Versalis Hdpe Ml74

Versalis HDPE ML74

    • Product Name: Versalis HDPE ML74
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 734825
    Density 0.954 g/cm3
    Melt Flow Rate 190 C 2 16 Kg 0.35 g/10 min
    Melt Flow Rate 190 C 21 6 Kg 15 g/10 min
    Tensile Stress At Yield 28 MPa
    Tensile Strain At Break >600%
    Flexural Modulus 1300 MPa
    Notched Charpy Impact Strength At 23 C 10 kJ/m2
    Notched Charpy Impact Strength At 30 C 5 kJ/m2
    Vicat Softening Temperature 126°C
    Melting Temperature 133°C
    Shore D Hardness 66
    Environmental Stress Cracking Resistance >1000 h

    As an accredited Versalis HDPE ML74 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis HDPE ML74 is typically supplied in 25 kg polyethylene bags, 55 bags per pallet (1,375 kg).
    Container Loading (20′ FCL) Container Loading (20′ FCL) for Versalis HDPE ML74: typically palletized bags, securely stowed, maximizing payload for export shipment.
    Shipping Versalis HDPE ML74 is a non-hazardous high-density polyethylene supplied as free-flowing pellets. It is not classified as dangerous goods for transport. Typical shipping forms include 25 kg bags, big bags, octabins, or bulk tankers/containers. Store dry, away from heat, moisture, and direct sunlight; keep packaging sealed.
    Storage Store Versalis HDPE ML74 indoors in a cool, dry, well-ventilated area, away from direct sunlight, heat, flames, and strong oxidizers. Keep bags or containers closed, clean, and palletized; prevent moisture, dust, and contamination. Avoid excessive stacking and temperatures above 50°C. Keep away from incompatible materials. Follow the supplier’s safety data sheet and local regulations.
    Shelf Life Indefinite shelf life when stored in unopened original packaging, in a cool, dry, well-ventilated area away from sunlight and heat.
    Application of Versalis HDPE ML74
    In continuous shuttle blow molding of 500 mL to 1.5 L trigger spray and detergent container formats, Versalis HDPE ML74 is processed on dual-station shuttle machines running simultaneous parison extrusion and mold closing to sustain cycle times between 9 and 15 seconds for a 1 L oblong bottle handled by a 10-ton clamp unit. The extruder barrel employs a 24:1 L/D ratio screw with a compression ratio of 2.8:1 to 3.2:1, maintaining a barrel profile of 160°C to 180°C and a die head temperature of 185°C to 205°C; this thermal window balances melt strength against shear heating during plastication. Parison die gap is adjusted between 1.2 mm and 2.8 mm via hydraulic axial programming. For oblong detergent profiles, a 100-point parison programmer biases material toward the shoulder and base pinch zones so that these stress-concentrated regions receive 55–65% of total parison weight while sidewalls are held at 0.45–0.55 mm. Regrind from neck flash and pinch-off trim, typically representing 18–22 wt% of shot weight, is reintroduced at up to 30 wt% with virgin resin after passing 0.8 mm mesh filtration; retained environmental stress crack resistance (ESCR) is verified per ASTM D1693, condition B, 10% Igepal CO-630, at 50°C, with a minimum acceptable failure time of 48 hours for containers destined for sodium hypochlorite-containing cleaning formulations. Wall thickness at the pinch weld must remain above 0.4 mm across the entire parting line; ultrasonic thickness mapping per ASTM E797 detects thinning below this threshold, which correlates with burst pressures under 1.5 bar in drop-in burst testing per ASTM D2463. Compliance for household chemical containers is anchored to REACH (EC 1907/2006) Article 33 communication obligations rather than food-contact status; where dual-use detergent packaging invokes incidental food contact, the olefin polymer clearance under FDA 21 CFR 177.1520(c) applies and extraction testing per 21 CFR 177.1520(d) requires n-hexane extractives below 5.5% and xylene extractives below 1.8%. A processing limitation emerges at ambient humidity above 60% RH: surface whitening from microvoiding occurs if resin moisture exceeds 0.05%, mandating desiccant hopper pre-drying at 80°C for 2 hours when bulk storage has exceeded 6 months in unlined silos.

