, holding a cushion above 8 mm increases residence time and can yellow the UV-stabilised package after 20 min of interruption. Clamp force requirement is approximately 4–6 kN/cm² of projected part area; a 2500 kN machine is adequate for a 4-cavity crate mould with shot weights up to 1.2 kg.

    The U suffix denotes a UV-stabilised formulation intended to retard photo-oxidative chain scission during outdoor service. Unstabilised HDPE exposed to ultraviolet radiation in the 290–400 nm wavelength range undergoes rapid loss of elongation and surface microcracking. When grades of this type are assessed under accelerated weathering according to ISO 4892-2:2013, cycle 1, retained tensile elongation after 1000 h is a relevant quality-control indicator, but grade-specific data for MM 80 U is not currently published in the technical datasheet; therefore end-use validation should be performed on moulded parts rather than extrapolated from resin data alone. Outdoor exposure of natural-white mouldings in temperate climates typically requires a minimum wall thickness of 1.5 mm to avoid premature UV embrittlement; black or coloured masterbatch systems with 2–3 wt% carbon black provide additional screening. The grade should not be exposed to repeated steam sterilisation above 121°C or long-term contact with strong oxidising acids, because these conditions consume the phenolic and phosphite antioxidants and reduce the protective effect of the UV package.

    When the End-Use Part Requires Food Contact and Regulatory Conformity

    For food contact applications, Versalis HDPE MM 80 U falls within the scope of polyethylene homopolymer provisions, provided the grade meets the extractable fraction and migration limits specified in the applicable jurisdiction. In the European Union, compliance is evaluated under Commission Regulation (EU) No 10/2011 and its amendments, with an overall migration limit of 10 mg/dm² for food contact materials. In the United States, the base polymer is considered suitable for food contact under 21 CFR 177.1520 when the end-use article meets the prescribed extractable content and density conditions. REACH Regulation (EC) No 1907/2006 requires that the supplier be consulted for SVHC content above 0.1 wt%; the current safety data sheet does not list Candidate List SVHCs above this threshold. RoHS Directive 2011/65/EU is not directly applicable to HDPE packaging but may be required by downstream buyers for electrical and electronic equipment housings; the grade contains no intentionally added lead, cadmium, mercury, hexavalent chromium, PBB, or PBDE above the 0.1 wt% threshold.

    Regulatory compliance checklist for MM 80 U
    Standard or regulationScopeStatus or requirement
    Commission Regulation (EU) No 10/2011Plastic food contact materialsOverall migration limit 10 mg/dm²
    21 CFR 177.1520Olefin polymers for food contactCompliance based on extractable fraction and density
    REACH Regulation (EC) No 1907/2006SVHC contentNo listed SVHC above 0.1 wt%
    RoHS Directive 2011/65/EUHeavy metal restrictionsNo intentionally added restricted substances above 0.1 wt%

    The differentiation of MM 80 U from other Versalis HDPE grades rests primarily on MFR, density, and stabiliser package. Lower-MFR Versalis grades intended for extrusion blow moulding, such as those with MFR below 1 g/10 min, show better parison stability but require higher extruder torque and are unsuitable for thin-wall injection moulding. Grades with MFR above 20 g/10 min shorten cycle times but exhibit lower environmental stress crack resistance in fatty food and detergent contact because lower molecular weight reduces the tie-molecule density. Compared with metallocene-catalysed HDPE grades of similar MFR, MM 80 U may have a broader molecular weight distribution, which improves injection processing but can reduce impact strength and ESCR. The UV-stabilised formulation distinguishes it from non-UV HDPE grades of similar flow; however, the specific light stabiliser chemistry is not disclosed in public technical literature. End users replacing polypropylene in crates and closures must account for the lower flexural modulus of HDPE relative to PP and the lower service temperature resistance; HDPE MM 80 U is generally limited to continuous service below 80°C under mechanical load, and stacking loads should be reduced above 50°C because creep modulus declines with temperature.

    Top