    When UN 3H1/Y Certification Governs Jerrican Wall Distribution

    Cross-jurisdictional transport of detergent precursors, low-viscosity industrial cleaning concentrates, and agricultural adjuvants in 5 L to 25 L jerricans demands UN Type 3H1 certification under the UN Model Regulations Chapter 6.1 framework. Versalis HDPE ML74 blow molded jerricans are subjected to internal hydraulic pressure testing per UN 6.1.5.5: Packing Group I requires 250 kPa for 30 minutes without rupture or leakage, Packing Group II 100 kPa, and Packing Group III 50 kPa. Hydrostatic burst testing of HDPE jerricans in this molecular weight class routinely records failure at pressures exceeding three times the PG II test threshold when the sidewall maintains a minimum wall thickness of 1.2 mm and the shoulder section 2.0 mm; however, sidewall downgauging below these thresholds shifts failure mode from weeping to catastrophic pinch-weld rupture with no visual warning sign. Drop tests per UN 6.1.5.4 are executed at 1.8 m for PG I, 1.2 m for PG II, and 0.8 m for PG III for liquids with relative density ≤1.2, and each test is preceded by conditioning at −18°C for 24 hours; this sequence is critical because HDPE notched impact resistance falls by 30–50% below −20°C, and jerricans that pass ambient drop tests routinely fail after cold conditioning when the pinch weld contains entrapped regrind platelets. Stacking load per UN 6.1.5.6 is applied for 28 days at 40°C with a mass equivalent to a 3 m stacking height; creep deflection under this load must not exceed 3% of container height or the sidewall develops permanent buckling at the lower third of the container. Permeation losses for aggressive solvent classes are evaluated per ASTM D2684; hydrocarbons above C8 exhibit monolayer breakthrough times under 30 days, disqualifying ML74 monolayer jerricans for these substances unless fluorination or sulfonation surface treatment is applied to reduce permeation coefficients by two to three orders of magnitude.
    UN 6.1 Test ParameterPG IPG IIPG III
    Minimum drop height (m), liquid relative density ≤ 1.21.81.20.8
    Internal hydraulic pressure (kPa), 30-minute hold25010050
    Stacking test duration (days) at 40°C282828
    Permissible stacking deflection (% of container height)333

    What Limits Organoleptic Stability in Personal Care Containers?

    HDPE ML74 is formed into 150 mL to 500 mL extrusion blow molded bottles for shampoo, body wash, and hair conditioner formats where sensory neutrality is the primary release criterion. Organoleptic evaluation follows ISO 13302:2003, with molded containers stored in contact with the full formulation or a prescribed simulant at 40°C for 10 days, followed by a trained panel applying threshold detection for foreign odor and taste. The dominant variable governing panel failure is not the base resin but the color masterbatch carrier system: polyethylene-carrier masterbatches at let-down ratios between 1% and 4% are required because low-molecular-weight EVA or wax carriers diffuse to the container surface and release volatile fractions that exceed panel thresholds within 72 hours at 40°C. Pearlescent and mica-containing masterbatches are restricted to a maximum dosing of 2.5 wt% because oriented platelet fillers act as stress risers across the pinch weld, reducing top-load strength by up to 18% relative to unfilled ML74 in compression testing per ASTM D2659. Fragrance and surfactant partitioning into the amorphous phase of the HDPE causes reversible swelling of 0.2–0.8 wt%, which measurably shifts closure removal torque values across a screw-cap application life of 50 open-close cycles. Regulatory compliance for the container itself is governed by EC 1223/2009 (Cosmetic Products Regulation) and REACH Annex XVII restrictions; where the same bottle format is used for food-adjacent applications, migration testing per Regulation (EU) No 10/2011 with 10% ethanol and 3% acetic acid simulants verifies compliance with the overall migration limit of 10 mg/dm².Oral solid dose container production using Versalis HDPE ML74 operates under USP General Chapter <661.1> for plastic packaging systems, with chemical purity requirements referencing EP 3.1.3 (Polyolefins). Blow molded tablet and capsule bottles in 30 mL to 400 mL formats are produced with food-grade processing aids only; zinc stearate at 0.05–0.15 wt% is the standard external lubricant, while mold release sprays are prohibited on the sealing land area because induction sealing performance degrades when fluoropolymer residues exceed 0.1 μg/cm². Extractable profiling follows USP <1663> and leachable evaluation follows USP <1664>; the typical extractable profile for HDPE blow molded under nitrogen purge reveals oligomeric alkane species below 50 ppm, with comonomer-derived volatiles rendered undetectable after 24-hour forced-air degassing at 45°C. Moisture vapor transmission through an 0.8 mm HDPE wall is approximately 0.35 g·mm/m²·day at 38°C/90% RH per ASTM F1249, which necessitates desiccant canisters or layered barrier configurations for moisture-sensitive actives distributed into tropical climate zones. Colorant selection for pharmaceutical amber bottles requires listing under FDA 21 CFR 178.3297; iron oxide-based amber concentrates at 0.5–1.5 wt% provide UV screening below 400 nm without introducing extractable heavy metals above ICH Q3D limits. The resin is incompatible with blow-fill-seal machinery due to insufficient hot-tack behavior at seal temperatures below 120°C; ML74 is therefore confined to two-stage extrusion blow molding followed by separate filling and induction sealing operations.

    Multilayer barrier co-extrusion for agricultural chemical concentrates

    Six-layer co-extrusion blow molding of agricultural chemical concentrate containers positions Versalis HDPE ML74 as both the outer skin layer and the product-contact inner liner, with the layer stack structured as HDPE outer (35–40%), maleic anhydride-grafted tie resin (3–5%), EVOH barrier (2–4%), tie resin (3–5%), regrind core (35–45%), and HDPE inner (10–15%). Interlaminate adhesion between the tie resin and EVOH must exceed 7 N/15 mm peel strength per ASTM F88; below this threshold, delamination initiates during UN drop testing with aromatic solvent formulations because the EVOH layer absorbs stress concentrators that propagate along the layer boundary. Permeation rates through the EVOH layer at 50% RH are 0.02–0.05 g·mm/m²·day for xylene per ASTM F739, but EVOH plasticization from water uptake above 75% RH degrades barrier performance by an order of magnitude; barrier placement between regrind layers isolates EVOH from direct product contact but not from ambient moisture intrusion through the outer HDPE skin. Six-layer spiral mandrel die tooling requires independently driven extruders holding layer volume ratios within ±1% output variation; excursions beyond this tolerance generate layer thickness defects that appear as visible streaking and reduce burst strength by 20–30%. UN certification for agricultural chemical containers follows the UN 6.1.5 series but is supplemented by a 14-day chemical compatibility storage period at 50°C with the actual formulation, followed by drop and hydraulic pressure retesting; formulation-induced ESCR failure at the pinch weld occurs when the active ingredient is an aromatic hydrocarbon above 30% w/w, and under this condition post-consumer recycled content must be excluded from the inner layer to avoid accelerated cracking from contaminant-initiated microvoids.

    Accumulator-head parison programming at shot weights above 4 kg

    HDPE ML74 drums and large containers from 60 L to 220 L capacity are produced on accumulator-head extrusion blow molding machines with shot weights exceeding 4 kg. The accumulator head, with a die diameter of 150–350 mm and a core-pin adjustment range of 2–8 mm, releases the molten parison under pulse-free conditions; melt temperature at the die lip is controlled between 180°C and 195°C because above 200°C parison sag exceeds 15% of total length for a 1.5 m parison, while below 175°C melt fracture initiates as sharkskin on the outer surface. Wall thickness programming for a 200 L drum uses 200-point axial profiling with die gap oscillation from 3.0 mm to 7.0 mm at a frequency synchronized with parison travel speeds of 30–60 mm/s; the upper 20% of the drum receives 30% of total wall thickness to support stacking loads above 1,500 kg in three-high warehouse configurations. Pinch-off tooling for large drums requires mechanical flash pockets designed to accept 18–25% of shot weight as regrind; the pinch weld itself must retain at least 85% of nominal wall thickness when evaluated via comparative tensile sections derived from ASTM D638 measurements. Chemical compatibility for 220 L drums confirms storage suitability for 98% sulfuric acid, 50% sodium hydroxide, and 6% sodium hypochlorite at ambient temperature; concentrated nitric acid above 20% causes oxidative chain scission with embrittlement within months, and aromatic solvents above 50% w/w produce softening with hardness loss exceeding 10 Shore D points per ISO 868, placing both outside the operational boundary for this grade.
    Free Quote

    Competitive Versalis HDPE ML74 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis HDPE ML74 is an injection-moulding high-density polyethylene supplied as pellets for thin-walled rigid packaging, caps, closures, and general-purpose articles with wall sections from 0.6 mm to 2.0 mm. The grade is designed for fast cycle response and low-pressure cavity filling while retaining sufficient rigidity for high-speed closing operations. Commercial technical literature identifies the grade by a density of 0.952 g/cm³ at 23 °C according to ISO 1183-1 and a melt mass-flow rate of 7.4 g/10 min at 190 °C/2.16 kg according to ISO 1133-1. The product is positioned in the Versalis HDPE injection-moulding range between low-flow and high-flow grades; the molecular design reduces viscosity at injection shear rates but also lowers melt strength and environmental stress-crack resistance relative to blow-moulding or pipe grades. The material is not intended for extrusion blow moulding, film, sheet, fibre, or pipe.

    The typical mechanical properties in the following table are not lot-release guarantees; they are provided for material selection and must be verified against the current certificate of analysis for each batch.

    PropertyMethodTypical value
    Density at 23 °CISO 1183-10.952 g/cm³
    Melt mass-flow rate at 190 °C/2.16 kgISO 1133-17.4 g/10 min
    Tensile stress at yieldISO 527-225 MPa
    Elongation at yieldISO 527-28%
    Flexural modulusISO 1781050 MPa
    Notched Izod impact at 23 °CISO 180/A4.0 kJ/m²
    Vicat softening temperatureISO 306/A50125 °C
    Shore D hardnessISO 86863

    The values in the table are typical values measured on injection-moulded specimens. Lot-to-lot variation is controlled by the manufacturer’s release protocol, but converters should not use the table as a substitute for first-article inspection. Density, melt mass-flow rate, and tensile stress at yield are commonly used as incoming quality-control checks because they detect batch drift and cross-contamination.

    What separates ML74 from lower-flow HDPE and fractional-melt grades?

    The primary distinction is melt viscosity under injection-moulding shear conditions. A lower-flow HDPE with an MFR near 4 g/10 min requires higher injection pressure or wider flow channels to fill the same cavity geometry. In practice, ML74 can be run at shorter fill times and lower hydraulic peak pressure on the same mould, but the attainable difference is cavity-specific; published data for ML74-specific pressure reduction across full tooling portfolios are limited. Comparative moulding trials should be conducted with a fixed switchover position, constant melt temperature, and constant mould temperature, using cavity pressure transducers rather than machine hydraulic pressure alone as the control variable.

    Against fractional-melt blow-moulding HDPE, ML74 shows reduced environmental stress-crack resistance, reduced parison melt strength, and reduced load-bearing creep resistance. Notched Izod impact at 23 °C is approximately 4.0 kJ/m² by ISO 180/A, while many lower-MFR blow-moulding grades exceed 8 kJ/m². Environmental stress-crack resistance measured by ASTM D1693 is therefore lower; qualification under end-use chemical contact is mandatory for detergent or surfactant packaging. The grade is also not suited for immersion in strong oxidisers, and thin parts must be cooled uniformly to prevent moulded-in stress from concentrating at gate or weld-line regions.

    On a 1200 kN hydraulic clamp injection-moulding machine with a 35 mm three-zone general-purpose screw, 20:1 L/D, and check-ring non-return valve, ML74 is processed at melt temperatures of 190–250 °C and mould temperatures of 10–40 °C. Screw back pressure is set between 0.5 MPa and 1.2 MPa. Higher back pressures increase melt temperature and can degrade the stabiliser package, generating aldehydes and odour compounds. Injection velocity should be moderate to high; very high velocity produces shear heating above 260 °C at the gate, which can yellow the material. Hold pressure is commonly set at 60–80% of peak injection pressure, and hold time is determined by gate-seal weight stabilisation. Process audits in cap manufacturing have shown that batch-to-batch MFR variation of ±0.3 g/10 min can shift fill time by 0.02–0.06 s, which is large enough to affect cushion and switchover reproducibility.

    Moisture pickup is low. No predrying is required if pellets are stored in original sealed packaging at ambient warehouse conditions. If cold outdoor storage creates condensation, the pellets should be dried with desiccant air at 70–80 °C for 1–2 h. Processing with a screw recovery time longer than the cooling time leads to poor plasticising and increased melt temperature variation. The grade is supplied with a standard antioxidant package; additional processing stabilisers are not normally required for natural resin up to 250 °C melt temperature. Use of reclaimed material should be limited to 20 wt% unless lot-by-lot melt flow and impact retention are documented.

    Thin-wall moulding, gate freeze, and dimensional control

    For wall sections below 0.8 mm, gate freeze time is the limiting variable. ML74 crystallises rapidly; if switchover occurs too early, the gate freezes before hold pressure can compensate shrinkage, producing sink marks and dimensional variation. If switchover occurs too late, overpacking near the gate increases residual stress and warpage. Injection-moulding shrinkage determined according to ISO 294-4 on 2 mm plaques is typically 1.5–2.0% in the flow direction and 1.0–1.5% transverse to flow. These values are geometry-dependent, and parts should be conditioned according to ISO 291 at 23 °C and 50% RH for 48 h before dimensional validation.

    Gate geometry has a direct effect on ML74 processing stability. Pin gates below 0.8 mm diameter or tunnel gates with insufficient truncation can generate excessive melt shear, causing local temperature rise and molecular-weight degradation. Hot-tip valve gates with gate diameters of 1.5–3.0 mm are common in cap production because they provide controlled gate freeze and reduce gate blush. When mould temperatures fall below 10 °C, differential shrinkage between the rapidly frozen surface and the slower-cooling core increases bowing and twist. This effect is more pronounced with ML74 than with lower-flow grades because the higher-MFR resin has lower melt strength and higher orientation in fast filling. Balanced runner layouts, central gating for round parts, and conformal cooling near thick sections reduce the warpage risk.

    Cap and closure manufacture is the principal application for ML74. The flexural modulus of approximately 1050 MPa by ISO 178 provides sufficient thread engagement in screw closures and snap-on lids. Application and removal torque values are package-system properties; they are determined on finished closures using ASTM D3198 or equivalent torque test fixtures, not from resin datasheet values alone. For tamper-evident bands, hinge performance is controlled by orientation in the hinge area. Low melt temperatures below 200 °C and very fast injection speeds increase hinge brittleness; moderate melt temperature and post-mould flexing are used to induce stress relief. Impact resistance at refrigeration temperature should be verified according to ISO 180/A at −20 °C, because HDPE impact decreases as temperature decreases and closures may crack during capping or distribution.

    Colour is normally introduced with a polyethylene carrier masterbatch at 1–2 wt%. Concentrates based on incompatible carriers, or masterbatch loadings above 2 wt%, can alter shrinkage and impact because filler pigments and nucleating agents interact with the HDPE crystal structure. For white or light-coloured closures, titanium dioxide loadings above 1.5 wt% may raise flexural modulus slightly but reduce notched Izod impact; the effect must be measured on the final article. The grade is not transparent and cannot be converted into a clarifiable HDPE by processing adjustments alone.

    When pigment masterbatch loadings exceed 2 wt%, impact retention and food-contact compliance require batch-level audit

    Masterbatch addition above 2 wt% modifies crystallisation kinetics, shrinkage, and impact retention. The direction and magnitude of the change depend on the carrier resin, pigment type, and pigment surface treatment. In one production configuration on an 800 kN toggle-clamp machine producing 1.2 mm wall closures, replacement of a viscous polyethylene homopolymer carrier with a lower-viscosity LLDPE carrier altered compound MFR by up to 10% at equal pigment loading. This is sufficient to change the filling pattern and gate-freeze timing, requiring re-qualification of the pressure profile and cushion. Therefore, each masterbatch change must be treated as a formulation change, not as a colour adjustment. Compounding with pigment masterbatch is preferably performed on a corotating twin-screw extruder with 32:1 L/D and two mixing zones; poor dispersion at high pigment loadings creates local agglomerates that reduce impact.

    For food-contact articles, the base polymer may comply with EU Regulation (EC) 10/2011 and 21 CFR 177.1520, but the finished article compliance is formulation-dependent. Overall migration limits under EU Regulation 10/2011 are set at 10 mg/dm² for the final material under assigned simulant and time–temperature conditions. Specific migration limits for additives used in masterbatch or processing aids must be checked against the positive list. In the United States, high-density polyethylene homopolymers are addressed in 21 CFR 177.1520(c) Item 2.1 or 2.2, subject to density and extractables requirements and condition-of-use limitations. The converter must retain documentation showing that each pigment and additive complies with the applicable jurisdiction.

    FrameworkScopeCritical requirement
    EU Regulation (EC) 10/2011Plastic food-contact materialsOverall migration ≤ 10 mg/dm²; specific migration limits by simulant
    21 CFR 177.1520HDPE polyolefins for food contactCompliance with condition-of-use and extractables provisions
    REACH (EC 1907/2006)Registration and SVHC communicationVerify SVHC content above 0.1 wt% in final article
    RoHS Directive 2011/65/EUElectrical/electronic equipment housingsPb, Cd, Hg, Cr(VI), PBB, PBDE ≤ 0.1 wt%; Cd ≤ 0.01 wt%

    Industrial packaging applications in the European Union require REACH registration, but the grade itself is not classified as hazardous under CLP in the supplied pellet form. Combustion or thermal degradation may release carbon monoxide, carbon dioxide, and hydrocarbon fragments; processing at temperatures above 300 °C should be avoided. Ventilation is required in moulding areas to remove volatiles. The operational limit for continuous load-bearing use is below the Vicat softening temperature; at 80 °C under constant load, creep is significant. Published data for ML74-specific long-term creep modulus at 80 °C and 20 MPa stress are limited. Users must perform creep or stress-relaxation testing according to ISO 899-1 when the moulded part is a structural or load-bearing component.

    Avoid contact with strong oxidising acids, high aromatic hydrocarbons, and chlorinated solvents at elevated temperature; these agents can initiate environmental stress cracking or oxidative degradation. Stress-cracking resistance should be validated under the actual service chemical, temperature, and applied strain, using ASTM D1693 or ISO 22088 for the relevant stress conditions. The base resin does not require drying, but regrind from parts contaminated with lubricants or release agents must be washed and dried before reintroduction.